• 제목/요약/키워드: Hwangtoh

검색결과 53건 처리시간 0.025초

활성황토를 사용한 콘크리트의 염소이온 침투 저항성에 관한 실험적 연구 (Experimental Study on the Resistance of Chloride Infiltration of Concrete Using Activated Hwangtoh Admixture)

  • 이강우;장종호;최희용;구자술;황혜주;김무한
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2001년도 가을 학술발표회 논문집
    • /
    • pp.781-786
    • /
    • 2001
  • The Salt attack is one of the primary factors that cause the deterioration of durability in steel reinforced concrete structure. And to depreciate the deterioration from the Salt attack in concrete structure, pozzolanic materials are used widely in recent years. In this study, experiments about the resistance of chloride infiltration of concrete according to the replacement rations of Activated Hwangtoh and various pozzolanic materials(silica fume, fly ash, blast furnace slag and non Activated/Activated Hwangtoh) are performed and the results of this study were shown as follows; 1) As the replacement ratios of Activated Hwangtoh were getting higher, the strength of concrete was increased and in case of various pozzolanic materials, strength of Activated Hwangtoh in specimen was better than that of fly ash, blast furnace slag and non Activated Hwangtoh. 2) As the replacement ratios of Activated Hwangtoh were getting higher, the resistance of chloride infiltration of concrete was increased and in case of various pozzolanic materials, silica fume is better than any other pozzolanic materials and Activated Hwangtoh was better than that of fly ash, blast furnace slag and non Activated Hwangtoh.

  • PDF

황토와 고로슬래그를 첨가한 콘크리트의 건조수축 및 크리프 특성에 관한 연구 (A Study of Properties of Drying Shrinkage and Creep of Concrete Incorporating Hwangtoh and Blast Furnace Slag)

  • 강홍기;양근혁;이영호;황혜주;정헌수
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2004년도 춘계 학술발표회 제16권1호
    • /
    • pp.612-615
    • /
    • 2004
  • The objective of this experimental study was to understand inelastic strain of concrete incorporating hwangtoh or combination of hwangtoh and slag. Main variables were replacement level of admixtures, hwangtoh and slag. We studied the properties of concrete such as heat of hydration, drying shrinkage and creep according to the replacement level of hwangtoh and slag. Test results showed that the heat of hydration of concrete decrease with increasing hwangtoh and slag replacement. Also drying shrinkage and creep of concrete increase with increasing hwangtoh replacement.

  • PDF

Characteristics of Alkali-activated Natural Hwangtoh Paste Utilizing Microwave Heating

  • Kim, Baek-Joong;Yi, Chong-Ku;Kang, Kyung-In
    • 한국건축시공학회지
    • /
    • 제12권5호
    • /
    • pp.503-509
    • /
    • 2012
  • In this study, the potential use of indigenous natural loess(Hwangtoh) as a new construction material, via alkali activation in conjunction with microwave heating, was investigated. Hwangtoh pastes with three different mix proportions of varying alkali liquid concentrations at a constant liquid-to-Hwangtoh ratio of 0.55 were prepared. Through the investigation it was found that it is possible to prepare Hwangtoh paste with $19.02N/mm^2$ at the age of 4 hours with the alkali solution of 8M NaOH and 1:4.5 mass ratio of liquefied $Na_2SiO_3$ at the curing temperature of $60^{\circ}C$ by microwave heating. The strength development at early age of the alkali activated Hwangtoh paste specimens may be attributed to both a higher rate of reaction and moisture evaporation due to microwave heating.

