The properties and wear behavior of HVOF spray coating layer of Co-alloy powder

  • Cho, Tong-Yul;Yoon, Jae-Hong;Kim, Kil-Su;Youn, Suk-Jo;Back, Nam-Ki;Chun, Hui-Gon
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.16 no.6
    • /
    • pp.273-277
    • /
    • 2006
  • High velocity of oxy-fuel (HVOF) thermal spray coating is progressively replacing the other classical hard coatings such as chrome plating and ceramic coating by the classical methods, since the very toxic $Cr^{6+}$ ion is well known as carcinogen causing lung cancer, and the ceramic coatings are brittle. Co-alloy T800 powder is coated on the Inconel 718 substrates by the HVOF coating procesess developed by this laboratory. For the study of the possibility of replacing of chrome plating, the wear properties of HVOF Co-alloy T800 coatings are investigated using the reciprocating sliding tester with a counter sliding SUS 304 ball both at room and at an elevated temperature of $1000^{\circ}F\;(538^{\circ}C)$. The possibility as durability improvement coating is studied for the application to the high speed spindles vulnerable to frictional heat and wear. Wear mechanisms at the reciprocating sliding wear test are studied far the application to the systems similar to the sliding test such as high speed spindles. Wear debris and frictional coefficients of T800 coatings both at room and at an elevated temperature of $538^{\circ}C$ are drastically reduced compared to those of non-coated surface of Inconel 718 substrates. Wear traces and friction coefficients of both coated and non-coated surfaces are drastically reduced at a high temperature of $538^{\circ}C$ compared with those at room temperature. These show that the coating is highly recommendable far the durability Improvement coating on the surfaces vulnerable to frictional heat and wear.

A Study on the Coated Characteristics of Ceramic Tools (세라믹공구 재료의 피복특성에 관한 연구)

  • Lee, Myeong-Je;Im, Hong-Seop;Yu, Bong-Hwan
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.24 no.4 s.175
    • /
    • pp.900-906
    • /
    • 2000
  • Ceramic, PCD and CBN tools are available for the difficult-to-cut-materials such as hardened carbon tool steel, stainless steel, Inconel 718 and etc. Ceramic tools are likely to be chipped and abruptly broken before the appearance of normal wear in turning. Ceramic tools are suitable for continuous in turning, not for intermittent in milling. In this study, TiN/TiCN multi-layer coated ceramic tools were found to restrain the chipping, breaking and early fracture and to increase the critical cutting speed owing to TiN/TiCN multi-layer coating in Arc Ion Plating of PVD method.

Stress Corrosion Cracking Lifetime Prediction of Spring Screw (스프링 체결나사의 응력부식균열 수명예측)

  • Koh, S.K.;Ryu, C.H.
    • Proceedings of the KSME Conference
    • /
    • 2004.11a
    • /
    • pp.7-12
    • /
    • 2004
  • A lifetime prediction of holddown spring screw in nuclear fuel assembly was performed using fracture mechanics approach. The spring screw was designed such that it was capable of sustaining the loads imposed by the initial tensile preload and operational loads. In order to investigate the cause of failure and to predict the stress corrosion cracking life of the screw, a stress analysis of the top nozzle spring assembly was done using finite element analysis. The elastic-plastic finite element analysis showed that the local stresses at the critical regions of head-shank fillet and thread root significantly exceeded than the yield strength of the screw material, resulting in local plastic deformation. Normalized stress intensity factors for PWSCC life prediction was proposed. Primary water stress corrosion cracking life of the Inconel 600 screw was predicted by using integration of the Scott model and resulted in 1.78 years, which was fairly close to the actual service life of the holddown spring screw.

  • PDF

Characteristics of manual welding process on carbon steel repair welding using buttering bead (버터링 비드를 이용한 탄소강 보수용접에서 수동 용접 프로세스의 특성)

  • Song, Geun-Ho;Kim, In-Su;Lee, Myeong-Yeol
    • Proceedings of the KWS Conference
    • /
    • 2007.11a
    • /
    • pp.42-44
    • /
    • 2007
  • Methods of repair welding are different to production welding for welding position, welding process, welding power source, heating methods. This study investigated proper the welding process used the welding process SMAW and GTAW in the weldment of inconel filler metals. Mechanical test showed that SMAW and GTAW process had higher mechanical properties than those of material specification. Both SMAW and GTAW welding process can appy the repair welding. In comparison, GTAW welding process had more higher mechanical properties in the weldment.

  • PDF

A Study on ODSCC of OPR 1000 Steam Generator Tube (OPR 1000 증기발생기 전열관의 ODSCC 고찰)

  • Suk, Dong Hwa;Oh, Chang Ha;Lee, Jae Woog
    • Transactions of the Korean Society of Pressure Vessels and Piping
    • /
    • v.6 no.2
    • /
    • pp.16-19
    • /
    • 2010
  • In this study, the axial ODSCC occurrence of domestic OPR 1000 steam generator tube was caused by the tube weakness and the sludge accumulation in the secondary side of steam generator. Inconel 600 HTMA used as tube material is related to most of tube leakage accidents in the world and also these ODSCCs were detected mainly at the 5th TSP(Tube Support Plate) to the 8th TSP of hot leg side. These elevations(5th TSP to 8th TSP) pave the way for the sludge accumulation. As a result of EC(Eddy Current) Bobbin and RPC data analysis, ODSCCs were occurred at contact points of tube and tube support plate. The more accumulated sludge, the higher occurrence frequency of ODSCC.

