The effective properties of saturated concrete healed by EDM with the ITZs

  • Chen, Qing;Jiang, Zhengwu;Zhu, Hehua;Ju, J.W.;Yan, Zhiguo;Li, Haoxin
    • Computers and Concrete
    • /
    • v.21 no.1
    • /
    • pp.67-74
    • /
    • 2018
  • A differential scheme based micromechanical framework is proposed to obtain the effective properties of the saturated concrete repaired by the electrochemical deposition method (EDM) considering the interfacial transition zone (ITZ) effects. The constituents of the repaired concrete are treated as different phases, consisting of (micro-)cracks, (micro-)voids and (micro-)pores (occupied by water), deposition products, intrinsic concrete made up by the three traditional solid phases (i.e., mortar, coarse aggregates and their interfaces) and the ITZs. By incorporating the composite sphere assemblage (CSA) model and the differential approach, a new multilevel homogenization scheme is utilized to quantitatively estimate the mechanical performance of the repaired concrete with the ITZs. The CSA model is modified to obtain the effective properties of the equivalent particle, which is a three-phase composite made up of the water, deposition products and the ITZs. The differential scheme is employed to reach the equivalent composite of the concrete repaired by EDM considering the ITZ effects. Moreover, modification procedures considering the ITZ effects are presented to attain the properties of the repaired concrete in the dry state. Results in this study are compared with those of the existing models and the experimental data. It is found that the predictions herein agree better with the experimental data than the previous models.

Solidification Cracking in Welds and its Control (용접부 응고균열 발생 및 제어)

  • Yoon, Jong-Won
    • Proceedings of the KWS Conference
    • /
    • 2010.05a
    • /
    • pp.22-22
    • /
    • 2010
  • Eutectic composition phase with low melting point which solidifies at the final stage affects the solidification cracking at the intercellular or interdendritic area of welds and castings. If sufficient amount of eutectic composition liquid does not exist between the solidifying phases, the discontinuities remain as cracks. However, abundant amount of liquid eutectic composition existing in the final stage can flow into the discontinuities easily and heal the cracks. By flowing of liquid eutectic and healing of discontinuities, the possibility of cracking can be reduced when the amount of eutectic liquid is sufficient. For the solidification of pure metals, liquid eutectic does not exist and the interlocking of growing solid phases can be realized without interruption of liquid film. Therefore there is little possibility of solidification cracking in the case of welds and castings of pure metal. In a practical sense, the effective way to reduce or prevent the solidification cracking is making the composition of molten pool or melts near to the eutectic composition.

  • PDF

Morphology of Bone-like Apatite Formation on Sr and Si-doped Hydroxyapatite Surface of Ti-6Al-4V Alloy after Plasma Electrolytic Oxidation

  • Yu, Ji-Min;Choe, Han-Cheol
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2017.05a
    • /
    • pp.79-79
    • /
    • 2017
  • Metallic biomaterials have been mainly used for the fabrication of medical devices for the replacement of hard tissue such as artificial hip joints, bone plates, and dental implants. Because they are very reliable on the viewpoint of mechanical performance. This trend is expected to continue. Especially, Ti and Ti alloys are bioinert. So, they do not chemically bond to the bone, whereas they physically bond with bone tissue. For their poor surface biocompatibility, the surface of Ti alloys has to be modified to improve the surface osteoinductivity. Recently, ceramic-like coatings on titanium, produced by plasma electrolytic oxidation (PEO), have been developed with calciumand phosphorus-enriched surfaces. A lso included the influences of coatings, which can accelerate healing and cell integration, as well as improve tribological properties. However, the adhesions of these coatings to the Ti surface need to be improved for clinical use. Particularly Silicon (Si) has been found to be essential for normal bone, cartilage growth and development. This hydroxyapatite, modified with the inclusion of small concentrations of silicon has been demonstrating to improve the osteoblast proliferation and the bone extracellular matrix production. Strontium-containing hydroxyapatite (Sr-HA) was designed as a filling material to improve the biocompatibility of bone cement. In vitro, the presence of strontium in the coating enhances osteoblast activity and differentiation, whereas it inhibits osteoclast production and proliferation. The objective of this work was to study Morphology of bone-like apatite formation on Sr and Si-doped hydroxyapatite surface of Ti-6Al-4V alloy after plasma electrolytic oxidation. Anodized alloys was prepared at 270V~300V voltages with various concentrations of Si and Sr ions. Bone-like apatite formation was carried out in SBF solution. The morphology of PEO, phase and composition of oxide surface of Ti-6Al-4V alloys were examined by FE-SEM, EDS, and XRD.

