  • Purpose: The purpose of this study was to colorimetrically evaluate the masking effect of different opacity of ingots on the final shade of IPS Empress Esthetic$^{(R)}$ laminate veneer restorations using the CIE $L^*a^*b^*$ system. Materials and methods: Six porcelain disks of IPS Empress Esthetic$^{(R)}$ system (translucency: E 01, E 03, E 0C-1, E TC-1, E TC-2, E TC-3) were fabricated with 7 mm in diameter and 0.6 mm in thickness. Six extracted human incisors (shade: A1, A3, A4, B2, B3, C3) were used as the abutment specimens. The incisors were prepared using a diamond wheel and made with a flat labial surface on the middle 1/3. For each combination of different shades of abutments and copings, the change in color was measured with a colorimeter. CIE $L^*a^*b^*$ coordinates were recorded for each specimen. Color differences (${\Delta}E$) were calculated. Descriptive statistical analysis was done. Results: ${\Delta}E$ values were significantly affected by coping translucency and abutment shade (P<.05). The color differences (${\Delta}E$) of laminate veneers among abutments with A3, B3, C3, and A4 shade were mostly below 2.7 which was within the clinically acceptable range, while color differences between A4 and B2, A3 and B2, and A1 and A4 showed more than 2.7. Conclusion: The final color of IPS Empress Esthetic$^{(R)}$ laminate veneers were significantly influenced by translucency of the coping and shade of abutment teeth. The large value difference of abutment teeth limited the masking ability by laminate veneers.

FRACTURE STRENGTH OF THE IPS EMPRESS CROWN : THE EFFECT OF OCCLUSAL DEPTH AND AXIAL INCLINATION ON LOWER FIRST MOLAR (IPS Empress 도재관의 파절강도: 하악 제1대구치에서 교합면 두께와 축면경사도에 따른 영향)

  • Kim Sung-Hoon;Lee Jin-Han;Kim Yu-Lee;Dong Jin-Keun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.41 no.1
    • /
    • pp.48-60
    • /
    • 2003
  • The purpose of this study was to compare the fracture strength of the IPS Empress ceramic crown according to the occlusal depth (1.5mm, 2.0mm, 2.5mm) and axial inclination ($4^{\circ},\;8^{\circ},\;12^{\circ}$) of the lower First Molar. After 10 metal dies were made for each group, the IPS Empress ceramic crowns were fabricated and cemented with resin cement(Bistite resin cement, Tokuyama Soda Co. LTD., Japan). The cemented crowns were mounted on the testing jig with inclination of 30 degrees and the universal testing machine(Zwick Z020, Zwick, Germany)was used to measure the fracture strength. The results of this study were as follows : 1. The fracture strength of the ceramic crown with 2.5mm depth and $12^{\circ}$ inclination was the highest (1789 N). Crowns of 1.5mm depth and $4^{\circ}$ inclination had the lowest strength (1091 N). 2. There were no significant differences in the fracture strength by axial inclination of the same occlusal depth group. 3. Most fracture lines began at the loading area and extended through proximal surface perpendicular to the margin, irrespective of occlusal depth. Size of fragment was affected by the amount of occlusal reduction.

FRACTURE STRENGTH OF THE IPS EMPRESS CROWN : THE EFFECTS OF INCISAL REDUCTION AND AXIAL INCLINATION ON UPPER CANINE (IPS Empress 도재관의 파절강도 : 상악 견치에서 절단연 삭제량과 축면 경사도에 따른 영향)

  • Shin Dong-Kuk;Kang Han-Joong;Park Yong-Suck;Park Kwang-Soo;Dong Jin-Keun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.43 no.1
    • /
    • pp.30-40
    • /
    • 2005
  • Purpose. The purpose of this study was to compare the fracture strength of the IPS Empress ceramic crown according to the incisal reduction (2.0mm, 2.5mm, 3.0mm) and axial inclination ($4^{\circ}$, $8^{\circ}$, $12^{\circ}$) of the upper canine. Material and methods. After 10 metal dies were made for each group, the IPS Empress ceramic crowns were fabricated and each crown was cemented on each metal die with resin cement. The cemented crowns mounted on the testing jig were inclined 30 degrees and the universal testing machine was used to measure the fracture strength. Results. 1. The fracture strength of the ceramic crown with 3.0mm depth and $12^{\circ}$ inclination was the highest (839N) Crowns of 2.0mm depth and $12^{\circ}$ inclination had the lowest strength (559N). 2. There was no significant difference in the fracture strength by axial inclination in the same incisal reduction group. 3. The fracture mode of the crowns was similar. Most of fracture lines began at the loading area and extended through proximal surface perpendicular to the margin irrespective of incisal reduction.

