차체 구조용 섬유직물 복합재의 평면 전단(mode II) 층간분리 거동에 대한 시험적 연구 (A Study on Sliding Shear(Mode II) Delamination of Woven Fabric composites for Carbody Structure)

  • 김승철;김정석;윤혁진;서승일
    • 한국철도학회:학술대회논문집
    • /
    • 한국철도학회 2010년도 춘계학술대회 논문집
    • /
    • pp.557-563
    • /
    • 2010
  • Mode II interlaminar fracture toughness was measured and fractured surfaces were observed of carbon/epoxy and glass/epoxy woven fabric composites for carbody structure. Woven fabric carbon/epoxy and glass/epoxy composites that made with prepreg and epoxy resin(RS1222) are used in carbody structure of Korean tilting train(TTX) and low floor bus. ENF(End Notched Flexure) specimens having $120mm{\times}20m{\times}5mm$ shape and 35mm initial crack were made with each composites and three point bending tests according to ASTM D790 were conducted for these specimens. Crack lengths in tests were recorded using optical microscope and digital camcorder. NL(Non Linear), 5% offset and Max. load points in load -displacement curves were checked and mode II interlaminar fracture toughness of these points were calculated and compared. Fractured surfaces of specimens were observed using optical microscope and mode II delamination behavior of each composites was discussed.

  • PDF

국부적 적층분리결함을 갖는 섬유금속적층판의 기계적 거동 특성 (Mechanical Behavior of Fiber Metal Laminates with Local Delamination Defects)

  • 최흥섭;최형집;최원종;하민수
    • 항공우주시스템공학회지
    • /
    • 제1권1호
    • /
    • pp.25-35
    • /
    • 2007
  • In this paper, the interlaminar crack problems of a fiber metal laminate (FML) under generalized plane deformation are studied using the theory of anisotropic elasticity. The crack is considered to be embedded in the matrix interlaminar region (including adhesive zone and resin rich zone) of the FML. Based on Fourier integral transformation and the stress matrix formulation, the current mixed boundary value problem is reduced to solving a system of Cauchy-type singular integral equations of the 1st kind. Within the theory of linear fracture mechanics, the stress intensity factors are defined on terms of the solutions of integral equations and numerical results are obtained for in-plane normal (mode I) crack surface loading. The effects of location and length of crack in the 3/2 and 2/1 ARALL, GLARE or CARE type FML's on the stress intensity factors are illustrated.

  • PDF

층간 분리가 있는 지능 복합재 적층판의 동적특성에 대한 연구 (Study on Dynamic Characteristics of Delaminated Smart Composite Laminates)

  • 김흥수;김재환;최승복
    • 한국소음진동공학회논문집
    • /
    • 제15권4호
    • /
    • pp.395-403
    • /
    • 2005
  • The dynamic characteristics of delaminated smart composite laminates are studied using animproved layerwise laminate theory. The theory is capable of capturing interlaminar shear stresses that are critical to delamination. The presence of discrete delamination is modeled through the use of Heaviside unit step functions. Stress free boundary conditions are enforced at all free surfaces. Continuity in displacement field and transverse shear stresses are enforced at each ply level. In modeling piezoelectric composite plates, a coupled piezoelectric-mechanical formulation is used in the development of the constitutive equations. Numerical analysis is conducted to investigate the effect of nonlinearity in the transient vibration of bimodular behavior caused by the contact impact of delaminated interfaces. Composite plates with delamination, subject to external loads and voltage history from surface bonded sensors, are investigated and the results are compared with corresponding experimental results and plates without delamination.

콘크리트 보강용 하이브리드 FRP 리바의 특성 (The properties of hybrid FRP rebar for concrete structures)

  • 원종필;박찬기;황금식;윤종환
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2003년도 봄 학술발표회 논문집
    • /
    • pp.255-260
    • /
    • 2003
  • The corrosion of steel rebars has been the major cause of the reinforced concrete deterioration. It is FRP rebar that is developed to solve problem of such steel rebar. FRP rebar in concrete structures should be used as a substitute of steel rebars for that cases in which aggressive environment produce high steel corrosion, or lightweight is an important design factor, or transportation cost increase significantly with the weight of the materials. But FRP rebar have only linearly elastic behavior; whereas, steel rebar has linear elastic behavior up to the yield point followed by large plastic deformation and strain hardening. Thus, the current FRP rebars are not suitable concrete reinforcement where a large amount of plastic deformation prior to collapse in required. The main objective of this study was to develop new type of hybrid FRP rebar. The manufacture of the hybrid FRP rebar was achieved pultrusion, braiding and filament winding techniques. Tensile and interlaminar shear test results of hybrid FRP rebar can provide its excellent tensile strength-strain behavior and interlaminar stress-strain behavior.

  • PDF

탄소섬유/에폭시 프리프레그의 플라즈마 표면처리 연구 (A Study on Graphite/Epoxy Prepreg Treatment Using Oxygen Plasma)

  • 김민호;이경엽;백영남;김현주;정동호
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2006년 창립20주년기념 정기학술대회 및 국제워크샵
    • /
    • pp.223-225
    • /
    • 2006
  • In this study, the graphite/epoxy prepregs were surface-treated using oxygen plasma, and optimal treatment time was determined measuring the contact angle en the prepreg surface. Interlaminar fracture behavior of surface-treated graphite/epoxy composite was compared with that of regular (untreated) graphite/epoxy composites. The results showed that the contact angle was a minimum when treated for 30 minutes. The interlaminar fracture toughness of surface-treated specimen was improved about 15% compared with that of regular specimen.

