  • Ion beam assisted deposition(IBAD) technique was used to synthesize hard coatings including diamond-like carbon(DLC), carbon nitride(CN) and metal-ceramic multilayered films. It was found that DLC films formed at low energy ion bombardment possess more $Sp^3$ bonds and much higher hardness. The films exhibited an excellent wear resistance. Nanometer multialyered Fe/TiC films was deposited by ion beam sputtering. The structure and properties were strongly dependent on the thickness of the individual layers and modulation wave length. It was disclosed that both hardness and toughness of the films could be enhanced by adjusting the deposition parameters. The CN films synthesized by IBAD method consisted of tiny crystallites dispersed in amorphous matrix, which were identified by electron diffraction pattern to be $\beta -C_3N_4$.

  • PDF

Influence of Deposition Method on Refractive Index of SiO2 and TiO2 Thin Films for Anti-reflective Multilayers

  • Song, Myung-Keun;Yang, Woo-Seok;Kwon, Soon-Woo;Song, Yo-Seung;Cho, Nam-Ihn;Lee, Deuk-Yong
    • Journal of the Korean Ceramic Society
    • /
    • v.45 no.9
    • /
    • pp.524-530
    • /
    • 2008
  • Anti-Reflective (AR) thin film coatings of $SiO_2$ (n= 1.48) and $TiO_2$ (n=2.17) were deposited by ion-beam assisted deposition (IBAD) with End-Hall ion source and conventional electron beam (e-beam) evaporation to investigate the effect of deposition method on the refractive indicies (n) of the fIlms. Green-light generation using a GaAs laser diode was achieved via excitation of the second harmonic. The latter resulted from the transmission of the fundamental guided-mode wave of 1064 nm through periodically poled $LiNbO_3$. Large differences in the refractive indicies of each of the layers in the multilayer coating may improve AR performance. IBAD of $SiO_2$ reduced its refractive index from 1.45 to 1.34 at 1064 nm. Conversely, e-beam evaporation of $TiO_2$ increased its refractive index from 1.80 to 2.11. In addition, no fluctuations in absorption at the wavelength of 1064 nm were found. The results suggest that films prepared by different deposition methods can increase the effectiveness of multilayer AR coatings.

Research for Deposition of $CeO_2$ Buffer Layer on Coated Conductor by Electron Beam Evaporation (전자빔 증발법에 의한 박막형 고온초전도체의 $CeO_2$ 버퍼층 증착 연구)

  • Lee, J.B.;Park, S.K.;Kim, H.J.;Moon, S.H.;Lee, H.G.;Hong, G.W.
    • Progress in Superconductivity
    • /
    • v.11 no.2
    • /
    • pp.123-127
    • /
    • 2010
  • The properties of buffer layer for thermal and chemical stability in coated conductor is a very important issue. $CeO_2$ has desirable thermal and chemical stability as well as good lattice match. In this study, $CeO_2$ was deposited by electron beam deposition. The MgO(001) single crystal and LMO buffered IBAD substrate(LMO/IBAD-MgO/$Y_2O_3/Al_2O_3$/Hastelloy) were used as substrates, which have $\Delta\phi$ values of ${\sim}8.9^{\circ}$. The epitaxial $CeO_2$ films was deposited with high deposition rate of $12{\sim}16\;{\AA}/sec$. During deposition, the change of oxygen partial pressure(${\rho}O_2$) does not cause change in c-axis texture. In case of $CeO_2$ on MgO single crystal, the substrate temperature was optimized at $750^{\circ}C$ with superior $\Delta\phi$ and $\Delta\omega$ value. Otherwise, In case of LMO buffered IBAD substrate, It was optimized at $650^{\circ}C$ with increasing its deposition thickness of $CeO_2$, which was finally obtained with best $\Delta\phi$ value of $5.5^{\circ}$, $\Delta\omega$ value of $2^{\circ}$ and Ra value of 2.2 nm.

