유한요소법을 이용한 Inconel 718의 열간단조공정시 동적재결정거동 예측 (Prediction of the Behavior of dynamic Recrystallization in Inconel 718 during Hot Forging using Finite Element Method)

  • 최민식;강범수;염종택;박노광
    • 소성∙가공
    • /
    • 제7권3호
    • /
    • pp.197-206
    • /
    • 1998
  • This paper presents the prediction of dynamic recrystallization behavior during hot forging of Inconel 718. Another experiment of pancake forging was also carried out to examine the recrystallization ration dynamically recrystallizaed grain size, and grain growth in the forging. In experiments cylindrical billets were forged by two operations with variations of forging temperature, reduction ration of deformation. and preheating process at each forging step. Also the finite element program, developed here for the prediction using the metallurgical models was used for the analysis of to Inconel 718 upsetting and the results were compared with experimental ones.

  • PDF

변형률 에너지법을 이용한 Inconel 617의 저주기피로 수명 예측 (Prediction of Low Cycle Fatigue Life for Inconel 617 using Strain Energy Method)

  • 김덕회;김기광;김재훈;이영신;박원식
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2004년도 추계학술대회
    • /
    • pp.285-290
    • /
    • 2004
  • Low cycle fatigue tests are performed on the Inconel 617 that be used for a hot gas casing. The relation between strain energy density and numbers of cycles to failure is examined in order to predict the low cycle fatigue life of Inconel 617. The life predicted by the strain energy method is found to coincide with experimental data and results obtained from the Coffin-Manson method. Also the cyclic behavior of Inconel 617 is characterized by cyclic hardening with increasing number of cycle at room temperature.

  • PDF

인코넬 690 합금의 크리프거동 (Creep Behaviours of Inconel 690 Alloy)

  • 황경충;윤종호;최재하;김성청
    • 한국공작기계학회논문집
    • /
    • 제11권4호
    • /
    • pp.54-61
    • /
    • 2002
  • Inconel 690 alloy has widely been used in power plant and high temperature facilities because it has high thermal resistance and toughness. But we have little design data about the creep behaviors of the alloy. Therefore, in this study, an apparatus has been designed and built for conducting creep tests under constant load conditions. A series of creep tests on Inconel 690 alloy have been performed to get the basic design data and life prediction of inconel products and we have gotten the following results. First, the stress exponents decrease as the test temperatures increase. Secondly, the creep activation energy gradually decreases as the stresses become bigger. thirdly, the constant of Larson-Miller Parameters on this alloy is estimated about 10. And last the fractographs at the creep rupture show both the ductile and the brittle fracture according to the creep conditions.

상온 대기 중에서 인코넬 600과 690의 슬라이딩 마모 (Sliding wear of Inconel 600 and 690 in room temperature air)

  • 홍동석;김경국;김준기;김선진
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2003년도 추계학술발표강연 및 논문개요집
    • /
    • pp.91-91
    • /
    • 2003
  • Sliding wear behaviors of Inconel 600 and 690 were investigated at room temperature in air. In the present study, Archard's equation which has low reliability was modified. In the prediction of wear volume by Archard's equation, the reliabilities of Inconel 600 and 690 were about from 26.3% to 45.7% and from 69. l% to 88.6%, respectively, The sliding wear behaviors of Inconel 600 and 690 turned out to be influenced by their stacking fault energy, and the fact was confirmed by using TEM and micro-hardness test Based on experimental results, the wear coefficient was modified as a function of the sliding distance. The calculation with the modified wear equation showed that the reliability of Inconel 600 tested with 409 ferritic stainless steel increased from 45.7% to 93.4%.

  • PDF

Inconel 617의 결정립 미세화에 의한 내부산화거동이 크렉 전파에 미치는 영향

  • 임정훈;조태선;김대경;김영도
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2010년도 춘계학술발표대회
    • /
    • pp.50.2-50.2
    • /
    • 2010
  • 니켈기 초내열합금 Inconel 617은 수소생산용 초고온 가스 냉각로의 열 교환기와 고온 가스관 등의 고온 배관용 후보재료로써, Cr, Mo, 와 W등의 첨가물이 함유된 고용 강화된 합금으로, 우수한 고온 강도, 크립 저항성, 내부식성 및 내산화성을 가지고 있는 것으로 알려져 있다. 본 연구에서는 결정립 미세화가 고온열화에 의해 입계를 따라 형성되는 internal oxide에 미치는 영향에 대해 평가하였고, 이러한 internal oxide가 인장응력 하에서 크렉 형성 및 전파에 미치는 영향을 평가하기 위하여 3-point bending test를 수행하였다. 미세한 결정립을 가지는 Inconel 617은 냉간압연 후 재결정을 통해 확보하였으며, as-received(AR)과 grain-refined(GR) Inconel 617은 $950^{\circ}C$에서 2000시간 동안 He분위기 하에서 열화시험을 수행하였다. AR과 GR에 형성된 internal oxide은 깊이와 분포 등의 뚜렷한 차이를 보였으며, 이러한 차이로 인해 인장응력 하에서 크렉 전파의 큰 차이를 나타내었다.