  • PDF

Econazole Induces p53-Dependent Apoptosis and Decreases Metastasis Ability in Gastric Cancer Cells

  • Choi, Eun Kyoung;Park, Eun Jung;Phan, Tien Thuy;Kim, Hea Dong;Hoe, Kwang-Lae;Kim, Dong-Uk
    • Biomolecules & Therapeutics
    • /
    • v.28 no.4
    • /
    • pp.370-379
    • /
    • 2020
  • Econazole, a potent broad-spectrum antifungal agent and a Ca2+ channel antagonist, induces cytotoxicity in leukemia cells and is used for the treatment of skin infections. However, little is known about its cytotoxic effects on solid tumor cells. Here, we investigated the molecular mechanism underlying econazole-induced toxicity in vitro and evaluated its regulatory effect on the metastasis of gastric cancer cells. Using the gastric cancer cell lines AGS and SNU1 expressing wild-type p53 we demonstrated that econazole could significantly reduce cell viability and colony-forming (tumorigenesis) ability. Econazole induced G0/G1 phase arrest, promoted apoptosis, and effectively blocked proliferation- and survival-related signal transduction pathways in gastric cancer cells. In addition, econazole inhibited the secretion of matrix metalloproteinase- 2 (MMP-2) and MMP-9, which degrade the extracellular matrix and basement membrane. Econazole also effectively inhibited the metastasis of gastric cancer cells, as confirmed from cell invasion and wound healing assays. The protein level of p53 was significantly elevated after econazole treatment of AGS and SNU1 cells. However, apoptosis was blocked in econazole-treated cells exposed to a p53-specific small-interfering RNA to eliminate p53 expression. These results provide evidence that econazole could be repurposed to induce gastric cancer cell death and inhibit cancer invasion.

Thermo-Mechanical Properties of Al2TiO5 Ceramics Stabilized with MgO and ZrO2 Additives (MgO와 ZrO2가 첨가된 Al2TiO5 세라믹의 열·기계적 물성)

  • Kim, Da-Mi;Kim, Hyung-Tae;Kim, Hyeong-Jun;Kim, Ik-Jin;Choi, Seong-Cheol;Kim, Yong-Chan;NamKung, Jung;Ryu, Sung-Soo
    • Journal of Powder Materials
    • /
    • v.19 no.4
    • /
    • pp.253-258
    • /
    • 2012
  • The characteristics of $Al_2TiO_5$ ceramics were influenced by the additives and the heat treatment that controls the microcrack behavior at grain boundaries. The effect of additives on $Al_2TiO_5$ ceramics were investigated in terms of mechanical properties and thermal expansion at high temperature. The $Al_2TiO_5$ were synthesized at $1500^{\circ}C$, $1550^{\circ}C$ and $1600^{\circ}C$ for 2h by reaction sintering. The formation of $Al_2TiO_5$ phase was increased by additives that enhanced the volume of the microcrack that can lead to low thermal expansion. The mechanical properties of the stabilized $Al_2TiO_5$ ceramics were increased remarkably at $1100^{\circ}C$, $1200^{\circ}C$ and $1300^{\circ}C$ due to the oneset of mechanical healing of grain-bondary microcracks at a high temperature. The amount of microcrack was decreased at lower sintering temperature that causes the increase of mechanical properties at high temperature.

In vitro and In vivo Activities Studies of Chois Mastic Using Self-microemulsifying Drug Delivery System (SMEDDS) against Helicobactor pylori (자가미세유화시스템을 이용한 매스틱의 헬리코박터파일로리 대한 In vitro 및 In vivo 활성 연구)

