• Title/Summary/Keyword: High-strength resin teeth

Search Result 24, Processing Time 0.023 seconds

Comparative Study on Wear Resistance and Hardness of Several Artificial Resin Teeth (수종의 인공 레진 치아의 마모저항성과 경도에 관한 비교 연구)

  • Choi, Yu-Sung;Lee, Joon-Seok;Cho, In-Ho
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.24 no.2
    • /
    • pp.129-146
    • /
    • 2008
  • The aim of this study was to compare and analyze wear resistance of acrylic resin tooth in denture opposing to different types of restoration materials. Also, it aimed to compare and analyze the hardness of three various types of resin artificial teeth when using five different types of denture detergents. In this study three types of artificial teeth were used. As ordinary acrylic resin tooth $Trubyte^{(R)}Biotone^{(R)}$ (Dentsply, U.S.A.) was used, and as high hardness resin tooth Endura $Posterio^{(R)}$ (Shofu, Japan) and Physio $Duracross^{(R)}$ (Nissin, Japan) were used. To compare wear resistance, gold alloy, dental porcelain, and composite resin were used as opposing restorations. In addition, with three types of resin tooth stated above, five types of denture detergents, which are $Yuhanrox^{(R)}$ (Yuhanclorox, Korea), $Polident^{(R)}$ (Yuhan Co., Korea), $Cidex^{(R)}OPA$ (Johnson & Johnson Medical Co., Korea), $Hexamedin^{(R)}$ (Bukwang Pharm Co., Korea) and Daihan sterile $water^{(R)}$ (Daihan Pharm Co., Korea) were used to compare and analyze the effects denture detergents have on the surface hardness. The results of this study were as follow : 1. When composite resin and dental porcelain were used as the opposing restorations, $Trubyte^{(R)}$ $Biotone^{(R)}$, Endura $Posterio^{(R)}$, Physio $Duracross^{(R)}$ in ascending order showed decrease of cusp height with significant difference (p<0.05). 2. When gold alloy was used as opposing restoration, there was decrease in the cusp height in order of $Trubyte^{(R)}Biotone^{(R)}$, Endura $Posterio^{(R)}$, Physio $Duracross^{(R)}$ and $Trubyte^{(R)}$ $Biotone^{(R)}$ especially showed significant decrease in high cusp height as compared to two other types of artificial tooth (p<0.05). 3. When composite resin, gold alloy and dental porcelain were used as opposing restorations, $Trubyte^{(R)}$ $Biotone^{(R)}$, Endura $Posterio^{(R)}$, Physio $Duracross^{(R)}$ in order decreased greatly in weight and these three materials showed significant difference (p<0.05). 4. Comparing the experiment values, decrease in strength had significant difference in all resin artificial teeth before and after the denture detergents were used (p<0.05). 5. When resin artificial teeth were subsided in $Yuhanrox^{(R)}$, $Cidex^{(R)}OPA$, and $Hexamedin^{(R)}$, $Trubyte^{(R)}$ $Biotone^{(R)}$, Endura $Posterio^{(R)}$, Physio $Duracross^{(R)}$ in order showed decrease in hardness, and $Trubyte^{(R)}$ $Biotone^{(R)}$ especially showed significant high decrease hardness as to other two types of artificial teeth (p<0.05). Therefore, Physio $Duracross^{(R)}$ seems to have superior wear resistance, and together with Endura $Posterio^{(R)}$, it presents excellent hardness as compared to $Trubyte^{(R)}$ $Biotone^{(R)}$. However, since this study is fragmentary, it should be given careful consideration and more study need to be done before making a definitive conclusion.

MICROTENSILE BONDING OF RESIN FIBER REINFORCED POST TO RADICULAR DENTIN USING RESIN CEMENT (레진 시멘트를 이용한 레진 파이버 강화 레진포스트의 치근 상아질에 대한 미세인장결합강도)

