• Title/Summary/Keyword: Ion scattering

Search Result 184, Processing Time 0.03 seconds

Thermal Conductivity in Individual Single-Crystalline PbTe Nanowires (단결정 PbTe 단일 나노선의 열전도도)

  • Roh, Jong Wook;Jang, So Young;Kang, Joohoon;Lee, Seunghyun;Noh, Jin-Seo;Park, Jeunghee;Lee, Wooyoung
    • Korean Journal of Metals and Materials
    • /
    • v.48 no.2
    • /
    • pp.175-179
    • /
    • 2010
  • We investigated the thermal conductivity of individual single-crystalline PbTe nanowires grown by chemical vapor transport method. Suspended MEMS was utilized to precisely measure the thermal conductivity of an individual nanowire. The thermal conductivity of a PbTe nanowire with diameter of 292 nm was measured to be $1.8W/m{\cdot}K$ at 300 K, which is about two thirds of that of bulk PbTe. This result indicates that the thermal conduction through a PbTe nanowire is effectively suppressed by the enhanced phonon boundary scattering. As the diameter of a PbTe nanowire decreases, the corresponding thermal conductivity linearly decreases.

Photoluminescence properties of Mn4+-activated Li2ZnSn2O6 red phosphors

  • Choi, Byoung Su;Lee, Dong Hwa;Ryu, Jeong Ho;Cho, Hyun
    • Journal of Ceramic Processing Research
    • /
    • v.20 no.1
    • /
    • pp.80-83
    • /
    • 2019
  • The Mn4+-activated Li2ZnSn2O6 (LZSO:Mn4+) red phosphors were synthesized by the solid-state reaction at temperatures of 1100-1400 ℃ in air. The synthesized LZSO:Mn4+ phosphors were confirmed to have a single hexagonal LZSO phase without the presence of any secondary phase formed by the Mn4+ addition. With near UV and blue excitation, the LZSO:Mn4+ phosphors exhibited a double band deep-red emission peaked at ~658 nm and ~673 nm due to the 2E → 4A2 transition of Mn4+ ion. PL emission intensity showed a strong dependence on the Mn4+ doping concentration and the 0.3 mol% Mn4+-doped LZSO phosphor produced the strongest PL emission intensity. Photoluminescence emission intensity was also found to be dependent on the calcination temperature and the optimal calcination temperature for the LZSO:Mn4+ phosphors was determined to be 1200 ℃. Dynamic light scattering (DLS) and field-effect scanning electron microscopy (FE-SEM) analysis revealed that the 0.3 mol% Mn4+-doped LZSO phosphor particles have an irregularly round shape and an average particle size of ~1.46 ㎛.

Characteristics of Poly(vinyl phenol) Ionomers Neutralized by LiOH and Their Miscibility with Poly(methyl methacrylate) (Li으로 중화된 폴리비닐페놀 이오노머의 특성 및 폴리메틸메타크릴레이트와의 혼화성)

  • 노진영;김진환
    • Polymer(Korea)
    • /
    • v.24 no.6
    • /
    • pp.886-892
    • /
    • 2000
  • Poly(4-vinyl phenol) (PVPh) was neutralized by LiOH and PVPh ionomers (PVPh-Li) with different Li neutralization extents were synthesized. The variation in $T_{g}$ with Li neutralization was determined by DSC and the results show that the $T_{g}$ increases by 3.$8^{\circ}C$ per Li mol%. When comparing this result with the 3.$2^{\circ}C$ per Na mol% reported for poly (styrene-co-hydroxy styrene), the greater value for PVPh-Li may be due to a strong interaction between unneutralized free -OH and -OLi produced. No distinct small angle X-ray scattering (SAXS) peak was observed for these PVPh ionomers in bulk. In the 50/50 blend of PVPh-Li with PVPh, the miscibile blend was obtained when the Li neutralization in PVPh-Li was 10 mol%. On the contrary, the 50/50 PVPh-Li/PMMA was immiscible when the Li neutralization was 5 mol%. It can be concluded that, even if the starting blend is miscible owing to hydrogen bonding, the miscibility of blend becomes diminished by introducing small amount of ion groups into one of the constituent polymers and the blend can be immiscible as long as any new strong intermolecular ion-dipole interaction is not generated.

