CrW 전율고용체 첨가 내열 알루미늄 합금에 관한 연구 (The Study of Heat Resistant Aluminum Alloy with CrW Homogeneous Solid Solution)

  • 김진평;성시영;한범석;김상호
    • 한국주조공학회지
    • /
    • 제33권3호
    • /
    • pp.122-126
    • /
    • 2013
  • Recently, heat-resistant aluminum alloy has been re-focused as a downsizing materials for the internal combustion engines. Heat-resistant Al alloy development and many researches are still ongoing for the purpose of improving thermal stability, high-temperature mechanical strength and fatigue properties. The conventional principle of heat-resistant Al alloy is the precipitation of intermetallic compounds by adding a variety of elements is generally used to improve the mechanical properties of Al alloys. Heat resistant aluminum alloys have been produced by CrW homogeneous solid solution to overcome the limit of conventional heat resistant aluminum alloy. From EPMA, it is found that CrW homogeneous soild solution phases with the size of $50-100{\mu}m$ have been dispersed uniformly, and there is no reaction between aluminum and CrW alloy. In addition, after maintaining at high temperature of 573 K, there is no growth of hardening phase, nor desolved, but CrW still exists as a homogeneous solid solution.

알루미나이징 강의 마모특성에 관한 연구 ( 1 ) - Rolling-Sliding 마찰의 초기마모영역을 중심으로 - (A Study on the Wear Characteristics of Aluminizing Steel ( 1 ) - Wear in Run-in Period on Rolling-Sliding Contact -)

  • 이규용
    • 수산해양기술연구
    • /
    • 제14권2호
    • /
    • pp.69-78
    • /
    • 1978
  • 알루미나이징강에 대하여 초기마모영역에서 rolling-sliding 마모시험을 한 결과를 요약하면 다음과 같다. 1) 2차 확산재의 내마모성이 가장 우수하고 처녀재에 비하여 저응력 레벨에서 약 18%, 고응력에서 약 40%의 마모감소를 나타낸다. 2) 2차 확산재는 피복층과 합금층 경계부근의 공공생성으로 인하여 예상보다 내마모성이 낮다. 3) 알루미나이징강의 rolling-sliding 접촉에 의한 마모파양의 형태는 spalling 이며 spalling crack은 합금속의 경계부근에서 발생한다.