• 제목/요약/키워드: Hardening layer depth

검색결과 42건 처리시간 0.029초

단순화된 설계인자에 의한 레이저표면경화공정의 퍼지제어기 설계 (Fuzzy Logic Controller Design By Means Of Characteristic Design Parameters in a LASER Surface Hardening Process)

  • 박영준;김재훈;조형석
    • 제어로봇시스템학회:학술대회논문집
    • /
    • 제어로봇시스템학회 2000년도 제15차 학술회의논문집
    • /
    • pp.292-292
    • /
    • 2000
  • Since high-power CO$_2$ Laser can be make a high densed energy to Local processing area, manufacturing processes using the laser can be processed for very Localized areas at a very fast rate with minimal or no distortion. Accordingly, the laser has been widely used in the fields of thermal manufacturing processes such as welding, fusion cutting, grooving, and heat treatment of metals. In particular, interest in the laser heat treatment process has grown tremendously in the past few years. In this process, maintaining the uniform hardening depth is important problem to obtain good quality products and to reduce heat induced distortion and residual stress. For achieving this objective, we introduced a new design technique of a fuzzy logic controller that greatly simplified the design procedure by defining several simplified design parameters. In the design procedure, the major design parameters of the controller are characterized by identifying several common aspects. From a series of simulation results, we found that the proposed design technique can be effectively used to design of a fuzzy logic controller for the LASER surface hardening process.

  • PDF

YAG LASER에 의한공구강의 표면개질에 관한 연구 (A Study on the Surfaces Modification of Tool Steel by YAG LASER)

  • 강형식
    • 한국생산제조학회지
    • /
    • 제9권2호
    • /
    • pp.66-71
    • /
    • 2000
  • Laser induced surface hardening of Tool steel(STC5) can be achieved either with or without surface melting. In trans-formation hardening as the surface is heated to a temperature below its melting point and is rapidly cooled solidified microstructures are usually much finer and stronger than those of the base matals. For this reason surface modification of tool steel by YAG laser irradiation has been studied as a function of processing parameters such as power density pulse width defocusing distance and molten depth. The high energy density changes and refines the microstructure of the near surface layer. In the case of beam passes martensite formed in the melt zone exhibited very high vickers hardness values. Molten depth and width depend on defocusing distance and energy of black color painting is more absorptive than other color painting.

  • PDF

주조용 티타늄 신합금 개발 (Development of New Titanium Alloys for Castings)

  • 김승언;정희원;현용택;김성준;이용태
    • 연구논문집
    • /
    • 통권29호
    • /
    • pp.163-171
    • /
    • 1999
  • A new titanium alloy system. Ti-xFe-ySi (x,y=0-4 wt%). was designed and characterized with the point at low cost and high strength for casting applications. Fe improved room and elevated temperature mechanical properties owing to solid solution hardening and beta phase stabilization. Si yielded titanium silicides and Si addition over 1 wt% resulted in poor ductility due to coarse silicide chains at prior beta boundaries. The optimum composition was found to be Ti-4Fe-(0.5-1)Si in the viewpoint of tensile strength and ductility which are comparable to the Ti-6Al-4V. The metal-mould reaction was also examined for Ti-xFe and Ti-xSi binary alloy system. The thickness of surface reaction layer w as not affected significantly with Fe content, while it was decreased with Si content. In the Ti-4Si alloy, no reaction layer was found. The depth of surface hardening layer was about $200\mum$ regardless of the mould materials.