  • Kim, Su-Ji;Jeong, Sang-Young;Gil, Young-Sig;Shin, Byung-Cheol;Hwang, Sung-Joo;Cho, Sun-Hang
    • YAKHAK HOEJI
    • /
    • v.55 no.1
    • /
    • pp.1-10
    • /
    • 2011
  • Mastic is a bleed resin formed in pistacia lentiscus tree extract form the anacatdiaceae family. Mastic is used as a food ingredient in the Mediteraanean resin, and has been used by local inhabitants as a traditional medicine for relief of upper abdominal discomfort, dyspepsiaand peptic ulcer. Clinically, mastic has been effective in the treatment of benign gastric and duodenal, ulcers, giving symptomatic relief and endoscopically proven healing. In this study, to enhance activiteies of poorly water soluble Mastic with oils, surfactants and cosurfactants and then the mixure was microemulsified in aqueous media under condition of gentle agitation and digestive motility that would be encountered in the gastrointestinal tract. Formulation development and screening were based on phase diagrams and characteristics of resultant microemulsion. For optimum mastic formulation, microemulsions with various ratio (w/w%) of mastics, oils, surfactants and cosurfactants were prepared and their solubility was evaluated by monitoring particles size in their buffer through visual asessment and electrophoretic light scattering spectrophotomerter (ELS). In vitro activity of self microemulsified mastic (SME mastic) was determined by minimum ingibition concentration (MIC) test against a panel of Helicobacter pylori (H. pylori) clinical strains. Additionally, in vivo activity of SME masitc was investigated us mouse infected by CH275 of H. pylori. The mean diameter of SME mastic was less then 100 nm in water and SME mastic was showed similar antiboisis effect compared to tometronidazole, clarithromycin and omeproazole. Consequently, SME mastic would be effective system to exterminate H. pylori. If mastic were dose with combined treatment, mastic might augur well for effect of H. pylori eradication as good remedy.

Marginal bony changes in relation to different vertical positions of dental implants

  • Yi, Jung-Myung;Lee, Jae-Kwan;Um, Heung-Sik;Chang, Beom-Seok;Lee, Min-Ku
    • Journal of Periodontal and Implant Science
    • /
    • v.40 no.5
    • /
    • pp.244-248
    • /
    • 2010
  • Purpose: The purpose of this study was to radiographically evaluate marginal bony changes in relation to different vertical positions of dental implants. Methods: Two hundred implants placed in 107 patients were examined. The implants were classified by the vertical positions of the fixture-abutment connection (microgap): 'bone level,' 'above bone level,' or 'below bone level.' Marginal bone levels were examined in the radiographs taken immediately after fixture insertion, immediately after second-stage surgery, 6 months after prosthesis insertion, and 1 year after prosthesis insertion. Radiographic evaluation was carried out by measuring the distance between the microgap and the most coronal bone-to-implant contact (BIC). Results: Immediately after fixture insertion, the distance between the microgap and most coronal BIC was $0.06{\pm}0.68\;mm$; at second surgery, $0.43{\pm}0.83\;mm$; 6 months after loading, $1.36{\pm}0.56\;mm$; and 1 year after loading, $1.53{\pm}0.51\;mm$ ($mean{\pm}SD$). All bony changes were statistically significant but the difference between the second surgery and the 6-month loading was greater than between other periods. In the 'below bone level' group, the marginal bony change between fixture insertion and 1 year after loading was about 2.25 mm, and in the 'bone level' group, 1.47 mm, and in 'above bone level' group, 0.89 mm. Therefore, the marginal bony change was smaller than other groups in the 'above bone level' group and larger than other groups in the 'below bone level' group. Conclusions: Our results demonstrated that marginal bony changes occur during the early phase of healing after implant placement. These changes are dependent on the vertical positions of implants.

Therapeutic strategies to manage chronic wounds by using biofilm dispersal mechanisms (생물막 분산기작을 이용한 만성창상의 치료전략)

  • Kim, Jaisoo;Kim, Min-Ho
    • Korean Journal of Microbiology
    • /
    • v.55 no.2
    • /
    • pp.87-102
    • /
    • 2019
  • Most chronic wounds persist in the inflammatory phase during wound healing due to the biofilm. Biofilms are resistant to antibiotics, weakening penetration, resistance to biocides and weakening local immune responses. The biofilm is firmly attached to the surrounding tissues and is very difficult to remove. Therefore, strategies to remove hard biofilms without damaging surrounding tissue are very important. One of possible strategies is dispersal. So many studies have been done to develop new strategies using dispersal mechanisms. In this review paper, especially chemotaxis, phage therapy, polysaccharides, various enzymes (glycosidases, proteases, and deoxyribonucleases), surfactants, dispersion signals, autoinducers, inhibitors were introduced. Combination therapies with other therapies such as antibiotic therapy were also introduced. It is expected that the possibility of treatment of chronic wound infection using the knowledge of the biofilm dispersal mechanisms presented in this paper will be higher.