Bond Strength of Mortar mixed Activated Hwangtoh

  • Go, Seong-Seok;Yeo, Sang-Ku;Lee, Hyun-Chul
    • 한국건축시공학회지
    • /
    • 제12권5호
    • /
    • pp.468-477
    • /
    • 2012
  • This study aimed to mix and test mortar incorporating activated Hwangtoh to improve the Hwangtoh brick bond strength of brick structures. To do this, the bond strength correlation of mortar was analyzed by means of materials and experiment factors and levels, and the optimum conditions were suggested after analyzing the physical properties of brick and the mix ratio of mortar and additive. Furthermore, the compressive strength and bond strength were found to be in inverse proportion, and in terms of the materials and mixing level, W/C ratio, substitution ratio of activated Hwangtoh, and fine aggregate grading were shown to have a considerable influence on the strength. In conclusion, the optimum mixing conditions to improve the bond strength are found to set W/C ratio at 65% and replacmenet ratio of activated Hwangtoh at 10%.

황토와 슬래그를 첨가한 콘크리트의 강도 및 응력-변형률 관계 (The Stress-Strain Relationship and Compressive Strength of Concrete Containing Hwangtoh and Slag)

  • 강홍기;양근혁;이영호;황혜주;정헌수
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2004년도 춘계 학술발표회 제16권1호
    • /
    • pp.672-675
    • /
    • 2004
  • The objective of this study was to understand the effect of hwangtoh and slag on various properties of concrete. Main variables were replacement level of admixtures, hwangtoh and slag, and curing temperature. Test results indicated that the compressive strength of concrete replaced by either hwangtoh and slag was significantly influenced by curing temperature. The elasticity modulus and compressive peak strain of concrete showed a small increase with increasing hwangtoh replacement.

  • PDF

황토 마감재의 배합비에 따른 압축강도 특성과 사용성 평가 (Usability and Strength Characteristics of Loess(Hwangtoh) Finishing Material by Different Ratios of Ingredients)

  • 리신호;윤성수;서교;송창섭;한충수
    • 농촌계획
    • /
    • 제11권3호
    • /
    • pp.53-57
    • /
    • 2005
  • Up to recently building are constructed focusing on the convenience of residential condition. However, environmental-friendly materials is required for construction as people are spending more time inside buildings and causes of many problems like sick-building syndrome are known due to the noxious gases and polluted air originated from construction materials. Although loess(hwangtoh) is an environmental-friendly material, it has limitations in compressive strength far a construction material. The purpose of this study is to suggest the optimal ratio of loess(hwangtoh) mortar by tests of compressive strength comparing with standard strength of floor finishing mortar and evaluate the usability of loess(hwangtoh) mortar for floor finishing material through an impact test, a cracking test and a abrasion test. Based on the results of this study, 86% of loess(hwangtoh) and 14% of inorganic binder is suggested for the optimal mixture ratio of loess(hwangtoh) mortar. Moreover, the characteristics of loess(hwangtoh) is suitable for floor finishing material in impact, crack, abrasion.

활성 황토 콘크리트 보의 전단 및 부착 강도 (Shear and Bond Strength of Activated Hwangtoh Concrete Beam)

  • 이남곤;박홍근;황혜주
    • 콘크리트학회논문집
    • /
    • 제22권5호
    • /
    • pp.685-694
    • /
    • 2010
  • 지금까지 환경 친화적 재료로서 황토에 관한 연구는 포틀랜드 시멘트를 부분적 대체하거나, 완전 대체하는 연구로 진행되어 왔다. 기존의 대부분의 연구에서는 압축강도, 건조수축, 크리프 등 황토 콘크리트의 역학적 성질에 초점이 맞춰졌다. 이 연구에서는 황토 콘크리트로 제작된 보 실험체의 전단강도를 실험하였다. 또한 황토 콘크리트에 정착된 인장 철근의 부착강도를 실험하였다. 이번 실험에서 시멘트를 20% 대체하는 활성 황토와 시멘트를 100% 대체하는 활성 황토를 사용한 콘크리트가 사용되었다. 실험 결과, 시멘트 20% 대체 활성 황토와 무시멘트 활성 황토 콘크리트 보의 전단 강도는 일반 포틀랜드 시멘트 콘크리트 보와 동등하였다. 반면에, 무시멘트 활성 황토 콘크리트의 부착 강도는 일반 포틀랜드 시멘트 콘크리트보다 작았다.

