High Temperature Corrosion in Carbon-Rich Gases

  • Young, D.J.
    • Corrosion Science and Technology
    • /
    • v.7 no.2
    • /
    • pp.69-76
    • /
    • 2008
  • Common methods for large scale hydrogen production, such as steam reforming and coal gasification, also involve production of carbonaceous gases. It is therefore necessary to handle process gas streams involving various mixtures of hydrocarbons, $H_2$, $H_2O$, CO and $CO_2$ at moderate to high temperatures. These gases pose a variety of corrosion threats to the alloys used in plant construction. Carbon is a particularly aggressive corrodent, leading to carburisation and, at high carbon activities, to metal dusting. The behaviour of commercial heat resisting alloys 602CA and 800, together with that of 304 stainless steel, was studied during thermal cycling in $CO/CO_2$ at $650-750^{\circ}C$, and also in $CO/H_2/H_2O$ at $680^{\circ}C$. Thermal cycling caused repeated scale separation, which accelerated chromium depletion from the alloy subsurface regions. The $CO/H_2/H_2O$ gas, with $a_C=2.9$ and $p(O_2)=5\times10^{-23}$ atm, caused relatively rapid metal dusting, accompanied by some internal carburisation. In contrast, the $CO/CO_2$ gas, with $a_C=7$ and $p(O_2)=10^{-23}-10^{-24}$ atm caused internal precipitation in all three alloys, but no dusting. Inward diffusion of oxygen led to in situ oxidation of internal carbides. The very different reaction morphologies produced by the two gas mixtures are discussed in terms of competing gas-alloy reaction steps.

Creep Damage Evaluation of High Temperature Material Using Small Punch Test Method (소형펀치실험법을 이용한 고온재료의 크리프 손상 평가)

  • Yu, Hyo-Sun;Lee, Song-In;Baek, Seung-Se;Na, Sung-Hun
    • Proceedings of the KIEE Conference
    • /
    • 2000.11a
    • /
    • pp.265-268
    • /
    • 2000
  • In this study, a small punch creep (SP-Creep) test using miniaturized specimen has been described for the development of the new creep test method for high temperature structural components such as headers and tubes of boiler, turbine casing and rotor, and reactor vessel. The SP-Creep testing technique has been applied to 1Cr-0.5Mo steel used widely as boiler header material and the creep test temperature are varied at $550^{\circ}C{\sim}600^{\circ}C$. From the experimental results, e.g. SP-Creep curve behaviors, the creep rate in steady state and creep rupture life with test temperature and load, the load exponential value(n, m), the activation energy($Q_{spc}$), the Monkman-Grant relation and the creep life assessment equation etc., it can be summarized that the SP-Creep test may be a useful test method to evaluate the creep properties of the heat resisting material such as boiler header.

  • PDF

Determination of Preheating Temperature for Box Girder Welding (강교용 박스거더의 용접예열 온도 선정에 관한 연구)

  • Cho, Jae-Hun;Moon, Seung-Jae;Yoo, Hoseon
    • Plant Journal
    • /
    • v.7 no.1
    • /
    • pp.49-55
    • /
    • 2011
  • This study analyzed causes and status of cracks to suggest preventives for welding cracks generated on fillet welding zone of atmosphere corrosion resisting steel box girder. Penetrant testing, a sort of non-destructive testing, was conducted for inspection of crack status on welding zone. As a result of test, welding cracks were found on the point of start, center and end to fillet welding zone of 32 mm-thickness. The result of carbon equivalent composition of materials was 0.452%. According to welding specification, to preheat prevent welding crack, preheat temperature of $100{\sim}200^{\circ}C$ should be kept before welding execution. It was failed to keep preheat temperature because it had been executed on winter season and the structure of box girder had wide heat transfer area. As a result of examination of time varying preheating temperature of 32mm-thickness material, it was understood that preheat temperature of above $230^{\circ}C$ on both 130mm-long sides of welded joint can prevent welding crack.

