• Title/Summary/Keyword: In densification

Search Result 817, Processing Time 0.022 seconds

Structural and Dielectric Properties of PLT Thin Plates (PLT 박편의 구조 및 유전특성)

  • Lee, Jae-Man;Park, Ki-Cheol
    • Journal of Sensor Science and Technology
    • /
    • v.7 no.1
    • /
    • pp.51-60
    • /
    • 1998
  • La-modified $PbTiO_{3}$(PLT) thin plates were prepared for the fabrication of PLT pyroelectric IR sensors. The effects of the preparation parameters such as tile sintering temperature, the La content, and the ambient powder quantity, on the microstructural and dielectric properties of PLT thin plates were investigated by X-ray diffraction, scanning electron microscope, and measurements of relative density and dielectric properties. With an increased La content, the tetragonality c/a was decreased but the densification and the grain size were increased, which is considered to be due to the increased Pb vacancy concentration to maintain charge neutrality at the increased of La content. When the quantity of the ambient powder wvas increased, the tetragonality was slightly increased, which is believed io be due to the reduced evaporation of PbO. But the e(fect is insignificant compared to that of La content. The dielectric constant at room temperature was increased and the Curie temperature was decreased in accordance with the decreased tetragonality ratio c/a with the increase of La content. The dielectric constant and tan ${\delta}$ of $500{\mu}m$ thick PLT thin plate with 10 wt% excess PbO and 10 mol% La contant sintered at $1250^{\circ}C$ for 2 hours in ambient powder of $0.02\;g/cm^{3}$ were 360 and 0.02, respectively.

  • PDF

The Piezoelectric Properties of (Na0.5K0.5)NbO3-K5.4Cu1.3Ta10O29 Ceramics with Various K5.4Cu1.3Ta10O29 Doping and Sintering Temperatures

  • Yoon, Jung Rag;Lee, Chang-Bae;Lee, Serk Won;Lee, Heun-Young
    • Transactions on Electrical and Electronic Materials
    • /
    • v.13 no.6
    • /
    • pp.283-286
    • /
    • 2012
  • (1-X)$(Na_{0.5}K_{0.5})NbO_3-XK_{5.4}Cu_{1.3}Ta_{10}O_{29}$ (NKN-KCT) lead-free piezoelectric ceramics have been synthesized by the conventional solid state sintering method, and their sinterability and piezoelectric properties were investigated. Typically, this material is sintered between 1,025 and $1,100^{\circ}C$ for 2 hours to achieve the required densification. Crystalline structures and Microstructures were analyzed by X-ray diffraction and scanning electron microscope. The density, dielectric constant (${\varepsilon}_r$), piezoelectric constant $d_{33}$, electromechanical coupling factor $k_p$ and mechanical quality factor $Q_m$ value of the NKN ceramics depended upon the KCT content and the sintering temperature. In particular, the KCT addition to NKN greatly improved the mechanical quality factor $Q_m$ value. The ceramic with X = 1.0 mol% sintered at $1,050^{\circ}C$ exhibited optimum properties (${\varepsilon}_r$=246, $d_{33}$=95, $k_p$=0.38 and $Q_m$=1,826). These results indicate that the ceramic is a promising candidate material for applications in lead free piezoelectric transformer and filter materials.

Electrical and Optical Properties of Solution-Based Sb-Doped SnO2 Transparent Conductive Oxides Using Low-Temperature Process (저온 공정을 이용한 용액 기반 Sb-doped SnO2 투명 전도막의 전기적 및 광학적 특성)

  • Koo, Bon-Ryul;Ahn, Hyo-Jin
    • Korean Journal of Materials Research
    • /
    • v.24 no.3
    • /
    • pp.145-151
    • /
    • 2014
  • Solution-based Sb-doped $SnO_2$ (ATO) transparent conductive oxides using a low-temperature process were fabricated by an electrospray technique followed by spin coating. We demonstrated their structural, chemical, morphological, electrical, and optical properties by means of X-ray diffraction, X-ray photoelectron spectroscopy, field-emission scanning electron microscopy, atomic force microscopy, Hall effect measurement system, and UV-Vis spectrophotometry. In order to investigate optimum electrical and optical properties at low-temperature annealing, we systemically coated two layer, four layer, and six layers of ATO sol-solution using spin-coating on the electrosprayed ATO thin films. The resistivity and optical transmittance of the ATO thin films decreased as the thickness of ATO sol-layer increased. Then, the ATO thin films with two sol-layers exhibited superb figure of merit compared to the other samples. The performance improvement in a low temperature process ($300^{\circ}C$) can be explained by the effect of enhanced carrier concentration due to the improved densification of the ATO thin films causing the optimum sol-layer coating. Therefore, the solution-based ATO thin films prepared at $300^{\circ}C$C exhibited the superb electrical (${\sim}7.25{\times}10^{-3}{\Omega}{\cdot}cm$) and optical transmittance (~83.1 %) performances.

