• 제목/요약/키워드: IPS Empress ceramic

검색결과 76건 처리시간 0.023초

MARGINAL FIDELITY AND FRACTURE STRENGTH OF IPS EMPRESS $2^{(R)}$ CERAMIC CROWNS ACCORDING TO DIFFERENT CEMENT TYPES

  • Cho Hyun-Ok;Kang Dong-Wan
    • 대한치과보철학회지
    • /
    • 제40권6호
    • /
    • pp.545-559
    • /
    • 2002
  • There has been increasing use of IPS Empress $2^{(R)}$ owing to easy fabrication method, high esthetics similar to natural teeth, good marginal accuracy, and sufficient fracture strength. However, in clinical application, although a luting agent and the tooth cementation bonding procedure influence the marginal accuracy and fracture strength restoration, there has been a controversy in the selection of proper luting agent. This study was to measure the marginal fidelites and fracture strength of IPS Empress crowns according to three cement types, Protec $cem^{(R)}$, Variolink $II^{(R)}$ and Panavia $21^{(R)}$. After construction of 12 experimental dies for each group, IPS Empress $2^{(R)}$ crowns were fabricated and luted the metal master die prepartion of the maxillary right premolar. Marginal gaps before cementation and after cementation were measured. Buccal incline on the functional cusp of specimens were loaded until the catastrophic failure and fracture strength was measured. The results of this study were as follows: 1. The range of gap was $34.04{\pm}4.84{\mu}m$ before cementation and $37.88{\pm}5.00{\mu}m$ after cementation, which showed significant difference by paired t-test (p<0.05). The difference in the results from marginal accuracy according to measuring point proved to be not statistically significant by two-way ANOVA test (p>0.05). 2. The difference in the results from marginal accuracy according to three cement types Proved that The Variolink $II^{(R)}$ cement group had the least gap, $35.43{\pm}5.03{\mu}m$, and showed superior marginal accuracy while there existed statistic significance in Protec $cem^{(R)}$ cement group, $39.06{\pm}4.41{\mu}m$ or Panavia $21^{(R)}$ cement group, $39.16{\pm}4.39{\mu}m$ by two-way ANOVA test & multiple range test (p<0.05). 3. The difference in the results from fractures strength testing according to three cement type groups proved to be statistically significant (p<0.05). The Variolink $II^{(R)}$ cement group shows highest fracture strength of $1257.33{\pm}226.77N$, Panavia $21^{(R)}$ cement group has $1098.08{\pm}138.45N$, and Protec $cem^{(R)}$ cement group represents the lowest fracture strength of $926.75{\pm}115.75N$. 4. Three different cement groups of different components showed acceptable marginal fidelity and fracture strength. It is concluded that IPS Empress $2^{(R)}$ crowns luted using Variolink $II^{(R)}$ cement group had stronger fracture strength and smaller marginal gap than the other cement groups. Although Variolink $II^{(R)}$ resin cement seemed acceptable to clinical applications in IPS Empress $2^{(R)}$ system, the IPS Empress $2^{(R)}$ system still requires long-term research due to the lack of data in clinical applications.

수종의 post와 IPS-Empress Ingot 두께가 전부 도재 수복물 최종색조에 미치는 영향 (INFLUENCE OF SEVERAL POSTS AND IPS-EMPRESS INGOT THICKNESS ON THE FINAL SHADE OF ALL-CERAMIC CROWNS)