  • PDF

A Study on Resisting Force of H-Shaped Beam Using Glass Web Plate (유리 웨브를 사용한 H형 합성보의 내력에 관한 연구)

  • Son, Ki-Sang;Jeon, Chang-Hyun
    • Journal of the Korean Society of Safety
    • /
    • v.21 no.3 s.75
    • /
    • pp.73-80
    • /
    • 2006
  • Generally beam design depends on the yielding and maximum strength of each member varying with its section shape. Web plate of H-shape beam has not been substituted with glass plate, because it is known that its strength and heat properties are different and it is limited to substitute the existing steel web with glass element. Ceiling height of each room should be decreased with more than 60-80cm due to the beam. Differently from this condition, glass web beam has a good point to see through it and sunshine can be penetrate into the other size especially when it is installed as of outside wall. And also, it can be safer due to controlling room inside easier, if the strength is applicate. This study is to show some applicability after finding out the properties using the test. The test members with a size of $1,600{\times}200{\times}300{\times}9mm$ being SS41 rolled steel having THK 9mm flange while having 8,10mm and reinforced glass 12mm thickness is bonded with epoxy bond under the condition of temperature $28^{\circ}C$, humidity 50%, bonding power 24Mpa. It is show reinforced glass has 5 times of fracture stress more than the common glass but $50{\sim}150%$ difference between these 2 kinds of glass was shown. Reinforce glass did not support the original upper flange after fracture but the common glass did the upper flange after unloading. Generally reinforced glass is stronger than the common one but the common glass having a part of crack on it, compared with reinforced glass having the overall fracture could be more useful in case of needing ductility.

Degradation Degree Evaluation of Heat Resisting Steel by Electrochemical Technique Part 2 : Effect of Testing Conditions on Evaluation Value of Degradation Degree and Changes of Mechaical Properties (전기화학적 방법에 의한 내열강의 열화도측정 제2보 : 열화도측정치에 미치는 측정조건들의 영향과 기계적성질 변화에 대해서)

  • 정희돈;권영각;장래웅
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.17 no.2
    • /
    • pp.300-312
    • /
    • 1993
  • The material deterioration of service-exposed boiler tube steels in fossil power plant was evaluated by using the electrochemical technique namely, modified electrochemical potentiokinetic reactivation(EPR). It was focused that the passivation of Mo$_{6}$C carbide which governs the mechanical properties of Mo alloyed steels did not occur even in the passivity region of steel in sodium molybdate solution and the reactivation peak current (Ip) observed as the result of non-passivation indicating the precipitation of Mo$_{6}$C carbides. To obtain the optimal test conditions for the field test by using the specially designed electrochemical cell, the effects of scan rate, the surface roughness and the pH of electrolyte on Ip value were also investigated. Furthermore, the change of mechanical properties occurred during the long time exposure at high temperature was evlauated quantitatively by small punch(SP) tests and micro hardness test taking account of the metallurgical changes. It is known that reactivation peak current (Ip) has a good relationship with Larson-Miller Parameter(LMP) which represents the information about material deterioration occurred at high temperature environment. In addition it was possible to estimate the ductile-brittle transition temperature (DBTT) by means of the SP test. The Sp test could be, therefore, suggested as a reliable test method for evaluating the material degradation of boiler tube steels. From the good correaltion between the SP DBTT and Ip values shown in this study, it was knows that the change of mechanical properties could be evaluated non-destructively by measurring only Ip values.ues.

