• Title/Summary/Keyword: Insulation breakdown voltage

Search Result 342, Processing Time 0.019 seconds

Electrical Characteristics Analysis According to Electrode Shape and Distance Between Electrodes (전극 형태와 전극 간 거리에 따른 전기적 특성 분석)

  • Tae-Hee Kim;Soon-Hyung Lee;Mi-Yong Hwang;Yong-Sung Choi
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.36 no.4
    • /
    • pp.408-412
    • /
    • 2023
  • In this paper, in order to analyze high electrical insulation and cooling performance using mineral oil, the liquid insulating oil was changed in electrode shape and distance between electrodes to compare and analyze electrical characteristics according to equal electric field, quasi-equivalent electric field, and unequal electric field. As a result, the breakdown voltages were 36,875 V and 36,875 V in the form of sphere-sphere and plate-plate electrodes with equal electric fields. The breakdown voltage was 31,475 V in the sphere-plate electrode type, which is a quasi-equilibrium field, and the breakdown voltage was 28,592 V, 27,050 V, and 22,750 V in the needle-needle, sphere-needle, and needle-plate electrode types, which are unequal fields. Through this, it is possible to know the difference in breakdown voltage according to the type of electric field. The more equal the field, the higher the breakdown voltage, and the more unequal field, the lower the breakdown voltage. The difference in insulation breakdown voltage could be seen depending on the type of electric field, the insulation breakdown voltage was higher for the more equal electric field, and the insulation breakdown voltage was lower for the more unequal electric field. Also, it was confirmed that the closer the distance between the electrodes, the higher the insulation breakdown voltage, the higher the insulation breakdown current, and the insulation breakdown voltage and the insulation breakdown current were proportional.

Electrical Breakdown Properties of Oil-paper Insulation under Pulsating Voltage Influenced by Temperature

  • Bao, Lianwei;Li, Jian;Zhang, Jing;Li, Xudong
    • Journal of Electrical Engineering and Technology
    • /
    • v.11 no.6
    • /
    • pp.1735-1743
    • /
    • 2016
  • Insulation of valve-side windings in converter transformer withstands pulsating voltages, which will produce more serious insulation problems. In this paper, the electric breakdown experiments of oil-paper insulation specimens were executed at pulsating voltages and different temperatures. Experiment and analysis results showed that the breakdown voltage decreased with increasing temperature under pulsating voltage. The influence of temperature proves to be more significant once the temperature exceeds a limitation threshold. A fitting formula between breakdown voltage and the temperature was reported. Finally, in order to clearly understand the breakdown properties under pulsating voltage, the electric field distribution and space charge behavior under pulsating voltage at different temperature were discussed.

Characteristics of Insulation Diagnosis and Failure in Gas Turbine Generator Stator Windings

  • Kim, Hee-Dong
    • Journal of Electrical Engineering and Technology
    • /
    • v.9 no.1
    • /
    • pp.280-285
    • /
    • 2014
  • In order to evaluate the insulation deterioration in the stator windings of five gas turbine generators(137 MVA, 13.8 kV) which has been operated for more than 13 years, diagnostic test and AC dielectric breakdown test were performed at phases A, B and C. These tests included measurements of AC current, dissipation factor, partial discharge (PD) magnitude and capacitance. ${\Delta}I$ and ${\Delta}tan{\delta}$ in all three phases (A, B and C) of No. 1 generator stator windings showed that they were in good condition but PD magnitude indicated marginally serviceable and bad level to the insulation condition. Overall analysis of the results suggested that the generator stator windings were indicated serious insulation deterioration and patterns of the PD in all three phases were analyzed to be internal, slot and spark discharges. After the diagnostic test, an AC overvoltage test was performed by gradually increasing the voltage applied to the generator stator windings until electrical insulation failure occurred, in order to determine the breakdown voltage. The breakdown voltage at phases A, B and C of No. 1 generator stator windings failed at 28.0 kV, 17.9 kV, and 21.3 kV, respectively. The breakdown voltage was lower than that expected for good-quality windings (28.6 kV) in a 13.8kV class generator. In the AC dielectric breakdown and diagnostic tests, there was a strong correlation between the breakdown voltage and the voltage at which charging current increases abruptly ($P_{i1}$, $P_{i2}$).

