• 제목/요약/키워드: Hot isostatic pressing(HIP)

검색결과 53건 처리시간 0.025초

Stellite bearings for liquid Zn-/Al-Systems with advanced chemical and physical properties by Mechanical Alloying and Standard-PM-Route

  • Zoz, H.;Benz, H.U.;Huettebraeucker, K.;Furken, L.;Ren, H.;Reichardt, R.
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2000년도 춘계학술강연 및 발표대회 강연 및 발표논문 초록집
    • /
    • pp.9-10
    • /
    • 2000
  • An important business-field of world-wide steel-industry is the coating of thin metal-sheets with zinc, zinc-aluminum and aluminum based materials. These products mostly go into automotive industry. in particular for the car-body. into building and construction industry as well as household appliances. Due to mass-production, the processing is done in large continuously operating plants where the mostly cold-rolled metal-strip as the substrate is handled in coils up to 40 tons unwind before and rolled up again after passing the processing plant which includes cleaning, annealing, hot-dip galvanizing / aluminizing and chemical treatment. In the liquid Zn, Zn-AI, AI-Zn and AI-Si bathes a combined action of corrosion and wear under high temperature and high stress onto the transfer components (rolls) accounts for major economic losses. Most critical here are the bearing systems of these rolls operating in the liquid system. Rolls in liquid system can not be avoided as they are needed to transfer the steel-strip into and out of the crucible. Since several years, ceramic roller bearings are tested here [1.2], however, in particular due to uncontrollable Slag-impurities within the hot bath [3], slide bearings are still expected to be of a higher potential [4]. The today's state of the art is the application of slide bearings based on Stellite\ulcorneragainst Stellite which is in general a 50-60 wt% Co-matrix with incorporated Cr- and W-carbides and other composites. Indeed Stellite is used as the bearing-material as of it's chemical properties (does not go into solution), the physical properties in particular with poor lubricating properties are not satisfying at all. To increase the Sliding behavior in the bearing system, about 0.15-0.2 wt% of lead has been added into the hot-bath in the past. Due to environmental regulations. this had to be reduced dramatically_ This together with the heavily increasing production rates expressed by increased velocity of the substrate-steel-band up to 200 m/min and increased tractate power up to 10 tons in modern plants. leads to life times of the bearings of a few up to several days only. To improve this situation. the Mechanical Alloying (MA) TeChnique [5.6.7.8] is used to prOduce advanced Stellite-based bearing materials. A lubricating phase is introduced into Stellite-powder-material by MA, the composite-powder-particles are coated by High Energy Milling (HEM) in order to produce bearing-bushes of approximately 12 kg by Sintering, Liquid Phase Sintering (LPS) and Hot Isostatic Pressing (HIP). The chemical and physical behavior of samples as well as the bearing systems in the hot galvanizing / aluminizing plant are discussed. DependenCies like lubricant material and composite, LPS-binder and composite, particle shape and PM-route with respect to achievable density. (temperature--) shock-reSistibility and corrosive-wear behavior will be described. The materials are characterized by particle size analysis (laser diffraction), scanning electron microscopy and X-ray diffraction. corrosive-wear behavior is determined using a special cylinder-in-bush apparatus (CIBA) as well as field-test in real production condition. Part I of this work describes the initial testing phase where different sample materials are produced, characterized, consolidated and tested in the CIBA under a common AI-Zn-system. The results are discussed and the material-system for the large components to be produced for the field test in real production condition is decided. Outlook: Part II of this work will describe the field test in a hot-dip-galvanizing/aluminizing plant of the mechanically alloyed bearing bushes under aluminum-rich liquid metal. Alter testing, the bushes will be characterized and obtained results with respect to wear. expected lifetime, surface roughness and infiltration will be discussed. Part III of this project will describe a second initial testing phase where the won results of part 1+11 will be transferred to the AI-Si system. Part IV of this project will describe the field test in a hot-dip-aluminizing plant of the mechanically alloyed bearing bushes under aluminum liquid metal. After testing. the bushes will be characterized and obtained results with respect to wear. expected lifetime, surface roughness and infiltration will be discussed.

  • PDF

핵융합로부품 시험을 위한 고열부하 시험시설 KoHLT-1 구축 (Development of a High Heat Load Test Facility KoHLT-1 for a Testing of Nuclear Fusion Reactor Components)

  • 배영덕;김석권;이동원;신희윤;홍봉근
    • 한국진공학회지
    • /
    • 제18권4호
    • /
    • pp.318-330
    • /
    • 2009
  • 본 한국원자력연구원에서는 국제열핵융합실험로(ITER)의 일차벽을 개발하기 위해 그라파이트 히터를 이용한 고열부하 시험시설 KoHLT-1(Korea Heat Load Test facility-1)을 구축하였으며, 현재 정상적으로 가동되고 있다. KoHLT-1의 주목적은 Be-CuCrZr-SS의 이종 금속이 HIP 방법에 의해 접합된 ITER 일차벽 mockup의 접합 건전성을 확인하는데 있다. KoHLT-1은 판형 그라파이트 히터, 냉각 jacket이 부착된 상자형 시험용기, 직류 전원, 냉각계통, He 기체 공급계통과 각종 진단계통으로 구성되어 있으며, 이 모든 시설은 Be 처리가 가능한 특수 정화계통이 설치된 실험실에 설치되었다. 그라파이트 히터는 두개의 시험 대상물 사이에 설치되며, 시험대상물과의 거리는 $2{\sim}3\;mm$이다. 시험 대상물의 크기와 요구되는 열유속에 따라 여러 가지의 그라파이트 히터를 설계, 제작하였으며, 전기 저항은 고온 운전 중에 $0.2{\sim}0.5{\Omega}$이 되도록 하였다. 히터는 100V/400 A의 직류전원에 연결되어 있으며, PC와 multi function module로 구성된 전류 조정계통에 의해 미리 프로그램되어 있는 패턴으로 전류를 자동 조절하게 된다. 두 시험대상물에 인가되는 열유속은 calorimetry법에 의해 냉각수의 입, 출구 온도와 유량을 측정하여 얻게 된다. 여러 가지 형태의 ITER 일차벽 Be mockups에 대해 고열부하 시험을 수행하였으며, 시험을 통하여 KoHLT-1 고열부하 시험 시설의 성능이 확인되었고, 24시간 이상의 연속 운전에 있어서도 그 신뢰성이 입증되었다.

