알루미늄 합금 용접부의 피로균열성장거동에 관한 파괴력학적 연구 (A Fracture Mechanics Study on the Fatigue Crack Growth Behaviors in Aluminum Alloy Weldments)

  • 차용훈
    • 한국생산제조학회지
    • /
    • 제5권3호
    • /
    • pp.31-39
    • /
    • 1996
  • The objective of this study is to investigate the influence of welding residual stresses on the fatigue crack growth behavior of cracks located transverse to the weld bead. For this purpose, G. T. A (Gas Tungsten Arc) welding was performed on hte Al alloy 1100-O plate and the same initial crack is made on HAZ(Heat Affected Zone), weld metal and base meta respectively. Specimens were used CT(Compact Tension) specimens. Initial welding residual stresses were measured by using strai gage sectioning method. All specimens were tested under constant amplitude load with stress ratio R=0.1, It is possible to predict fatigue crack growth behaviors and the fatigue life, using numerical analysis together with distribution of initial residual stress and the values of C and m obtained from $da/dN-{\Delta}K$

  • PDF

변형후 형상의 최적화를 위한 동맥과 PTFE 문합의 직경비 연구 (The Study on the Diameter Ratio of the Artery-PTFE Anastomosis for the Optimized Deformed Shape)

  • 이성욱;심재준;한근조
    • 대한의용생체공학회:의공학회지
    • /
    • 제24권2호
    • /
    • pp.113-119
    • /
    • 2003
  • 본 연구에서는 end-to-end 문합시 변형된 직경의 불일치로 인하여 발생하게 되는 혈관질환을 방지하기 위하여 기계역학적 거동을 유한요소 법을 이용하여 해석한 결과를 나타내었다. 이 연구에서는 서로 다른 직경을 가지는 동맥과 인공혈관인 PTFE의 문합시 봉합으로 인한 예변형을 고려하였으며, 봉합된 문합부에 수축기혈압인 120mmHg(16.0KPa)을 작용시켜 혈관의 변형을 분석하였다. 변형 후 최종 문합부의 형상은 동맥과 PTFE의 초기 직경비(R$_{I}$)와 PTFE의 두께에 대하여 분석하였다. 그리고 동맥과 PTFE의 초기 직경비가 문합부에서 발생되는 응력에 어떠한 영향을 미치는지에 대하여 해석하여 다음과 같은 결과를 얻었다. 1. 혈관내막의 증식등을 고려하지 않고 봉합으로 인한 예변형과 수축기 혈압만을 고려할 경우 가장 이상적인 초기 직경비(R$_{I}$)는 1.073이다. 2. 상당응력과 원주방향응력은 초기 직경비(R$_{I}$) 증가에 따라 증가하며 모두 접합부에서 PTFE측으로 0.4mm 떨어진 지점에서 최대값이 발생하였다.

X선 잔류응력을 이용한 냉간압연강의 피로손상 모델링에 관한 연구 (A Study on Fatigue Damage Modelling in Cold Rolled Steel using X-ray Residual Stress)

  • 조석수;주원식
    • 한국해양공학회지
    • /
    • 제13권4호통권35호
    • /
    • pp.55-62
    • /
    • 1999
  • Cold rolled steel has much plastic strain in the material surface produced by manufacturing process. The strain causes the variation of surface residual stress, in which influences the fatigue behavior under repeated loading. As experimental results, it was confirmed that the behavior of residual stress ${\sigma}_r$, with cycle N consisted of three stages except stress amplitude near fatigue limit in SPCC steel. On the first stage compressive residual stress decreased rapidly, on the second stage gradually, and on the last stage slightly. The relation between ${\sigma}_r$, and log N appeared linear behavior except the early part of cycle ratio $N/N_f$. The average gradient of ${\sigma}_r$, with respect to log N seemed to take a constant value without initial cycle ratio. On the other hand, the $N_f$ line was regressed by the first-order polynomial equation on ${\sigma}_r-log\;N_f$ diagram. Therefore, this study showed that both the gradient of ${\sigma}_r$, with respect to log N and the $N_f$ line was useful in predicting the cycle ratio $N/N_f$.

