혼성물리화학기상 증착법에 의한 알루미나 완충층을 가진 실리콘 기판 위의 $MgB_2$ 박막제조에 대한 연구 (Deposition of $MgB_2$ Thin Films on Alumina-Buffered Si Substrates by using Hybrid Physical-Chemical Vapor Deposition Method)

  • 이태경;박세원;성원경;허지영;정순길;이병국;안기석;강원남
    • Progress in Superconductivity
    • /
    • 제9권2호
    • /
    • pp.177-182
    • /
    • 2008
  • [ $MgB_2$ ] thin films were fabricated using hybrid physical-chemical vapor deposition (HPCVD) method on silicon substrates with buffers of alumina grown by using atomic layer deposition method. The growth war in a range of temperatures $500\;{\sim}\;600^{\circ}C$ and under the reactor pressures of $25\;{\sim}\;50\;Torr$. There are some interfacial reactions in the as-grown films with impurities of mostly $Mg_2Si$, $MgAl_2O_4$, and other phases. The $T_c$'s of $MgB_2$ films were observed to be as high as 39 K, but the transition widths were increased with growth temperatures. The magnetization was measured as a function of temperature down to the temperature of 5 K, but the complete Meissner effect was not observed, which shows that the granular nature of weak links is prevailing. The formation of mostly $Mg_2Si$ impurity in HPCVD process is discussed, considering the diffusion and reaction of Mg vapor with silicon substrates.

  • PDF

Thermodynamic Control in Competitive Anchoring of N719 Sensitizer on Nanocrystalline $TiO_2$ for Improving Photoinduced Electrons

  • Lim, Jong-Chul;Kwon, Young-Soo;Song, In-Young;Park, Sung-Hae;Park, Tai-Ho
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2011년도 제41회 하계 정기 학술대회 초록집
    • /
    • pp.68-69
    • /
    • 2011
  • The process of charge transfer at the interface between two semiconductors or between a metal and a semiconductor plays an important role in many areas of technology. The optimization of such devices requires a good theoretical description of the interfaces involved. This, in turn, has motivated detailed mechanistic studies of interfacial charge-transfer reactions at metal/organic, organic/organic, and organic/inorganic semiconductor heterojunctions. Charge recombination of photo-induced electron with redox species such as oxidized dyes or triiodide or cationic HTM (hole transporting materials) at the heterogeneous interface of $TiO_2$ is one of main loss factors in liquid junction DSSCs or solid-state DSSCs, respectively. Among the attempts to prevent recombination reactions such as insulating thin layer and lithium ions-doped hole transport materials and introduction of co-adsorbents, although co-adsorbents retard the recombination reactions as hydrophobic energy barriers, little attention has been focused on the anchoring processes. Molecular engineering of heterogeneous interfaces by employing several co-adsorbents with different properties altered the surface properties of $TiO_2$ electrodes, resulting to the improved power conversion efficiency and long-term stability of the DSSCs. In this talk, advantages of the coadsorbent-assisted sensitization of N719 in preparation of DSSCs will be discussed.

  • PDF

환형수조를 이용한 머드유동층의 연행부상률 산정 (Estimation of Entrainment Rate of Fluid Mud using Annular Flume)

  • 김동호;김원규;황규남
    • 한국해안·해양공학회논문집
    • /
    • 제28권5호
    • /
    • pp.257-264
    • /
    • 2016
  • 본 연구에서는 머드유동층의 연행부상률 산정을 목적으로 국내 최초로 환형수조를 이용하여 고령토 머드유동층에 대한 연행부상 실험이 수행되었다. 고령토로 제작된 머드유동층의 초기농도를 변화시키면서 총 6회의 연행부상 실험이 수행되었으며, 머드유동층의 연행부상률이 정량적으로 산정되었다. 본 연구결과에 따르면, 머드유동층의 부상률과 반대방향으로 작용하는 토사의 침강의 영향으로 인하여, 경계면에서 난류 운동에너지의 부가 손실이 유발되고, 결과적으로 리차드슨 수가 높은 경우에 염수 성층 구조일 때 보다 상당히 감소된 부상률이 초래되는 것으로 나타났다. 또한, 과거 타 연구결과와의 비교 검토를 통하여 본 연구에서 사용된 환형수조는 성능 상에 문제가 없음이 간접적으로 확인되었으며, 연행부상 실험 방법 및 실험 결과의 타당성이 입증되었다.

