Stress distribution of near the interface on high temperature fatigue in ceramic/metal bonded joints (세라믹/금속접합재의 고온피로에 따른 접합계면의 응력분포)

  • 박영철;허선철;윤두표;김광영
    • Journal of Ocean Engineering and Technology
    • /
    • v.10 no.2
    • /
    • pp.106-119
    • /
    • 1996
  • The ceramic has various high mechanical properties such as heat, abrasion, corrosion resistance and high temperature strength compared with metal. It also has low speciffic weight, low thermal expansibillity, low thermal conductivity. However, it could not be used as structural material since it is brittle and difficult for the machining. Therefore, there have been many researches to attempt to join ceramic with metal which is full of ductillity in order to compensate the weakness of ceramic.The problem is that residual stress develops around the joint area while the ceramic/metal joint material is cooled from high joining temperature to room temperature due to remarkable difference of thermal expansion coefficients between ceramic and metal. Especially, the residual stress at both edges of the specimen reduces the strngth of joint to a large amount by forming a singular stress field. In this study, two dimensional finite element method is attempted for the thermal elastic analysis. The joint residual stress of ceramic/metal developed in the cooling process is investigated and the change of joint residual stress resulted from the repetitive heat cycle is also examined. In addition, it is attempted to clarify the joint stress distribution of the case of tensile load and of the case of superposition of residual stress and actual loading stress.

  • PDF

Structural Analysis and Safety Assessment for Constricted Bridges (협착교량의 구조해석 및 안전성 평가)

  • Jeong, Jae-Hun;Kim, Moon-Ok;Choi, Hyun-Ho;Kim, Jang-Hwan
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.26 no.6
    • /
    • pp.33-38
    • /
    • 2022
  • As the intense heat continues, many cases of highway pavement blow up and bridge expansion joints damages have been inspected. Especially, Expansion joint closure of bridges is an important problem that can threat the safety of the bridge structure or reduce long-term durability. This paper proposed a structural analysis method for bridges having expansion joint closure and structural analysis was performed to verify the effects according to bridge types. Analysis bridges were divided into four types: concrete and steel bridges, shallow and piled foundations. To induce the situation of abutments and bridge decks are jammed, the following loads were additionally considered; lateral flow pressure, pavement expansion by alkali-aggregate reaction, creep settlement of backfill. The structural analysis method was verified by comparing the structural analysis results with the actually measured joint gap data. In addition, behavioral analysis due to joint closure was conducted to confirm the change in safety ratio by type of superstructure as the axial force increased.

Singular Stress Field Analysis and Strength Evaluation in Ceramic/.Metal Joints (세라믹/금속접합재의 열사이클피로에 따른 접합계면의 잔류응력분포 특성)

  • 박영철;김현수;허선철;강재욱
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 1996.04a
    • /
    • pp.709-713
    • /
    • 1996
  • The ceramic has such high qualities as light weight, abrasion resistance, heat resistance compared with metal, but since it is breakable, it can't be used as structural material and it is desirable to joining metal which is full of toughness, but, according as the ceramic/metal joint is executed at high temperature, the joint residual stress develops near the joint sides in the process of cooling the high temperature down to the suitable temperature due to difference of the thermal expansion coefficient between ceramic and metal, and the joint residualstress lowers the fracture strength. In this study, to ensure security and improvement of bending strength, 1 studies on see distribution shape of residual stress according to high thermal cycle, and the influnence of theraml cycle and distribution shape of residual stess on joint-strength.

  • PDF

Sensitivity Analysis on Hydraulic Expanded Tube-to-Tubesheet Joints for Tube Layout Patterns (튜브 배열에 따른 튜브/튜브시트 수압 확관 접합의 민감도 해석)

  • Kim, Dong-Yeong;Kim, Tae-Wan
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.23 no.11 s.170
    • /
    • pp.1896-1903
    • /
    • 1999
  • The basic requirements to improve the joints quality of tube-to-tubesheet for heat exchangers are to obtain high residual contact pressures between the tubes and the tubesheet as well as low residual stresses in the transition zone of the tubes. The residual contact pressures and residual stresses which govern the joint quality are influenced by parameters such as material properties, geometric dimension of tube and tubesheet and expansion pressures. There are two types of tube layout patterns, triangular and square, which are frequently used for heat exchangers. The purpose of the present work is to examine the superior tube layout patterns considering the joints quality by comparing numerical results from sensitivity analyses which were performed for both of tube layout patterns.

Effect of the Joint Condition between Muffler Shell and Baffle on Radiated Noise (배기계 방사소음에 대한 소음기 셀/격벽간 접합구조의 영향)

  • Yang, Chul-Ho
    • Transactions of the Korean Society for Noise and Vibration Engineering
    • /
    • v.16 no.3 s.108
    • /
    • pp.233-239
    • /
    • 2006
  • The effect of the joint condition of automotive muffler shell and baffle on radiated noise from muffler shell Is studied. Shell vibration characteristics, especially shift In natural frequency and change in of response amplitude, was identified from finite element analysis and modal tests for various joint conditions between shell and baffle. When there is heat expansion and inner pressure from the exhaust 9as in the muffler with elliptical cross section, the shell expands out, and construct gap with baffles. This gap causes more degrees of freedom of shell vibration and natural frequency shift. By welding the muffler shell to the baffles or using a dual shell muffler, the radiated noise problem could be mitigated supplying more a rigid joint and damping, respectively.