Update/Revision of Digital Map by Using the Drawing of Work Completion Surveying (준공측량도면을 이용한 수치지도 수정/갱신)

  • Kim, Won-Dae;Lee, Kang-Won;Park, Hong-Gi
    • Journal of Korean Society for Geospatial Information Science
    • /
    • v.8 no.1 s.15
    • /
    • pp.85-95
    • /
    • 2000
  • There is a recent emphasis on the need for updating and revision of existing digital maps as more digital maps are used and produced. Various type of data sources, such as photographs, ground surveyed data and satellite images, are used in the revision and the updating process. The process is very time consuming and costly, especially for small regional areas. This study, attempts to present an effective update/revision method using the as-built surveying drawings and the accuracy of the digital map which has been updated and revised using this method was also investigated. This study showed that by using as-built surveying drawings of scale 1/1,200 to update a digital map of scale 1/1,000, the resulting accuracy satisfied the requirements of the national digital map accuracy specification for the corresponding scale. The necessity of the existence of the necessary drawings and maps is a requirement of this process and it is also suggested that densification of local control points especially in the urban areas is necessary for producing accurate as-built surveying drawings. This would require the establishment of rules and regulations which would require constructions to perform as-built surveying, immediately after the construction has been completed.

  • PDF

Time Evolution of Water Permeability Coefficient of Carbonated Concrete (탄산화된 콘크리트의 투수계수에 대한 시간단계별 해석)

  • Yoon, In-Seok;Lee, Jeong-Yun;Cho, Byung-Young;Kim, Young-Geun
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2008.04a
    • /
    • pp.1053-1056
    • /
    • 2008
  • Permeability coefficient of concrete is a substantial key parameter for understanding the durability performance of concrete and its micro-structural densification. Many researches to deal with the issue have been accomplished, however, it is very rare to deal with the theoretical study on permeability coefficient in connection with carbonation of concrete and the effect of volumetric fraction of cement paste or aggregate on the permeability coefficient. The majority of these researches have not dealt with this issue combined with carbonation of concrete, although carbonation can significantly impact on the permeability coefficient of concrete. The purpose of this study is to establish a fundamental approach to compute the permeability coefficient of (non)carbonated concrete. When simulating micro-structural characteristics as a starting point for deriving a model for the permeability coefficient by the numerical simulation program for cementitious materials, HYMOSTRUC, a more realistic formulation can be achieved. For several compositions of cement pastes, the permeability coefficient is calculated with the analytical formulation, followed by a microstructure-based model. Emphasis is on the micro-structural changes and its effective change of the permeability coefficient of carbonated concrete. The results of micro-structural water permeability coefficient model will be compared with results achieved from permeability experiments.

  • PDF

Fabrication, Microstructure and Compression Properties of AZ31 Mg Foams

  • Zhao, Rui;Li, Yuxuan;Jeong, Seung-Reuag;Yue, Xuezheng;Hur, Bo-Young
    • Korean Journal of Materials Research
    • /
    • v.21 no.6
    • /
    • pp.314-319
    • /
    • 2011
  • Melt foaming method is one of cost-effective methods to make metal foam and it has been successfully applied to fabricate Mg foams. In this research, AZ31 Mg alloy ingot was used as a metal matrix, using AlCa granular as thickening agent and $CaCO_3$ powder as foaming agent, AZ31 Mg alloy foams were fabricated by melt-foaming method at different foaming temperatures. The porosity was above 41.2%~73.3%, pore size was between 0.38~1.52 mm, and homogenous pore structures were obtained. Microstructure and mechanical properties of the AZ31 Mg alloy foams were investigated by optical microscopy, SEM and UTM. The results showed that pore structure and pore distribution were much better than those fabricated at lower temperatures. The compression behavior of the AZ31 Mg alloy foam behaved as typical porous materials. As the foaming temperature increased from $660^{\circ}C$ to $750^{\circ}C$, the compressed strength also increased. The AZ31 Mg alloy foam with a foaming temperature of $720^{\circ}C$ had the best energy absorption. The energy absorption value of Mg foam was 15.52 $MJ/m^3$ at a densification strain of 52%. Furthermore, the high energy absorption efficiencies of the AZ31 Mg alloy foam kept at about 0.85 in the plastic plateau region, which indicates that composite foam possess a high energy absorption characteristic, and the Vickers hardness of AZ31 Mg alloy foam decreased as the foaming temperature increased.