  • PDF

XAS Studies of Ion Irradaited MgO Thin Films

  • Suk, Jae-Kwon;Gautam, Sanjeev;Song, Jin-Ho;Lee, Jae-Yong;Kim, Jae-Yeoul;Kim, Joon-Kon;Song, Jong-Han;Chae, Keun-Hwa
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2012.02a
    • /
    • pp.312-312
    • /
    • 2012
  • Magnesium oxide has become focus for research activities due to its use in magnetic tunnel junctions and for understanding of do ferromagnetism. Theoretical investigations on such type of system indicate that the presence of defects greater than a threshold value is responsible for the magnetic behaviour. It has also been shown experimentally that by decreasing the film thickness and size of nanoparticles, enhancement/increase in magnetization can be achieved. Apart from the change in dimension, swift heavy ions (SHI) are well known for creating defects and modifying the properties of the materials. In the present work, we have studied the irradiation induced effects in magnesium oxide thin film deposited on quartz substrate via X-ray absorption spectroscopy (XAS). Magnesium oxide thin films of thickness 50nm were deposited on quartz substrate by using e-beam evaporation method. These films were irradiated by 200 MeV Ag15+ ion beam at fluence of $1{\times}10^{11}$, $5{\times}10^{11}$, $1{\times}10^{12}$, $3{\times}10^{12}$ and $5{\times}10^{12}ions/cm^2$ at Nuclear Science Centre, IUAC, New Delhi (India). The grain size was observed (as studied by AFM) to be decreased from 37 nm (pristine film) to 23 nm ($1{\times}10^{12}ions/cm^2$) and thereafter it increases upto a fluence of $5{\times}10^{12}ions/cm^2$. The electronic structure of the system has been investigated by X-ray absorption spectroscopy (XAS) measurements performed at the high energy spherical grating monochromator 20A1 XAS (HSGM) beamline in the National Synchrotron Radiation Research Center (NSRRC), Taiwan. Oxides of light elements like MgO/ZnO possess many unique physical properties with potentials for novel application in various fields. These irradiated thin films are also studied with different polarization (left and right circularly polarized) of incident x-ray beam at 05B3 EPU- Soft x-ray scattering beamline of NSRRC. The detailed analysis of observed results in the wake of existing theories is discussed.

  • PDF

Magnetoresistance of Single-type and Dual-type GMR-SV Multilayer Thin Films with Top and Bottom IrMn Layer (상부와 하부 IrMn층을 갖는 단일구조 및 이중구조 거대자기저항-스핀밸브 다층박막의 자기적 특성 비교 분석)

  • Choi, Jong-Gu;Kim, Su-Hee;Choi, Sang-Heon;Lee, Sang-Suk
    • Journal of the Korean Magnetics Society
    • /
    • v.27 no.4
    • /
    • pp.115-122
    • /
    • 2017
  • The antiferromagnet IrMn based four different GMR-SV multilayers on Corning glass were prepared by using ion beam deposition and DC magnetron sputtering system. The magnetoresistance (MR) properties for single-type and dual-type GMR-SV multilayer films were investigated through the measured major and minor MR curves. The exchange bias coupling field ($H_{ex}$) and coercivity ($H_c$) of pinned layer, the $H_c$ and interlayer exchange coupling field ($H_{int}$) of free layer for the dual-type structure GMR-SV multilayer films consisted of top IrMn layer were 410 Oe, 60 Oe, 1.6 Oe, and 7.0 Oe, respectively. The minor MR curve of two free layers was performed the squarelike feature having a MR ratio of 8.7 % as the sum of 3.7 % and 5.0 %. The value of average magnetic field sensitivity (MS) was maintained at 2.0 %/Oe. Also, the magnetoresistance properties of the single-type and dual-type structure GMR-SV multilayer films consisted of bottom IrMn layer were decreased more than those of top IrMn layer. Two antiparallel states of magnetization spin arrays of the pinned and free layers in the dual-type GMR-SV multilayer films occurred the maximum MR value by the effect of spin dependence scattering.

