YBCO 초전도체막을 위한 Cu 판의 배향화 및 중간 산화층의 제조 (Texturing of Cu Sheets and Fabrication of Oxide Buffer Layers for YBCO Superconductor Films)

  • 김명희;김유진;한상철;성태현;김상준;노광수
    • 한국초전도학회:학술대회논문집
    • /
    • 한국초전도학회 1999년도 High Temperature Superconductivity Vol.IX
    • /
    • pp.352-357
    • /
    • 1999
  • The Cu sheets were selected for the substrate of the superconductor films. Pure Cu sheets with the thickness of 50${\mu}$m were fabricated using hot and cold rolling. The Cu sheets were heat treated to induce the biaxial texturing. The z-axis and x-y plane texturing of Cu sheets heat treated at different conditions were analyzed using XRD and a best heat treatment condition for the texturing was selected. ZrO$_2$ film was dip coated on Cu sheets heat treated at the best condition to prevent possible reaction between Cu sheets and YBCO superconductors, to reduce possible cracking due to thermal expansion mismatch and to decrease the lattice mismatch for biaxial texturing. The texturing of the oxide buffer layers were also studied.

  • PDF

붕소함유 냉간단조용 비조질강의 경화능 및 기계적 특성평가 (Characterization of Hardenability and Mechanical Properties of B-Bearing Microalloyed Steels for Cold Forging)

  • 박현균;김남규;최회진
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 춘계학술대회 논문집
    • /
    • pp.395-399
    • /
    • 2004
  • Four microalloyed steels containing B were investigated in terms of hardenability, mechanical properties and microstructure depending upon the cooling rates in order to develop the steel grade for the cold forged fasners. The alloy with the largest DI value among 4 alloys, which contains $0.12\%\;C,\;1.54\%\;Mn,\;0.65\%\;Cr,\;0.11\%V,\;0.040\%Ti\;and\;0.0033\%B$, showed the larest shift to the right hand side in the TTT diagram, implying the wide allowable cooling rate range subsequent to hot rolling in long bar processing, Mechanical tests indicated that yield strength are dependent upon the DI value in water quenched specimens but other properties showed almost the same values. In the same grade of steel, the increase in cooling rates causes the decrease in elongation but the increase in strength, reduction of area and Charpy impact values. Microstructural examination in steel grade with the larest DI values revealed martensitic structure In the water quenched state, a mixture of martensite and bainite in the oil quenched, and ferrite + pearlite in the air cooled and the forced air cooled but the latter showed finer microstructure.

  • PDF

Development of character recognition system for the mixed font style in the steel processing material

  • Lee, Jong-Hak;Park, Sang-Gug;Park, Soo-Young
    • 제어로봇시스템학회:학술대회논문집
    • /
    • 제어로봇시스템학회 2005년도 ICCAS
    • /
    • pp.1431-1434
    • /
    • 2005
  • In the steel production line, the molten metal of a furnace is transformed into billet and then moves to the heating furnace of the hot rolling mill. This paper describes about the development of recognition system for the characters, which was marked at the billet material by use template-marking plate and hand written method, in the steel plant. For the recognition of template-marked characters, we propose PSVM algorithm. And for the recognition of hand written character, we propose combination methods of CCD algorithm and PSVM algorithm. The PSVM algorithm need some more time than the conventional KLT or SVM algorithm. The CCD algorithm makes shorter classification time than the PSVM algorithm and good for the classification of closed curve characters from Arabic numerals. For the confirmation of algorithm, we have compared our algorithm with conventional methods such as KLT classifier and one-to-one SVM. The recognition rate of experimented billet characters shows that the proposing PSVM algorithm is 97 % for the template-marked characters and combinational algorithm of CCD & PSVM is 95.5 % for the hand written characters. The experimental results show that our proposing method has higher recognition rate than that of the conventional methods for the template-marked characters and hand written characters. By using our algorithm, we have installed real time character recognition system at the billet processing line of the steel-iron plant.

