마찰용접을 적용한 Cu-Al Busbar의 전기적 물성 연구 (Electrical Properties of Friction Welded joints between Cu-Al)

  • 김기영;최인철;;오명훈
    • 열처리공학회지
    • /
    • 제33권6호
    • /
    • pp.284-289
    • /
    • 2020
  • Since the dissimilar bonded interface usually consists of intermetallic compounds (IMCs) layer and cracks, their mechanical and electrical properties can be influenced by microstructure at interface between two different metals. In this study, the friction welded Cu-Al busbar, which is widely used to connect a secondary battery and their component, is selected to analyze the influence of interfacial characteristic on their tensile strength and electric conductivity. Then, the electrical characteristics of Cu busbar and Cu-Al busbar were investigated by thermal flow analysis and temperature rise test. In addition, the relationship between the maximum saturation temperature and the electrical conductivity were discussed in terms of interfacial characteristics of the friction welded Cu-Al busbar.

에너지 발생소자응용을 위한 수열합성법기반 ZnO 나노로드/Polystylene 하이브리드 나노구조 제조 (Fabrication of ZnO Nanorod/polystyrene Nanosphere Hybrid Nanostructures by Hydrothermal Method for Energy Generation Applications)

  • 백성호;박일규
    • 한국분말재료학회지
    • /
    • 제22권6호
    • /
    • pp.391-395
    • /
    • 2015
  • We report on the successful fabrication of ZnO nanorod (NR)/polystyrene (PS) nanosphere hybrid nanostructure by combining drop coating and hydrothermal methods. Especially, by adopting an atomic layer deposition method for seed layer formation, very uniform ZnO NR structure is grown on the complicated PS surfaces. By using zinc nitrate hexahydrate $[Zn(NO_3)_2{\cdot}6H_2O]$ and hexamine $[(CH_2)_6N_4]$ as sources for Zn and O in hydrothermal process, hexagonal shaped single crystal ZnO NRs are synthesized without dissolution of PS in hydrothermal solution. X-ray diffraction results show that the ZnO NRs are grown along c-axis with single crystalline structure and there is no trace of impurities or unintentionally formed intermetallic compounds. Photoluminescence spectrum measured at room temperature for the ZnO NRs on flat Si and PS show typical two emission bands, which are corresponding to the band-edge and deep level emissions in ZnO crystal. Based on these structural and optical investigations, we confirm that the ZnO NRs can be grown well even on the complicated PS surface morphology to form the chestnut-shaped hybrid nanostructures for the energy generation and storage applications.

Sn-Zn 무연솔더를 사용한 BGA패키지의 계면반응 및 신뢰성 평가 (Reliability Investigation and Interfacial Reaction of BGA packages Using the Pb-free Sn-Zn Solder)

  • 전현석;윤정원;정승부
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2005년도 춘계학술발표대회 개요집
    • /
    • pp.25-27
    • /
    • 2005
  • Sn-9Zn solder balls were bonded to Cu and ENIG (Electroless Nickel/Immersion Gold) pads, and the effect of aging on their joint reliability was investigated. The interfacial products were different from the general reaction layer formed in a Sn-base solder. The intermetallic compounds formed in the solder/Cu joint were $Cu_{5}Zn_{8}$ and $Cu_{6}Sn_{5}$. After aging treatment, voids formed irregularly at the bottom side of the solder because of Sn diffusion into the $Cu_{5}Zn_{8}$ IMC. In the case of the solder/ENIG joint, $AuZn_{3}$ IMCs were formed at the interface. In the case of the Sn-9Zn/ENIG, the shear strength remained nearly constant in spite of aging for 1000 hours at $150^{\circ}C$. On the other hand, in the case of the Sn-9Zn/Cu, the shear strength significantly decreased after aging at $150^{\circ}C$ for 100hours and then remained constant by further prolonged aging. Therefore, the protective plating layer such as ENIG must be used to ensure the mechanical reliability of the Sn-9Zn/Cu joint.

  • PDF

스퍼터링 코팅층을 중간재로 사용한 동(Cu)의 저온 접합(제1보) (Low Temperature Bonding of Copper with Interlayers Coated by Sputtering(Part 1))

  • 김대훈
    • 연구논문집
    • /
    • 통권24호
    • /
    • pp.63-79
    • /
    • 1994
  • This article reports a experimental study of the method to achieve a bond joint at lower temperature in a short time. DC magnetron sputtering of Sn, Sn/Pb, Sn/In and Sn/Cu on copper substrate was provided as an interlayer for Cu to Cu bonding under the air environment. Various examination was conducted and investigated on the effect of experimental parameters such as coating materials, coating time(or coating thickness), bonding temperature and bonding time etc. Bonding was performed at the temperature of $210^\circC-320^\circC$ for 0sec and interfacial reaction between the coated layer and copper substrate was examined using optical, scanning electron microscope and x-ray diffractometer. From the obtained results, it was found that intermetallic compounds layer consisted of $\eta-phase(Cu_6Sn_5)$ and $\beta-phase(Cu_3Sn)$ was formed at the joint interface for almost all coating materials. But the dominant phase formed in the preetched Cu substrate coated with Sn was $\beta-phase$. A characteristic morphology looks like a reaction ring, which was believed as the strong interconnecting regions between two substrates, was found to be formed on the reaction surface of copper substrates. The morphologies and compositions of the intermetallics, which depends on the regions of the reaction surface, was appeared as greatly different. Based on above results, the new bonding process to make the joint at lower temperature for short time can be admitted as a feasible process.

