High Temperature Oxidation Behavior and Surface Defect in Fe-25Mn-1.5Al-0.5C Steel (Fe-25Mn-1.5Al-0.5C강의 고온 산화 거동과 표면 결함)

  • Park, Shin Hwa;Hong, Soon Taik;Kim, Tai Wung;Chung, In-Sang
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.13 no.3
    • /
    • pp.158-162
    • /
    • 2000
  • The high temperature oxidation behavior and the surface defect in Fe-25Mn-1.5A1-0.5C steel was investigated by XRD (X-ray Diffractin) and electron microscopy. The intra- and inter-granular oxides were formed by the selective oxidation of manganese and aluminum, which were identified to MnAl2O4 phase. Aluminum nitride (AlN) was formed in front of these oxides. The ${\gamma}$-matrix was transformed to ${\alpha}$- and ${\varepsilon}$- phases by the selective oxidation of manganese. The surface defect, micro-scab was induced by the difference of the high temperature ductility between the matrix and the inter-granular oxide.