• 제목/요약/키워드: High-carbon steel

검색결과 772건 처리시간 0.022초

탄소주강과 경강선재간의 미끄럼 마멸특성 (The Sliding Wear Characteristics of Carbon Steel Castings against High Carbon Steel Wire Rods)

  • 류중북;채영훈;김석삼
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2001년도 제33회 춘계학술대회 개최
    • /
    • pp.319-326
    • /
    • 2001
  • The sliding wear characteristics of carbon steel castings were Investigated using a ball on disk type tester. The experiment was conducted using high carbon steel wire rods as ball material and carbon steel castings as disk material and different operating conditions, at room temperature under a lubrication and dry conditions. The results showed that the carbon steel castings appeared average wear volume Is lowed after annealing under a lubrication conditions and wear curve linear Increased. The specific wear rate of carbon steel castings Increased with wire diameter lubrication and dry also Increased 125 times In Ory. The sliding wear mechanism were Investigated due to fatigue wear lubrications and abrasive wear dries also wire Included fatigue and abrasive wear by plastic flow.

  • PDF

강의 마찰용접에 미치는 탄소당량의 영향

  • 나석주;양영수
    • Journal of Welding and Joining
    • /
    • 제4권3호
    • /
    • pp.32-42
    • /
    • 1986
  • In this study, the influence of carbon equivalents on friction welds of dissimilar steels was investigated. Four types of carbon steels with 10mm diameter were welded to a high-speed tool steel SKH 9. Main experimental results could be summarized as follows (1) Under constant friction pressure, the friction time increased almost linearly with the increasing burn-off length, while the forge length decreased almost linearly. (2) The maximum hardness in carbon steels increased almost linearly with the increasing carbon equivalent, but was much lower than that in the high speed steel. (3) After quenching and tempering of dissimilar steel friction welds, the hardness in carbon steel weldments became similar as that in the base metal, while the hardness in SKH 9 weld was still higher that of the base metal. (4) Relative movement in the friction phae occurred not at the interface of the weldments, but in the high speed steed steel near the interface. (5) For considered material combinations and welding parameters, most of fractures in tension and twisting tests occurred in the base metal. And welds with so high strength could produced in a wide range of welding parameters.

  • PDF

고탄소 연구강의 잠입귀열 방지에 관한 연구 (Study on Prevention of Quench Crack in Martensitic High Carbon Tool Steel)

  • 김학신;방성한;최종술;영형영
    • 한국표면공학회지
    • /
    • 제14권3호
    • /
    • pp.142-150
    • /
    • 1981
  • The present paper clarified mechanism of quench crack formation in high carbon steel dur-ing quenching, and, in order to prevent the quench crack, proposed two basic guides in alloy design of high carbon tool steel. They are to raise Ms temperature of high carbon tool steel by addition of alloying elemen-ts such as Al and Co, and to decrease grain size of the carbon tool steel by addition of alloying elements of Al, B, Ti, Zr, and V, and by grain-refining heat treatment.

  • PDF

신선가공조건에 따른 고탄소강 선재 Pearlite 층상구조의 유한요소해석 (FEM analysis of Pearlite Lamella Structure of High Carbon Steel on Drawing Process Conditions)

  • 김현수;배철민;이충열;김병민
    • 대한기계학회논문집A
    • /
    • 제29권2호
    • /
    • pp.325-332
    • /
    • 2005
  • This paper presents a study on defects in pearlite lamella structure of high carbon steel by means of finite-element method(FEM) simulation. High carbon pearlite steel wire is characterized by its nano-sized microstructure feature of alternation ferrite and cementite. FEM simulation was performed based on a suitable FE model describing the boundary conditions and the exact material behavior. Due to the lamella structure in high carbon pearlite steel wire, material plastic behavior was taken into account on deformation of ferrite and cementite. The effects of many important parameters(reduction in area, semi-die angle, lamella spacing, cementite thickness) on wire drawing process can be predicted by DEFORM-2D. It is possible to obtain the important basic data which can be guaranteed in the ductility of high carbon steel wire by using FEM simulation.

