• 제목/요약/키워드: High velocity oxy-fuel (HVOF)

검색결과 21건 처리시간 0.025초

HVOF 용사총의 기체역학에 관한 연구 (A Study of Gas Dynamics of the High-Velocity Oxy-Fuel Thermal Spray Gun)

  • 조필재;김희동
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2003년도 추계학술대회
    • /
    • pp.574-579
    • /
    • 2003
  • The present study addresses an analytical investigation to understand the characteristics of gas flow in the High-Velocity Oxy-Fuel(HVOF) thermal spray gun. One-dimensional analysis is extended to involve the effects of the wall friction and powder particle diameter. From the present analysis it is well known that the flow characteristics inside and outside the thermal spray gun is varied depending on the combustion chamber pressure. The thermal spray gun flow is characterized by six different patterns. The powder particle size and wall friction significantly influence the powder particle velocity. The particle velocity decreases with an increase in the powder particle size. This implies that the combustion chamber pressure should be increased to achieve a higher velocity of the powder particle.

  • PDF

실링재 및 실링방법이 HVOF 용사된 CrC-NiCr 코팅의 내식성에 미치는 영향 (Effect of Sealing Materials and Parameters on the Corrosion Resistance of HVOF-Sprayed CrC-NiCr Coatings)

  • 정영훈;남욱희;변응선;강태일;강정윤
    • 한국표면공학회지
    • /
    • 제47권6호
    • /
    • pp.323-329
    • /
    • 2014
  • Effects of sealant and sealing procedure on corrosion resistance of high velocity oxy-fuel (HVOF) sprayed coatings were studied. HVOF-sprayed CrC-20NiCr coatings were sealed using three commercial sealants based on phenolics and epoxy. Penetration depth of sealants, measured by fluorescent microscope technique, was between $19{\mu}m$ and $340{\mu}m$ depending on sealant, sealing condition or sealing procedure. It was found that sealing on rotation status was more effective than that on stationary specimen due to the Coriolis effect of fluid in pores of the coating. From the CASS results, corrosion resistance of properly sealed CrC-20NiCr coatings was equal to that of hexa-valent chromium plating.

HVOF 용사된 NiCoCrAlY 코팅의 산호막 관찰 (Microstructural Observation of Scales formed on HVOF-sprayed NiCoCrAlY Coatings)

  • 고재황;이동복
    • 한국재료학회지
    • /
    • 제14권2호
    • /
    • pp.110-114
    • /
    • 2004
  • High velocity oxy-fuel sprayed NiCoCrAlY coatings were oxidized between 1000 and $1200^{\circ}C$ in air, and the oxide scales were examined by XRD, SEM/EDS, and EPMA. The unoxidized coatings consisted mainly of ${\gamma}$'$-Ni_3$Al, with some ${\gamma}$-Ni. The major oxide formed on the coatings was $\alpha$ $-Al_2$$O_3$. Additionally, (CoCr$_2$$O_4$, $CoAl_2$$O_4$) spinels and $Al_{5}$ $Y_3$$O_{12}$ coexisted. NiO was not found, despite of high amount of Ni in the coating. Below the oxide layer, internally formed $Al_2$$O_3$ existed.

노즐 형상변화에 따른 HVOF 용사총에서의 유동특성에 관한 수치적 연구 (A Numerical Study on Flow Characteristics in HVOF Thermal Spray with Various Torch Shapes)

  • 백재상;김윤제
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2007년도 춘계학술대회B
    • /
    • pp.3062-3067
    • /
    • 2007
  • HVOF thermal spray guns are now being widely used to produce protective coatings, on the surfaces of engineering components. HVOF technology employs a combustion process to heat the gas flow and melt the coating materials which are particles of metals, alloys or cermets. Particle flow which is accelerated to high velocities and combustion gas stream are deposited on a substrate. In order to obtain good quality coatings, the analysis of torch design must be performed. The reason is that the design parameters of torch influence gas dynamic behaviors. In this study, numerical analysis is performed to predict the gas dynamic behaviors in a HVOF thermal spray gun with various torch shapes. The CFD model is used to deduce the effect of changes in nozzle geometry on gas dynamics. Using a commercial code, FLUENT which uses Finite Volume Method and SIMPLE algorithm, governing equations have been solved for the pressure, velocity and temperature distributions in the HVOF thermal spray torch.