  • PDF

9Cr-3W 강의 크리프 특성에 미치는 Mo 첨가의 영향 (Effect of Mo addition on the Creep Properties of 9Cr-3W Steel)

  • 김용래;장진성;김태규
    • 한국주조공학회지
    • /
    • 제33권1호
    • /
    • pp.1-7
    • /
    • 2013
  • The effect of the Mo addition on the high temperature creep properties of the 9Cr-3W steel was also evaluated. Two experimental steels, (9Cr-3W and 9Cr-3W-0.5Mo), were prepared using a vacuum induction melting process, followed by hot rolling and heat treatment processes. Three types of precipitates, ($M_{23}C_6$, Nb-rich MX and V-rich MX) were observed in a typical tempered martensitic matrix. Significant effects of the Mo addition on the tensile properties were not observed. However, the creep properties at $650^{\circ}C$ under applied stresses of 140 and 150 MPa were considerably enhanced by the Mo addition. The microstructural observation after the creep test indicated that the addition of Mo could function to retain the recovery of the martensitic matrix, thus resulting in the enhanced creep properties of the 9Cr-3W-0.5Mo steel. Furthermore coarsening of the $M_{23}C_6$ carbides and formation of Laves phases were observed in both samples after the creep tests.

고강도${\cdot}$고인성의 알루미늄 연속 주조기용 롤쉘 개발 (Development of Roll Shell for Aluminium Continuous Casters of High Strength and High Toughness)

  • 김병훈;박영철;김정태;이우동
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 제5회 압연심포지엄 신 시장 개척을 위한 압연기술
    • /
    • pp.216-222
    • /
    • 2004
  • The caster roll shells have the good thermal conductivity and the low thermal expansion and have to exhibit high enough strength and good ductility at temperature up to $600^{\circ}C$. Thermal stress in particular is very high due to the contact with the liquid aluminium. The main stresses are of thermal origin, which bring a plastic fatigue on surface. This paper will represent one survey about the investigation of the failure of roll shells for continuous casters and an analysis using the simulation of the temperature distribution and the state of stress during hot rolling. Moreover, there will be a discussion on the roll shell of Mod. HAR 5 which is developed by heat treatment process. Mod. HAR 5 has advantages of high strength, high toughness and increased thermal stress resistance while maintaining the same productivity as the conventional roll.

  • PDF

In-Line Trimming Shear 개발 (Development of In-Line Trimming Shear)

  • 이종일;강성구;서경수
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1999년도 제3회 압연심포지엄 논문집 압연기술의 미래개척 (Exploitation of Future Rolling Technologies)
    • /
    • pp.119-125
    • /
    • 1999
  • At Wire Rod Mill Plant, wire is made of the billet produced at continuous casting machine, or rolled bloom produced at billeting mill, and the product can be classified of wire of 5.5${\Phi}$ and bar in coil of 14∼42${\Phi}$ in diameter(bar in coil will be referred to as coil as below). At present, wire is produced at POSCO No.1, 2, 3 WRM, coil at garret line of No. 2 WRM. Head and tail of coil are properly cut and treated to scrap to fulfill the customer's satisfaction. This above cutting is done off line, and small size coil can be cut manually with clipper, large size coil with hydraulic cutter. Nowadays, it is being investigated to cut automatically in line with trimming shear after passing mill stand. At the moment, Because the coil produced at the garret line of No.2 WRM is hot 400∼600$^{\circ}C$ and trimming is done manually with cutter, there are always interference from manual operation or safety problem of bad working condition. Not only because of the diversity of the coil size 14∼42${\Phi}$ in diameter, but because of the rolling speed 2.5∼22m/sec, it is required to be equipped with several trimming shear. But this can be accomplished with only one shear installed proper place at this paper.

  • PDF

루버를 이용한 대형공장 내부 자 연환기유동 개선에 관한 연구 (Improvement for Natural Ventilation Flow inside a Large Factory Building Using Louver-t ype Ventilator)