  • Kim, Jin-Woo;Yu, Mi-Kyung;Lee, Se-Joon;Lee, Kwang-Won
    • Restorative Dentistry and Endodontics
    • /
    • v.28 no.1
    • /
    • pp.80-88
    • /
    • 2003
  • Object The purpose of this study were to evaluate the microtensile bond strength of resin fiber reinforced post to radicular dentin using resin cement according to various dentin surface treatment and to observe the inter face between post and root dentin under SEM Material and Method A total 16 extracted human single rooted teeth were used. A lingual access was made using a #245 carbide bur in a high-speed handpiece with copious air water spray. The post space was mechanically enlarged using H-file(up to #60) and Gates Glidden bures(#3). This was followed by refining of the canal space using the calbrating drill set provided in ER Dentinpost(GEBR, BRASSELER GmbH&Co. KG). The 16 teeth were randomly distributed into 4 group of 4 teeth. Group 1 teeth had their post space prepared using 10% phosphoric acid as root canal surface treatment agent during 20s. The canal was then rinsed with saline and dried with paper point. Group 2 teeth had their post space prepared using 3% NaOCl as root canal surface treatment agent during 30min. The canal was then rinsed with saline and dried with paper point. Group 3 teeth had their post space prepared using 17% EDTA as root canal surface treatment agent during 1min. The canal was then rinsed with saline and dried with paper point. Group 4 teeth had their post space prepared using 17% EDTA as root canal surface treatment agent during 1min. After rinsing with saline, the canal was rinced 10m1 of 3% NaOCl for 30min. After drying with paper point, the post(ER Dentinpost, GEBR, BRASSELER GmbH&Co. KG) was placed in the treated canals using resin cement. Once the canal was filled with resin cement(Super bond C&B sunmedical co. Ltd.), a lentulo was inserted to the depth of the canal to ensure proper coating of the root canal wall. After 24 hours, acrylic resin blocks($10{\cdot}10{\cdot}50mm$) were made. The resin block was serially sectioned vertically into stick of $1{\cdot}1mm$. Twenty sticks were prepared from each group. After that, tensile bond strengths for each stick was measured with Microtensile Tester. Failure pattern of the specimen at the interface between post and dentin were observed under SEM. Results 1. Tensile bond strengths(meen{\pm}SD$) ) were expressed with ascending order as follows group 4, $12.52{\pm}6.60$ ; group 1, $7.63{\pm}5.83$ ; group 2, $4.13{\pm}2.31$ ; group 3, $3.31{\pm}1.44$. 2. Tensile bond strengths of Group 4 treated with 17% EDTA +3%NaOCl were significant higher than those of group 1, 2 and 3 (p<0.05). 3. Tensile bond strengths of Group 1 treated with 10% phosphoric acid were significant higher than those of group 2 (p<0.05). Tensile bond strengths of Group 4 treated with 17% EDTA +3% NaOCl was significant higher than those of other groups.

A STUDY OF THE EFFECT OF LOW INTENSITY INITIAL LIGHT CURING ON THE BOND STRENGTH OF RESIN RESTORATION (초기 저광도 광중합이 레진 수복물의 결합강도에 미치는 영향에 관한 연구)

  • Han, Mi-Ran;Kwon, Soon-Won;Kim, Jong-Soo
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.28 no.1
    • /
    • pp.45-53
    • /
    • 2001
  • Recently some studies have shown that low light intensity followed by final cure at high light intensity may result in a smaller marginal gap and may be no negative effect on material properties. The purpose of this study was to evaluate the influence of the initial cure with low intensity on the shear bond strength of dentin and the microhardness of composite resin. Twenty intact bovine teeth were prepared for shear bond strength test and each tooth sectioned to three specimens. The specimens were randomly divided into three groups according to the light intensity and curing time as follows; Group I. $450mmW/cm^2$ 40sec Group II. $300mmW/cm^2$ 20sec and $600mmW/cm^2$ 20sec Gropu III. $250mmW/cm^2$ 20sec and $450mmW/cm^2$ 20sec. Samples of each group were restored with light-cured composite resin after dentin bonding and then the shear bond strength of each specimen were measured using universal testing machine. Ten resin specimens per group were prepared. After 24 hours, the Vickers microhardness value was measured at the top and bottom surfaces. The result are as follows; 1. Mean value of low initial intensity groups(II, III) were higher than the control group(I) in shear bond strength, but no significant difference could be found. 2. No significant difference could be found between three groups in microhardness.

