Cracking Threshold Analysis for Nanoindetation Using 3D Finite-Element Method (3차원 유한요소법을 이용한 나노압입에 의한 균열발생 하한계 해석)

  • Koo, Jae-Mean
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.28 no.3
    • /
    • pp.304-310
    • /
    • 2004
  • In this paper, cracking threshold for nanoindentation is analyzed by using 3D finited-element method. The analysis by maximum principal stress criterion can obtain the reliable results for determining to crack initiation location and load. Because the ratio of maximum principal stress to indentation depth for Victors indentation is smaller than flat-plane-column indentation and cracking for Victors indentation occurs from the inner part of specimen difficult to measure crack length, the nanoindentation facture test for flat-plane-column indentation is more effective.

Strength Evaluation of Aluminum Alloy Bolt by Nano-Indentation Hardness Test

  • KUBOTA Yoshihiro;NAKAMURA Tamotsu;KOBAYASHI Mitsuo;FUKUDA Katsumi
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2003.10b
    • /
    • pp.123-126
    • /
    • 2003
  • A high strength aluminum alloy bolt (A7050, T7 temper treatment) has been developed by the authors. The bolt has a small grain size in the whole area of the bolt because of the large equivalent strain followed by thermo-mechanical treatment. As the bolt made of A 7050 has a risk of stress corrosion cracking, each grain should be strengthened the grain inside than the grain boundary in order to improve the stress corrosion cracking resistance. It has been confirmed that the nano-indentation hardness at each grain inside increased with the increasing equivalent strain by thermo-mechanical treatment processing.

  • PDF

Analysis of Cracking Characteristics with Indenter Geometry Using Cohesive Zone Model (Cohesive Zone Model을 이용한 압입자 형상에 따른 균열특성분석)

  • Hyun, Hong Chul;Lee, Jin Haeng;Lee, Hyungyil;Kim, Dae Hyun;Hahn, Jun Hee
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.37 no.12
    • /
    • pp.1453-1463
    • /
    • 2013
  • In this study, we investigated the effect of the indenter geometry on the crack characteristics by indentation cracking test and FEA. We conducted various cohesive finite element simulations based on the findings of Lee et al. (2012), who examined the effect of cohesive model parameters on crack size and formulated conditions for crack initiation and propagation. First, we verified the FE model through comparisons with experimental results that were obtained from Berkovich and Vickers indentations. We observed whether nonsymmetrical cracks formed beneath the surface during Berkovich indentation via FEA. Finally, we examined the relation between the crack size and the number of cracks. Based on this relation and the effect of the indenter angle on the crack size, we can predict from the crack size obtained with an indenter of one shape (such as Berkovich or Vickers) the crack size for an indenter of different shape.

A Study on Mechanical Characteristics of Interface of Ceramic/Metal Composites (세라믹/금속 이종재료 계면의 기계적 특성에 관한 연구)

  • Seo, Do-Won;Kim, Hak-Kun;Song, Jun-Hee;Lim, Jae-Kyoo;Park, Chan-Gyung
    • Proceedings of the KSME Conference
    • /
    • 2000.04a
    • /
    • pp.121-126
    • /
    • 2000
  • Metal/Ceramic structures have many attractive properties, with great potential for applications that demand high stiffness, as well as chemical and biological stability, thermal and electrical insulation. They are currently in use for mechanical and thermal protection in cutting tool and engine parts. With all their great advantage, ceramics suffer from one major problem they are brittle, and are especially susceptible to cracking from surface contacts. Delamination at the interfaces with adjacent layers is a particularly disturbing problem, and can cause premature failure of a composite system. so determination of adhesive properties of coating is one of the most important problems for the extension of the use of coated materials. In this work, mechanical characteristics of Interface of ceramic/Metal composites are evaluated by means of hardness test, indentation test apparent interfacial toughness and bonding strength test. The interface indentation test provides a relation between the applied load(P) and the length of the crack(a) created at the interface between the coating and the substrate.