  • PDF

Step-Up 구조를 갖는 다층박막 초소형 구동소자의 초기변형 최소화에 관한 연구 (Minimization of Initial Deflection of Multi-Layered Micro-Actuator with Step-Up Structure)

  • 이희중;강신일
    • 대한기계학회논문집A
    • /
    • 제26권11호
    • /
    • pp.2415-2420
    • /
    • 2002
  • In the present study, a new anchor design was proposed to minimize the initial deflection of micro multi-layer cantilever beam with step-up structure, which is a key component of thin film micro-mirror array. It is important to minimize the initial deflection, caused by residual stress, because it reduces the performance of the actuation. Theoretical and experimental studies were conducted to examine the cause of the initial bending deflection. It was found that the bending deflection at the anchor of the cantilever beam was the primary source of initial deflection. Various anchor designs were proposed and the initial deflections for each design were calculated by finite element analysis. The analysis results were compared with experiments. To reduce the initial deflection a secondary support was added to the conventional structure. The optimal shapes were obtained by simulation and experiment. It was found from the analysis that the ratio or horizontal and vertical dimensions of secondary support was the governing factor, which affected the initial deflection.

단순봉합모델을 이용한 문합에서 탄성경계층의 두께 변화에 따른 기계역학적 거동에 관한 연구 (The Study on the Mechanical Behavior of the Anastomosis with respect to the Thickness Variation of Elastic Foundation Using Simplified Suturing Model)

  • 이성욱;한근조;심재준;한동섭;김태형
    • 한국정밀공학회지
    • /
    • 제21권8호
    • /
    • pp.188-195
    • /
    • 2004
  • In this paper we analyzed the mechanical behavior with respect to the thickness variation of elastic foundation(fatty tissue) in end-to-end anastomosis. This study considered the preliminary deformed shape induced by suturing in the anastomosis of coronary artery and PTFE with different diameters using simplified suturing model and the fatty tissue surrounding heart and coronary artery for more accurate result using finite element method. Area compliance(CA) was used to analyze the final deformed shape of the anastomotic part with respect to the thickness variation of fatty tissue under mean blood pressure, 100mmHg(13.3㎪). And Equivalent and circumferential stresses in the anastomosis were also analyzed with respect to the change of initial diameter ratio( $R_1$) and fatty tissue thickness( $T_{F}$). The results obtained were as follows : 1 When the elastic foundation, assumed to be incompressive material, surrounded the grafts in anastomosis, the compliance mismatch of artery and PTFE was reduced by 47 -72%. 2. As the initial diameter ratio( $R_1$) became larger, the higher difference of compliance was induced in spite of elastic foundation surrounding grafts. 3. The maximum nondimensional circumferential stress is twice or three times as high as the maximum nondimensional equivalent stress in the anastomotic part.t.

Data-driven SIRMs-connected FIS for prediction of external tendon stress

  • Lau, See Hung;Ng, Chee Khoon;Tay, Kai Meng
    • Computers and Concrete
    • /
    • 제15권1호
    • /
    • pp.55-71
    • /
    • 2015
  • This paper presents a novel harmony search (HS)-based data-driven single input rule modules (SIRMs)-connected fuzzy inference system (FIS) for the prediction of stress in externally prestressed tendon. The proposed method attempts to extract causal relationship of a system from an input-output pairs of data even without knowing the complete physical knowledge of the system. The monotonicity property is then exploited as an additional qualitative information to obtain a meaningful SIRMs-connected FIS model. This method is then validated using results from test data of the literature. Several parameters, such as initial tendon depth to beam ratio; deviators spacing to the initial tendon depth ratio; and distance of a concentrated load from the nearest support to the effective beam span are considered. A computer simulation for estimating the stress increase in externally prestressed tendon, ${\Delta}f_{ps}$, is then reported. The contributions of this paper is two folds; (i) it contributes towards a new monotonicity-preserving data-driven FIS model in fuzzy modeling and (ii) it provides a novel solution for estimating the ${\Delta}f_{ps}$ even without a complete physical knowledge of unbonded tendons.

Mean Stress를 고려한 11.7Cr-1.1Mo강의 고온저주기 피로특성에 관한 연구 (A Study of Low Cycle Fatigue Characteristics of 11.7Cr-1.1Mo Heat Resisting Steel with Mean Stress)

  • 홍상혁;홍춘희;이현우
    • 한국자동차공학회논문집
    • /
    • 제14권3호
    • /
    • pp.133-141
    • /
    • 2006
  • The Low cycle fatigue behavior of 11.7Cr-1.1Mo heat-resisting steel has been investigated under strain-controlled conditions with mean stresses at room temperature and $300^{\circ}C$. For the tensile mean stress test, the initial high tensile mean stress generally relaxed to zero at room temperature, however, at $300^{\circ}C$ initial tensile mean stress relaxed to compressive mean stress. Low cycle fatigue lives under mean stress conditions are usually correlated using modifications to the strain-life approach. Based on the fatigue test results from different stain ratio of -1, 0, 0.5, and 0.75 at room temperature and $300^{\circ}C$, the fatigue damage of the steel was represented by using cyclic strain energy density. Total strain energy density considering mean stress indicated well better than not considering mean stress at $300^{\circ}C$. Predicted fatigue life using Smith-Watson-Topper's parameter correlated fairly well with the experimental life at $300^{\circ}C$.