  • PDF

Zirconia resin-bonded fixed partial denture in maxillary single-tooth edentulous area: A case report (상악 전치부 단일치 상실 환자에서 지르코니아 레진접착성 고정성 국소의치를 이용한 수복 증례)

  • Rojee Oh;Hee-Won Jang;Na-Hong Kim;Joo-Hyuk Bang;Keun-Woo Lee;Yong-Sang Lee
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.61 no.2
    • /
    • pp.135-142
    • /
    • 2023
  • Resin-bonded fixed partial denture (RBFPD)as known as Maryland bridge is is a well-known conservative method for its minimized invasion of the teeth for an anterior single tooth edentulous area. Despite of its various advantages, RBFPD was not widespread because of its high debonding rates, non-esthetic look or weak structure for material property. Currently, with the introduction of zirconia to dental material for RBFPD, Maryland bridge entered upon a new phase. Zirconia surmounts poor esthetics of metal framework, having proper strength, and overcomes ceramic's structural weakness, being sufficiently esthetic. In this case, edentulous area of maxillary left lateral incisor was restored using zirconia resin-bonded fixed partial denture. Restoration of missing tooth in anterior area was achieved using non-invasive and esthetic prosthesis, then we report this case as satisfactory results were obtained for both the operator and the patient.

Evaluation of Shear Bond Strength and Microleakage of Bulk-fill Resin Composites (Bulk-fill 복합레진의 상아질 전단결합강도 및 미세누출)

  • Lee, Hanbyeol;Seo, Hyunwoo;Lee, Juhyun;Park, Howon
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.42 no.4
    • /
    • pp.281-290
    • /
    • 2015
  • The aim of this study was to evaluate shear bond strength (SBS) of bulk-fill resin composites (RCs) to dentin and their micro-leakage. One high-viscosity bulk-fill RC and 2 low-viscosity bulk-fill RCs were compared with 1 conventional RC. 7thgenerationbondingagentswereused. In order to evaluate SBS values, 40 permanent molars were selected and divided into 4 groups. The bulk-fill RCs were applied in 4 mm thickness, whereas the conventional RC was applied in 2 mm thickness. In order to evaluate micro-leakage, class I cavities ($5{\times}2{\times}4mm$) were prepared in 32 permanent molars. The teeth were divided into 4 groups and restored with resin composites in an increment of 4 mm for the bulk-fill RC and in 2 horizontal increments of 2 mm for the conventional RC. The mean SBS value of conventional RC showed no statistically significant difference when compared with those of low-viscosity bulk-fill RCs. However, the mean SBS value of high-viscosity bulk-fill RC was significantly lower than that of conventional RC (p < 0.05). There were no statistically significant differences in micro-leakage between the 4 groups. For SBS and micro-leakage, the use of low-viscosity bulk-fill RCs might help clinicians simplify the procedure.

Fiber Reinforced Inlay Adhesion Bridge

  • Cho, Lee-Ra;Yi, Yang-Jin;Song, Ho-Yong
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.38 no.3
    • /
    • pp.366-374
    • /
    • 2000
  • FRC/ceromer system provides the clinician with a durable, flexible, and esthetic alternative to conventional porcelain fused to metal crowns. FRC is the matrix which is silica-coated and embedded in a resin matrix. The ceromer material which is a second generation indirect composite resin contains silanized, microhybrid inorganic fillers embedded in a light-curing organic matrix. FRC/ceromer restoration has a several advantages: better shock absorption, less wear of occluding teeth, translucency, color stability, bonding ability to dental hard tissues, and resiliency. It has versatility of use including inlay, onlay, single crown, and esthetic veneers. With adhesive technique, it can be used for single tooth replacement in forms of inlay adhesion bridge. In single tooth missing case, conventional PFM bridge has been used for esthetic restoration. However, this restoration has several disadvantages such as high cost, potential framework distortion during fabrication, and difficulty in repairing fractures. Inlay adhesion bridge with FRC/ceromer would be a good alternative treatment plan. This article describes a cases restored with Targis/Vectris inlay adhesion bridge. Tooth preparation guide, fabrication procedure, and cementation procedure of this system will be dealt. The strength/weakness of this restoration will be mentioned, also. If it has been used appropriately in carefully selected case, it can satisfy not only dentist's demand of sparing dental hard tissue but also patient's desire of seeking a esthetic restorations with a natural appearance.