핵융합로용 플라즈마 대향부품 개발을 위해 제작된 텅스텐/FM강 HIP 접합 목업의 수명 평가 해석

  • 이동원;신규인;김석권;진형곤;이어확;윤재성;문세연;홍봉근
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2014년도 제46회 동계 정기학술대회 초록집
    • /
    • pp.452-452
    • /
    • 2014
  • 블랑켓 일차벽이나 디버터와 같은 핵융합로 플라즈마 대향부품은 플라즈마로부터 입사되는 중성자 및 입자들을 차폐하여 구조물을 보호하고, 발생열을 에너지로 변환하기 위해 냉각재를 활용한 열제거 기능을 담당한다. 특히, 고속중성자와 입사 열부하 및 여러 입자들로부터 블랑켓 및 내부 구조물을 보호하기 위해 차폐체와 구조물로 구성된다. 세계적으로 차폐체로서는 텅스텐 혹은 텅스텐 합금, 구조물용 재료로는 저방사화 Ferritic Martensitic (FM) 강이 유력한 후보재료로 개발, 연구 중에 있다. 국내에서는 국제핵융합로(ITER) 사업을 통해 고온등방가압(HIP, Hot Isostatic Pressing)을 이용한 이종금속간 접합기술과 한국형 저방사화 고온구조재료인 ARAA (Advanced Reduced Activation Alloy)가 개발되고 있으며, 이를 활용한 설계, 접합법 개발, 제작목업의 건전성 평가 등이 수행되고 있다. 한국원자력연구원에서는 핵융합 기초사업의 일환으로 전북대와 공동으로 수행 중인 건전성 평가체계 개발을 위해, 기 개발된 접합법을 활용한 $45mm(H){\times}45mm(W){\times}2mm(T)$의 W/FM강 목업을 제작한 바 있으며, 이를 국내 구축된 고열부하 시험 장비인 KoHLT-EB (Electron Beam)를 활용한 고열부하 인가 건전성 평가시험을 준비 중에 있다. 이종금속간 접합 특성은 기계적 평가를 위한 파괴시험을 통해 검증, 이를 활용한 목업이 제작되었으며, 제작된 목업에 대한 초음파를 이용한 접합면의 비파괴 검사를 통해 결함이 없음을 확인하였다. 최종적으로 실제 사용되는 핵융합 운전조건과 유사 혹은 가혹한 조건에서 고열부하를 인가하여, 그 건전성을 평가가 이루어질 것이다. 고열부하 시험을 위해서는 냉각조건, 인가 열부하, 수명평가를 통한 반복 고열부하 인가 횟수 등이 사전에 결정되어야 한다. 이를 위해 상업용 열수력, 구조해석 코드인 ANSYS-CFX와 -mechanical을 이용한 시험조건 모의 및 수명 평가가 수행되었다. 구축 장비의 냉각계통을 고려하여 냉각수의 온도 및 속도는 $25^{\circ}C$, 0.15 kg/sec로, 열부하는 0.5 및 $1.0MW/m^2$에 대해 모의를 수행하였다. 정상상태 시 텅스텐의 최대 온도는 각 열부하 조건에 따라 $285.3^{\circ}C$$546.8^{\circ}C$였으며, 이에 도달하는 시간을 구하기 위해 천이해석을 수행하였고, 이를 통해 30초에 최대온도 95 %이상의 정상상태 온도에 도달함을 확인하였다. 또한, 목업의 초기 온도에 도달하는 냉각시간도 동일한 천이해석을 통해 30초로 가능함을 확인하였고, 최종 시험 조건을 30초 가열, 30초 냉각으로 결정하였다. 결정된 반복 열부하 인가 조건에서 이종금속 접합체가 받는 다른 열팽창 정도에 따른 응력을 계산하여 목업의 수명을 도출하였고, 이를 시험해야 할 반복 횟수로 결정하였다. 각 열부하 조건에 따른 온도조건을 ANSYS-mechanical 코드를 활용하여 열팽창과 이에 따른 접합면의 응력분포로 계산하였다. 0.5 및 $1.0MW/m^2$에 대해, 목업이 받는 최대 응력은 334.3 MPa와 588.0 MPa 였으며, 이 때 텅스텐과 FM강이 받는 strain을 도출하여 물성치로 알려진 cycle to failure 값을 도출하였다. 열부하에서 예상되는 수명은 0.5 및 $1.0MW/m^2$에 대해, 100,000 사이클 이상과 2,655 사이클로 계산되었으며, 시간적 제약을 고려 최종 평가는 $1.0MW/m^2$에 대해, 3,000사이클 정도의 실험을 통해 그 수명까지 접합건전성이 유지되는 지 실험을 통해 평가할 예정이다.

  • PDF