  • 복원미;최근배;박찬운;안승근
    • 대한치과보철학회지
    • /
    • 제42권5호
    • /
    • pp.514-523
    • /
    • 2004
  • Statement of problem: All-ceramic restorations have been advocated for superior esthetics. Various post and core systems have been used to improve the strength of damaged teeth, but it is unclear whether they affect the final shade of finished all-ceramic restorations. Purpose: The influence of different types of post and core systems on light transmission through all-ceramic crowns was assessed by spectrophotometric analysis. Also the masking effect of different thickness of ceramic ingot was evaluated. Material and Methods : Forty-five sample disks (15mm in diameter) at several thickness(1.0, 1.5, 2.0mm) and value(shade 100, 200, 300) were made in heat pressed ceramic(IPS-Empress). Background specimens simulating gold-alloy cast posts(Type III casting gold alloy), metal posts(Ni-Cr casting alloy) and ceramic posts(CosmoPost) were fabrica-ted. Resin composite(Z250, A3 shade) was used as a tooth substrate reference. For each combination, the change in color was measured with a spectrophotometer. Readings were performed for 2 conditions (1) ability of ceramic to mask the core in relation to its thickness(1.0, 1.5, or 2.0mm) ; (2) influence of post and core types on the final color of the ceramic. Data were recorded according to the CIE $L^*a^*b^*$ systems and color difference($\Delta$E) was calculated. Results: 100 shade ingot: when ceramic thickness was 1.0mm, $\Delta$E value for ceramic post larger than 1 but $\Delta$E value for metal and gold post was larger than 2. For ceramic thickness of 1.5mm, only $\Delta$E value for metal was larger than 2, and the other samples' $\Delta$E value was smaller than 2. For ceramic thickness of 2.0mm, $\Delta$E values for all specimens was smaller than 2. 200 shade ingot: when ceramic thickness was 1.0mm, $\Delta$E value for ceramic post was smaller than 1 but $\Delta$E value for metal and gold post was larger than 2. For ceramic thickness of 1.5 mm, only the $\Delta$E value for metal was larger than 2, and the other samples' $\Delta$E value was smaller than 2. For ceramic thickness of 2.0mm, $\Delta$E values for all specimens was smaller than 1. 300 shade ingot: when ceramic thickness was 1.0mm, only $\Delta$E value for metal was larger than 2 and the other samples' $\Delta$E value was smaller than 2. For ceramic thickness of 1.5mm, $\Delta$E values for all specimens was smaller than 1. For ceramic thickness of 2.0mm, $\Delta$E values for all specimens was smaller than 1. Conclusion: The final esthetic result of the IPS-Empress glass-ceramic restoration was not affected by the presence of different core materials when the thickness was more than 2.0 mm. When ceramic thickness decreases to 1.5mm, it is advised to take the substrate aspects into consideration. If the ceramic thickness is less than 1.0mm, using the tooth color matched substrate is strongly recommended.

금속 다우엘코어에 사용된 수종의 전부도재관의 색조변화에 관한 연구 (A STUDY THE SHADE CHANCE OF SEVERAL KINDS OF ALL CERAMIC CROWNS USED FOR METAL DOWEL CORE)

  • 허성일;임헌송;임주환;조인호
    • 대한치과보철학회지
    • /
    • 제39권5호
    • /
    • pp.477-491
    • /
    • 2001
  • The purpose of this study is to compare and analyze the shade changes(${\Delta}E^*$) about $In-Ceram^{(R)}$, $IPS-Empress^{(R)}$, $OPC^{(R)}$ by using of the spectrophotometer arising from inital status and before and after cementation of the resin cement mounted on the metal core. We used a couple of statistics such as 'One- Way ANOVA' and 'Multiple Range Test.' We could be able to verify significantly what is being discussed here up to 95%. The results drawn from our research are as follows : 1. At the time of our experiments regarding the initial shapes of all-ceramic and mounting status of all-ceramic on the metal crown(${\Delta}E^*1$), and a comparison of mounting of all ceramic on the metal crown with all-ceramic cemented on the metal core(${\Delta}E^*2$), at the time of shade change of initial shapes and after we cemented on the metal core. (1) no significant difference among all-ceramics was found. (2) no particular difference was found regarding the $In-Ceram^{(R)}$. (3) a significant difference between the ${\Delta}E^*1$ and ${\Delta}E^*2$ regarding the $IPS-Empress^{(R)}$ was found(P<0.05). (4) a significant difference between the ${\Delta}E^*1$ and ${\Delta}E^*2$ regarding the $OPC^{(R)}$ was found(P<0.05). 2. When we compared the shade changes(${\Delta}E^*$) resulted from before and after the cementation on each of the parts involved of some all-ceramic, we could be able to find shade change increase form incisal third, middle third. and cervical third in that order in $In-Ceram^{(R)}$(spinell), IPS $Empress^{(R)}$, and $OPC^{(R)}$ all. In addition. we could be able to find a significant difference between cervical third and incisal third, middle third. (P<0.05) From what we have just seen, we might conclude that there is a significant shade change difference before and after the cementation with respect to $IPS-Empress^{(R)}$ and $OPC^{(R)}$. In addition, we could also be able to find more shade change difference at the cervical third rather than incisal third and middle third depending on the parts involved.