황토팩 제품의 규격 (Standard of Hwangtoh Pack Product)

  • 손영택
    • Journal of Pharmaceutical Investigation
    • /
    • 제35권6호
    • /
    • pp.467-469
    • /
    • 2005
  • The purpose of this study was to investigate main ingredients of Hwangtoh (Korean yellow ochre), especially ferric oxide $(Fe_{2}O_{3})$ content. In this study, X-ray fluorescence spectrophotometry was employed to analyze the ingredients of Hwangtoh. The ferric oxide $(Fe_{2}O_{3})$ contents of Hwangtoh from Hwa Sun, Ham An, Chil Gok, Sun Chun, Ha Dong, San Chung, Go Chang, Kim Che and Jeong Eup were 1.5, 5.66, 11.76, 6.63, 2.74, 11.4, 4.84, 7.21 and 6.23%, respectively. Based on the above results, any Hwangtoh sample didn't meet the ferric oxide $(Fe_{2}O_{3})$ content criterion.

Mechanical Properties of Hwangtoh-Based Alkali-Activated Concrete

  • Yang, Keun-Hyeok;Hwang, Hey-Zoo;Lee, Seol
    • Architectural research
    • /
    • 제11권1호
    • /
    • pp.25-33
    • /
    • 2009
  • This study presents the testing of 15 hwangtoh-based cementless concrete mixes to explore the significance and limitations of the development of eco-friendly concrete without carbon dioxide emissions while maintaining various beneficial effects. Hwangtoh, which is a kind of kaolin, was incorporated with inorganic materials, such as calcium hydroxide, to produce a cement-less binder. The main variables investigated were the water-to-binder ratio and fine aggregate-to-total aggregate ratio to ascertain the reliable mixing design of hwangtoh-based cementless concrete. The variation of slump with elapsed time was recorded in fresh concrete specimens. Mechanical properties of hardened concrete were also measured: including compressive strength gain, splitting tensile strength, moduli of rupture and elasticity, stress-strain relationship, and bond resistance. In addition, mechanical properties of hwangtoh-based cement-less concrete were compared with those of ordinary portland cement (OPC) concrete and predictions obtained from the design equations specified in ACI 318-05 and CEB-FIP for OPC concrete, wherever possible. Test results show that the mechanical properties of hwangtoh-based concrete were significantly influenced by the water-to-binder ratio and to less extend by fine aggregate-to-total aggregate ratio. The moduli of rupture and elasticity of hwangtoh-based concrete were generally lower than those of OPC concrete. In addition, the stress-strain and bond stress-slip relationships measured from hwangtoh-based concrete showed little agreement with the design model specified in CEB-FIP. However, the measured moduli of rupture and elasticity, and bond strength were higher than those given in ACI 318-05 and CEB-FIP. Overall, the test results suggest that the hwangtoh-based concrete shows highly effective performance and great potential as an environmental-friendly building material.

활성 황토 콘크리트 보의 휨 성능 (Flexural Performance of Activated Hwangtoh Concrete Beam)

  • 이남곤;황혜주;박홍근
    • 콘크리트학회논문집
    • /
    • 제22권4호
    • /
    • pp.567-574
    • /
    • 2010
  • 지금까지 환경 친화적 재료로서 황토에 관한 연구는 포틀랜드 시멘트를 부분적 대체하거나, 완전 대체하는 연구로 진행되어 왔다. 기존의 대부분의 연구에서는 압축강도, 건조수축, 크리프 등 황토 콘크리트의 역학적 성질에 초점이 맞춰졌다. 이 연구에서는 황토 콘크리트로 제작된 보 실험체의 휨 성능을 실험하였다. 이번 실험에서는 시멘트를 20% 대체하는 활성 황토를 사용한 콘크리트와 시멘트를 100% 대체하는 활성 황토 콘크리트가 사용되었다. 단순보 실험은 2점 정적 재하 하중으로 실험하였다. 휨 강도, 균열 모멘트, 처짐, 연성도 등의 결과를 일반 포틀랜드 시멘트 콘크리트로 제작된 보의 실험 결과와 비교하였다.