INFLUENCE OF THICKNESS OF EMPRESS 2 CERAMIC ON FRACTURE STRENGTH (Empress 2 도재의 두께에 따른 파절강도에 관한 연구)

  • Koh, Jung-Woo;Yang, Jae-Ho;Lee, Sun-Hyung
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.38 no.4
    • /
    • pp.446-460
    • /
    • 2000
  • All-ceramic restorations have had a more limited life expectancy than metal ceramic crowns be-cause of their lower strength. The relatively lower strength has limited the use of all-ceramic crowns to the areas where occlusal loads are lower Therefore many researches have been done to increase the strength of all-ceramic crowns. IPS Empress 2 is a new type of lithium disilicate glass-ceramic with enhanced physical characteristics which has been in use clinically since 1998. Previous researches reported that the flexural strength of all-ceramic material was greater than 300 MPa, and all-ceramic crowns can be used in staining or layering technique. The objective of this study was to investigate the influence of the thickness of IPS Empress 2 ceramic on fracture strength. Both staining technique and layering technique was investigated. Vita VMK was used as control. For all three groups, five specimens each of 0.8mm, 1.0mm, 1.4mm, 1.8mm, and 2.2mm thick-ness (a total of 75 specimens) were prepared. Control group : Vita VMK Porcelain specimens were prepared with dentine ceramic and liquid glazing was done. Group I : IPS Empress 2 were prepared with staining technique and stained twice and glazed once. Group II : IPS Empress 2 were prepared with layering technique and glazed after wash firing. The thickness and diameter of the specimen were measured and controlled after specimen preparation. Biaxial Flexure Test (ASTM Standard F394-78) was adopted as this test method produces results least affected by the edge condition of the specimens. Fracture strength was measured with Instron Universal Testing Machine. Conclusions are as follow : 1. The fracture strength was increase in order of control group, test group I, test group II. 2. Fracture strength of the group I (Empress 2 Staining) was 65.54 N in 0.8mm, 155.2 N in 1.0mm, 233.5 N in 1.4mm, 434.5 N in 1.8mm, and 600.1 N in 2.2mm. 3. Fracture strength of the group II (Empress 2 Layering) was 190.0 N in 0.8mm, 283.5 N in 1.0mm. 437.2 N in 1.4mm, 732.0 N in 1.8mm, and 1115.0 N in 2.2mm. 4. No statistical difference was found in flexural strengths according to thickness in a specified group(p>0.05).

  • PDF

A STUDY ON THE MICROSTRUCTURE OF IPS EMPRESS CERAMICS ACCORDING TO THE HEAT TREATMENT AND SPRUE TYPE (주입선 및 열처리에 따른 IPS Empress 도재의 미세구조에 관한 연구)

  • Dong, Jin-Keun;Oh, Sang-Chun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.36 no.5
    • /
    • pp.772-785
    • /
    • 1998
  • This study was undertaken to clarify the microstructure of the different IPS Empress ingots by etching and to observe the change of leucite crystal structure according to subsequent heat treatment and the crystal distribution according to sprue types(${\phi}2.8mm$, single sprue; ${\phi}1.8mm$, double sprue) by scanning electron microscopy. IPS Empress T1, O1 ingots used for staining technique, and Dentin(A2) ingots used for layering technique were selected for this study. To observe the microstructures of these ingots before pressing, the specimens were prepared in splinters($3{\times}3{\times}3mm$) taken from the original ingots. And to estimate crystal distribution and microstructural change by sprue type and subsequent heat treatment. the specimens($3{\times}3{\times}3mm$) were heat-pressed through the two types of sprues with different diameters and numbers, and all specimens were fired according to the recommended firing schedule. The observed surface was ground with waterproof papers($#800{\sim}#1800$) on the grind polisher and was cleaned ultrasonically. All specimen were etched with 0.5% hydrofluoric acid. After etching, the surface was treated by ion sputter coating for SEM observation at an accelerating voltage of 20kV. In all specimens, the central area of ground surface was observed because there was less difference in microstructure between the peripheral area and the central area. The results were as follows ; 1. In the microstructure according to the ingot type, there was a wide difference between the staining (T1,O1) and layering(Dentin A2) ingots, but there was not a considerable difference between the T1 ingot and the O1 ingot for staining technique. 2. In all specimens, the crystal dispersion of IPS Empress ceramic using double sprue was significantly more scattered than that of IPS Empress ceramic using single sprue. The degree of scattering was strongest in the Dentin(A2) specimen and weakest in the O1 ingot. 3. In the microstructural change according to the subsequent heat treatment, all of ingots had some microcracks in the inside of the leucite crystal and the glass matrix after pressing. The inner splinters of the leucite crystal became smaller, and more microcracks occurred in the glass matrix due to increasing heat treatment times. 4. The size of leucite crystals varied from $1{\mu}m\;to\;5{\mu}m$. The mean size of mature crystals was about $5{\mu}m$. The form of the crystal was similar to a circle when it was smaller and similar to an ellipse when it was larger.