Rodent peri-implantitis models: a systematic review and meta-analysis of morphological changes

  • Ren Jie Jacob Chew;Jacinta Xiaotong Lu;Yu Fan Sim;Alvin Boon Keng Yeo
    • Journal of Periodontal and Implant Science
    • /
    • v.52 no.6
    • /
    • pp.479-495
    • /
    • 2022
  • Purpose: Rodent models have emerged as an alternative to established larger animal models for peri-implantitis research. However, the construct validity of rodent models is controversial due to a lack of consensus regarding their histological, morphological, and biochemical characteristics. This systematic review sought to validate rodent models by characterizing their morphological changes, particularly marginal bone loss (MBL), a hallmark of peri-implantitis. Methods: This review was conducted following the Preferred Reporting Items for Systematic Reviews and Meta-Analysis (PRISMA) guidelines. A literature search was performed electronically using MEDLINE (PubMed), and Embase, identifying pre-clinical studies reporting MBL after experimental peri-implantitis induction in rodents. Each study's risk of bias was assessed using the Systematic Review Center for Laboratory animal Experimentation (SYRCLE) risk of bias tool. A meta-analysis was performed for the difference in MBL, comparing healthy implants to those with experimental peri-implantitis. Results: Of the 1,014 unique records retrieved, 23 studies that met the eligibility criteria were included. Peri-implantitis was induced using 4 methods: ligatures, lipopolysaccharide, microbial infection, and titanium particles. Studies presented high to unclear risks of bias. During the osseointegration phase, 11.6% and 6.4%-11.3% of implants inserted in mice and rats, respectively, had failed to osseointegrate. Twelve studies were included in the meta-analysis of the linear MBL measured using micro-computed tomography. Following experimental peri-implantitis, the MBL was estimated to be 0.25 mm (95% confidence interval [CI], 0.14-0.36 mm) in mice and 0.26 mm (95% CI, 0.19-0.34 mm) in rats. The resulting peri-implant MBL was circumferential, consisting of supra- and infrabony components. Conclusions: Experimental peri-implantitis in rodent models results in circumferential MBL, with morphology consistent with the clinical presentation of peri-implantitis. While rodent models are promising, there is still a need to further characterize their healing potentials, standardize experiment protocols, and improve the reporting of results and methodology.

Effect of Epidermal Growth Factor with Collagen Matrix on Increasing Gingival Thickness: A Pilot Preclinical Investigation

  • Hyun-Chang Lim;Yeek Herr;Jong-Hyuk Chung;Seung-Yun Shin;Seung-Il Shin;Ji-Youn Hong
    • Journal of Korean Dental Science
    • /
    • v.16 no.2
    • /
    • pp.172-181
    • /
    • 2023
  • Purpose: To investigate the effect of epidermal growth factor (EGF) with collagen matrix (CM) for increasing gingival thickness. Materials and Methods: In five mongrel dogs, bilateral gingival defects were surgically made on the maxillary canines. After two months, either a subepithelial connective tissue graft (group SCTG) or CM with EGF (0.1 ug/ml, group EGF) was grafted, and the flap was coronally positioned to cover the graft materials. The animals were sacrificed after three months. Intraoral scanning was performed for soft tissue analysis. Histologic and histomorphometric analyses were performed. Result: Two animals exhibited wound dehiscence during the healing phase, leaving three for analysis. No statistically significant difference was found in soft tissue changes (P>0.05). The level of gingival margin (GM) increased in both groups (1.02±0.74 mm in group SCTG vs. 1.24±0.83 mm in group EGF). Linear increases at the GM pre-augmentation in the soft tissue profile were 1.08±0.58 mm in group SCTG and 0.96±0.73 mm in group EGF. Histomorphometric parameters (keratinized tissue height, tissue thickness, and rete peg density) were not significantly different between the groups (P>0.05). Conclusion: EGF loaded onto CM led to comparable gingival phenotype enhancement to SCTG.