• 제목/요약/키워드: Industrial Ceramic

검색결과 597건 처리시간 0.026초

마이크로에멀젼법을 이용한 나노 CoFe2O4 분말의 실리카 코팅 (Silica Coating of Nanosized CoFe2O4 Particles by Micro-emulsion Method)

  • 김유진;유리;박은영;피재환;최의석
    • 한국세라믹학회지
    • /
    • 제46권1호
    • /
    • pp.69-73
    • /
    • 2009
  • We report the preparation of nanocrystalline cobalt ferrite, $CoFe_2O_4$ particles and their surface coating with silica layers using micro emulsion method. The cobalt ferrite nanoparticles with the size 7nm are firstly prepared by thermal decomposition method. Hydrophobic nanoparticles were coated with silica using micro-emulsion method with surfactant, $NH_4OH$, and tetraethylorthosilicate (TEOS). Monodispersed and spherical silica coated cobalt ferrite nanoparticles have average particle diameter of 38 nm and narrow sized distribution.

Gas transport properties of alumina composite membranes

  • Lee, Hong-Joo;Hiroyuki Yamauchi;Hiroyuki Suda;Kenji Haraya
    • 한국막학회:학술대회논문집
    • /
    • 한국막학회 2004년도 Proceedings of the second conference of aseanian membrane society
    • /
    • pp.128-131
    • /
    • 2004
  • The composite mesoporous ceramic membranes were prepared with ${\gamma}$-alumina and poly (2, 6-dimethyl-l, 4-pyphenylene oxide) (PPO) on the surface of the macroporous $\alpha$-alumina ceramic membranes and the permeation results were compared with those of the $\alpha$-alumina membrane for large-scale applications. In the results of the transport experiments, the ceramic membranes gave high gas permeances mainly due to Knudsen diffusion and surface diffusion as an additional mechanism. And, the polymer modification increased the permeances of the strongly adsorbing gas components. In this study the modifications of alumina ceramic membranes could increase the gas permeation performances especially for the strongly absorbing gas components.

  • PDF

일부 요업사업장의 분진, 결정형 유리규산 및 납의 폭로에 관한 연구 (A Study on Work's Exposure to Dust, Crystalline Free Silica and Lead in Ceramic Industry)

  • 오세민;신용철;박동욱;이나루;박승현;이광용;문영한
    • 한국산업보건학회지
    • /
    • 제4권2호
    • /
    • pp.168-179
    • /
    • 1994
  • In some ceramic industries, worker exposure to dust, crystalline free silica and lead were determined and evaluated. The conclusions are as follows. 1. Crystalline silica in bulk samples was 10.5 % in sanitary ware industry, 9.4 % in tile industry, and 2.1 % in ceramic insulator industry respectively. The free silica content of air filter sample was 8.03 % in table ware industry, 5.59 % in sanitary ware industry, and 1.32 % in ceramic insulator industry. Because silica content in ceramic dust is relatively high, it is should be considered silica as important factor in evaluating for ceramic industry. 2. The silica contents in dust from tile, sanitary ware and table ware industries are above 5%, it should be classified as "Type" 2 dust. 3. The airborne concentration of respirable crystalline silica was $27.9{\mu}g/m^3$ in a sanitary ware factory and $5.8{\mu}g/m^3$ in a ceramic insualtor factory. Three of ten samples sampled the above factories were exceeded the occupational exposure levels, $100{\mu}g/m^3$. 4. Geometric mean(GM) of total dust in 11 factories was $1.00mg/m^3$ and GM of respirable dust concentration in 5 factories was $0.33mg/m^3$. Sanitary ware industry had the highest concentration of total dust, $1.62mg/m^3$ and of respirable dust, $0.88mg/m^3$. 5. Average lead concentration in air was $0.05mg/m^3$ in glazing process of 2 factories manufacturing table ware. Five of ten sample(50%) were exceeded $0.05mg/m^3$. Therefore lead exposure in pottery industry should be considered as important problem.

  • PDF

Multifunctionality in Ceramic/Metal Nanocomposites

  • Sekino, Tohru;Kondo, Hiroki;Niihara, Koichi
    • 한국분말재료학회지
    • /
    • 제8권3호
    • /
    • pp.186-191
    • /
    • 2001
  • Several fabrication processes, corresponding nanostructural features and multifunctionality as well has been investigated for oxide ceramic based nanocomposites with metal nanodispersion (i.e., ceramic/metal nanocomposites). Transition metal (Ni, Co, etc) dispersed alumina and zirconia based nanocomposites have been synthesized by reducing and hot-press sintering of ceramic and metal oxide mixtures prepared by several method. Improved fracture strength (1.1 and 1.9 GPa for $Al_2O_3/Ni$ and $ZrO_2/Ni$ nanocomposites, respectively) of these composites have been achieved according to their nanostructures. In addition, ferromagnetic characteristic has been kept. The variation of magnetization with an applied stress has found to be more sensitive as smaller as the magnetic metal dispersion is. This result thus suggests the possibility of fracture and/or stress sensing of the composites by simple magnetic measurement.