  • PDF

IPS Empress 도재관의 파절강도: 하악 중절치에서 절단연 삭제량과 축면 경사도에 따른 영향 (Fracture Resistance and Stress Distribution of All Ceramic Crowns with Two Types of Finish Line on Maxillary Central Incisor)

  • 남영성;김계순;정영찬;김유리;동진근
    • 구강회복응용과학지
    • /
    • 제19권3호
    • /
    • pp.207-217
    • /
    • 2003
  • The purpose of this study was to compare the fracture strength of the IPS Empress ceramic crown according to the incisal depth (1.5mm, 2.0mm, 2.5mm) and axial inclination ($4^{\circ}$, $8^{\circ}$, $12^{\circ}$) of the lower central ncisor. After 10 metal dies were made for each group, the IPS Empress ceramic crowns were fabricated and each crown was cemented on each metal die with resin cement. The cemented crowns mounted on the testing jig were inclined 30 degrees and a universal testing machine was used to measure the fracture strength. The results of this study were as follows : The fracture strength of the ceramic crown with 2.0mm depth and $12^{\circ}$ inclination was the highest (648 N). Crowns of 1.5mm depth and $4^{\circ}$ inclination had the lowest strength (482 N). There were no significant differences of the fracture strength by axial inclination in same incisal depth group. The fracture mode of the crowns was similar. Most of fracture lines began at the loading area and extended through proximal surface perpendicular to the margin irrespective of incisal depth. There had correlation between fracture strength and fractured surface area.

즉시 Frialit-2 implant 식립, 즉시 임시치관 제작 그리고 IPS Empress 2 crown을 이용한 상악중절치의 심미적 수복 (Esthetic reconstruction of upper central incisor using immediate Frialit-2 implant placement, immediate temporary crown fabrication and IPS Empress 2 crown)

  • 김유리;오상천
    • 구강회복응용과학지
    • /
    • 제19권1호
    • /
    • pp.43-48
    • /
    • 2003
  • During the past several years, significant advances have occurred in the utilization of osseointegrated implants for the treatment of partially edentulous patients. One of the biggest purposes for treating of these patients is the high demand for improved esthetics, especially in the anterior region. For this esthetics, the new trend in dental implants is the immediate placement and immediate superstructure fabrication. The refined surgical technique, the skillful soft tissue management, and the proper prosthetic coordination are the main factors to achieve natural looking of implant supported prosthesis. The customized provisional restoration and the customized impression coping are recommended for the optimal peri-implant soft tissue contour. The basic concept of Frialit 2 system was the immediate replacement of a tooth with root-analog fixture after extraction. This system guarantees an ideal result in function and esthetics. The ceramic abutment system offers improved quality in the respect of esthetics, fitness, translucency, and biocompatibility. In this clinical report, the final restoration made with IPS Empress 2 crown on the CeraBase abutmen of Frialit 2 system allowed the reproduction of the natural vitality of tooth and adjacent gingiva.