  • PDF

The comparison between experimental and FEA results for crack initiation due to corrosion of reinforcement (콘크리트 구조물의 철근부식으로 인한 균열발생에 관한 실험적, 해석적 결과의 비교)

  • 장상엽;김용철;조용범
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2003.05a
    • /
    • pp.693-698
    • /
    • 2003
  • Corrosion of reinforcement and deterioration of concrete short the lifetime of reinforced concrete structure and affect the safety of the structure. In particular, the corrosion of reinforcement causing the inner pressure of the interface between the concrete and reinforcement is known to significantly contribute to the premature deterioration of concrete structure. Several attempts have been made to predict the cracking time of the concrete structure. However, problems such as the lack of reproducibility of concrete tests and non-uniformity of materials have hampered thess kinds of studies. Thus, the mechanism of the concrete cracking due to reinforcement corrosion is in the way. This studymeasured the mechanical properties of corrosion products using the nano-indentation test method. Likewise, the critical thickness of corrosion products for the cracking of concrete cover was investigated using the finite element and experimental methods.

  • PDF

Evaluation of Indentation Fracture Toughens in Brittle Materials Based on FEA Solutions (유한요소해에 기초한 취성재료의 압입파괴인성평가)

  • Hyun, Hong Chul;Lee, Jin Heang;Felix, Rickhey;Lee, Hyungyil
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.37 no.12
    • /
    • pp.1503-1512
    • /
    • 2013
  • In this study, we proposed an indentation evaluation method for fracture toughness using cohesive finite element simulations. First, we examined the effect of material properties (yield strain, Poisson's ratio, and elastic modulus) on crack size during Vickers indentation and then generated a regression formula that explains the relations among fracture toughness, indentation load, and crack size. We also proposed another indentation formula for fracture toughness evaluation using the contact size a and E/H (H: hardness). Finally, we examined the relation between the crack size and the indenter shapes. Based on this, we can generate from the formula obtained using the Vickers indenter a formula for an indenter of different shapes. Using the proposed method, fracture toughness is directly estimated from indentation data.

The Evaluation of Mechanical Property of X20CrMoV12.1 Boiler Tube Steels (X20CrMoV12.1강의 열화에 따른 기계적특성 평가)

  • Kim, B.S.;Lee, S.H.;Kim, D.S.;Jung, N.G.
    • Journal of Power System Engineering
    • /
    • v.8 no.3
    • /
    • pp.18-22
    • /
    • 2004
  • Boiler is one of the most important utilities providing steam to turbine in order to supply mechanical energy in thermal power plant. It is composed of thousands of tubes for high efficient heat transfer. The material for boiler tubes is used in such high temperature and pressure condition as $540^{\circ}C$, 22MPa. The boiler tube material is required to resist creep damage, fatigue cracking, and corrosion damages. 2.25%Cr-1Mo steel is used for conventional boiler tubes, and austenitenite stainless steel is used for higher temperature boiler tubes. But the temperature and pressure of steam in power plant became higher for high plant efficiency. So, the property of boiler tube material must be upgaded to fit the plant property. Several boiler tube material was developed to fit such conditions. X20CrMoV12.1 steel is also developed in 1980's and used for superheater and reheater tubes in supercritical boilers. The material has martensite microstructures which is difficult to evaluate the degradation. In this thesis, degrade the X20CrMoV12.1 steel at high temperatures in electric furnace, and evaluate hardness with Vickers hardness tester and strengths with Indentation tester.

  • PDF

Effect of Microstructure on the Environmentally Induced Cracking Behavior of Al-Zn-Mg-Cu-Zr Aluminum Alloy