Effect of the thickness of CeO$_2$ buffer layer on the YBCO coated conductor

  • Dongqi Shi;Ping Ma;Ko, Rock-Kil;Kim, Ho-Sup;Ha, Hong-Soo;Chung, Jun-Ki;Kyu-Jeong, Song;Park, Chan;Moon, Seung-Hyun
    • Progress in Superconductivity and Cryogenics
    • /
    • v.6 no.4
    • /
    • pp.1-4
    • /
    • 2004
  • Three group samples with difference thickness of $CeO_2$ capping layer deposited by PLD were studied. Among them, one group $CeO_2$ films were deposited on stainless steel tape coated with IBAD- YSZ and $CeO_2$ buffer layer ($CeO_2$/IBAD-YSZ/SS); other two groups of $CeO_2 YSZ Y_2O_3$multi-layer were deposited on NiW substrates for fabrication of YBCO coated conductor through RABiTS approach. The pulsed laser deposition (PLD) and DC magnetron sputtering were employed to deposit these buffer layers. On the top of buffer layer, YBCO film was deposited by PLD. The effect of thickness of $CeO_2$ film on the texture of $CeO_2$ film and critical current density ($J_c$) of YBCO film were analyzed. For the case $CeO_2$ on $CeO_2$/IBAD-YSZ/SS, there was a self-epitaxy effect with the increase of $CeO_2$ film. For $YSZ/Y_2O_3$ NiW which was deposited by PLD or DC magnetron sputtering, there is not self-epitaxy effect. However, the capping layer of $CeO_2$ film deposited by PLD improved the quality of buffer layer for $YSZ/Y_2O_3$ which was deposited by DC magnetron sputtering, therefore increased the $J_c$ of YBCO film.

A Study on the MgO Protective Layer Deposited by Oxygen-Neutral-Beam-Assisted Deposition in AC PDP (산소 중성빔으로 보조증착된 MgO 보호막을 갖는 AC PDP의 특성에 관한 연구)

  • Li, Zhao-Hui;Kwon, Sang-Jik
    • Journal of the Korean Vacuum Society
    • /
    • v.17 no.2
    • /
    • pp.96-101
    • /
    • 2008
  • The magnesium oxide (MgO) protective layer plays an important role in plasma display panels (PDPs). Our previous work demonstrated that the properties of MgO thin film could be improved, which were deposited by Ion-Beam-Assisted Deposition (IBAD). However arc discharge always occurs during the IBAD process. To avoid this problem, Oxygen-Neutral-Beam-Assisted Deposition (NBAD) is used to deposit MgO thin films in this paper. The energy of the oxygen neutral beam was used as the parameter to control the deposition. The experimental results showed that the oxygen neutral beam energy was effective in determining in structural and discharge characteristics. The lowest firing inception voltage, the highest brightness and the highest luminous efficiency were obtained when the MgO thin film was deposited with an oxygen neutral beam energy of 300eV. The surface morphology of MgO thin film was also analyzed using AFM (Atomic Force Microscopy) and SEM (Scanning Electron Microscopy).

Fabrication of Thick SmBCO/IBAD-MgO coated conductor (후막 SmBCO/IBAD-MgO 초전도 박막선재의 제조)

  • Lee, J.H.;Kang, D.K.;Ha, H.S.;Ko, R.K.;Oh, S.S.;Kim, H.K.;Yang, J.S.;Jung, S.W.;Moon, S.H.;Youm, D.;Kim, C.J.
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2009.05a
    • /
    • pp.9-9
    • /
    • 2009
  • Coated conductor is required to have good critical current property for high efficiency of electric power applications. Until now, long coated conductor does not show high Jc over 3 MA/$cm^2$ in thick superconducting layer because of texture degradation by thick superconducting layer. In this study, in order to overcome this issue, thicker superconducting layer was deposited with optimized conditions to reduce the degradation of critical current density. SmBCO superconducting coated conductor was deposited with 1~3 um of thickness at $750\sim850^{\circ}C$ under 15~20 mTorr of oxygen partial pressure using batch type EDDC( evaporation using drum in dual chamber). The buffered substrate for superconducting layer deposition was used IBAD-MgO template with the architecture of $LaMnO_3/MgO/Y_2O_3/Al_2O_3$/Hastelloy. After fabrication of coated conductor, critical current was measured by 4-prove method under self-magnetic field and 77K. In addition, surface morphology and texture were analyzed by SEM and XRD, respectively. 3 um thick SmBCO coated conductor shows highest $I_C$ values of 638A/cm-w in 1 m long in the world.