  • PDF

Full-mouth rehabilitation with CAD/CAM monolithic zirconia in dentinogenesis imperfecta: a case report (상아질 형성 부전증 환자에서 CAD/CAM 단일 구조 지르코니아를 이용한 완전구강회복 증례)

  • Kim, Min-Kyoo;Kim, Sung-Hun;Lee, Jai-Bong;Han, Jung-Suk;Yeo, In-Sung;Ha, Seung-Ryong
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.52 no.4
    • /
    • pp.317-323
    • /
    • 2014
  • Dentinogenesis Imperfecta, with a high incidence rate of 1 : 6 - 8000, is inherited by autosomal dominant genetic transmission. This dental disorder causes discoloration of the teeth and the enamel and dentin show hypoplastic or hypocalcified defects which lead to frequent fractures and rapid attrition. Therefore, timely treatment is necessary for the preservation of the remaining teeth. In this particular case, a 19-year-old patient suffering from Type 1 dentinogenesis imperfecta showed signs of brownish hued teeth with multiple fractures, a loss of vertical dimension, excessive interdental space in the maxillary anterior teeth, and a lack of 5 posterior teeth. To improve the esthetic appearance of the anterior teeth, the vertical dimension was increased. Resin caps were used to alleviate the difficulty of taking an impression of multiple teeth at once. Monolithic zirconia materials used in this case showed high fracture strength and the ability to mask the discoloration of the teeth and therefore, functionally and esthetically favorable results were achieved.

Effect of adhesive hydrophobicity on microtensile bond strength of low-shrinkage silorane resin to dentin (접착시스템의 소수성이 Low-shrinkage silorane resin과 상아질의 미세인장강도에 미치는 영향)

  • Cho, So-Yeun;Kang, Hyun-Young;Kim, Kyoung-A;Yu, Mi-Kyung;Lee, Kwang-Won
    • Restorative Dentistry and Endodontics
    • /
    • v.36 no.4
    • /
    • pp.280-289
    • /
    • 2011
  • Objectives: The purpose of this study was to evaluate ${\mu}TBS$ (microtensile bond strength) of current dentin bonding adhesives which have different hydrophobicity with low-shrinkage silorane resin. Materials and Methods: Thirty-six human third molars were used. Middle dentin was exposed. The teeth were randomly assigned to nine experimental groups: Silorane self-etch adhesives (SS), SS + phosphoric acid etching (SS + pa), Adper easy bond (AE), AE + Silorane system bonding (AE + SSb), Clearfil SE bond (CSE), CSE + SSb, All-Bond 2 (AB2), AB2 + SSb, All-Bond 3 (AB3). After adhesive's were applied, the clinical crowns were restored with Filtek LS (3M ESPE). The 0.8 mm ${\times}$ 0.8 mm sticks were submitted to a tensile load using a Micro Tensile Tester (Bisco Inc.). Water sorption was measured to estimate hydrophobicity adhesives. Results: ${\mu}TBS$ of silorane resin to 5 adhesives: SS, 23.2 MPa; CSE, 19.4 MPa; AB3, 30.3 MPa; AB2 and AE, no bond. Additional layering of SSb: CSE + SSb, 26.2 MPa; AB2 + SSb, 33.9 MPa; AE + SSb, no bond. High value of ${\mu}TBS$ was related to cohesive failure. SS showed the lowest water sorption. AE showed the highest solubility. Conclusions: The hydrophobicity of adhesive increased, and silorane resin bond-strength was also increased. Additional hydrophobic adhesive layer did not increase the bond-strength to silorane resin except AB2 + SSb. All-Bond 3 showed similar ${\mu}TBS$ & water sorption with SS. By these facts, we could reach a conclusion that All-Bond 3 is a competitive adhesive which can replace the Silorane adhesive system.