  • 강종훈;이상준
    • 한국전산유체공학회:학술대회논문집
    • /
    • 한국전산유체공학회 2008년도 춘계학술대회논문집
    • /
    • pp.705-706
    • /
    • 2008
  • When heat generated inside a large factory building is not discharged due to a stagnant flow, the working environment of workers becomes worse and the cooling of high-temperature products such as hot-rolling coils is delayed. To investigate the natural ventilation inside a large factory building, experimental studies were carried out using wind-tunnel tests. The scale-down factory building models were placed in an atmospheric boundary layer (ABL) and the mean and fluctuating velocity fields were measured using a particle image velocimetry (PIV) technique. For the prototype factory model, the outdoor air is only entrained into the factory building through the one-third open windward wall, and stagnant flow is formed in the rear part of the target area. In order to improve the indoor ventilation environment of the factory building, three different louver-type ventilators were attached at the upper one-third open windward wall of the factory model. Among the three louver ventilators tested in this study, the ventilator model #3 with the outer louver (${\theta}_o$ = 90$^{\circ}$) and the inner louver (${\theta}_i$ = -70$^{\circ}$) was found to improve the natural ventilation inside the factory building model effectively. The flow rate of the entrained air was increased with aligning the outer louver blades with the oncoming wind and guiding the entrained air down to the ground surface with elongated inner louver blades.

  • PDF

9mm 합금타이타늄 중간 선재 연구 (A Study on The Φ 9mm Titanium Alloy Wire)

  • 김상연
    • 한국산학기술학회논문지
    • /
    • 제13권1호
    • /
    • pp.8-13
    • /
    • 2012
  • Ti-3Al-2.5V 잉고트를 제작하고 직경 9mm 합금타이타늄 wire로 가공하여 수입소재와 비교하여 그 특성을 조사하였다. 잉고트는 산소함량이 0.11wt%이고 철 함량이 0.085wt%로서 ASTM Gr.9 규격을 만족하였다. 9mm 합금 타이타늄 wire 경도는 225-250Hv로 비슷한 결과를 얻었고, 인장강도는 수입소재가 804MPa이고, 국내 개발품은 734MPa이었다. 연신율은 수입소재가 12%이고 국내 개발품은 22%였다. 직경 400mm 잉고트에서 단조 및 다단 열간 압연공정을 통해 직경 9.0mm 타이타늄합금선재를 제작하는 새로운 제작공정을 개발하였다.

알루미늄캔의 재활용(再活用) 기술현황(技術現況) (The Present Status of Recycling Technology of Aluminum Can)

  • 임차용;강석봉
    • 자원리싸이클링
    • /
    • 제9권2호
    • /
    • pp.3-10
    • /
    • 2000
  • 알루미늄 폐캔은 중요한 재활용 자원으로서 알루미늄 캔용 원소재 판재는 물론 알루미늄의 국내소요량을 전량 수입에 의존하고 있는 우리나라로서는 활용 가능한 알루미늄폐캔의 재활용율을 높여야 하는 것은 외화절약과 환경보호 측면에서 대단히 중요하다. 사용한 알루미늄 캔을 다시 캔으로 재활용 하는 단계는 폐캔의 수집, 파쇄, 선별, 도료제거, 용해 및 2차지금을 제조하는 단계와 이 2차지금을 이용하여 열처리, 열간 및 냉간압연, 중간소둔처리 등을 거쳐 다시 캔을 성형하는 2단계로 나눌수 있다. 본 자료에서는 이러한 알루미늄 캔의 재활용 기술에 대한 우리나라와 선진국들의 현황과 전망을 소개하였다.

  • PDF

분사주조한 Al기지 입자강화 복합재료의 마모특성 (Characterization of Wear Resistance of Particle Reinforced Al Matrix Composite Manufactured by Centrifugal Spray Casting)

  • 배차헌;최학규;방국수
    • 한국주조공학회지
    • /
    • 제24권2호
    • /
    • pp.108-114
    • /
    • 2004
  • $Al_2O_3$, SiC reinforced Al matrix composites were fabricated by centrifugal spray casting method and their wear resistance characteristics have been studied. Particles are generally uniformly distributed in the microstructure of as-cast specimens. In order to investigate the effect of secondary deformation, hot rolling was performed for each specimen of pure Al matrix composites with a reduction of 10, 20, 30, 40 and 50% at $400{\sim}500^{\circ}C$, respectively. Microstructure of specimen showed that particle distribution density and hardness increased because of increasing of reduction ratio. Wear test with a various sliding velocity of 1.98, 2.38, 2.88 and 3.53m/sec showed that the wear resistance characterization of composite improved remarkably compared to the normal alloy and performs without reinforced particles. Microstructural observation for the worn surface of pure Al specimens without particles showed that a change in wear mechanism seemed to separate layer by surface fatigue. In other case of Al composite reinforced with $Al_2O_3$ and SiC, the grinder type of wear mechanism was shown.