Development of High Temperature Creep Properties Evaluation Method using Miniature Specimen (미소시험편을 이용한 고온 크리프 특성 평가법 개발)

  • Yu, Hyo-Sun;Baek, Seung-Se;Lee, Song-In;Ha, Jeong-Soo
    • Proceedings of the KSME Conference
    • /
    • 2000.04a
    • /
    • pp.43-48
    • /
    • 2000
  • In this study, a small punch creep(SP-Creep) test using miniaturized specimen$(10{\times}10{\times}0.5mm)$ has been described for the development of the newly semi-destructive creep test method for high temperature structural components such as headers and tubes of boiler turbine casino and rotor and reactor vessel. The SP-Creep testing technique has been applied to 2.25Cr-1Mo(STBA24) steel used widely as boiler tube material and the creep test temperature are varied at $550^{\circ}C{\sim}600^{\circ}C$. The overall deformations of SP-Creep curves are definitely depended with applied load and creep test temperature and show the creep behaviors of three steps like conventional uniaxial creep curves. The steady state creep rate${\delta}_{ss}$ of SP-Creep curve for miniaturized specimen increases with increasing creep temperature, but the exponential value with creep loading is decreased. The activation energy$(Q_{spc})$ during SP-Creep deformation with various test temperatures shows 605.7kJ/mol that is g.eater than 467.4kJ/mol reported in uniaxial creep test. This may be caused by the difference of stress states during creep deformation In two creep test. But from the experimental results, e.g. SP-Creep curve behaviors, the steady state creep rate${\delta}_{ss}$ with creep temperature, and the exponential value(n) with creep loading, it can be summarized that the SP-Creep test may be a useful test method to evaluate the creep properties of the heat resisting material.

  • PDF

An Experimental Study on Friction Welding and Heat Treatment of Engine Exhaust Valve Steels ( SCr4-21-4 N , SUH3-21-4-N (기관배기 밸브용 강 ( SCr4-21-4N , SUH3-21-4N ) 의 마찰압접과 열처리에 관한 실험적 연구)

  • 오세규
    • Journal of the Korean Society of Fisheries and Ocean Technology
    • /
    • v.14 no.2
    • /
    • pp.79-87
    • /
    • 1978
  • This is an experimental study on friction welding and heat treatment of engine exhaust valve materials whose welding combination is SCr4 as stem to 21-4N as head and SUH3 to 21-4N. In this study, not only the experiments of friction welding under the selected optimum welding condition and the examination of the mechanical properties were carried out, but also the heat treatment of friction welded specimens under the two selected conditions was taken to obtain the better welding character, eliminating the latent stress and the hardness peak which appeared at the welded zones of heat resisting steel(21-4N, SUH3) and low alloyed steel ($SCr_4$) friction weldments. The results obtained by the experiments and consideration in this study are as follows: I) It was experimentally proved quite reasonable that 'speed=3,OOO rpm, heating pressure Pl=8 kg/ mm2, upsetting pressure p, = 20 kg/mm', heating time $t_1$ = 3 see, upsetting time TEX>$t_2$ = 2.5 sec' was selected as the optimum welding condition for friction-welding the engine exhaust valve materials $SCr_4$ to 21-4 Nand SUH 3 to 21-4 N. 2) The results of the previous study and this one on friction welding of such dissimilar materials as SUH 3-SUH 31, SCr 4-SUH 31, SCr 4-SUH 3, SUH 3-CRK 22, SCr4-21-4 Nand SUH3-21-4 N agreed with each other substantially in the friction welding characteristics at welded interface zones. 3) It was also certified quite satisfactory that '600\ulcornerCX30 min. Xroom air cooling' as an optimum heat treatment condition of the friction welded materials SCr 4-21-4 Nand SUH 3-21-4 N was experimentally determined to eliminate the latent stress and the hardness peak at welded zones. 4) About 20% of the tensile strength before heat treatment of friction welded specimens was decreased after heat treatment 600\ulcornerCX30 min. Xair cooling, but the location of fracture was moved from heat affected zone to parent $SCr_4$ & SUH3. 5) Microscopic examination of the weld joints friction-welded and heat-treated under the above mentioned conditions revealed that the weld zone is very narrow and has a fine grained intermixed structure without any welding defects. 6) The above mentioned conditions can be also utilized as friction welding parameters of the other dissimiar materials for engine valve production.