Comparison of flexural strength and modulus of elasticity in several resinous teeth splinting materials (여러 레진계 치아고정 재료의 굴곡강도 및 탄성계수 비교)

  • Yoo, Je-In;Kim, Soo-Yeon;Batbayar, Bayarchimeg;Kim, Jin-Woo;Park, Se-Hee;Cho, Kyung-Mo
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.32 no.3
    • /
    • pp.169-175
    • /
    • 2016
  • Purpose: Direct splinting material should have high flexural strength to withstand force during mastication and low modulus of elasticity to provide some movement while force applied for relief of stress. The purpose of this study was to compare flexural strength and modulus of elasticity of several resinous splinting materials. Materials and Methods: Four materials; Super-Bond C&B, G-FIX, G-aenial Universal Flo, FiltekTM Z350 XT; were used in this study. Fifteen rectangular bar specimens of each material were prepared. Three-point bending test were performed to determine physical properties. Maximum load at fracture was recorded and flexural strength and modulus of elasticity were calculated. One-way analysis of variance (ANOVA) and Scheffe's tests at a 0.05 level of significance were conducted on all test results. Results: Statistical analysis reveals that Super-Bond C&B had significant low mean value for flexible strength and the other three materials showed no significant difference. For modulus of elasticity, Super-Bond C&B exhibited statistically lower modulus of elasticity. G-FIX presented intermediate result, showing statistically higher modulus of elasticity than Super-Bond C&B but lower than G-aenial Universal Flo and FiltekTM Z350 XT. There was no significant difference on modulus of elasticity between G-aenial Universal Flo and FiltekTM Z350 XT. Conclusion: Using a G-FIX, the newly commercially available splinting material, which shows higher fracture resistance properties comparable to flowable and restorative composite resin and a relatively flexible nature might be a beneficial for stabilizing teeth mobility.

MARGINAL FIDELITY AND FRACTURE STRENGTH OF IPS EMPRESS $2^{(R)}$ CERAMIC CROWNS ACCORDING TO DIFFERENT CEMENT TYPES

  • Cho Hyun-Ok;Kang Dong-Wan
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.40 no.6
    • /
    • pp.545-559
    • /
    • 2002
  • There has been increasing use of IPS Empress $2^{(R)}$ owing to easy fabrication method, high esthetics similar to natural teeth, good marginal accuracy, and sufficient fracture strength. However, in clinical application, although a luting agent and the tooth cementation bonding procedure influence the marginal accuracy and fracture strength restoration, there has been a controversy in the selection of proper luting agent. This study was to measure the marginal fidelites and fracture strength of IPS Empress crowns according to three cement types, Protec $cem^{(R)}$, Variolink $II^{(R)}$ and Panavia $21^{(R)}$. After construction of 12 experimental dies for each group, IPS Empress $2^{(R)}$ crowns were fabricated and luted the metal master die prepartion of the maxillary right premolar. Marginal gaps before cementation and after cementation were measured. Buccal incline on the functional cusp of specimens were loaded until the catastrophic failure and fracture strength was measured. The results of this study were as follows: 1. The range of gap was $34.04{\pm}4.84{\mu}m$ before cementation and $37.88{\pm}5.00{\mu}m$ after cementation, which showed significant difference by paired t-test (p<0.05). The difference in the results from marginal accuracy according to measuring point proved to be not statistically significant by two-way ANOVA test (p>0.05). 2. The difference in the results from marginal accuracy according to three cement types Proved that The Variolink $II^{(R)}$ cement group had the least gap, $35.43{\pm}5.03{\mu}m$, and showed superior marginal accuracy while there existed statistic significance in Protec $cem^{(R)}$ cement group, $39.06{\pm}4.41{\mu}m$ or Panavia $21^{(R)}$ cement group, $39.16{\pm}4.39{\mu}m$ by two-way ANOVA test & multiple range test (p<0.05). 3. The difference in the results from fractures strength testing according to three cement type groups proved to be statistically significant (p<0.05). The Variolink $II^{(R)}$ cement group shows highest fracture strength of $1257.33{\pm}226.77N$, Panavia $21^{(R)}$ cement group has $1098.08{\pm}138.45N$, and Protec $cem^{(R)}$ cement group represents the lowest fracture strength of $926.75{\pm}115.75N$. 4. Three different cement groups of different components showed acceptable marginal fidelity and fracture strength. It is concluded that IPS Empress $2^{(R)}$ crowns luted using Variolink $II^{(R)}$ cement group had stronger fracture strength and smaller marginal gap than the other cement groups. Although Variolink $II^{(R)}$ resin cement seemed acceptable to clinical applications in IPS Empress $2^{(R)}$ system, the IPS Empress $2^{(R)}$ system still requires long-term research due to the lack of data in clinical applications.