  • PDF

Welding Residual Stress and Strength of Thick 9% Nickel Steel Plate (9% 니켈강 후판 용접부의 강도 및 잔류응력)

  • Kim, Young-Kyun;Kim, Young-Wann;Kim, Jae-Hoon
    • Journal of Power System Engineering
    • /
    • v.18 no.4
    • /
    • pp.85-90
    • /
    • 2014
  • In this paper, the transient thermal and residual stress analysis of the welding of 9% Ni steel plates using the FEA software ABAQUS are presented. The 9% Ni steel plates are welded manually with welding consumables of 70% Ni based Inconel type super-alloys (YAWATA WELD B (M)), producing a multi-pass/multi-layer butt weld. For these materials, temperature dependant mechanical and thermal material properties are used in the analysis. The back gouging is considered in welding process simulation. The FE thermal results are validated by comparing the real fusion profile and heat affected zone (HAZ). In addition, the continuous indentation test was conducted to measure the strength of base metal, HAZ and weld metal.

The Evaluation of Surface Crack in Paramagnetic Material by FEF Technique (FEF 탐상법을 이용한 상자성체 표면결함 평가)

  • Kim, Hoon
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.24 no.5
    • /
    • pp.532-537
    • /
    • 2004
  • FEF(Focused Electromagnetic Field) technique was newly developed that is based on the induction principle exciting electromagnetic field. The technique consists of an induction wire and a sensor for detecting electromagnetic field, and is applied in a non-contact mode. In this study, the technique was applied to the evaluation of EDM slits in some conductive materials - aluminum alloy, stainless steel and Inconel alloy. The voltage in the non-defect region is depended upon the measurement lift-off. The voltage signals on defects are measured with peak values, and the peak values changed with the depth of defects. The voltage distributions for all conductive materials are the same trend.

Improvement of Oxidation-resisting Characteristic for SOFC Interconnect Material by Use of Thin Film Coating (박막 코팅을 이용한 SOFC 분리판 재료의 내산화성 향상)

  • Lee, Chang-Bo;Bae, Joong-Myeon
    • Transactions of the Korean Society of Mechanical Engineers B
    • /
    • v.30 no.12 s.255
    • /
    • pp.1211-1217
    • /
    • 2006
  • This study is focused on oxidation prevention of STS430, which is generally used as solid oxide fuel cell(SOFC) interconnect at intermediate operating temperatures with oxidation-proof coatings. Inconel, $La_{0.6}Sr_{0.4}CoO_3(LSCo)$ and $La_{0.6}Sr_{0.4}CoO_3(LSCr)$ were chosen as coating materials. Using a radio frequency magnetron sputtering method, each target material was deposited as thin film on STS430 and was analyzed to find out favorable conditions. In this study, LSCr-coated STS430 can reduce electrical resistance to 1/3 level, compared with uncoated STS430. Also, long-term durability test at $700^{\circ}C$ for 1000 hours tells that LSCr thin layer performs an important role to prohibit serious degradations. Superior oxidation-resistant characteristic of LSCr-coated STS430 is attributed to the inhibition of spinel structure formation such as $MnCr_2O_4$.

Mechanical Properties for Welding Part on Ni Base Superalloy Material According to Heat Treatment Parameters (열처리조건에 따른 Ni기지 초합금 용접부의 기계적 특성)

  • Yang, Sung-Ho;Park, Sang-Yeol;Choi, Hee-Sook;Ko, Won;Chae, Na-Hyun;Kim, Moon-Young
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.31 no.4
    • /
    • pp.525-531
    • /
    • 2007
  • The operating temperature has been increased to improve the efficiency of gas turbine. The most advanced Gas turbine is operated at above $1,500^{\circ}C$. Improvement in material and cooling method permit hot gas path component to run at increased temperature. But, the repair of blades which are developed with advanced manufacture technique is difficult to use normal welding. Most of gas turbine blades are made of precipitation harden nickel base superalloy, which is very hard to weld. Therefore, the employment of welding filler on blade is solid solution nickel base superalloy(Hastelloy X, Inconel 617). In this study, Tensile test in high temperature was conducted on welded GTD111DS with GTD111 to evaluate effect of variation of pre, post treatment. The result of this study showed that the specimen was treated with optimum pre and post treatment(preweld HT($1200^{\circ}C$), Post treatment($1100^{\circ}C$ HIP, $1200^{\circ}C$ + $1100^{\circ}C$ + $800^{\circ}C$ HT) is mush superior.

A Study on the Corrosion Characteristics Evaluation for Reactor Material of Waste Water Treatment (폐수처리 반응기용 재질의 부식특성 평가에 대한 연구)

  • Kim, Ki-Tae;Lee, Tae-Gu;Moon, Seung-Jae;Lee, Jae-Heon
    • Plant Journal
    • /
    • v.4 no.2
    • /
    • pp.60-65
    • /
    • 2008
  • As the operating conditions in a supercritical oxidation reactor are set in high temperature with high pressure causing a reactor suffering from the harsh circumstances. It means the reactor adopts itself with Fe-Cr alloy in acidic atmosphere with low pH value and Ni alloy in basic atmosphere with high pH value due to its superior corrosion resistance. The study, whose target waster water is pertinent to the latter part, has selected Ni alloy such as ostenite type stainless steel 304 and 316, superstainless steel AL6XN, Inconel 625, MAT 21, and titanium Gr. 5 in order to measure corrosion resistance against those samples under the same conditions of temperature and pressure applied for a supercritical oxidation reactor. The result shows the identifiable difference in corrosion resistance by observing the surface states through a scanning probe microscope as well as measuring the weight loss through making the samples above deposited in wastewater for two-week and four-week stay. The purpose of this corrosion experiment is to identify the most corrosion-resistant material among sample species pre-selected according to pH concentration of wastewater in pursue of applying for a reactor exposed to the extreme corrosion environment. It is because such a reactor made of a verified material enables to safeguard a stable operation under the supercritical wastewater processing facility.

  • PDF