Esthetic restoration of anterior dentition using Empress 2 system: A clinical report

  • Kim, Min-Ho;Yang, Jae-Ho
    • 대한치과보철학회지
    • /
    • 제38권6호
    • /
    • pp.821-828
    • /
    • 2000
  • Metal - ceramic restorations have been the standard of fixed oral rehabilitation for over 30 years, and while many advances have been made in materials and research, the esthetic challenges of the light reflective metal substructure will always put clinician in an esthetic dilemma, for only a very talented ceramist / dentist team can create esthetics that rival nature on a repeatable basis. All ceramic restorations have also been a choice in our restorative armamentarium, but in the past, the materials have also had their own limitation, number on being question-able strength to withstand occlusal forces generated during mastication. IPS Empress 2 offers dentistry a metal free alternative to traditional restorative techniques. This clinical report describes the treatment of patients with esthetic problem of anterior dentition using Empress 2 system.

  • PDF

변연형태와 레진시멘트에 따른 IPS Empress 도재관의 변연누출에 관한 연구 (A STUDY ON THE MICROLEAKAGE OF THE IPS EMPRESS CERAMIC CROWN ACCORDING TO MARGIN TYPES AND RESIN CEMENT)

  • 정원엽;오상천;동진근
    • 대한치과보철학회지
    • /
    • 제36권6호
    • /
    • pp.789-805
    • /
    • 1998
  • The purpose of this study was to compare the microleakage of the IPS Empress ceramic crown according to 1) margin types such as rounded shoulder and bevel, 2) margin locations such as enamel and dentine, 3) resin cement types such as Variolink and Bistite. For this study, 80 extracted premolar teeth were used. After 10 experimental dies were prepared for each group, the IPS Empress ceramic crowns were fabricated on the dies and cemented with one of two types of resin cement. After 1,000 cycles of thermal changes were given with the thermocycling unit, each specimen was sectioned with a low speed diamond saw in both the buccolingual and the mesiodistal direction. The microleakage was then measured with a stereo microscope. The obtained results were as follows : 1. Every experimental group showed microleakage. The microleakage of the crowns which had a rounded shoulder on enamel cemented with Variolink was the lowest of all. The resulting rank of the mean microleakage was rounded shoulder on enamel using Variolink(0.601mm), rounded shoulder on enamel using Bistite (0.794mm), bevel on enamel using Variolink (0.826mm), rounded shoulder on dentine using Variolink(1.054mm), bevel on enamel using Bistite(1.087mm), rounded shoulder on dentine using Bistite(1.176mm), bevel on dentine using Variolink(1.258mm), and bevel on dentine using Bistite(1.467mm). 2. The statistically significant differences in the microleakage were found in 4 cases: rounded shoulder on enamel using Variolink and bevel on dentine using Variolink, rounded shoulder on enamel using Variolink and bevel on dentine using Bistite, rounded shoulder on enamel using Bistite and bevel on dentine using Bistite, bevel on enamel using Variolink and bevel on dentine using Bistite. 3. The microleakage of rounded shoulder finish line was lower than that of bevel finish line. The statistically significant differences were found with respect to the type of finish lines. 4. The microleakage of the finish line on enamel was lower than that of finish line on dentine. The statistically significant differences were found with respect to the location of the finish lines. 5. The microleakage of the Variolink cement was lower than that of the Bistite cement. The statistically significant differences were found with respect to the resin cements.

  • PDF

Zirconia ceramic의 표면처리 방법이 레진시멘트의 결합강도에 미치는 영향 (EFFECT OF SURFACE TREATMENTS OF ZIRCONIA CERAMIC ON THE BOND STRENGTH OF RESIN CEMENTS)