  • PDF

Planarization of SUS310 Metal Substrate Used for Coated Conductor Substrate by Chemical Solution Coating Method (화학적인 용액 코팅방법에 의한 박막형 고온초전도체에 사용되는 SUS310 금속모재의 평탄화 연구)

  • Lee, J.B.;Lee, H.J.;Kim, B.J.;Kwon, B.K.;Kim, S.J.;Lee, J.S.;Lee, C.Y.;Moon, S.H.;Lee, H.G.;Hong, G.W.
    • Progress in Superconductivity
    • /
    • v.12 no.2
    • /
    • pp.118-123
    • /
    • 2011
  • The properties of $2^{nd}$ generation high temperature superconducting wire, coated conductor strongly depend on the quality of superconducting oxide layer and property of metal substrate is one of the most important factors affecting the quality of coated conductor. Good mechanical and chemical stability at high temperature are required to maintain the initial integrity during the various process steps required to deposit several layers consisting coated conductor. And substrate need to be nonmagnetic to reduce magnetization loss for ac application. Hastelloy and stainless steel are the most suitable alloys for metal substrate. One of the obstacles in using stainless steel as substrate for coated conductor is its difficulties in making smooth surface inevitable for depositing good IBAD layer. Conventional method involves several steps such as electro polishing, deposition of $Al_2O_3$ and $Y_2O_3$ before IBAD process. Chemical solution deposition method can simplify those steps into one step process having uniformity in large area. In this research, we tried to improve the surface roughness of stainless steel(SUS310). The precursor coating solution was synthesized by using yttrium complex. The viscosity of coating solution and heat treatment condition were optimized for smooth surface. A smooth amorphous $Y_2O_3$ thin film suitable for IBAD process was coated on SUS310 tape. The surface roughness was improved from 40nm to 1.8 nm by 4 coatings. The IBAD-MgO layer deposited on prepared substrate showed good in plane alignment(${\Delta}{\phi}$) of $6.2^{\circ}$.

BONE RESPONSE OF THREE DIFFERENT SURFACE IMPLANTS : HISTOMORPHOMETRIC, PERIO TEST VALUE AND RESONANCE FREQUENCY ANALYSIS IN BEAGLE DOGS

  • Choi, Joon-Eon;Suh, Kyu-Won;Lee, In-Ku;Ryu, Jae-Jun;Shin, Sang-Wan
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.45 no.3
    • /
    • pp.362-374
    • /
    • 2007
  • Statement of problem. The intial stability for osseointegration of implant has been an interesting factor. Especially, in the case of poor bone quality or immediately loaded implant, various strategies have been developed focusing on the surface of materials to improve implant fixation to bone. The microscopic properties of implant surfaces play a major role in the osseous healing of dental implants. Purpose. The aims of this study are to perform a histologic and histomorphometric comparison of the healing characteristics of three different surfaces and the comparison of resonance frequency analysis (RFA) values measured by $Osstell^{TM}$ and perio-test values (PTV) measured by Periotest. Material and methods. A total of 24 screw titanium implants (Dentium Co., Seoul, Korea) with 6mm in length and 3.4mm in diameter, were placed in the mandible of 4 beagle dogs. Implants were divided into three groups following the surface treatment methods: Group I is machined(control group). Group II is anodically oxidized. Group III is coated 500nm in thickness with hydroxyapatite(HA) by ion beam assisted deposition(IBAD) on the anodized oxidization. Bone blocks from 2 dogs were caught after 3 weeks of covered healing and another blocks from 2 dogs after 6 weeks. RFA values and PTV were measured right after insertion and at 3 and 6weeks. Histomorphometric analysis was made with Kappa Image Base System to calculate bone-to-implant contact (BIC) and bone area inside the threads. Pearson's correlation analyses were performed to evaluate the correlation between RFA and PTV, BIC and bone area ratio of three different surfaces at 3 and 6 weeks. Results. 1) In all surface treatment methods, the RFA values decreased and the PTV values increased until 6 weeks in comparison to initial values. 2) At 3 weeks, no significant difference was found from bone-to-implant contact ratio and bone area ratio of three different surface treatment methods(P>0.05). However, at 6 weeks, different surface treatment methods showed significantly different bone-toimplant contact ratio and bone area ratio(P<0.05). 3) In the implants with the IBAD on the anodic oxidization, significant difference was found between the 3 weeks and the 6 weeks bone area ratio(P<0.05). 4) Correlation was found between the RFA values and the bone area ratio at 3 and 6 weeks with significant difference(P<0.05). Conclusions. These results indicate that the implants with the IBAD on the anodic oxidization may have a high influence on the initial stability of implant.