  • PDF

Fracture strength of the IPS Empress crown :The effect of incisal reduction and axial inclination on upper central incisor (IPS Empress 도재관의 파절강도 : 상악 중절치에서 절단연 삭제량과 축면 경사도에 따른 영향)

  • Song, Byung-Kwen;Lee, Hae-Hyoung;Dong, Jin-Keun
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.16 no.3
    • /
    • pp.237-245
    • /
    • 2000
  • The purpose of this study was to compare the fracture strength of the IPS Empress ceramic crown according to the incisal depth(2.0mm, 2.5mm, 3.0mm) and axial inclination($4^{\circ}$, $8^{\circ}$, $12^{\circ}$) of the upper central incisor. After 10 metal dies were made for each group, the IPS Empress ceramic crowns were fabricated and each crown was cemented on each metal die with resin cement. The cemented crowns mounted on the testing jig were inclined 30 degrees and a universal testing machine was used to measure the fracture strength. The results were : 1. The fracture strength of the ceramic crown with 2.5mm depth and $8^{\circ}$ inclination was the highest(965N). Crowns of 2.0mm depth and $4^{\circ}$ inclination had the lowest strength(713N). There were no significant differences of the fracture strength by axial inclination in same incisal depth group. 2. The fracture mode of the crowns was similar. Most of fracture lines began at the loading area and extended through proximal surface perpendicular to the margin irrespective of incisal depth. There had correlation between fracture strength and fractured surface area.

  • PDF

Fracture Strength of IPS Empress Crown : The Effect of Incisal Reduction and Axial Inclination on Lower Canine (IPS Empress 도재관의 파절강도 : 하악 견치에서 절단연 삭제량과 축면 경사도에 따른 영향)

  • Jung, Young-Chan;Shin, Dong-Kuk;Park, Eun-Ju;Kim, Min-Jeong;Dong, Jin-Keun
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.20 no.1
    • /
    • pp.19-29
    • /
    • 2004
  • The purpose of this study was to compare the fracture strength of the IPS Empress ceramic crown according to the incisal reduction(2.0mm, 2.5mm, 3.0mm) and axial inclination ($4^{\circ}$, $8^{\circ}$, $12^{\circ}$) of the lower canine. After 10 metal dies were made for each group, the IPS Empress ceramic crowns were fabricated and each crown was cemented on each metal die with resin cement. The cemented crowns mounted on the testing jig were inclined 30 degrees and a universal testing machine was used to measure the fracture strength. The results of this study were as follows : 1. The fracture strength of the ceramic crown with 3.0mm depth and $12^{\circ}$ inclination was the highest(1377N). Crowns of 2.0mm depth and $4^{\circ}$ inclination had the lowest strength (731 N). 2. There were no significant differences of the fracture strength by axial inclination in same incisal reduction group. 3. The fracture mode of the crowns was similar. Most of fracture lines began at the loading area and extended through proximal surface perpendicular to the margin irrespective of incisal reduction.

Esthetic reconstruction of upper central incisor using immediate Frialit-2 implant placement, immediate temporary crown fabrication and IPS Empress 2 crown (즉시 Frialit-2 implant 식립, 즉시 임시치관 제작 그리고 IPS Empress 2 crown을 이용한 상악중절치의 심미적 수복)

  • Kim, Yu-Lee;Oh, Sang-Chun
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.19 no.1
    • /
    • pp.43-48
    • /
    • 2003
  • During the past several years, significant advances have occurred in the utilization of osseointegrated implants for the treatment of partially edentulous patients. One of the biggest purposes for treating of these patients is the high demand for improved esthetics, especially in the anterior region. For this esthetics, the new trend in dental implants is the immediate placement and immediate superstructure fabrication. The refined surgical technique, the skillful soft tissue management, and the proper prosthetic coordination are the main factors to achieve natural looking of implant supported prosthesis. The customized provisional restoration and the customized impression coping are recommended for the optimal peri-implant soft tissue contour. The basic concept of Frialit 2 system was the immediate replacement of a tooth with root-analog fixture after extraction. This system guarantees an ideal result in function and esthetics. The ceramic abutment system offers improved quality in the respect of esthetics, fitness, translucency, and biocompatibility. In this clinical report, the final restoration made with IPS Empress 2 crown on the CeraBase abutmen of Frialit 2 system allowed the reproduction of the natural vitality of tooth and adjacent gingiva.