고분자 태양전지를 위한 비공액형 고분자 전해질 (Non-Conjugated Polymer Electrolytes for Polymer Solar Cells)

  • 라마티아 피트리 빈티 나스룬;사브리나 아우파 살마;김주현
    • 공업화학
    • /
    • 제31권5호
    • /
    • pp.467-474
    • /
    • 2020
  • 고분자태양전지는 용액공정에 의한 생산이 가능하여, 경량, 저비용, 기계적 유연성 및 고효율과 같은 많은 이점이 있다. 이들은 지난 수십 년 동안 많은 관심을 끌어왔다. 공액 고분자 전해질(conjugated polymer electrolyte, CPE) 및 비공액 고분자 전해질(non-conjugated polymer electrolyte, NPE) 재료는 기존의 금속 산화물 중간층과 관련된 일반적인 약점(전하 수집능력 저하 및 금속/고분자 계면에서의상용성 저하 등)을 극복하기 위해 사용되었다. 그러나 CPE의 합성은 매우 복잡한 합성과정이 필요하며, 대량합성이 어려운 단점이 있다. 따라서 상대적으로 합성이 용이한 NPE를 개발 혹은 기존에 개발되어 있는 NPE를 이용하면 보다 쉽게 단점을 극복할 수 있다. 이온 그룹이 포함되어 있는 경우 NPE는 특히 고분자 태양전지를 구현함에 있어 많은 이점을 제공할 수 있으며, 이에 본 총설에서는 그 동안 개발 혹은 응용되었던 NPE에 대한 내용을 다루었다.

Si 웨이퍼의 UBM층 도금두께에 따른 무플럭스 플라즈마 솔더링 (Fluxless Plasma Soldering with Different Thickness of UBM Layers on Si-Wafer)

  • 문준권;강경인;이재식;정재필;주운홍
    • 한국표면공학회지
    • /
    • 제36권5호
    • /
    • pp.373-378
    • /
    • 2003
  • With increasing environmental concerns, application of lead-free solder and fluxless soldering process have been taken attention from the electronic packaging industry. Plasma treatment is one of the soldering methods for the fluxless soldering, and it can prevent environmental pollution cased by flux. On this study fluxless soldering process under $Ar-H_2$plasma using lead free solders such as Sn-3.5 wt%Ag, Sn-3.5 wt%Ag-0.7 wt%Cu and Sn-37%Pb for a reference was investigated. As the plasma reflow has higher soldering temperature than normal air reflow, the effects of UBM(Under Bump Metallization) thickness on the interfacial reaction and bonding strength can be critical. Experimental results showed in case of the thin UBM, Au(20 nm)/Cu(0.3 $\mu\textrm{m}$)/Ni(0.4 $\mu\textrm{m}$)/Al(0.4 $\mu\textrm{m}$), shear strength of the soldered joint was relatively low as 19-27㎫, and it's caused by the crack observed along the bonded interface. The crack was believed to be produced by the exhaustion of the thin UBM-layer due to the excessive reaction with solder under plasma. However, in case of thick UBM, Au(20 nm)/Cu(4 $\mu\textrm{m}$)/Ni(4 $\mu\textrm{m}$)/Al(0.4 $\mu\textrm{m}$), the bonded interface was sound without any crack and shear strength gives 32∼42㎫. Thus, by increasing UBM thickness in this study the shear strength can be improved to 50∼70%. Fluxed reflow soldering under hot air was also carried out for a reference, and the shear strength was 48∼52㎫. Consequently the fluxless soldering with plasma showed around 65∼80% as those of fluxed air reflow, and the possibility of the $Ar-H_2$ plasma reflow was evaluated.