  • PDF

강과 알루미늄의 레이저 접합에 관한 연구 Part 1 : 접합 변수의 최적 조건에 관한 연구 (A Study on Laser Joining of Low Carbon Steel and Aluminum Alloy Part 1 : Process Parameters)

  • 박태완;조정호;나석주
    • Journal of Welding and Joining
    • /
    • 제23권5호
    • /
    • pp.25-29
    • /
    • 2005
  • Steel has been mainly used in the automotive industry, because of good mechanical properties, weldability and so on. However, there has been increase in using aluminum to reduce the weight of vehicle. This leads to improve fuel efficiency and to reduce air pollution. A steel-aluminum hybrid body structure is recently used not only to reduce the weight of vehicle but also to increase safety. In this paper, the laser beam joining method is suggested to join steel and aluminum. To avoid making brittle intermetallic compounds(IMC) that reduce mechanical properties of the joint area, only aluminum is melted by laser irradiation and wetted on the steel surface. The brittle IMC layer is formed with small thickness at the interface between steel and aluminum. By controlling the process parameters, brittle IMC layer thickness is suppressed under 10 micrometers which is a criterion to maintain good mechanical properties.

브레이징한 Ti/Cu 접합계면부의 미세조직 특성 (A Characteristic of Microstructures in Bonding Interlayer of Brazed Titanium to Copper)

  • 김우열;정병호;이성렬
    • Journal of Welding and Joining
    • /
    • 제13권3호
    • /
    • pp.106-115
    • /
    • 1995
  • To know the bonding phenomena of Ti/Cu brazed joint, a characteristic of microstructures in bonding interlayer of vacuum brazed pure Ti to Cu has been studied in the temperature range from 1088 to 1133K for various bonding times using Ag-28wt%Cu filler metal. Also intermediate phases formed in bonded interlayer and behavior of layer growth have been investigated. The obtained results in this study are as follows: 1) Liquid insert metal width at the each brazing temperature was proportional to the square root of brazing time, and it was considered that the liquid insert metal width was controlled by the diffusion rate process of primary .alpha.-Cu formed at the Ti side. 2) Intermediate phases formed near the Ti interface were .betha.-Ti and intermetallic compounds TiCu, Ti$_{2}$Cu, Ti$_{3}$Cu, and TiCu. 3) .betha.-Ti formed in Ti base metal durig brazing transformed to lamellar structure, .alpha.-Ti + Ti$_{2}$Cu. The structure came from the eutectoil decomposition reaction in cooling. And the width of .betha.-Ti layer was proportional to the square root of brazing time, and it was considered that the growth of .betha.-Ti layer was controlled by interdiffusion rate process in .betha.-Ti. 4) The layer growth of TiCu, Ti$_{3}$Cu$_{4}$ and TiCu, phases formed near the Ti interface was linerface was linearly proportional to the brazing time, and it was considered that the layer growth of these phases was controlled by the chemical reaction rate at the interface.

  • PDF

SKD61 금형강의 소착 반응층 두께에 미치는 Al-9wt%Si-0.3wt%Mg 합금의 Fe, Mn 영향 (Effect of Fe, Mn Contents of Al-9wt%Si-0.3wt%Mg Alloys on the Thickness of Die Soldering Reaction Layer for SKD61 Die Steel)

  • 김헌주;조치만;정창렬
    • 한국주조공학회지
    • /
    • 제29권4호
    • /
    • pp.169-175
    • /
    • 2009
  • Effect of iron and manganese contents on die soldering reaction has been studied in Al-9wt.%Si-0.3wt.%Mg alloy. Ternary ${\alpha}_{hcp}-Al_8Fe_2Si$ and ${\alpha}_{bcc}-Al_8Fe_2Si$ intermetallic compounds formed by interaction diffusion between Al-Si-Mg system alloy melt and SKD61 die steel surface. Thickness of soldering reaction layer in die steel surface decreased as Fe and Mn contents of the melts increased : When Fe content of Al-9wt.%Si-0.3wt.%Mg melts at constant 0.5wt%Mn content was 0.15wt.%, 0.45wt.% and 0.6wt.%, thickness of soldered layer of each alloy was $64.5{\mu}m,\;57.3{\mu}m$ and $46.9{\mu}m$ respectively. For Mn content of the alloy melts at constant 0.45wt.%Fe content was 0.30wt.%, 0.50wt.% and 0.70wt.%, thickness of soldered layer of each alloy was $66.1{\mu}m,\;57.3{\mu}m$ and $48.3{\mu}m$ respectively.