The Effects of $SrTiO_3$ Addition on the Microstructure and Magnetic Properties of YIG (YIG ($Y_3$$Fe_5$O_{12}$)의 미세구조 및 자성 특성에 대한 $SrTiO_3$첨가 영향)

  • Jang, Hak-Jin;Yun, Seok-Young;Kim, Tae-Ok
    • Korean Journal of Materials Research
    • /
    • v.11 no.3
    • /
    • pp.203-206
    • /
    • 2001
  • The effects of SrTiO$_3$ addition and sintering temperature on the microstructure and magnetic properties of yttrium iron garnet (YIG) were investigated. The lattice Parameter increasing of sintered YlG with small amount of SrTiO$_3$ addition was supposed to be substituted $Y^{+3}$, Fe$^{+3}$ ions to Sr$^{+2}$,Ti$^{+4}$ ions which are relatively large in ionic ranius. A YIG specimen sintered at 142$0^{\circ}C$ with 0.2mol% SrTiO$_3$ showed above 98% densification of theoretical density. Saturation magnetization (M$_s$) at room temperature decreased a little bit with increasing SrTiO$_3$, addition but no great chance. In addition, the coercivity (H$_c$) was almost not changed by sintering temperature.

  • PDF

The Effect of Powder Oxidation on the Thermoelectric Properties of β-FeSi2 (β-FeSi2의 열전변환특성에 미치는 분말산화의 영향)

  • ;Kunihito Koumoto
    • Journal of the Korean Ceramic Society
    • /
    • v.40 no.11
    • /
    • pp.1106-1112
    • /
    • 2003
  • For the purpose of making clear the role of oxygen in the thermoelectric properties of FeSi$_2$, thermoelectric measurements and spectroscopic characterization were conducted for the oxidized specimens fabricated from ($\alpha$+$\varepsilon$)-phases and/or $\beta$-phase. Addition of oxygen to FeSi$_2$ prevented both densification during sintering and transformation from metallic phases to semiconducting phase during annealing treatment. In an specimens, electrical conductivity and thermal conductivity decreased with oxidation time. The Seebeck coefficient was positive and small for pure FeSi$_2$. And/or the oxidized specimens fabricated from ($\alpha$+$\varepsilon$)-phases. However, it was negative and showed a maximum peak at about 500 K for the oxidized FeSi$_2$ fabricated from $\beta$-phase. The value of maximum peak increased with oxidation time.

Fabrication of Nanostructured Ti from Ti and TiH2 by Rapid Sintering and Its Mechanical Properties (급속소결에 의한 Ti와 TiH2로부터 나노구조의 Ti 제조 및 기계적 특성)

  • Kim, Na-Ri;Cho, Sung-Wook;Kim, Won-Baek;Shon, In-Jin
    • Korean Journal of Metals and Materials
    • /
    • v.50 no.1
    • /
    • pp.34-38
    • /
    • 2012
  • Titanium has good deformability, high hardness, high biocompatibility, excellent corrosion resistance and low density. Due to these attractive properties, it has been used in many industrial applications. Dense nanostructured Ti was sintered from mechanically activated Ti and $TiH_2$ powders by high frequency induction heating under pressure of 80 MPa. The advantage of this process is that it allows very quick densification to near theoretical density and inhibition of grain growth. $TiH_2$ powder was decomposed to Ti during sintering. The hardness of Ti increased and the average grain size of Ti decreased with increasing milling time. The average grain sizes of Ti samples sintered from Ti and $TiH_2$ powder milled for 5 hrs were about 26 nm, 44 nm, respectively. The hardness of Ti sintered from Ti and $TiH_2$ powder milled for 5 h was $504kg/mm^2$ and $567kg/mm^2$, respectively.

Mechanical Properties and Fabrication of Nanostructured Al2TiO5 Compound by Pulsed Current Activated Sintering (펄스전류 활성 소결에 의한 나노구조 Al2TiO5 화합물 제조 및 기계적 특성)

  • Kang, Hyun-Su;Park, Hyun-Kuk;Doh, Jung-Mann;Yoon, Jin-Kook;Park, Bang-Ju;Shon, In-Jin
    • Korean Journal of Metals and Materials
    • /
    • v.50 no.11
    • /
    • pp.817-822
    • /
    • 2012
  • Nano powders of $Al_2O_3$ and $TiO_2$ compounds made by high energy ball milling were pulsed current activated sintered for studying their sintering behaviors and mechanical properties. The advantage of this process is that it allows very quick densification to near theoretical density and inhibition of grain growth. Nano-structured $Al_2TiO_5$ with small amount of $Al_2O_3$ and$TiO_2$ was formed by sintering at $1300^{\circ}C$ for 5 minute, in which average grain size was about 96 nm. Hardness and fracture toughness of the nano-structured $Al_2TiO_5$ compound with a small amount of $Al_2O_3$ and$TiO_2$ were $602kg/mm^2$ and $2.6MPa{\cdot}m^{1/2}$, respectively.