A Study on the Insulation Characteristics for Stator Windings of IGBT PWM Inverter-Fed Induction Motors

  • Hwang, Don-Ha;Kang, Dong-Sik;Kim, Yong-Joo;Lim, Tae-Hoon;Bae Sung-Woo;Kim Dong-Hee;Ro Chae-Gyun
    • Journal of Power Electronics
    • /
    • v.3 no.3
    • /
    • pp.159-166
    • /
    • 2003
  • The winding insulation of low-voltage induction motors in adjustable-speed drive system with voltage-fed Inverters is substantially stressed due to the uneven voltage distribution and excessive voltage stress (dv/dt), which result in the premature insulation breakdown In this paper, the detailed insulation test results of 26 low-voltage induction motors are presented. Six different types of insulation techniques are applied to 26 motors. The insulation characteristics are analyzed with partial discharge, discharge inception voltage, AC current, and dissipation factor tests Also, insulation breakdown tests by high voltage pulses are performed, and the corresponding breakdown voltages obtained.

Effect of Conductor Radius of Polyesterimide- Polyamideimide Enameled Round Wire on Insulation Breakdown Voltage and Insulation Lifetime

  • Park, Jae-Jun;Shin, Seong-Sik;Lee, Jae-Young;Han, Se-Won;Kang, Dong-Pil
    • Transactions on Electrical and Electronic Materials
    • /
    • v.16 no.3
    • /
    • pp.146-150
    • /
    • 2015
  • Insulation breakdown voltage and insulation lifetime were investigated in straight lines or twisted pairs with polyesterimide-polyamideimide enameled round wires (EI/AIW ). The enamel thickness was 50 μm and the conducting copper radius was 0.50, 0.75, 1.09, and 1.50 mm, respectively. There were many air gaps in a twisted pair therefore, when voltage was applied to the twisted pair, enamel erosion took place in the air gap area because of partial discharge according to Paschen's law. Insulation breakdown voltage and insulation lifetime were highest in the sample of 0.75 mm conductor radius, which was higher than those values for 0.50 mm or 1.09 and 1.55 mm.

Assessment of Insulation Deterioration in Stator Windings of High Voltage Motor (고압전동기 고정자 권선의 절연열화 평가)

  • Kim, Hee-Dong;Kong, Tae-Sik
    • The Transactions of The Korean Institute of Electrical Engineers
    • /
    • v.61 no.5
    • /
    • pp.711-716
    • /
    • 2012
  • To assess the insulation deterioration of stator windings, diagnostic and AC breakdown tests were performed on the eleven high voltage (HV) motors rated at 6kV. After completing the diagnostic tests, the AC overvoltage test was performed by gradually increasing the voltage applied to the stator windings until electrical insulation failure occurred, to obtain the breakdown voltage. Stator winding of motors 1, 3, and 8 failed at above rated voltage at 14 kV, 13.8kV, and 16.4kV, respectively. The breakdown voltage of three motors was higher than expected for good quality windings in 6kV motors. Based on deterioration evaluation criteria, the stator winding insulation of eleven HV motors are confirmed to be in good condition. The turning point of the current, $P_{i2}$, in the AC current vs. voltage characteristics occurred between 5kV and 6kV, and the breakdown voltage was low between 13.8kV and 16.4kV. There was a strong correlation between the breakdown voltage and various electrical characteristics in diagnostic tests including Pi2.

Analysis of Insulation Condition in Traction Motor Stator Windings (견인전동기 고정자 권선의 절연상태 분석)

  • Kim, Hee-Dong;Park, Young
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.20 no.7
    • /
    • pp.631-635
    • /
    • 2007
  • Diagnostic, surge and ac breakdown tests are widely used to evaluate the insulation condition of stator winding in traction motor. Diagnostic test included ac current, tan delta and maximum partial discharge. The result of diagnostic test indicates that five kinds of stator windings are good condition. Surge test was peformed to confirm the healthy of turn insulation in stator windings. This test is very easy to detect the turn insulation failure between normal and defect stator windings. After completing the diagnostic test, ac breakdown test has conducted gradually increasing ac voltage, until the stator winding punctured. No. 5 stator windings failed near rated voltage of 18.9 kV The breakdown voltage of No. 1 stator windings was 13.0 kV The ac breakdown voltage of normal winding is about 1.45 times higher than that of defect windings. The failure was located in a line-end coil at the exit from the core slot.