The drained deformation characteristics of sand subjected to lateral cyclic loading

  • Junhua Xiao;Jiapei Ma;Jianfeng Xue;Zhiyong Liu;Yingqi Bai
    • Geomechanics and Engineering
    • /
    • 제34권5호
    • /
    • pp.481-489
    • /
    • 2023
  • Drained cyclic triaxial tests were conducted on a saturated sand to examine its deformation characteristics under either axial or lateral cyclic loading condition. To apply lateral cyclic loading, the cell pressure was cycled while maintaining a constant vertical stress. The strain accumulations and flow direction in the soil were presented and discussed considering various initial stress ratios (η0), cyclic stress amplitudes and cyclic stress paths. The results indicate that axial strain accumulation shows an exponential increase with the maximum stress ratio (ηmax). The initial deviatoric stress has comparable effects with lateral cyclic stress amplitude on the accumulated axial strain. In contrast, the accumulated volumetric strain is directly proportional to the lateral cyclic stress amplitude but not much affected by η0 values. Due to the anisotropy of the soil, the accumulated axial and lateral bulging strains are greater in lateral cyclic loading when compared to axial cyclic loading even though ηmax is the same. It is also found that ηmax affects soil's lateral deformation and increasing the ratio could change the lateral deformation from contraction to bulging. The flow direction depends on ηmax in the sand under lateral cyclic loading, regardless of η0 values and the cyclic stress amplitudes, and a large ηmax could lead to great deviatoric strain but a little volumetric strain accumulation.

복합조직강의 미시조직변화가 피로파괴전파에 미치는 영향 (The Effects of the Microstructural Change of Dual Phase Steel on Fatigue Fracture Propagation)

  • 오세욱;김웅집
    • 한국해양공학회지
    • /
    • 제5권2호
    • /
    • pp.58-66
    • /
    • 1991
  • Not only difference of fatigue crack growth and propagation behavior resulted from the grain size, the hardness ratio and volume fraction in M.E.F. dual phase steel composed of martensite in hard phase and ferrite in soft phase, but also the effects of the plastic constraint were investigated by fracture mechanics and microstructural method. The main results obtained are as follows: 1) The fatigue endurance of M.E.F. steel increases with decreasing the grain size, increasing the ratio of hardness and volume fraction. 2) The initiation of slip and crack occures faster as the stress level goes higher. These phenomena result from the plastic constraint effect of the second phase. 3) The crack propagation rate in the constant stress level is faster as the grain size gets larger, the ratio of hardness lower and volume fraction smaller.

  • PDF

동결 온도와 재하속도에 따른 동결토의 일축압축 및 쪼갬인장 강도특성 (Experimental Study on Unconfined Compression Strength and Split Tensile Strength Properties in relation to Freezing Temperature and Loading Rate of Frozen Soil)

  • 서영교;최헌우
    • 한국해양공학회지
    • /
    • 제26권6호
    • /
    • pp.19-26
    • /
    • 2012
  • Recently the world has been suffering from difficulties related to the demand and supply of energy due to the democratic movements sweeping across the Middle East. Consequently, many have turned their attention to never-developed extreme regions such as the polar lands or deep sea, which contain many underground resources. This research investigated the strength and initial elastic modulus values of eternally frozen ground through a uniaxial compression test and indirect tensile test using frozen artificial soil specimens. To ensure accurate test results, a sandymud mixture of standard Jumunjin sand and kaolinite (20% in weight) was used for the specimens in these laboratory tests. Specimen were prepared by varying the water content ratio (7%, 15%, and 20%). Then, the variation in the strength value, depending on the water content, was observed. This research also established three kinds of environments under freezing temperatures of $-5^{\circ}C$, $-10^{\circ}C$, and $-15^{\circ}C$. Then, the variation in the strength value was observed, depending on the freezing environment. In addition, the tests divided the loading rate into 6 phases and observed the variation in the stress-strain ratio, depending on the loading rate. The test data showed that a lower freezing temperature resulted in a larger strength value. An increase in the ice content in the specimen with the increase in the water content ratio influenced the strength value of the specimen. A faster load rate had a greater influence on the uniaxial compression and indirect tensile strengths of a frozen specimen and produced a different strength engineering property through the initial tangential modulus of elasticity. Finally, the long-term strength under a constant water content ratio and freezing temperature was checked by producing stress-strain ratio curves depending on the loading rate.