  • PDF

The Study on Laser Cladding of Heat Resisting Steel Using EuTroLoy 16006 Powder(I) - Characteristics of 1 Pass Clad Layer with Process Parameters - (EuTroLoy 16006 분말을 이용한 내열강의 레이저 클래딩에 관한 연구(I) - 공정변수에 따른 1패스 클래드 층의 특성 -)

  • Kim, Jong Do;Lee, Eun Jin;Kim, Cheol Gyu
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.41 no.4
    • /
    • pp.299-305
    • /
    • 2017
  • Re-engineering is gaining attention due to severe environmental pollution and economic crisis. Although re-engineering in shipbuilding has been carried out steadily, technological advancements, domestic ship repair and maintenance industries are not as prevalent as shipbuilding industries. In order to solve this problems, laser cladding can significantly aid with technical development. Laser cladding produces an outstanding clad layer with minimal dilution and little porosity. In this study, prior to applying laser cladding to an exhaust valve face, the effects of various parameters that affect the characteristics of the 1 pass clad layer were investigated. When laser power was increased, the clad layer width became broader and the height was decreased. In addition, it was identified that the hardness of the clad layer was inversely proportional to the power, and the entire clad layer was diluted through an EDS chemical composition analysis.

A Study on the Spalling Properties of High Strength Concrete Using Synthetic Fiber (유기섬유를 혼입한 고강도 콘크리트의 폭렬 특성에 관한 실험적 연구)

  • Jeon, Chan Ki;Jeon, Joong Kyu
    • Journal of the Society of Disaster Information
    • /
    • v.8 no.1
    • /
    • pp.18-26
    • /
    • 2012
  • Accordingly architectural structure is getting high-rise and bigger, a use of high strength and high performance concrete has been increasing. High performance concrete has cons of explosion in a fire. This Explosion in the fire can cause the loss of the sheath on a concrete surface, therefore it effects that increasing a rate of heat transmission between the steel bar and inner concrete. Preventing this explosion of high performance concrete in the fire, many kinds of researches are now in progressing. Typically, researches with using Polypropylene-fiber and Steel-fiber can prove controling the explosion, but the reduction of mobility was posed as a problem of workability. Consequently, to solve the problem as mentioned above, concrete cans secure fire resisting capacity through the using of coating liquid, including Ester-lubricant and non-ionic characteristic surfactant. This research has been drawn a ideal condition in compressive strength areas of concrete by an experiment. When applying 13mm of polyamide-fiber, proper fiber mixing volume by compressive strength areas of concrete is $0.8kg/m^3$ in 60MPa, $1.0kg/m^3$ in 80MPa, $1.5kg/m^3$ in $100MPa/m^3$. These amount of a compound can control the explosion.

Fire Resistance of Circular Internally Confined Hollow Reinforced Concrete Column (원형 내부 구속 중공 철근콘크리트 기둥의 내화 성능)

  • Won, Deok-Hee;Han, Taek-Hee;Lee, Gyu-Sei;Kang, Young-Jong
    • Journal of Korean Society of Steel Construction
    • /
    • v.22 no.2
    • /
    • pp.139-150
    • /
    • 2010
  • Reinforced-concrete (RC) columns are frequently designed and constructed. other types of columns includes composite types such as concrete-filled tube columns (CFT). Hollow RC columns may be effective in reducing both the self weight of columns and total amount of materials used. This is due to the fact that a hollow RC column possesses larger moment of inertia than that of solid RC columns of same cross sectional area. Despite the effectiveness the hollow RC column has not been popular because of its poor ductility performance. While the transverse reinforcements are effective in controlling the brittle failure of the outside concrete, they are not capable of resisting the failure of concrete of inner face which is in unconfined state of stress. To overcome these drawbacks, the internally confined hollow reinforced concrete (ICH RC), a new column type, was proposed in the previous researches. In this study, the fire resistance performance of the ICH RC columns was analyzed through a series of extensive heat transfer analyses using the nonlinear-material model program. Also, effect of factors such as the hollowness ratio, thickness of the concrete, and thickness of the internal tube on the fire resistance performance were extensively studied. Then the factors that enhance the fire-resistant performance of ICH RC were presented and analyzed.