탄소강재(炭素鋼材)의 작은 표면결함(表面缺陷)에서 성장(成長)하는 표면피로(表面疲勞)균열의 성장특성(成長特性)에 관한 연구(硏究) (A Study on Growth Characteristics of the Surface Fatigue Crack Propagated from a Small Surface Defect in Carbon Steels)

  • 서창민;강용구
    • 대한조선학회지
    • /
    • 제21권1호
    • /
    • pp.35-42
    • /
    • 1984
  • In the present study, rotating bending fatigue tests have been carried out in three kinds of carbon steel specimens; an annealed low carbon steel, an annealed high carbon steel and quenched-tempered high carbon steel; with a small artificial surface defect that might exist in real structures. Fatigue crack lengths have been observed by a method of replication in order to investigate the growth characteristic of fatigue crack in the viewpoints of strength of materials and fracture mechanics. The main results obtained are as follows: 1) The effect of a small surface defect upon the reduction of fatigue limit is considerably large, and the rate of fatigue limit reduction grows in the following order; annealed low carbon steel(mild steel), annealed high carbon steel, quenched-tempered high carbon steel. 2) When the growth rate of surface crack length(2a) was investigated in the viewpoints of fracture mechanics based upon $ ${\Delta}K_{\varepsilon}$, the dependence of stress level and of surface defect size disappear, and there exists a linear relationships between d(2a)/dN and ${\Delta}K_{{\varepsilon}t},\;\Delta_{{\varepsilon}t}\sqrt{{\pi}a}$, on log. plot, i.e, $d(2a)/dN={C{\cdot}{\Delta}K_{\varepsilon}}^3_t$, where ${\Delta}_{{\varepsilon}t}\sqrt{{\pi}a}$ a is the cyclic total strain intensity factor range.

  • PDF

Neutron Radiography를 이용한 고탄소흑연강에서 붕소 분석 (Boron Analysis in High Carbon Graphitized Steel using Neutron Autoradiography)

  • 우기도;양창호;박희찬;이창희;심철무;장진성;김현경
    • 한국재료학회지
    • /
    • 제11권12호
    • /
    • pp.1074-1079
    • /
    • 2001
  • To study the distribution of boron and the boron effect for nucleation of graphite in high carbon steel, neutron induced autoradiography method is used. High carbon steel is easy to make the graphitization by addition of boron. It is easy to analysis of boron distribution using neutron radiography with neutron fluence of $1.9$\times${\times}10^{13}/cm^2$in the boron added high carbon steel. By the neutron induced autoradiography technique, it was found that the distribution of boron depended on boron content, graphitiging temperature and time. And by the analysis of secondary ion mass spectroscopy (SIMS) and electron probe micro analysis (EPMA), boron or boride were acted at nucleation site of graphite in high carbon steel.

  • PDF

일부실시 직교배열 실험설계에 의한 고성능 하이브리드 섬유보강 콘크리트 배합 최적화 (Optimum mixture of high performance hybrid fiber reinforced concrete using fractional experimental design by orthogonal array)

  • 박대효;노명현;박춘근
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2004년도 추계 학술발표회 제16권2호
    • /
    • pp.341-344
    • /
    • 2004
  • In the present research, slump, modulus of rupture (MOR) and flexural toughness $(I_{30})$ of high performance hybrid fiber reinforced concrete (HPHFRC) mixed with micro-fiber (carbon fiber) and macro-fiber (steel fiber) and replaced with silica fume were assessed with the analysis of variance (ANOVA). Steel fiber was a considerable significant factor in aspect of the response values of MOR and boo Based on the significance of factors related to response values from ANOVA, following assessments were available; Slump decrease: carbon fiber >> steel fiber > silica fume; MOR: steel fiber > silica fume > carbon fiber; $I_{30}$: steel fiber > carbon fiber > silica fume. Steel fiber $1.0\%$, carbon fiber $0.25\%$ and silica fume $5.0\%$, and Steel fiber $1.0\%$, carbon fiber $0.25\%$ and silica fume $2.5\%$ were obtained as the most optimum mixture.

