• Title/Summary/Keyword: Heat resistance reliability

Search Result 85, Processing Time 0.019 seconds

A study on the optimization of manufacturing processes of double wall bellows for dual fuel engine II - Optimization of welding process - (Dual Fuel 엔진용 이중관 벨로우즈 제작 공정의 최적화에 관한 연구 II - 용접공정의 최적화 -)

  • Kim, Pyung-Su;Kim, Jong-Do;Song, Moo-Keun
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.40 no.6
    • /
    • pp.504-509
    • /
    • 2016
  • Production processes of double wall bellows can be roughly categorized into two steps. In the first step, inner and outer bellows are made of STS316L in austenite stainless steel due to their excellent formability and corrosion resistance. In the second step, the double wall bellows are manufactured using the welding method with both the inner and outer bellows. The microstructure and defects of each weldment are observed to ensure the reliability of bellows since weldment is a highly vulnerable part, which can crack and fracture when bellows are formed or used. In this study, optimum welding conditions were derived from the analysis of microstructure and inspection of weldment of bellows that were produced using various welding procedure. Moreover, the mechanical properties were evaluated through hardness measurement of substrate, weldment and the heat-affected zone.

Porous Media Modelling and Verification of Thermal Analysis for Inlet and Outlet Ducts of Spent Fuel Storage Cask (사용후핵연료 저장용기 유로입출구의 다공성매질 모델링 및 열해석 검증평가)

  • Lee, Ju-Chan;Bang, Kyung-Sik;Choi, Woo-Seok;Seo, Ki-Seog;Ko, Sungho
    • Journal of Nuclear Fuel Cycle and Waste Technology(JNFCWT)
    • /
    • v.16 no.2
    • /
    • pp.223-232
    • /
    • 2018
  • Bird screen meshes are installed at the air inlet and outlet ducts of spent fuel storage casks to inhibit the intrusion of debris from the external environment. The presence of these screens introduces an additional resistance to air flow through the ducts. In this study, a porous media model was developed to simplify the bird screen meshes. CFD analyses were used to derive and verify the flow resistance factors for the porous media model. Thermal analyses were carried out for concrete storage cask using the porous media model. Thermal tests were performed for concrete casks with bird screen meshes. The measured temperatures were compared with the analysis results for the porous model. The analysis results agreed well with the test results. The analysis temperatures were slightly higher than the test temperatures. Therefore, the reliability and conservatism of the analysis results for the porous model have been verified.

Research of Diffusion Bonding of Tungsten/Copper and Their Properties under High Heat Flux

  • Li, Jun;Yang, Jianfeng
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2011.05a
    • /
    • pp.14-14
    • /
    • 2011
  • W (tungsten)-alloys will be the most promising plasma facing armor materials in highly loaded plasma interactive components of the next step fusion reactors due to its high melting point, high sputtering resistance and low deuterium/tritium retention. The bonding technology of tungsten to Cu alloy was one of the key issues. In this paper, W/CuCrZr diffusion bonding has been performed successfully by inserting pure metal interlay. The joint microstructure, interfacial elements migration and phase composition were analyzed by SEM, EDS, XRD, and the joint shear strength and micro-hardness were investigated. The mock-ups were fabricated successfully with diffusion bonding and the cladding technology respectively, and the high heat flux test and thermal fatigue test were carried out under actively cooling condition. When Ni foil was used for the bonding of tungsten to CuCrZr, two reaction layers, Ni4W and Ni(W) layer, appeared between the tungsten and Ni interlayer with the optimized condition. Even though Ni4W is hard and brittle, and the strength of the joint was oppositely increased (217 MPa) due primarily to extremely small thicknesses (2~3 ${\mu}m$). When Ti foil was selected as the interlayer, the Ti foil diffused quickly with Cu and was transformed into liquid phase at $1,000^{\circ}C$. Almost all of the liquid was extruded out of the interface zone under bonding pressure, and an extremely thin residual layer (1~2 ${\mu}m$) of the liquid phase was retained between the tungsten and CuCrZr, which shear strength exceeded 160 MPa. When Ni/Ti/Ni multiple interlayers were used for bonding of tungsten to CuCrZr, a large number of intermetallic compound ($Ni_4W/NiTi_2/NiTi/Ni_3T$) were formed for the interdiffusion among W, Ni and Ti. Therefore, the shear strength of the joint was low and just about 85 MPa. The residual stresses in the clad samples with flat, arc, rectangle and trapezoid interface were estimated by Finite Element Analysis. The simulation results show that the flat clad sample was subjected maximum residual stress at the edge of the interface, which could be cracked at the edge and propagated along the interface. As for the rectangle and trapezoid interface, the residual stresses of the interface were lower than that of the flat interface, and the interface of the arc clad sample have lowest residual stress and all of the residual stress with arc interface were divided into different grooved zones, so the probabilities of cracking and propagation were lower than other interfaces. The residual stresses of the mock-ups under high heat flux of 10 $MW/m^2$ were estimated by Finite Element Analysis. The tungsten of the flat interfaces was subjected to tensile stresses (positive $S_x$), and the CuCrZr was subjected to compressive stresses (negative $S_x$). If the interface have a little microcrack, the tungsten of joint was more liable to propagate than the CuCrZr due to the brittle of the tungsten. However, when the flat interface was substituted by arc interfaces, the periodical residual stresses in the joining region were either released or formed a stress field prohibiting the growth or nucleation of the interfacial cracks. Thermal fatigue tests were performed on the mock-ups of flat and arc interface under the heat flux of 10 $MW/m^2$ with the cooling water velocity of 10 m/s. After thermal cycle experiments, a large number of microcracks appeared at the tungsten substrate due to large radial tensile stress on the flat mock-up. The defects would largely affect the heat transfer capability and the structure reliability of the mock-up. As for the arc mock-up, even though some microcracks were found at the interface of the regions, all microcracks with arc interface were divided into different arc-grooved zones, so the propagation of microcracks is difficult.