  • PDF

Multi-Objective Design Optimization of Composite Stiffened Panel Using Response Surface Methodology

  • Murugesan, Mohanraj;Kang, Beom-Soo;Lee, Kyunghoon
    • Composites Research
    • /
    • 제28권5호
    • /
    • pp.297-310
    • /
    • 2015
  • This study aims to develop efficient composite laminates for buckling load enhancement, interlaminar shear stress minimization, and weight reduction. This goal is achieved through cover-skin lay-ups around skins and stiffeners, which amplify bending stiffness and defer delamination by means of effective stress distribution. The design problem is formulated as multi-objective optimization that maximizes buckling load capability while minimizing both maximum out-of-plane shear stress and panel weight. For efficient optimization, response surface methodology is employed for buckling load, two out-of-plane shear stresses, and panel weight with respect to one ply thickness, six fiber orientations of a skin, and four stiffener heights. Numerical results show that skin-covered composite stiffened panels can be devised for maximum buckling load and minimum interlaminar shear stresses under compressive load. In addition, the effects of different material properties are investigated and compared. The obtained results reveal that the composite stiffened panel with Kevlar material is the most effective design.

LIPCA에 공급되는 전기장의 변화가 PZT 특성과 적층배향에 미치는 영향 (The Effect of Variable Electric Fields on the PZT Characteristic and Laminate Configuration in LIPCA)

  • 김철웅;남인창;윤광준
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2006년도 춘계학술대회 논문집
    • /
    • pp.397-398
    • /
    • 2006
  • The advanced piezoelectric ceramic composite actuator, which is called LIPCA with the FRP and the optimization of the laminate configuration, was performed to maximize the stress transfer and the fiber bridging effect. This study evaluated the effect of variable electric fields on the PZT characteristic, laminate configuration and fatigue characteristics under the resonance frequency, which meant the largest performance range and the changes of its interlaminar phase were also evaluated by stages. In conclusions, Comparing with the fatigue lift of intact LIPCA, the fatigue life of LIPCA embedded by the artificial delamination was decreased up to 50%. The micro void growth and the coalescence of epoxy were actively made at the interlaminar phase subject to the large tensile stress.

  • PDF

경량화용 복합재 튜브의 적층구성이 흡수에너지 특성에 미치는 영향 (Influence of Stacking Sequence Conditions the Absorbed Energy Characteristics of Composite Tubes)

  • 김영남;김지훈;양인영
    • 한국정밀공학회지
    • /
    • 제18권11호
    • /
    • pp.34-41
    • /
    • 2001
  • This study is to investigate the energy absorption characteristics of CFRP(Carbon-Fiber Reinforced Plastics) tubes on static and dynamic tests. Axial static compression tests have been carried out using the static testing machine(Shin-gang buckling testing machine) and dynamic compression tests have been utilized using an vertical crushing testing machine. When such tubes are subjected to crushing loads, the response is complex and depends on the interaction between the different mechanisms that could control the crushing process. The collapse characteristics and energy absorption have been examined for various tubes. Energy absorption of the tubes are increased as changes in the lay-up which may increase the modulus of tubes. The results have been varied significantly as a function of ply orientation and interlaminar number.

  • PDF

흑연/에폭시 복합재료의 혼합모우드 층간분리 해석 (Analysis of Mixed Mode Delamination in Graphite/Epoxy Composite)

  • 염영진;유희
    • 한국자동차공학회논문집
    • /
    • 제4권4호
    • /
    • pp.171-178
    • /
    • 1996
  • DCB(pure mode I) and CLS(mixed mode) tests were performed to investigate the effect of fracture mode on the interlaminar fracture of composite laminate. Mode I critical strain energy release rate was found to be $133J/m^2$ from the DCB test and total strain energy release rate decreased from $1, 270J/m^2$ as thickness ratio(tl/t) varied from 0.333 to 0.667 from the crease from the CLS test. Crack length had no effect on the total strain energy release rate and load was almost constant during the crack growth of the specimen which had the specific thickness ratio. Crack initiated when the stress of the strap ply reached constant stress $42kgf/mm^2$ which was found to be independent of the thickness ratio.

  • PDF

차체구조용 복합재 박육부재의 축압괴 특성에 관한 연구 (The Study on the Axial Collapse Characteristics of Composite Thin-Walled Members for Vehicles)

  • 김영남;차천석;양인영
    • 한국자동차공학회논문집
    • /
    • 제9권6호
    • /
    • pp.195-200
    • /
    • 2001
  • Composites have wide applications in aerospace vehicles and automobiles because of the inherent flexibility in their design for improved material properties. Composite tribes in particular, are potential candidates for their use as energy absorbing elements in crashworthiness applications due to their high specific energy absorbing capacity and the stroke efficiency. Their failure mechanism however is highly complicated and rather difficult to analyze. This includes fracture in fibres, in the matrix and in the fibre-matrix interface in tension, compression and shear. The purpose of this study is to investigate the energy absorption characteristics of CFRP(Carbon Fiber Reinforced Plastics) tubes on static and impact tests. Static compression tests have been carried out using the static testing machine and impact tests have been carried out using the vertical crushing testing machine. Interlaminar number affect the energy absorption capability of CFRP tubes. Also, theoretical and experimental have the same value.

  • PDF