크롬질화처리한 저탄소강의 고분자 전해질 연료전지 분리판으로서의 표면특성 (Surface Properties of Chromium Nitrided Carbon Steel as Separator for PEMFC)

  • 최창용;강남현;남대근
    • 한국표면공학회지
    • /
    • 제44권5호
    • /
    • pp.173-178
    • /
    • 2011
  • Separator of stack in polymer electrolyte membrane fuel cell (PEMFC) is high cost and heavy. If we make it low cost and lighter, it will have a great ripple. In this study, low carbon steel is used as base metal of separator because the cost of low carbon steel is very cheaper commercial metal material than stainless steels, which is widely used as separator. Low carbon steel has not a good corrosion resistance. In order to improve the corrosion resistance and electrolytic conductivity, low carbon steel needs to be surface treated. We made Chromium electroplated layer of $5{\mu}m$, $10{\mu}m$ thickness on the surface of low carbon steel and it was nitrided for 2 hours at $1000^{\circ}C$ in a furnace with 100 torr nitrogen gas pressure. Cross-sectional and surface microstructures of surface treated low carbon steel are investigated using SEM. And crystal structures are investigated by XRD. Interfacial contact resistance and corrosion tests were considered to simulate the internal operating conditions of PEMFC stack. The corrosion test was performed in 0.1 N $H_2SO_4$ + 2 ppm $F^-$ solution at $80^{\circ}C$. Throughout this research, we try to know that low carbon steel can be replaced stainless steel in separator of PEMFC.

Tensile strength of bilayered ceramics and corresponding glass veneers

  • Anunmana, Chuchai;Champirat, Tharee;Jirajariyavej, Bundhit
    • The Journal of Advanced Prosthodontics
    • /
    • 제6권3호
    • /
    • pp.151-156
    • /
    • 2014
  • PURPOSE. To investigate the microtensile bond strength between two all-ceramic systems; lithium disilicate glass ceramic and zirconia core ceramics bonded with their corresponding glass veneers. MATERIALS AND METHODS. Blocks of core ceramics (IPS e.max$^{(R)}$ Press and Lava$^{TM}$ Frame) were fabricated and veneered with their corresponding glass veneers. The bilayered blocks were cut into microbars; 8 mm in length and $1mm^2$ in cross-sectional area (n = 30/group). Additionally, monolithic microbars of these two veneers (IPS e.max$^{(R)}$ Ceram and LavaTM Ceram; n = 30/group) were also prepared. The obtained microbars were tested in tension until fracture, and the fracture surfaces of the microbars were examined with fluorescent black light and scanning electron microscope (SEM) to identify the mode of failure. One-way ANOVA and the Dunnett's T3 test were performed to determine significant differences of the mean microtensile bond strength at a significance level of 0.05. RESULTS. The mean microtensile bond strength of IPS e.max$^{(R)}$ Press/IPS e.max$^{(R)}$ Ceram ($43.40{\pm}5.51$ MPa) was significantly greater than that of Lava$^{TM}$ Frame/Lava$^{TM}$ Ceram ($31.71{\pm}7.03$ MPa)(P<.001). Fluorescent black light and SEM analysis showed that most of the tested microbars failed cohesively in the veneer layer. Furthermore, the bond strength of Lava$^{TM}$ Frame/Lava$^{TM}$ Ceram was comparable to the tensile strength of monolithic glass veneer of Lava$^{TM}$ Ceram, while the bond strength of bilayered IPS e.max$^{(R)}$ Press/IPS e.max$^{(R)}$ Ceram was significantly greater than tensile strength of monolithic IPS e.max$^{(R)}$ Ceram. CONCLUSION. Because fracture site occurred mostly in the glass veneer and most failures were away from the interfacial zone, microtensile bond test may not be a suitable test for bonding integrity. Fracture mechanics approach such as fracture toughness of the interface may be more appropriate to represent the bonding quality between two materials.

Crystal Structure and Dielectric Responses of Pulsed Laser Deposited (Ba, Sr)$TiO_3$ Thin Films with Perovskite $LaNiO_3$ Metallic Oxide Electrode