  • 김창훈;전영찬;정창모;임장섭
    • 대한치과보철학회지
    • /
    • 제42권4호
    • /
    • pp.386-396
    • /
    • 2004
  • Statement of problem: It is not clear how to make a stable bonding between zirconia ceramic and resin cement. And the study about surface treatment of zirconia ceramic or bonding resin cement are not enough. Purpose: To measure and compare the shear bond strength of some resin cements on zirconia ceramic after different surface treatments. Material and method: 48 ceramic discs were made of 3 ceramic materials, zirconia ceramics (Zi-Ceram), heat-pressed ceramics (IPS Empress 2) and slip cast alumina ceramics (In-Ceram). According to the surface treatments of ceramic specimens and resin cements, specimens were classified into 6 groups and each group was composed of 8 specimens. For the surface treatment of Zi-Ceram group (test group), sandblasting and diamond bur preparation were applied and Superbond C&B and Panavia F were bonded respectively. For IPS Empress 2 group (control group), Variolink II was bonded after sandblasting, acid etching, silanization and for In-Ceram ALUMINA group (control group), Panavia F was bonded after sandblasting. After storing specimens in distilled water for 24 hours, the shear bond strength was measured by the universal testing machine. Results and conclusion: 1. Zi-Ceram group with Superbond C&B cement showed higher bond strength than with Panavia F cement regardless to the surface treatments (p<0.05). 2. In Zi-Ceram group with Superbond C&B cement, sandblasting treatment group (12.1MPa) showed higher bond strength than diamond bur treatment group (7.7MPa) (p<0.05). In Zi-Ceram group with Panavia F cement, there were no significant differences in the bond strength according to the surface treatments (p>0.05). 3. Zi-Ceram group with sandblasting and Superbond C&B cement (12.1MPa) showed the highest bond strength. The bond strength of this group was not significantly different from In-Ceram ALUMINA group (10.4MPa) (p>0.05) and lower than IPS Empress 2 group (15.9MPa) (p<0.05).

Celay/In-Ceram, Conventional In-Ceram, Empress 2 전부도재관의 변연적합도에 관한 비교 연구 (MARGINAL FIT OF CELAY/IN-CERAM, CONVENTIONAL IN-CERAM AND EMPRESS 2 ALL-CERAMIC SINGLE CROWNS)

  • 양재호;여인성;이선형;한중석;이재봉
    • 대한치과보철학회지
    • /
    • 제40권2호
    • /
    • pp.131-139
    • /
    • 2002
  • There have been many studies about marginal discrepancy of single restorations made by various systems and materials. But many of statistical inferences are not definite because of sample size, measurement number, measuring instruments. etc. The purpose of this study was to compare the marginal adaptations of the anterior single restorations made by different systems and to consider more desirable statistical methods in analysing the marginal fit. The in vitro marginal discrepancies of three different all-ceramic crown systems (Celay In-Ceram. Conventional In-Ceram. IPS Empress 2 layering technique) and one control group (PFM) were evaluated and compared. The crowns were made from one extracted maxillary central incisor prepared with a 1mm shoulder margin and $6^{\circ}$ taper walls by milling machine. 10 crowns per each system were fabricated. Measurements or a crown were recorded at 50 points that were randomly selected for marginal gap evaluation. Non-parametric statistical analysis was performed for the results. Within the limits of this study, the following conclusions were drawn: 1 Mean gap dimensions and standard deviations at the marginal opening for the maxillary incisor crowns were $98.2{\pm}40.6{\mu}m$ for PFM, $83.5{\pm}18.7{\mu}m$ for Celay In-Ceram, $104.9{\pm}44.1{\mu}m$ for conventional In-Ceram, and $45.5{\pm}11.5{\mu}m$ for IPS Empress 2 layering technique. The IPS Empress 2 system showed the smallest marginal gap (P<0.05). The marginal openings of the other three groups were not significantly different (P<0.05). 2 The marginal discrepancies found in this study were all within clinically acceptable standards ($100\sim150{\mu}m$). 3. When the variable is so controlled that the system may be the only one, mean value is interpreted to be the marginal discrepancy of a restoration which is made by each system and standard deviation is to be technique-sensitivity of each one. 4. From the standard deviations. the copy-milling technique (Celay/In-Ceram) was not considered to be technique-sensitive in comparison with other methods. 5. Parametric analysis is more reliable than non-parametric one in interpretation of the mean and standard deviation. The sample size of each group has to be more than 30 to use parametric statistics. The level of clinically acceptable marginal fit has not been established. Further studies are needed.