Hydrogelation Process Variables in Crystallization of Zeolite (Zeolite 결정 성장에 미치는 Hydrogel화의 영향)

  • 서정권;이광석;이정민;정필조
    • Journal of the Korean Ceramic Society
    • /
    • v.26 no.4
    • /
    • pp.575-582
    • /
    • 1989
  • The effects of raw material feeding procedures and gelation temperatures on zeolite synthesis are investigated. Thus, the synthesis of zeolite 4A from sodium aluminate and sodium silicate solutions is chosen as a model reaction, for which equi-molar hydrogelation is performed with variation of feeding procedures and gelation temperatures. The formation of crystal nuclei, often being referred to as precursors, is induced under different conditions, the variation being examined by means of viscosity and water contents. The final products of zeolite 4A are evaluated by XRD, SEM morphology, particle size analysis and cation exchange capacity. Evidence shows that the viscosity of the initial products and their water contents are markedly influenced by the feeding methods of the reactant materials and by the gelation temperature. Further, it is found that the gelation at an elevated temperatures near 7$0^{\circ}C$ can be made possible through modification of mixing procedures. This provides convenient means of controlling the particle size of the final products. In this regard, a continuous flow-type mixing technique is proposed, which is demonstrated to be superior to the conventional batch-type mixings. The significance of this finding may lie in savings of equipment as well as energy costs, especialy on a large scale commercialization of zeolite production.

  • PDF

First Hydrogelation of Discrete Metal Complexes. Structures and Fluxional Behavior of Cyclopalladium(II) Complexes

  • Na, Young-Mee;Noh, Tae-Hwan;Ha, Byung-Jo;Hong, Jong-Ki;Jung, Ok-Sang
    • Bulletin of the Korean Chemical Society
    • /
    • v.30 no.3
    • /
    • pp.573-576
    • /
    • 2009
  • The reaction of $(en)Pd(NO_3)_2$ (en = ethylenediamine) with 1,4-bis(dimethyl-4-pyridylsilyl)benzene (L) affords cyclodimer, $[(en)Pd(L)]_2(NO_3)_4$, whereas the reaction of $(tmeda)Pd(NO_3)_2$ (tmeda = N,N,N’,N’-tetramethylethylenediamine) with L gives cyclotrimer, $[(tmeda)Pd(L)]_3(NO_3)_6$. Both complexes exist as catenane in water. The catenated cyclodimer is rigid whereas the catenated cyclotrimer is dynamic in water. The catenated cyclotrimers afford hydrogel containing 98.5% water below 2 ${^{\circ}C}$. The hydrogel changes to its sol around 38 ${^{\circ}C}$, and to its clear solution at 78 ${^{\circ}C}$. Such a notable difference between $[(en)Pd(L)]_2(NO_3)_4$ and $[(tmeda)Pd(L)]_3(NO_3)_6$ might be explained by their different dynamic behavior via ring size effects.

Synthesis of P-type Zeolite Using Melting Slag from Municipal Incineration Ash (도시 소각재 용융슬래그로부터 P형 제올라이트 합성)

  • Lee Sung-Ki;Jang Young-Nam;Chae Soo-Chun;Ryu Kyoung-Won;Bae In-Kook
    • Journal of the Mineralogical Society of Korea
    • /
    • v.19 no.1 s.47
    • /
    • pp.7-14
    • /
    • 2006
  • Melting slag generated from the lots of municipal incineration ash, which causes the one of big urban problems in modern industrial society, was used as starting material for the hydrothermal synthesis of zeolite. P-type zeolite has been successfully synthesized by the combined process of both 'hydrogelation' and 'clay conversion' method. Commercial sodium silicate was used as Si source, and $NaAlO_2$ was prepared by the reaction in a $Na_{2}O/Al_{2}O_{3}$ molar ratio of 1.2. The optimum conditions for zeolite synthesis was found to be the $SiO_{2}/Al_{2}O_{3}$ ratio in the 3.2 and 4.2 range, the $H_{2}O/Na_{2}O$ ratio in the 70.7 and 80.0 range, and more than 15-hour reaction time at $80^{\circ}C$, In the synthesized zeolite, inhomogeneous melting slag particles were disappeared and homogeneous P-type zeolite crystal was grown. The cation exchange capacity of the synthesized zeolite was determined to be approx. 240 cmol/kg.

Preparation of Semi-solid Fibroin Gel and its Flow Property (반고형 피브로인 단백질 겔의 제조 및 유동특성)

  • Hur, Won;Lee, Shin-Young
    • KSBB Journal
    • /
    • v.24 no.6
    • /
    • pp.563-569
    • /
    • 2009
  • Fibroin is an insoluble structural protein from Bombyx mori. It can be solubilized by dissolving in a hot $CaCl_2$ solution and subsequent dialysis. The aqueous solution is unstable and a transition from aqueous fibroin molecules rich in random coil is undergo to one rich in $\beta$-sheet content, resulting in hydrogelation. However, fibroin gel is so fragile and plastic that its mechanical property should be reformed for various applications. In this report, a semi-solid form of fibroin gel was prepared using glycerol and ethanol and was investigated to analyze their flow properties. A fibroin gel with 80% glycerol showed pseudoplastic and thixotropic properties. The square root of its yield stress varied linearly with fibroin concentration and it extrapolated to zero shear stress at 0.2% fibroin. A fibroin gel with 40% ethanol was shown to be highly thixotropic but its shear-thinning behavior was only observed above a certain level of shear rate. Its pseudoplasticity was restored by a high rate of shear stress.

In situ Gel Forming Stereocomplex Composed of Four-Arm PEG-PDLA and PEG-PLLA Block Copolymers

  • Jun, Yeo-Jin;Park, Kyung-Min;Joung, Yoon-Ki;Park, Ki-Dong;Lee, Seung-Jin
    • Macromolecular Research
    • /
    • v.16 no.8
    • /
    • pp.704-710
    • /
    • 2008
  • Injectable hydrogels are quite promising materials due to their potential to minimize invasive implantation and this provides versatile fitness irrespective of the damaged regions and facilitates the incorporation of bioactive agents or cells. In situ gel formation through stereocomplex formation is a promising candidate for injectable hydrogels. In this paper, a new series of enantiomeric, four-arm, PEG-PLA block copolymers and their stereocomplexed hydrogels were prepared by bulk ring-opening polymerization of D-lactide and L-lactide, respectively, with stannous octoate as a catalyst. The prepared polymers were characterized by $^1H$ nuclear magnetic resonance (NMR) spectroscopy, Fourier-transform infrared (FT IR) spectroscopy, gel permeation chromatography (GPC) and thermal gravitational analysis (TGA), confirming the tailored structure and chain lengths. The swelling and degradation behavior of the hydrogels formed from a selected copolymer series were observed in different concentrations. The degradation rate decreased with increasing polymer content in the solution. The rheological behavior indicated that the prepared hydrogel underwent in situ gelation and had favorable mechanical strength. In addition, its feasibility as an injectable scaffold was evaluated using a media dependence test for cell culture. A Tris solution was more favorable for in situ gel formation than PBS and DMEM solutions were. These results demonstrated the in situ formation of hydrogel through the construction of a stereocomplex with enantiomeric, 4-arm, PEG-PLA copolymers. Overall, enantiomeric, 4-arm, PEG-PLA copolymers are a new species of stereocomplexed hydrogels that are suitable for further research into injectable hydrogels.