  • PDF

초듀랄류민(A2024-T3)의 절삭거동에 관한 연구 (The Study on the Cutting Behavior of Super Duralumin(A2024-T3))

  • 전태옥;박흥식;예규현
    • 한국정밀공학회지
    • /
    • 제9권4호
    • /
    • pp.147-153
    • /
    • 1992
  • This study was undertaken to investigate the cutting behaviour of super duralumin (A2024-T3) with sintered carbide tool(P20). The cutting test was carried out under different conditions such as cutting speed, cutting depth and rake angle, etc. The specific cutting force Kc and Kt of vertical and radial forces decreases as cutting speed increases, especially the decrease rate of Kt becomes larger than of Kc as cutting speed increases. Kc and Kt in small cutting depth are much affected by work-hardening of surface layer. The chip width and shear angle become layer as cutting depth increases, especially chip width at feed of 0.1mm almost approaches cutting width. Relation between the friction coefficient of chip side and tool rake angle side can make the modelization studying the built-up edge size. The shear angle model equation of super duralumin generally agree with theory of Ernst-Merchant.

  • PDF

Sursulf 처리후 고주파 표면경화된 저탄소강의 경도 및 마모특성에 미치는 Sursulf 처리시간 및 고주파 경화 이송속도의 영향 (The Effect of Sursulf Treating Time and Traveling Speed during Induction Hardening on Hardness and Wear Characteristics of Low Carbon Steel Combined-Heat-Treated)

  • 노용식;김영희;이평호;신호강;이상윤
    • 열처리공학회지
    • /
    • 제2권2호
    • /
    • pp.17-26
    • /
    • 1989
  • This study has been performed to investigate into some effects of the Sursulf treatment time and the traveling speed of surface hardening treatment on the hardness and the wear characteristics by applying the combined heat treating techniques of Sursulf process followed by induction hardening treatment to mild steel. It has been shown that increasing the Sursulf treatment time increases the case depth, but both hardness and wear resistance are not considerably improved. When the combined heat treating technique of high frequency induction heating after Sursulf treatment is applied, an improvement in case depth as well as wear resistance is obtained. In particular, the hardness in diffusion zone is greatly increased due mainly to the formation of martensite and possibly lower bainite. Iron oxides formed during induction heating and subsequent water spray cooling in the outermost part of compound layer may be considered to cause some increases in hardness and wear resistance.

  • PDF

수소주입시킨 다상조직강의 Subsurface Zone 내 취성화 거동 (A Behavior of Embrittlement at the Subsurface Zones of Multiphase Steels Charged with Hydrogen)

  • 강계명;박재우;최종운
    • 한국표면공학회지
    • /
    • 제46권1호
    • /
    • pp.48-53
    • /
    • 2013
  • In the present work, it was investigated a behavior of hydrogen embrittlement at the subsurface zones of 590 DP steels by using the micro-Vickers hardness test. The micro-Vickers hardnessess of DP steels were measured to evaluate the degree of embrittlement as the effective hardening depths of subsurface zones with hydrogen charging conditions. The results showed that the distributions of micro-Vickers hardness in width varied from maximum hardness 239.5 Hv to minimum hardness 174 Hv, while the depth of effective hardening layer at the subsurface zones of DP steels was from $320{\mu}m$ to $460{\mu}m$ with hydrogen charging conditions, respectively. It was proposed that the distribution of microhardness be used as the evaluation index of the degree of embrittlement. But the variations of martensite volume fractions were not affected along depth of hardening at the same changing time, hydrogen charging times were appeared as an effective factor of the degree of embrittlement. Therefore, the micro-Vickers hardness test is an attractive tool for evaluation of hydrogen embrittlement at the subsurface zones of these DP steels.

복합열처리(複合熱處理)한 연강(軟鋼)의 표면경화(表面硬化)에 관한 연구 (A Study on Surface Case Hardening of Blend Heat Treated Mild Steel)

  • 정인상;전해동;신석목
    • 열처리공학회지
    • /
    • 제5권1호
    • /
    • pp.23-31
    • /
    • 1992
  • It is investigated that Fe-C-N compound layer, defusion layer, and induction hardened layer produced by nitrocarburizing blend heat treatment in austenitic temperature with high frequency induction heating of mild steel specimen sprayed sursulf salt-bath. As the temperature of blend-heat treatment got increased, the thickness and hardness of compound layer and diffusion layer were increased. Compound layer(max. $35{\mu}m$), diffusion layer (max. 2.5mm) and induction hardened layer were gained in the shortest time 10 sec and in the case of $1000^{\circ}C$ total hardness depth of those was about 3.5mm. When the blend-heat treated specimen was reheated, maximum hardness of compound layer was dropped more than that of the reheated compound layer after sursulf treated, whereas hardness of diffusion layer was increased.