Residual Stress in U-Bending Deformations and Expansion Joints of Heat Exchanger Tubes (전열관의 굽힘 및 확관접합 잔류응력)

  • Jang, Jin-Seong;Bae, Gang-Guk;Kim, U-Gon;Kim, Seon-Jae;Guk, Il-Hyeon;Kim, Seong-Cheong
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.24 no.2 s.173
    • /
    • pp.279-289
    • /
    • 2000
  • Residual stress induced in U-bending and tube-to-tubesheet joint processes of PWR's row-1 heat exchanger tube was measured by X-ray method and Hole-Drilling Method(HDM). Compressive residual stresses(-) at the extrados surface were induced in U-bending, and its maximum value reached -319 MPa in axial direction at the position of $\psi$ = $0^{\circ}$. Tensile residual stresses(+) of $\sigma_{zz}$ = 45 MPa and $\sigma_{\theta\theta}$ = 25 MPa were introduced in the intrados surface at the position of $\psi$ = $0^{\circ}$. Maximum tensile residual stress of 170 MPa was measured at the flank side at the position of $\psi$ = $90^{\circ}$, i.e., at apex region. It was observed that higher stress gradient was generated at the irregular transition regions (ITR). The trend of residual stress induced by U bending process of the tubes was found to be related with the change of ovality. The residual stress induced by the explosive joint method was found to be lower than that by the mechanical roll method. The gradient of residual stress along the expanded tube was highest at the transition region (TR), and the residual stress in circumferential direction was found to be higher than the residual stress in axial direction.

Failure Analysis of Stress Reliever in Heat-Transport Pipe of District Heating System

  • Cho, Jeongmin;Chae, Hobyung;Kim, Heesan;Kim, Jung-Gu;Kim, Woo Cheol;Lee, Soo Yeol
    • Corrosion Science and Technology
    • /
    • v.21 no.4
    • /
    • pp.243-249
    • /
    • 2022
  • The objective of the present study was to perform failure analysis of double-layered bellow (expansion joint), a core part of stress reliever, used to relieve axial stresses induced by thermal expansion of heat-transport pipes in a district heating system. The bellow underwent tensile or compressive stresses due to its structure in terms of position. A leaked position sufferred a fatigue with a tensile component for decades. A cracked bellow contained a higher fraction of martensitic phase because of manufacturing and usage histories, which induced more brittleness on the component. Inclusions in the inner layer of the bellow acted as a site of stress concentration, from which cracks initiated and then propagated along the hoop direction from the inner surface of the inner layer under fatigue loading conditions. As the crack reached critical thickness, the crack propagated to the outer surface at a higher rate, resulting in leakage of the stress reliever.

A Counterplan of temperature crack control by a heat of hydration of Subway concrete box structure concerned External Temperature (대기온도를 고려한 지하철 콘크리트 Box 구조물의 수화열에 의한 온도균열제어 대책)

  • Roh, Hyun-Sup;Kim, Eun-Kyum;Yang, Sin-Chu
    • Proceedings of the KSR Conference
    • /
    • 2007.11a
    • /
    • pp.581-584
    • /
    • 2007
  • The subway concrete box structure can`t establish expansion joint because of animal power delivery of the subway rail. In this case, As increase of structure volume, it is subjected to cause temperature crack. The temperature crack due to the heat of hydration classified a nonstructural crack. but it has a bad effect on durability of concrete structures. especially, in case of a subway concrete box structure, when a water-proof facilities is beaked on an outer-wall, the water leakage occurs through a penetration crack generated from a wall of the concrete structure too. This paper, for the subway concrete box structure, examined a condition of temperature crack occurrence by a heat of hydration concerned external temperature from analysing by a three dimensional finite element method.

  • PDF

A study on the transverse shrinkage for the butt joint welding of plate (평판의 맞대기 이음 용접시의 가로수축에 관한 연구)

  • 이우수;왕지석
    • Journal of Welding and Joining
    • /
    • v.5 no.3
    • /
    • pp.46-52
    • /
    • 1987
  • The mechanism of transverse shrinkage for the butt joint weldig of plates is investigated in this paper. It was certified that the compressive plastic strain due to thermal expansion of materials during heating play an important role on the transverse shrinkage. It was also pointed out that the transverse shrinkage has to be treated with the samples of which the shapes are as close to real shapes of welded materials as possible, because the distribution of temperature and relative rigidity of materials during welding have great influence on the transverse shrinkage. The formulas for the calculation of transverse shrinkage were presented and the experiments were carried out in order to verify the formulas. the main results are as follows; 1. For the bead-on-plate welding, the transverse shrinkage in the begining parts of welding is the smallest, the end parts is next and the transverse shrinkage of mid section is the largest. 2. In bead-on-plate welding, the equations presented in this paper concerning transverse shrinkage coincide fairly well with the experimental values generally. 3. Transverse shrinkage increases generally as specific heat input per unit thickness increaes.

  • PDF

Design of exhaust manifold for pulse converters considering fatigue strength due to vibration

  • Cho, Kyung-Sang;Son, Kyung-Bin;Kim, Ue-Kan
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.37 no.7
    • /
    • pp.694-700
    • /
    • 2013
  • The design of the exhaust manifold for the pulse converters of a 4 strokes high power medium-speed diesel engine is presented in terms of fatigue analysis. The said system undergoes thermal expansion due to high temperature of exhaust gas and is exposed to intrinsic vibration of the internal combustion engine. Moreover, the exhaust pulse generates pressure pulsating along the runner inside manifold. Under such circumstances, the design and construction of exhaust manifold must be carried out in a way to prevent early failure due to fracture. To validate the design concept, a test rig was developed to simulate the combination of thermal and vibrational movements, simultaneously. Experimental results showed that a certain sense of reliability can be achieved by considering a field factor obtained from the results of engine bench tests.