  • Ghosh, Rahul;Venugopal, A.;Pradeep, PI;krishna, L. Rama;Narayanan, P. Ramesh;Pant, Bhanu;Cherian, Roy M
    • Corrosion Science and Technology
    • /
    • v.17 no.3
    • /
    • pp.101-108
    • /
    • 2018
  • AA7010 is an Al-Zn-Mg-Cu alloy containing Zr, developed as an alternate to traditional AA7075 alloy owing to their high strength combined with better fracture toughness. It is necessary to improve the corrosion resistance and surface properties of the alloy by incorporating plasma electrolytic oxidation (PEO) method. AA7010-T7452 aluminum alloy has been processed through the forging route with multi-stage working operations, and was coated with $10{\mu}m$ thick $Al_2O_3$ ceramic aluminina coating using the plasma electrolytic oxidation (PEO) method. The corrosion, stress corrosion cracking (SCC) and nano-mechanical behaviours were examined by means of potentiodynamic polarization, slow strain rate test (SSRT) and nano-indentation tests. The results indicated that the additional thermomechanical treatment during the forging process caused a fully recrystallized microstructure, which lead to the poor environmental cracking resistance of the alloy in 3.5% NaCl solution, despite the overaging treatment. Although the fabricated PEO coating improved general corrosion resistance, the brittle nature of the coating did not provide any improvement in SCC resistance of the alloy. However, the hardness and elastic modulus of the coating were significantly higher than the base alloy.

A study on Adhesion and Wear Resistance of Vanadium Carbide Coating on Die Steels by Immersing in Molten Borax Bath (용융 붕사욕 침지법에 의해 금형용 강에 형성된 VC coating층의 밀착성과 내마모성에 관한 연구)

  • Lee, B.K.;Nam, T.W.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.13 no.2
    • /
    • pp.71-84
    • /
    • 2000
  • A study on adhesion and wear resistance of VC(vanadium carbide) coating on die steels, STD11 and STD61, has been carried out. The VC coating on the die steels was made by immersing them in molten borax bath, a kind of TRD(thermo-reactive deposition and diffusion). Adhesion strength and wear resistance were investigated using scratch test, indentation test and plate-disc test(Ogoshi type) respectively. The influence of sliding distance on the amount of wear has been determined and dominant wear mechanisms has been characterized using optical microscopy, scanning electron microscopy and EDS spectroscopy. The critical adhesion strength($L_c$) between VC coating layer and substrate(STD11) was increased to 60N($L_c$) in the scratch test. In the case of STD61, the strength increased to 24N. The wear resistance of VC coated die steels was excellent because the diffusion layer formed just below the coating layer. The dominant wear mechanism was identified as adhesive wear for VC coating die steels which were worn by combination of cracking and plucking of VC fragments and disc.

  • PDF

A Study on Material Degradation Evaluation of 9Cr1MoVNb Steel by Micromechanics Test Method (미소역학 시험기법에 의한 9Cr1MoVNb강의 열화도 평가)

  • Baek, Seung-Se;Na, Sung-Hoon;Yoo, Hyun-Chul;Lee, Song-In;Ahn, Haeng-Gun;Yu, Hyo-Sun
    • Proceedings of the KSME Conference
    • /
    • 2000.11a
    • /
    • pp.105-110
    • /
    • 2000
  • The Micromechanics test is new test method which uses comparatively smaller specimen than that required in conventional material tests. There are several methods, such as small-specimen creep test, the continuous indentation test, and small punch(SP) test. Among them, the small punch(SP) test method has been applied to many evaluation fields, such as a ductile-brittle transition temperature, stress corrosion cracking, hydrogen embrittlement, and fracture properties of advanced materials like FGM or MMC. In this study, the small punch(SP) test is performed to evaluate the mechanical properties at high/low temperature from $-196^{\circ}C$ to $650^{\circ}C$ and the material degradation for virgin and aged materials of 9Cr1MoVNb steel which has been recently developed. The ${\Delta}P/{\Delta}{\delta}$ parameter defined a slope in plastic membrane stretching region of SP load-displacement curve decreases according to the increase of specimen temperature, and that of aged materials is higher than the virgin material in all test temperatures. And the material degradation degrees of aged materials with $630^{\circ}C$ -500hrs and $630^{\circ}C$ -1000hrs are $36^{\circ}C$ and $38^{\circ}C$ respectively. These behaviors are good consistent with the results of hardness($H_v$) and maximum displacement(${\delta}_{max}$).

  • PDF