  • PDF

유한요소법을 이용한 레이저 표면경화처리 공정변수의 민감도 해석 (Sensitivity Analysis of Processing Parameters for the Laser Surface Hardening Treatment by Using the Finite Element Method)

  • 이세환;양영수
    • Journal of Welding and Joining
    • /
    • 제19권2호
    • /
    • pp.228-234
    • /
    • 2001
  • A methodology is developed and used to evaluate the response sensitivity of the thermal systems to variations in their design parameters. Technique for computing the sensitivity of temperature distributions to changes in processing parameters needed to decide the more effective laser input parameters for laser surface hardening treatment is considered. In this study, a state equation governing the heat flow in laser surface treatment is analyzed using a three-dimensional finite element method and sensitivity data of the processing parameter obtained using a direct differentiation method is applied to the sensitivity analysis. The interesting processing parameters are taken as the laser scan velocity and laser beam radius ( $r_{ b}$), and the sensitivities of the temperature T versus v and $r_{b}$ are analyzed. These sensitivity results are obtained with another parameters fixed. To verify the numerical analysis results, hardened layer dimensions (width and depth) of the numerical analysis are compared with the experimental ones.nes.

  • PDF

훼로보론과 NaBF4 에 의한 강재의 침 경화처리에 관하여 (Study on the Boriding of Steel in Ferroboron and NaBF4 Powder Mixture)

  • 김문일;여운관
    • 한국표면공학회지
    • /
    • 제8권3호
    • /
    • pp.5-11
    • /
    • 1975
  • The boronizing method using ferroborn and NaBF4 powder mixture was studied for surface hardening of medium carbon steel. This boride layer was compared with a boride layer that was formed in ferroboron and KBF4 powder mixture. The frequency factor and activation energy were discussed in this paper. The main results obtained can be summerized as follow. 1) The optimum range of NaBF4 content is 10 to 15% of weight to obtain a thick and dense boride layer. 2) The depth of the boride layer was approximately expressed by the following equation : {{{{d=100 exp (-18,000/RT) SQRT { t} }} 3) The oxidating resistance of boronized steel proved to be good at 800$^{\circ}C$ but almost unacceptable near at 900 $^{\circ}C$. 4) The NaBF4 effect was the same as that reported for KBF4.

  • PDF

레이저 표면 경화처리 긍정변수의 민감도 해석에 관한 연구 (A study on the sensitivity analysis of processing parameters for the laser surface hardening treatment)

  • 이세환;양영수
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2000년도 특별강연 및 추계학술발표대회 개요집
    • /
    • pp.260-263
    • /
    • 2000
  • A methodology is developed and many used to evaluate the response sensitivity of the thermal systems to variations in their design parameters. Technique for computing the sensitivity of temperature distributions to changes in processing parameters needed for deciding the more effective laser input parameters for laser surface hardening treatment are considered. In this study, a state equation governing the heat flow in laser surface treatment is analyzed using a three-dimensional finite element method and sensitivity data of the processing parameter obtained using a direct differentiation method applied for sensitivity analysis. The interesting processing parameter is taken as the laser scan velocity and characteristic beam radius( $r_{b}$) of the sensitivity of the temperature T versus v and $r_{b}$ is analyzed. And these sensitivity results obtained in another parameters are fixed condition. To verifying the numerical analysis results, hardened layer dimensions (width and depth) of the numerical analysis compared with the results of an experimental data.ata.

  • PDF