Accelerated Insulation Life Estimation for PAI/Nano Silica Enamelled Wire under Inverter Surge and Temperature Stress (인버터 서지와 온도스트레스 하에서 PAI/Nano Silica 에나멜와이어의 가속절연수명 평가)

  • Park, Jae-Jun
    • The Transactions of The Korean Institute of Electrical Engineers
    • /
    • v.65 no.10
    • /
    • pp.1712-1720
    • /
    • 2016
  • AC and DC insulation breakdown voltage was studied for magnet wire coated with double layers of high flexural PAI layer and high anti-corona PAI/nanosilica (15 wt%) layer. The specimens were prepared at various drying temperatures (T/D): $22^{\circ}C$, $240^{\circ}C$, and $260^{\circ}C$, respectively. The increase effects of nanosilica on AC and DC insulation breakdown voltage were not so significant compared to that of magnet wire coil coated with original PAI. And the AC and DC insulation breakdown voltage was improved by decreasing diameter of winding coil. As T/D temperature increased, AC and DC insulation breakdown voltage decreased.

Dielectric Insulation Properties of Double Pancake Coil Type HTS Transformer (Double Pancake Coil형 고온초전도 변압기의 전기적 절연 특성)

  • 백승명;정종만;이현수;한철수;김상현
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.16 no.2
    • /
    • pp.151-156
    • /
    • 2003
  • High temperature superconductor can only be applied against an engineering specofication that has to be determined for each particular application form the design requirements for economic viability and for operation margins in service. However, in order to realize the HTS transformer, it is necessary to establish the high voltage insulation technique in cryogenic temperature. Therefore, the composite insulation of double pancake coil type transformer are described and AC breakdown voltage characteristics of liquid nitrogen(LN$_2$) under HTS pancake coil electrode made by Bi-2223/Ag are studied. The Breakdown of LN$_2$ is dominated electrode shape and distance. The influence of pressure on breakdown voltage is discussed with th different electrode. For the electrical insulation design of turn-to-turn insulation for the HTS transformer, we tested breakdown strength of insulation sheet under varying pressure. And we investigated surface flashover properties of LN$_2$ and complex conition of cryogenic gaseous nitrogen(CGN$_2$) obove a LN$_2$ surface. The surface voltage of GFRP was measured as a function of thickness and electrode distance in LN$_2$ and complex condition of CGN$_2$ above a LN$_2$ surface. this research presented information of electrical insulation design for double pancake coil(DPC) type HTS transformer.

Stator Insulation Quality Assessment for High Voltage Motors Based on Probability Distributions

  • Kim, Hee-Dong;Kim, Chung-Hyo
    • Journal of Electrical Engineering and Technology
    • /
    • v.3 no.4
    • /
    • pp.571-575
    • /
    • 2008
  • Stator insulation quality assessment for high voltage motors is a major issue for the reliable maintenance of industrial and power plants. To assess the condition of stator insulation, nondestructive tests were performed on the sixty coil groups of twelve motors. After completing the nondestructive tests, the AC voltage applied to the stator winding was gradually increased until insulation failure in order to obtain the breakdown voltage. The stator winding of each motor was classified into five coil groups; one group with healthy insulation and four groups with four different types of artificial defects. To analyze the breakdown voltage statistically, Weibull distribution was employed for the tests on the fifty coil groups of ten motors. The 50th percentile values of the measured breakdown voltages based on the statistical data of the five coil groups of ten motors were 26.1kV, 25.0kV, 24.4kV, 26.7kV and 30.5kV, respectively. Almost all of the failures were located in the line-end coil at the exit of the core slot. The breakdown voltages and the types of defects showed strong relation to the stator insulation tests such as in the case of dissipation factor and ac current. It is shown that the condition of the motor insulation can be determined from the relationship between the probability of failure and the type of defect.