  • Lee, Su-Jae;Kang, Kwang-Yong;Jung, Sang-Don;Kim, Jin-Woo;Han, Seok-Kil
    • The Korean Journal of Ceramics
    • /
    • 제6권3호
    • /
    • pp.258-261
    • /
    • 2000
  • Highly (h00)-oriented (Ba, Sr)TiO$_3$(BST) thin films were grown by pulsed laser deposition on the perovskite LaNiO$_3$(LNO) metallic oxide layer as a bottom electrode. The LNO films were deposited on SiO$_2$/Si substrates by rf-magnetron sputtering method. The crystalline phases of the BST film were characterized by x-ray $\theta$-2$\theta$, $\omega$-rocking curve and $\psi$-scan diffraction measurements. The surface microsturcture observed by scanning electron microscopy was very dense and smooth. The low-frequency dielectric responses of the BST films grown at various substrate temperatures were measured as a function of frequency in the frequency range from 0.1 Hz to 10 MHz. The BST films have the dielectric constant of 265 at 1 kHz and showed multiple dielectric relaxation at the low frequency region. The origin of these low-frequency dielectric relaxation are attributed to the ionized space charge carriers such as the oxygen vacancies and defects in BST film, the interfacial polarization in the grain boundary region and the electrode polarization. We studied also on the capacitance-voltage characteristics of BST films.

  • PDF

보강재에 도금된 Cu층이 Al/SiC복합재료의 젖음성에 미치는 영향 (Wetting improvement of SiC/Al Metal Matrix Composite by Cu Surface Treatment)

  • 이경구;조규종;이도재
    • 한국재료학회지
    • /
    • 제11권5호
    • /
    • pp.398-404
    • /
    • 2001
  • SiC 보강재 표면에 도금된 Cu금속층이 Al/SiC복합재료의 젖음성에 미치는 영향을 검토하였다. 보강재에 대한 금속층의 도금은 무전해도금법을 이용하였으며, Al/SiC 복합재료의 제조는 텅스텐 발열체 진공로의$ 670^{\circ}C$~$900^{\circ}C$에서 제조하여 보강재와 기지간의 접촉부위를 촬영하여 젖음성을 측정하였다 젖음성 측정 결과 보강재에 도금된 Cu층은 젖음성을 향상시켰고, 젖음성의 개선은 보강재에 도금된 금속층과 기지간의 반응에 의해 계면에너지를 변화시킴으로서 나타난 결과이며. 반응을 통한 산화피막의 배제도 영향을 미친 것으로 판단된다

  • PDF

공초점레이저주사현미경을 이용한 심미수복재와 상아질의 접착계면에 관한 연구 (A CONFOCAL LASER SCANNING MICROSCOPIC STUDY ON THE INTERFACE BETWEEN TOOTH COLORED RESTORATIVE MATERIALS AND DENTIN)

  • 박병철;조영곤;문주훈
    • Restorative Dentistry and Endodontics
    • /
    • 제25권3호
    • /
    • pp.313-320
    • /
    • 2000
  • The purpose of this study was to evaluate on the interfacial morphology between dentin and restorative materials. In this in vitro study, the cavity wall restorated with 3 different kinds of tooth colored restorative materials [resin-modified Glass Ionomer cement (Fuji II LC), composite resin (Z-100), compomer (Dyract)]. The thirty extracted human molar teeth without caries and/or restorations are used. The experimental teeth were randomly divided into three groups of ten teeth each. In each group, Wedge shaped cavities (width: 3mm, length: 2mm, depth: 1.5mm) were prepared at the cementoenamel junction on buccal and lingual surfaces. The adhesive of composite resin were mixed with rhodamine B. Primer of composite resin, Prime & Bond 2.1 of Dyract and liquid of Fuji II LC were mixed with fluorescein. In group 1, the cavity wall was treatment with dentin conditioner, and then restorated with Fuji II LC. In group 2, the cavity wall was treatment with Prime & Bond 2.1 and then restorated with Dyract. In group 3, the cavity wall was etching with 10% maleic acid, applied with primer and bonding agent and then restorated with Z-100. The interface between dentin and restorative materials was observed by fluoresence imaging with a confocal laser scanning microscope. The results were as follows : 1. In Glass ionomer group, adaptation of resin modified Glass-ionomer restoration against cavity wall is tight, but the crack formed inside of restoration were observed. 2. In Dyract group, the penetration of resin tag is shorter and the width of hybrid layer is narrower than composite resin group. 3. In Z-100 group, primer penetrated deeply through dentinal tubule. Also bonding agent was penetrated along the primer, but the penetration length is shorter than primer part, and in 3-D image, the resin tag is conical shape and lateral branch is observed.

  • PDF