  • PDF

A Study on the High Frequency Ultrasonic Attenuation Characterization in Artificially Aging Degraded 2.25Cr-1Mo Steel (2.25Cr-1Mo 강 인공 열화재의 고주파수 초음파 감쇠특성에 관한 연구)

  • Park, Ik-Keun;Park, Un-Su;Kim, Chung-Seok;Kim, Hyun-Mook;Kwun, Sook-In;Byeon, Jai-Won
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.21 no.4
    • /
    • pp.439-445
    • /
    • 2001
  • The destructive method is reliable and widely used lot the estimation of material degradation but, it have time-consuming and a great difficulty in preparing specimens from in-service industrial facilities. Therefore, the estimation of degraded structural materials used at high temperature by nondestructive evaluation such as electric resistance method, replica method, Barkhausen noise method, electro-chemical method and ultrasonic method are strongly desired. Ultrasonic nondestructive evaluation technique has been reported good to attain efficiency of measurement, high sensitivity of measurement, and rapidity and reliability of result interpretation. In this study, it was verified experimentally the feasibility of the evaluation of degraded 2.25Cr-1Mo steel specimens which were prepared by the isothermal aging heat treatment at $630^{\circ}C$ by high frequency longitudinal wave method investigating the change of attenuation coefficient by FFT analysis and wavelet transform. Because of carbide precipitation increase and spheroidization near grain boundary of microstructure to aging degradation, attenuation coefficient had a tendency to increase as degradation proceeded. It was identified possibly to evaluate degradation using the characteristics of high-frequency ultrasonics. Frequency dependence of ultrasonic attenuation coefficient to aging degradation appeared large, which made sure that attenuation coefficient is an important parameter for evaluation of aging degradation.

  • PDF

Comparative study on the performance of butt fusion-welding processes for nuclear safety class large-diameter thick-walled PE pipes

  • Zhenchao Wang;Bin Wang;Aimin Xiang;Di Jiao;Fa Yu;Qiuju Zhang;Xiaoying Zhao
    • Nuclear Engineering and Technology
    • /
    • v.56 no.10
    • /
    • pp.4184-4194
    • /
    • 2024
  • New technologies in polymer synthesis and pipe extrusion equipment have led to the commercialization of high-performance, large-diameter, thick-wall high density polyethylene (HDPE) pipes. They have been used in the field of seawater transport and cooling to replace metal pipes, due to their advantages of high corrosion resistance and extensibility. Connection of HDPE pipe is important as it determines the safety of the entire piping system. Butt fusion welding is commonly used for HDPE pipe connection but may cause the formation of weak points in the welded joints, interfering the reliability of the pipeline system in the application of nuclear power plants. At present, there is a lack of research on evaluating the performance of welded joint for large-diameter thick-wall HDPE pipes made by butt fusion-welding. The purpose of this study is to investigate the influence of three different butt fusion-welding processes, i.e., single low pressure (SLP), single high pressure (SHP) and dual low pressure (DLP), by evaluating the performance of their welded joints, including characterizing tensile strength, extensibility, crystallinity and hardness. In specific, a thick-wall HDPE pipe with OD of 812.8 mm and wall thickness of 74 mm which is certified for nuclear safety class was used for study. Representative specimen from the outer, middle and inner part across the wall of the main pipe body and welded joints were taken for testing. Different test methods and specimens were designed to assess the feasibility of evaluating the welding performance from different welding process. The results showed that the mechanical properties of different locations of the welded joints were different, and the tensile strength and fracture energy of the middle part of the joint were lower than that of the inner and outer parts, which could be caused by the difference in the crystallinity and thickness of the melting zone influenced by welding processes, as can be seen from the analysis of DSC test and morphology observation. Hardness testing was conducted on the section of the welded joints, and it revealed that the micromechanical properties of the welded joints in the region of the heat-affected zone were enhanced significantly, which may be due to the annealing effect caused by welding process. In summary, The DLP process resulted in the best extensibility of the welded joints among three processes, suggesting that the joining pressure from welding process plays an important role in affecting the extensibility of the welded joints.