A COMPARATIVE STUDY ON THE FLEXURE STRENGTH OF THE CERAMICS FOR ALL-CERAMIC CROWNS (All-ceramic Crown 용 도재의 굽힘강도에 관한 비교연구)

  • Yu Hyoung-Woo;Song Chang-Yong;Bae Tae-Seong;Song Kwang-Yeob;Park Chan-Woon
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.32 no.2
    • /
    • pp.195-211
    • /
    • 1994
  • The purpose of this study was to evaluate the fracture resistance of the four kinds of dental porcelains for the all-ceramic crown(Vita In-Ceram, Vita Hi-Ceram, IPS-Empress, Vitadur-N) and one kind for the metal-ceramic non(Vita VMK 68) was used as the control group. In order to determine the fracture resistance, the hi-axial flexure strength was measured at a crosshead speed of 0.5mm/min, and the Vickers hadrness was measured at an indentation load of 1kg for 20 seconds. The results obtained were summarized as follows ; 1. The maximum Weibull modulus of 24.61 for Vitadur-N and the minimum one of 852 for IPS-Empress were observed ; the maximum characteristic strength of 353.26MPa for Vita In-Ceram and the minimum that of 63.20MPa for Vitadur-N were also observed. 2. The maximum mean bi-axial flexure strength of 339.12MPa for Vita In-Ceram and thd minimum one of 61.99MPa for Vitadur-N were calculated. Results of the Scheffe test indicated that the statistically significant difference(P<0.05) existed between Vita In-Ceram or Vita Hi-Ceram and the others ; also between IPS-Empress and Vitadur-N. 3. The maximum mean hardness of $980.55kg/mm^2$ for Vita VMK 68 appeared. Results of the Scheffe test indicated that statistically significant difference(P<0.05) existed between Vita In-Ceram or Vita Hi-Ceram and the others ; also between IPS-Empress and Vita VMK 68.

  • PDF

A STUDY ON THE MARGINAL FIT OF ALL-CERAMIC CROWNS USING CCD CAMERA (CCD카메라를 이용한 수종 전부도재관의 변연적합도에 관한 연구)

  • Moon, Byoung-Hwa;Yang, Jae-Ho;Lee, Sun-Hyung;Chung, Hun-Young
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.36 no.2
    • /
    • pp.273-292
    • /
    • 1998
  • The purpose of this study was to evaluate marginal fit of four all-ceramic crown systems 1) conventional In-Ceram, 2) copy-milled In-Ceram using Celay system, 3) IPS Empress, 4) OPC(Optimal Pressable Ceramic). All ceramic crowns were made on epoxy dies. The fabricated crowns were sandblasted, cleaned with ultrasonic cleansing, silanated, and cemented with Bistite composite resin cement. the selected marginal areas of the crowns were the labial, lingual, mesial, and distal surface. Each selected area of surface was $0.6{\times}1.6mm$ in dimension. The image of each marginal area was captured to computer files using DT-55 Frame Grabber and light microscope connected CCD camera. The marginal gaps were measured every $70{\mu}m$ using computer image analysis program. The results obtained were summarized as follows : 1. The marginal fit of four all-ceramic crowns were significantly different from each other(p<0.01), and mean marginal fit values obtained were $31.42{\pm}16.52{\mu}m$ in conventional In-Ceram, $55.45{\pm}27.90{\mu}m$ in copy-milled In-Ceram using Celay system, $44.36{\pm}24.59{\mu}m$ in IPS Empress, $47.21{\pm}20.42{\mu}m$ in OPC. 2. In the marginal fit of conventional In-Ceraw and copy-milled In-Ceram crowns using Celay system there was no significant difference between mesiodistal and buccolingual surface, but in the marginal fit of IPS Empress and OPC crowns, there was significant difference between mesiodistal and buccolingual surface(p<0.01). 3. The marginal fit of four kinds of all-ceramic crowns was clinically acceptable.