Cu/Sn 비아를 적용한 일괄적층 방법에 의한 다층연성기판의 제조 (Fabrication of Laminated Multi-layer Flexible Substrate with Cu/Sn Via)

  • 이혁재;유진
    • 마이크로전자및패키징학회지
    • /
    • 제11권4호
    • /
    • pp.1-5
    • /
    • 2004
  • 다층 연성기판은 높은 전기 전도성과 낮은 절연상수로 잘 알려진 구리와 폴리이미드로 구성되어 있다. 본 연구에서는 이러한 다층연성기판을 패턴된 스테인리스 스틸 위에 구리선을 전기도금하고 폴리이미드를 코팅함에 의해서 균일한 형태의 $5{\mu}m$-pitch의 전도선을 제조하는데 성공하였다. 또한, 다층기판 형성시 비아흘은 UV 레이저로 형성시켰으며 구리와 주석을 전기 도금함으로 이를 채웠다. 그런다음 비아와 전도선이 붙은 채로 스테인리스 스틸에서 벗겨냈다. 이렇게 형성된 각각의 층을 한번에 적층하여 다층연성기판을 완성하였다. 적층시 주석과 구리사이에 고체상태 반응(Solid state reaction)이 발생하여 $Cu_6Sn_5$ and $Cu_3Sn$을 형성하였으며 비아패드에 비아가 수직으로 위치한 완전한 형태의 층간 연결을 형성하였다. 이러한 비아 형성 공정은 V형태의 비아나 페이스트 비아와 비교할 때 좋은 전기적 특성, 저가공정등의 여러 장점을 가지고 있다.

  • PDF

In Situ Transmission Electron Microscopy Study on the Reaction Kinetics of the Ni/Zr-interlayer/Ge System

  • Lee, Jae-Wook;Bae, Jee-Hwan;Kim, Tae-Hoon;Shin, Keesam;Lee, Je-Hyun;Song, Jung-Il;Yang, Cheol-Woong
    • Applied Microscopy
    • /
    • 제45권1호
    • /
    • pp.16-22
    • /
    • 2015
  • The reaction kinetics of the growth of Ni germanide in the Ni/Zr-interlayer/Ge system was investigated using isothermal in situ annealing at three different temperatures in a transmission electron microscope. The growth rate of Ni germanide in the Ni/Zr-interlayer/Ge system was determined to be diffusion controlled and depended on the square root of the time, with the activation energy of $1.04P{\pm}0.04eV$. For the Ni/Zr-interlayer/Ge system, no intermediate or intermixing layer between the Zr-interlayer and Ge substrate was formed, and thus the Ni germanide was formed and grew uniformly due to Ni diffusion through the diffusion path created in the amorphous Zr-interlayer during the annealing process in the absence of any intermetallic compounds. The reaction kinetics in the Ni/Zr-interlayer/Ge system was affected only by the Zr-interlayer.

A Study on the Eutectic Pb/Sn Solder Filip Chip Bump and Its Under Bump metallurgy(UBM)

  • Paik, Kyung-Wook
    • 마이크로전자및패키징학회지
    • /
    • 제5권1호
    • /
    • pp.7-18
    • /
    • 1998
  • In the flip chip interconnection on organic substrates using eutectic Pb/Sn solder bumps highly reliable Under Bump Metallurgy (UBM) is required to maintain adhesion and solder wettability. Various UBM systems such as 1$\mu$m Al/0.2$\mu$m Pd/1$\mu$m Cu, laid under eutectic Pb/Sn solder were investigated with regard to their interfacial reactions and adhesion proper-ties. The effects of numbers of solder reflow and aging time on the growth of intermetallic compounds (IMCs) and on the solder ball shear strength were investigated. Good ball shear strength was obtained with 1$\mu$m Al/0.2$\mu$m Ti/5$\mu$m Cu and 1$\mu$m Al/0.2$\mu$m ni/1$\mu$m Cu even after 4 solder reflows or 7 day aging at 15$0^{\circ}C$. In contrast 1$\mu$m Al/0.2$\mu$m Ti/1$\mu$m Cu and 1$\mu$mAl/0.2$\mu$m Pd/1$\mu$m 쳐 show poor ball shear strength. The decrease of the shear strength was mainly due to the direct contact between solder and nonwettable metal such as Ti and Al resulting in a delamination. In this case thin 1$\mu$m Cu and 0.2$\mu$m Pd diffusion barrier layer were completely consumed by Cu-Sn and pd-Sn reaction.