  • PDF

Inconel 713C와 SCM 440의 마찰용접 (Friction Welding of Inconel 713C and SCM 440)

  • 조현수;서성재
    • Journal of Welding and Joining
    • /
    • 제15권6호
    • /
    • pp.78-84
    • /
    • 1997
  • Friction welding technique was studied to weld the turbine wheel and shaft of a turbocharger. The welding parameters were selected to investigate the effects of variables on welding quality of Inconel 713C and SCM 440. Experimental results showed that the turbine wheel and shaft could be successfully welded by friction welding. The heat affected zone was identified to be 2 mm from the weld seam. After welding, the hardness profile was found to have sudden increase and decrease for inconel 713C and SCM 440 respectively. Tensile strength of welded specimens was higher than the required strength for all of the studied welding parameters. The central portion of fracture surfaces by bending had no defects such as crack.

  • PDF

Inconel 617 GTA 용접조건에 따른 미세조직 특성 및 기계적성질 (The Microstructures and Mechanical Properties on the GTA Welding conditions of Inconel 617)

  • 최성부;이봉근;강정윤
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2005년도 추계학술발표대회 개요집
    • /
    • pp.171-173
    • /
    • 2005
  • Inconel 617 is a solid solution, nickel-chromium-cobalt-molybdenum alloy with an exceptional combination of high temperature strength and oxidation resistance. The combination of high strenth and oxidation resistance at temperatures over $1800^{\circ}F$ makes Inconel 617 an attractive material for such components as ducting, transition liners in both aircraft and gas turbine. In this study, the weldability and weldment characteristics of Inconel 617 are considered in GTAW associated with the two welding current and with back shielding gas using or not. After GTAW with 120A and 150A current, microstructures and hardness test, bending test, tensile test on room and elevated temperature for the determination of optical welding condition.

  • PDF

nconel 600위에 증착된 TiN 박막의 고온 NaCl 수용액에서의 CPP 실험에 의한 핏팅저항성의 연구 (A Study on Pitting Resistance of TiN Film Coated on Inconel 600 by CPP Test in High Temperature NaCl Solution)

  • 김용일;정한섭;김홍회;이원종
    • 한국세라믹학회지
    • /
    • 제32권11호
    • /
    • pp.1301-1307
    • /
    • 1995
  • Pitting corrosion of TiN film deposited on Inconel 600 by plasma assisted chemical vapor deposition (PACVD) was investigated. Cyclic potentiodynamic polarization (CPP) tests were conducted in order to determine the pit nucleation potentials, Enp, of the TiN-deposited sample and the bare Inconel 600 in deaerated NaCl solution at 25, 135 and 20$0^{\circ}C$. The effects of the TiN film thickness, the solution temperature and the Cl- concentration on Enp were studied. Enp of the TiN-deposited sample which had the film thickness above 1${\mu}{\textrm}{m}$ were higher than those of the bare Inconel 600 by 300~600mV at all the solution temperatures, implying the pitting resistance improvement of the TiN film. The morphologies of the pits generated after immersion test were examined with a scaning electron microscopy. The higher was the solution temperature, the more corrosion products, mainly composed of Cr and Ni oxides, were formed.

  • PDF

Magnetic NDE for Sensitization of Inconel 600 Alloy

  • Kikuchi, Hiroaki;Sumimoto, Takaki;Kamada, Yasuhiro;Kobayashi, Satoru
    • Journal of Magnetics
    • /
    • 제18권3호
    • /
    • pp.348-351
    • /
    • 2013
  • Inconel 600 alloy, Ni base alloy, is widely used for steam generator tubings where sensitization occurs at grain boundaries and sensitization will induce tubing failures. This alloy has usually paramagnetic property, however, it transforms into ferromagnetic property along grain boundaries when sensitization occurs: this means NDE using magnetism for sensitization is possible. Therefore, in this study, Inconel 600 alloys were heat treated at 873 K from 0 to 400 hours so as to generate sensitization and their magnetic properties were investigated in detail. The saturation and the residual magnetization increase with increasing heat treatment time and take a maximum. On the other hand, the coercive force decreases with the increase in time of heat treatment. We confirmed that characteristics at only grain boundaries change into ferromagnetic phase by a MFM observation. As a trial for industrial application, heat treated Inconel 600 alloy was scanned by a magnetic field sensor, and the variations in magnetization were obtained nondestructively. The results indicate a feasibility of magnetic NDE for sensitization of Inconel 600 alloy.

국내 증기발생기 전열관 마열에 대한 실험적 연구 (Experimental studies on the fretting wear of domestic steam generator tubes)

  • 이영호;김형규;김인섭
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2002년도 제35회 춘계학술대회
    • /
    • pp.304-309
    • /
    • 2002
  • Fretting wear test in room temperature water was performed to evaluate the wear coefficient of Inconel 600,690 (Pressurized Water Reactor, PWR) and Alloy 800 (CANadian DeuteriumUranium, CANDU) steam generator (SG) tubes against ferritic and martensitic stainless steels. The main focus is to compare the wear behaviors between Alloy 800 and Inconel alloys. Test conditions are $10{\sim}30N$ of normal load, $200{\sim}450{\mu}m$ of sliding amplitude and 30Hz of frequency. The result indicated that the wear rate of Alloy 800 was higher than those of Inconel 690 at various test condition such as normal loads, sliding amplitudes etc. From the results of SEM observation, there was little evidence of plastic deformation layer that were dominantly formed on the worn surfaces of Inconel 690. Also, wear particles in Alloy 800 were released from contacting asperities deformed by severe plastic flow during fretting wear. Main cause of wear rate between Alloy 800 and Inconel 690 may be due to the difference of hardness between martensitic and ferritic stainless steel. The wear rate and wear mechanism of two tubes in room temperature water are discussed.