  • PDF

탄소주강품과 경강선재간의 미끄럼 마멸특성 (The Sliding Wear Characteristics of the Carbon Steel Castings against High Carbon Steel Wire Rods)

  • 류중북;채영훈;김석삼
    • Tribology and Lubricants
    • /
    • 제19권4호
    • /
    • pp.223-229
    • /
    • 2003
  • The sliding wear characteristics of the crane sheave were investigated using a pin-on-disk rig tester. The experiment was conducted using a high carbon steel wire that was upper material, also carbon steel castings that was disk material. There are various operating conditions in this work. At the room temperature, we carried out the wear test under a grease lubrication and dry condition. The results of wear test showed that an annealed-casted have lower, also the wear curves are linearly increased with increasing of sliding distance. For the specific wear rate of annealed-casted, the wear resistance was increased with decreasing diameter of wire. The wear of a wire and a disk have a different mechanism, the one is the abrasive wear due to fatigue wear under lubrication, another is the adhesion wear under dry condition.

선급용 고장력강 FSW접합부의 미세조직 및 기계적 성질 (Microstructures and Mechanical Properties of Friction Stir Welded High Strength Steels far Shipbuilding)

  • 장웅성;최기용
    • Journal of Welding and Joining
    • /
    • 제20권3호
    • /
    • pp.67-73
    • /
    • 2002
  • In an attempt to evaluate the feasibility of friction stir welding(FSW) for joining carbon steels, microstructures and mechanical properties of friction stir welded carbon steels with different grain structures were investigated. In comparison of O-type stir zone(SZ) appeared in various aluminium alloys, configuration of SZ in friction stir welded carbon steels displayed U-type. Plastically deformed pearlite band structure was identified to surround the SZ, indicating the existence of so-called thermo-mechanically affected zone(TMAZ). However, the TMAZ of carbon steels was much narrower than that of Al alloys. The microstructures of both stir zone and TMAZ revealed bainite matrix in a conventional carbon steel for shipbuilding, while, in the same region, ferrite matrix microstructures were formed in a low carbon fine grained steel. The conventional carbon steel showed superior stirring workability to that of the fine grained carbon steel. The yield and tensile strength of the friction stir welded joints were comparable to those of the base metals, and the elongation in welded joints demonstrated excellent ductility. Absorbed energy in SZ of the fine grained carbon steel was ten times higher than that obtained from conventional submerged arc weld metal of the same steel. Based on these results, the application FSW to carbon steels was found to be feasible.

Constitutive Relation of Alloy Steels at High Temperatures

  • Lee, Young-Seog
    • International Journal of Precision Engineering and Manufacturing
    • /
    • 제6권4호
    • /
    • pp.55-59
    • /
    • 2005
  • This paper presents a feasibility study whether Shida's constitutive equation being widely used for plain carbon steel in steel manufacturing industry can be extended to alloy steels with a due carbon equivalent model. T,he constitutive relation of the alloy steels (SAE9254, AISI52100 and AISI4140) is measured using hot deformation simulator (GLEEBLE 3500C) at high temperatures ($800^{\circ}C{\~}1000^{\circ}C$) within strain rates of $0.05{\~}40\;s^{-1}$. It has been found the predicted flow stress behavior (constitutive relation) of AISI52100 steel is in agreement with the measured one. On the other hand, the measured flow stress behavior of SAE9254 and AISI4140 steel partly concords with the predicted one when material experiences relatively high strain rate ($10{\~}40\;s^{-1}$) deformation at low temperature ($800^{\circ}C$). It can be deduced that, for AISI52100 steel, Shida's equation with the carbon equivalent model can be applicable directly to the roughing and intermediate finishing stand in hot rolling process for calculating the roll force and torque.