  • PDF

세라믹담체를 이용한 페놀계 산업폐수의 생물학적 처리 (Biological Treatment of Phenolic Industrial Wastewater by a Mixed Culture Immobilized on Ceramic Beads)

  • 오희목;구영환;안극현;장갑용;고영희;권기석;윤병대
    • 한국미생물·생명공학회지
    • /
    • 제23권6호
    • /
    • pp.755-762
    • /
    • 1995
  • A phenolic resin industrial wastewater containing about 41,000 mg/l of phenol and 2,800 mg/l of formaldehyde was biologically treated by a mixed culture GE2 immobilized on ceramic beads. This study was carried out with three experimental groups : Control-only added the sludge of papermill wastewater ; GE2 treatment-added GE2 to Control ; Ceramic treatment-applied ceramic carrier to GE2 treatment. When the original wastewater was diluted 80 times with aerated tap-water, influent COD$_{Mn}$ WaS 1,140 mg/l and that of the effluent was in the range of 22-35 mg/l, which was not much different among the experimental groups. However, at 20-times dilution, influent COD$_{Mn}$ was 4,800 mg/l and the effluent COD$_{Mn}$ of Control, GE2 treatment and Ceramic treatment was 179, 128 and 94 mg/l, respectively. COD$_{Mn}$, removal efficiency by Ceramic treatment was the highest, at 98.0%. At this time, the effluent phenol concentration of Control, GE2 treatment and Ceramic treatment was 10.71, 7.93 and 5.60, respectively. As the dilution times decreased, the removal efficiency of COD$_{Mn}$ and phenol did not change much, but COD$_{Mn}$ and phenol concentration of the effluent increased. Consequently, it is likely that the phenolic industrial wastewater containing phenol and formaldehyde can be biologically treated using a GE2 and ceramic carrier and that at 40-times dilution, the effluent completely meets the effluent standards for industrial wastewater treatment plant.

  • PDF

괘속조형(Ceramic SLA)과 고속가공을 이용한 단납금형 개발에 대한 연구 (Case Study of Hybrid Tooling using High Speed Cutting and Ceramic SLA (StereoLithography Apparatuses) Technologies)

  • 권홍규;홍정의
    • 산업경영시스템학회지
    • /
    • 제30권2호
    • /
    • pp.23-28
    • /
    • 2007
  • "Getting to market first" is extremely critical in this competitive business environment. The speed at which products are developed and released to market is tightly linked to profitability and market share. Many companies that have been very skeptical of Rapid Tooling (RT) technologies developed so far are working on Hybrid Tooling (HT) that can really meet the market standards. This paper describes the experimentation how HT process has been being successfully established and effectively applied with typical case study. Through the experimentation, Ceramic-filled HT was found to be aptly suited for the low grade mold, both in terms of the lead time, dimensional accuracy, and tooling cost.

압전 세라믹 액추에이터를 위한 소형 고전압 구동 증폭기 개발 (Development of Compact High Voltage Driving Amplifier for Piezo Ceramic Actuator)

  • 김순철;한정호;이수영
    • 한국산학기술학회논문지
    • /
    • 제13권11호
    • /
    • pp.5409-5415
    • /
    • 2012
  • 압전 세라믹 액추에이터는 스프레이, 디스펜서, 밸브제어와 같은 다양한 산업제품들에 응용된다. 압전 세라믹 소자의 기계적인 변위의 크기는 인가 전압의 크기에 의해 정해지므로, 압전 세라믹 액추에이터 구동을 위해서는 고전압 전원장치와 함께 전력증폭기가 필요하다. 본 논문에서는 간단하고 크기가 작은 H-브리지 형태의 전력증폭기와 플라이백 고전압 스위칭 모드 전원장치를 개발하였다. H-브리지 형태의 전력증폭기는 펄스폭 변조를 이용하여 압전 세라믹 액추에이터에 대한 에너지 입력의 크기를 쉽게 조절할 수 있다는 장점이 있다.

SiC계 세라믹 발열체 경제성 평가 (Economical Estimation of SiC Ceramic Heater)

  • 조현섭;유인호
    • 한국산학기술학회:학술대회논문집
    • /
    • 한국산학기술학회 2009년도 춘계학술발표논문집
    • /
    • pp.450-453
    • /
    • 2009
  • Compositional design and optimization of processing parameters are key factors for controlling and improving the properties of SiC-based electroconductive ceramic composites. Compare economic estimation of SiC ceramic heater with sheathe heater are as followings. (1) Temperature rising time of sheath heater is 1.1 times faster than SiC ceramic heater. (2) Heating insulation of SiC ceramic heater is 2.7 times larger than sheath heater. If SiC ceramic heater is one body type of a product application, contact resistance will decrease. I think that temperature initial rising time is faster than now. The more SiC ceramic heater is used for a long time, the more economic benefit is larger in the view point of heat insulation.

  • PDF

SiC 세라믹 하니컴 담체의 탄성 물성치 평가 (Estimation on Elastic Properties of SiC Ceramic Honeycomb Substrate)

  • 조석수
    • 한국산학기술학회논문지
    • /
    • 제14권12호
    • /
    • pp.6106-6113
    • /
    • 2013
  • 가솔린 엔진 차량용 삼원촉매담체는 주로 코제라이트 세라믹으로 제작되는 다공성 부품으로 엔진의 혼합기가 농후한 경우 삼원촉매의 열적 내구성이 급격히 떨어져 설계 내구 수명을 제대로 만족시키지 못하고 있다. 따라서 본 연구에서는 SiC 세라믹 촉매 담체의 내구성 평가에 사용할 기계적 물성치를 유한요소해석으로 구하기 위하여 등가물성평가방법을 이용하여 SiC 세라믹 하니컴 담체의 기계적 물성치를 유한요소해석용 시험편으로 구하였다. MOR과 탄성계수는 코제라이트 세라믹 하니컴 담체에 비하여 SiC 세라믹 하니컴 담체가 최소 2배와 9.3배 정도 크게 평가되고 있어 SiC 세라믹 하니컴 담체는 코제라이트 세라믹 하니컴 담체에 비하여 높은 구조 강도를 가지고 있다.