A Study on the Status of Fine Dust Generated from Construction Waste Intermediate Treatment Plants in Rural Area and Its Impact on Neighboring Areas (농촌지역 건설폐기물 중간처리 사업장에서 발생하는 미세먼지의 발생 현황 및 인근 지역에 미치는 영향 연구)

  • Jang, Kyong-Pil;Park, Ji-Sun;Kim, Byung-Yun
    • Journal of the Korean Institute of Rural Architecture
    • /
    • v.25 no.4
    • /
    • pp.9-16
    • /
    • 2023
  • In this study, the status and characteristics of fine dust and its impact on neighboring areas were investigated to proactively respond to the government's environmental regulations expected in the future and to minimize the damage by the fine dust generated at construction waste intermediate treatment plants. In addition, since there are no such plants that can affect the surroundings with no houses or other waste treatment sites nearby, an independently located construction waste intermediate treatment plant was selected to compare the characteristics of fine dust with that from the construction waste intermediate treatment sites located in the downtown area. The conclusions of the study are as follows. (1) The measurement results of PM10 at 4 points in the plant showed that the location where the crushing facility was operating had an elevated level of fine dust at 80㎍/m3 on average and a maximum of 124㎍/m3, and the level rose to 110㎍/m3 at points where vehicles frequent. (2) The PM2.5 measurement results inside the plant showed that the average concentration of the reference point was 16㎍/m3 and the maximum value was 20㎍/m3, which was distributed within the management standard. (3) It was found that the average concentration of PM10 in the nearby area ranged from 28 to 38㎍/m3, which was similar to or lower than 36㎍/m3 of the reference point. Therefore, the concentration of the fine dust generated in the plant had a negligible effect on the increase in concentration of fine dust in nearby areas. (4) The heavy metal contents were measured from the filter paper collected from the plant. The PM10 was found to be about 14 to 26ng/m3, and PM 2.5 was 25 to 28ng/m3, which was the average of domestic atmospheric concentrations. (5) The SEM-EDX analysis results showed that the PM10 contained Si and O around 40% similarly for both. The SiO2, a component of silica occupied the most and C was present as CaCO3, which was assumed to be a limestone component. The remaining components included NaO, Al2O3, and CaO as trace oxides. (6) The SEM-EDX analysis results showed that the PM 2.5 contained 5 to 7% of Cl, which is a chlorine ion, and a small amount of K was detected at 2.51% in the sample from the shutdown plant.

Evaluation of dose variation at the vertex during Total Skin Electron Beam (전신 피부 전자선 조사(TSEB)시 두정부(Vertex)에서의 선량 변화 평가)

  • Jeon Byeong-Chul;An Seung-Kwon;Lee Sang-Gyu;Kim Joo-Ho;Cho Kwang-Hwan;Cho Jung-Hee;Park Jae-Il
    • The Journal of Korean Society for Radiation Therapy
    • /
    • v.12 no.1
    • /
    • pp.112-116
    • /
    • 2000
  • Purpose : The vertex scalp is always tangentially irradiated during total skin electron beam(TSEB) This study was discuss to the dose distribution at the vertex scalp and to evaluate the use of an electron reflector. positioned above the head as a means of improving the dose uniformity. Methods and Materials Vetex dosimetry was performed using ion-chamber and TLD. Measurements were 6 MeV electron beam obtained by placing an acrylic beam speller in the beam line. Studies were performed to investigate the effect of electron scattering on vertex dose when a lead reflector $40{\times}40cm$ in area, was positioned above the phantom. Results : The surface dose at the vertex, in the without of the reflector was found to be less than $37.8\%$ of the skin dose. Use of the lead reflector increased this value to $62.2\%$ for the 6 MeV beam. Conclusion : The vertex may be significantly under-dosed using standard techniques for total skin electron beam. Use of an electron reflector improves the dose uniformity at the vertex and may reduce or eliminate the need for supplemental irradiation.

  • PDF

Preparation of a Hydrophobized Chitosan Oligosaccharide for Application as an Efficient Gene Carrier