  • PDF

Ti(Al,O)/$Al_2O_3$ 플라즈마 코팅한 SS41의 고온산화 거동 (High Temperature Oxidation Behavior of Plasma-sprayed Ti(Al,O)/$Al_2O_3$ Coatings on SS41 Steel)

  • 최갑송;우기도;이현범;전재열
    • 열처리공학회지
    • /
    • 제20권5호
    • /
    • pp.231-236
    • /
    • 2007
  • High velocity oxy-fuel (HVOF) spraying was used to coat Ti(Al,O)/$Al_2O_3$ powder onto the SS41 steel plate. Macrostructure of the coated specimen has been investigated by scanning electron micrograph (SEM). High temperature oxidation behavior of the coated specimen and SS41 steel have been studied. From the results of SEM observation, Ti(Al,O)/$Al_2O_3$ powder was coated well onto the substrate SS41 steel. Porosity onto the coated layer was only 0.38%. The oxidation results showed that Ti(Al,O)/$Al_2O_3$ powder coated SS41 steel have improved little oxidation resistance at $900^{\circ}C$ in air, but improved remarkably oxidation resistance at $800^{\circ}C $ in air compare to the substrate SS41 steel.

분무건조법에 의한 용사용 WC-17%Co 복합분말제조 및 HVOF(High Velocity Oxy-Fuel) 용사특성 (Fabrication of WC-17%Co Composite Powder for Thermal Spray by Spray-Drying Method and HVOF Thermal Spray Characteristics)

  • 설동욱;김병희;임영우;정민석;서동수
    • Journal of Welding and Joining
    • /
    • 제14권6호
    • /
    • pp.101-108
    • /
    • 1996
  • In this study, WC-l7wt% Co composite powder for thermal spray was fabricated by spray drying method. The agglomerated composite powder had spheroidal morphology and the particle size distribution was 20~60${\mu}{\textrm}{m}$. WC and Co were distributed homogeneously. However, the strength of the spray-dried agglomerate was low due to the pores within the agglomerate. Therefore, the spray-dried agglomerate was broken down during HVOF thermal spray and the microstructure was inhomogeneous with many pores within the coating layer. And the decomposition of WC to W and $W_{6}$ $C_{2.54}$ was accelerated. The strength and flowability of the agglomerate were greatly improved by sintering heat treatment(110$0^{\circ}C$, 1 hour, hi atmosphere), and then the coating layer showed dense and homogeneous microstructure with well-developed splats. The hardness of the coating layer was H $v_{300}$ = 1072.2.2.

  • PDF

HVOF용사 코팅한 SM490B 코팅층의 미시조직 특성 (The Micro Structure Characteristics of Coating Layer on SM490B with HVOF Coating)

  • 남기수;조원익;윤명진;김병문
    • 한국공작기계학회논문집
    • /
    • 제14권5호
    • /
    • pp.80-86
    • /
    • 2005
  • High velocity oxy-fuel thermally sprayed coating of the WC-Co cermet material is a well-established process for modifying the surface properties of the structural components exposed to the corrosive and wear attacks. The hard WC phase in the coating resists to the wear while the soft metallic Co increases the adhesive and cohesive bonding properties. The coating properties deposited by the HVOF process are greatly dependent on the feedstock materials and processing parameters. The effects of the feedstock material and process coating parameters including the in-flight particle parameters and resultant coating microstructures were observed in this paper.

A comparative study on corrosion behavior of WC-CoCr and WC-CrC-Ni coatings by HVOF

  • 주윤곤;조재영;장시홍;송기오;조동율;윤재홍
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2008년도 추계학술대회 초록집
    • /
    • pp.155-157
    • /
    • 2008
  • High velocity oxy-fuel (HVOF) thermal spraying coating has been used widely throughout the last 60 years mainly in defense, aerospace, and power plants. Recently this coating technique is considered as a promising candidate for the replacement of the traditional electrolytic hard chrome plating (EHC) which pollutes the environment and causes lung cancer by toxic hexa-valent $Cr^{6+}$. In this study, two kinds of cermet coatings, WC-CoCr and WC-CrC-Ni, are formed by HVOF spraying. The corrosion and electrochemical properties are evaluated by polarization tests in 3.5 wt% solutions.

  • PDF

유압실린더 세라믹코팅 기공률 최소화 방안 (Minimization of Porosity in Ceramic Coating on a Hydraulic Cylinder)

  • 정영호;문승재;유호선
    • 플랜트 저널
    • /
    • 제6권4호
    • /
    • pp.63-71
    • /
    • 2010
  • The best way to prevent the corrosion of piston rod is a selection of quality of the material and method of construction which minimize the porosity. The high velocity oxy fuel(HVOF) method, which generates lower porosity than existing plasma spray, was applied to ceramic laminated bond layer. Porosity percentage fell to bellow 2%, lower than that of plasma spray at 7%. Coating material of ceramic-coated main layer was selected as the $Cr_2O_3$ affiliation material, which is more dense than $Al_2O_3$ affiliation. To fill up the pores formed after the coating process, we sealed the bond layer and main layer. Sealing process was performed twice, once after the coating and once after the grinding. Upon the anti-corrosion test on the sealed sample and on the non-sealed sample, it is confirmed that the sealed sample was not corroded for 1,000 hours while the non-sealed sample was corroded within 48 hours.

  • PDF