  • Son Sohee;Chae Su Young;Choi Changyong;Kim Myung-Yul;Ngugen Vu Giang;Jang Mi-Kyeong;Nah Jae-Woon;Kweon Jung Keoo
    • Macromolecular Research
    • /
    • v.12 no.6
    • /
    • pp.573-580
    • /
    • 2004
  • To prepare chitosan-based polymeric amphiphiles that can form nanosized core-shell structures (nanopar­ticles) in aqueous milieu, chitosan oligosaccharides (COSs) were modified chemically with hydrophobic cholesterol groups. The physicochemical properties of the hydrophobized COSs (COSCs) were investigated by using dynamic light scattering and fluorescence spectroscopy. The feasibility of applying the COSCs to biomedical applications was investigated by introducing them into a gene delivery system. The COSCs formed nanosized self-aggregates in aqueous environments. Furthermore, the physicochemical properties of the COSC nanoparticles were closely related to the molecular weights of the COSs and the number of hydrophobic groups per COS chain. The critical aggregation concentration values decreased upon increasing the hydrophobicity of the COSCs. The COSCs effi­ciently condensed plasmid DNA into nanosized ion-complexes, in contrast to the effect of the unmodified COSs. An investigation of gene condensation, performed using a gel retardation assay, revealed that $COS6(M_n=6,040 Da)$ containing $5\%$ of cholesteryl chloroformate (COS6C5) formed a stable DNA complex at a COS6C5/DNA weight ratio of 2. In contrast, COS6, the unmodified COS, failed to form a stable COS/DNA complex even at an elevated weight ratio of 8. Furthermore, the COS6C5/DNA complex enhanced the in vitro transfection efficiency on Human embryonic kidney 293 cells by over 100 and 3 times those of COS6 and poly(L-lysine), respectively. Therefore, hydrophobized chitosan oligosaccharide can be considered as an efficient gene carrier for gene delivery systems.

Characterization of relationship between particle size and powder properties for $BaTiO_3$ ($BaTiO_3$의 입도와 분체특성과의 상관 관계 연구)

  • Chun, M.P.;Cho, J.H.;Kim, B.I.
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.15 no.6
    • /
    • pp.244-251
    • /
    • 2005
  • The relationship between particle size of hydro-thermally synthesized barium titanate powders (BT01, BT02, BT03, BT04, BT05) and the powder properties was investigated by means of particle size, specific surface area, zeta potential, XPS, XRD and SEM. Particle size determined by laser light scattering is closely related with specific surface area and the tetragonality (c/a) obtained from XRD. The specific surface area of the samples inversely decreased with increasing particle size except BT03 powder. BT03 sample showed higher surface area than BT04 sample of equivalent particle size, which was attributed mostly to the agglomeration of particles in terms of SEM image and XRD analysis. Zeta potential increased with increasing particle size with the exception of BT02 and BT03 which showed larger minus value of zeta potential in comparison with other BT powders. Beta potential results of BT02 and BT03 are considered to be related with the dissolution of $Ba^{2+}$ ion in these powers which was examined by XPS.

Variation of the surface structure of the Al / W(110) planes according to the substrate temperature and the coverage

  • Choi, Dae Sun
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2016.02a
    • /
    • pp.156.2-156.2
    • /
    • 2016
  • The variation of the surface structure of the Al adsorbed W(110) planes according to the coverage and the substrate temperature has been investigated using LEED and ISS When the Al atoms were adsorbed on the W(110) surface at room temperature, a p($1{\times}1$) of the fcc (111) face were found at the coverage higher than 4 ML. When the substrate temperature was kept at 900 K during Al adsorption and the coverage was 1.0 ML, the surface revealed a p($1{\times}1$) of the bcc(110) face and when the coverage is 1.5 ML, the surface showed a p($1{\times}1$) of the bcc (110) face together with a p($1{\times}1$) double domain structure (fcc (111) face) rotated ${\pm}3^{\circ}$ from the [100] direction of the W(110) surface. When Al atoms were adsorbed on the W(110) surface at the substrate temperature of 1000 K and the coverage was higher than 1.0 ML, the surface revealed a p($1{\times}1$) of the bcc(110) face together with p($1{\times}1$) double domain structure(fcc(111) face) rotated ${\pm}3^{\circ}{\sim}5^{\circ}$ from the [100] direction of the W(110) surface. When Al atoms were adsorbed on the W(110) surface at the substrate temperature of 1100 K and the coverage was 0.5 ML, Al atoms formed a p($2{\times}1$) double domain structure When the coverage was 1.0 ML, the double domain hexagonal structure (fcc(111) face) rotated ${\pm}5^{\circ}$ from the [100] direction of the W(110) surface and another distorted hexagonal structure was found. Low-energy electron diffraction results along with ion scattering spectroscopy results showed that the Al atoms followed the Volmer-Weber growth mode at high temperature.

  • PDF