• 제목/요약/키워드: Handness

검색결과 6건 처리시간 0.017초

오스템퍼 처리(處理)한 구상흑연주철(球狀黑鉛鑄鐵)의 강인화(强靭化)에 관(關)한 연구(硏究)(1) (The Study on the Strength and Toughness of Austempered Ductile Cast Iron)

  • 이영기;김석원;김동건;이방식
    • 한국주조공학회지
    • /
    • 제10권2호
    • /
    • pp.144-153
    • /
    • 1990
  • Ductile cast iron has good ductility and toughness, for the graphite morphology is spheroidal. It has been reported that the strengthening and toughening of the ductile cast iron was resulted from the modification of matrix structure by the heat treatment or the addition of alloying elements. In this study, effects of various special heat treatments (cyclic heat treatment and intermediate heat treatment) and Ni addition on the toughness and strength of the austempered ductile cast iron were studied. The results obtained from this study were as follows : 1. The amount of fine pearlite was increased with the Ni content and the number of cycle in cyclic heat treatment. 2. When the specimens treated and not by special heat treatment at 820 was austempered, in the former the austenite was formed on grain boundary entirely, but in the latter on grain boundary partially. 3. The impact energy was decreased with the Ni content, because the coarisen austenite pools formed with the Ni content was transformed into martensite during quenching. 4. The mechanical properties of austempered ductile cast iron containing 2%Ni treated cyclic heat treatment(5 cycles)was very excellent in handness 99(HRB), impact energy 12(kg-m) maximum fracture load 1500(kg-f).

  • PDF

유행성 출혈형 폐염양 질환의 병원체에 관한 연구 (Comparative Analysis of Leptospira Isolated in Korea and Leptospira from ATCC)

  • 김주덕;이태윤;이원영;이봉기
    • 대한미생물학회지
    • /
    • 제21권2호
    • /
    • pp.191-204
    • /
    • 1986
  • Leptospira isolated from the patients with so called epidemic pulmonary hemorrhagic fever were comparatively studied with standard strains obtained from ATCC. The specific aim of this study was to clarify the morphologic heterogeneity of the isolates, i. e., coexistence of spiral forms in both handness, right and left, rod and spherical forms in their population by comparing them with those of the ATCC strains. No differences between our strains and ATCC strains were noticed in their growth characteristics, responses to the culture media, temperature, antibiotics and antifungal agents. Furthermore, the morphologic heterogeneity had been repeatedly observed even in cultures of standard ATCC strains, which had been noticed in the cultures of bacteria isolated in this laboratory. The serologic analysis of our isolates demonstrated that the bacteria reacted with L. icterohaemorrhagiae and L. australis regardless their differences in time of isolation(1984, 1985). Thus, it was concluded that the spiral bacteria isolated in this laboratory are Leptospira of a new serovar which still remained to be determined. And the previous reports on the morphology of the Leptospira, which described that the Leprospira population has only spiral forms with right. handed coils might be reconsidered.

  • PDF

오스템퍼링 조건과 Mn의 양이 ADI의 기계적 성질에 미치는 영향 (Effect of Austempering Factors and Mn Addition on Mechanical Properties of ADI)

  • 서관수;예병준
    • 한국주조공학회지
    • /
    • 제12권5호
    • /
    • pp.390-396
    • /
    • 1992
  • In this study, we investigated effect of austempering factors and Mn addition on mechanical properties of ADI with ferrite-bainite matrix by pearlite-bainite transformation treatment. Ductile cast iron specimens containing various of Mn were austenitized at 875$^{\circ}C$ for 350 sec or 925$^{\circ}C$ for 160 sec and then austempered at 300$^{\circ}C$ or 400$^{\circ}C$ for the various periods(5 to 30 min). Manganese increased pearlite volume fraction in as cast ductile cast iron. The obtained results are as follows ; 1) In austenitizing, hardness of sepecimens austenitized at 875$^{\circ}C$ for 350 sec was higher than that of 925$^{\circ}C$ for 160 sec. 2) In effect of austempering temperature, tensile strength and handness of specimens austempered at 300$^{\circ}C$ was higher than that of 400$^{\circ}C$. However, elongation had reverse tendency. 3) Increasing austempering time decreased hardness due to the increment of bainite and retained austenite fractions. However, toughness are increased.

  • PDF

치과용 아말감의 미세경도에 관한 실험적연구 (AN EXPERIMENTAL STUDY ON THE MICROHARDNESS OF DENTAL AMALGAMS)

  • 신동훈
    • Restorative Dentistry and Endodontics
    • /
    • 제8권1호
    • /
    • pp.89-96
    • /
    • 1982
  • The purpose of this study is to identify the phases of four different types, low-copper lathe cut (Type II, class 1) and spherical (Type II, class 2) amalgam alloys which are made by Caulk company and high copper Dispersalloy (Type II, class 3) made by Johnson & Johnson and Tytin (Type I, class 2) made by S.S. White and to determine the Vickers hardness number on the individual phase and four different types of dental amalgam. After each amalgam alloy and Hg measured exactly by the balance was triturated by the mechanical amalgamator (De Trey), the triturated mass was inserted into the cylindrical metal mold which was 4 mm in diameter and 12mm in height and was pressed by the Instron Universal Testing machine (Model 1125) at the speed of 1mm/minute with 143$kg/cm^2$ according to the A.D.A. Specification No. 1. The Specimen removed from the mold, mounted and stored in the room temperature for 7 days. The speciman was polished with the emery paper from #220 to #1200 and finally on the polishing cloth with 0.3 and 0.05 um $Al_2O_3$ powder suspended in water. And then each specimen was etched by Allan's method and washed with Sodium Bisulfinite for 30 seconds. Finally differentiation and metallography on each phase were obtained by using metallographical microscope (Versamet, Union) and microhardness was obtained by using microhardness tester (MVH-2, Torsee). The results were as follows: 1. In the low-copper amalgam, the ${\gamma}$, ${\gamma}_1$ and ${\gamma}_2$ phase were observed and in the high-copper amalgam, the ${\gamma}$, ${\gamma}_1$. ${\epsilon}$ and ${\eta}$ phases were observed but ${\gamma}_2$ phase was not observed. 2. Among the microhardness of each amalgam phase measured under pressing a vickers diamond indenter with 2.0gm load for 30 seconds, e phase has the highest V.H.N (314 ${\pm}$ 20), and in low-copper amalgam 12 phase has the lowest V.H.N. (29${\pm}$1) and ${\eta}$ phase which was observed in high-copper amalgam has 230${\pm}$13 V.H.N and this phase is considerd to contribute to strengthen the handness in amalgam. 3. The V.H.N. measured under pressing a Vickers diamond indenter with 300.0gm load for 30 seconds in low-copper amalgam was lower than that of high-copper amalgam.

  • PDF

언어 중추 영역에 대한 기능적 자기공명영상: 시각적, 청각적 지시 과제에 관한 비교 (Functional MR Imaging of Language System : Comparative Study between Visual and Auditory Instructions in Word Generation Task)

  • 구은회;권대철;김동성;송인찬
    • 대한의용생체공학회:의공학회지
    • /
    • 제24권4호
    • /
    • pp.241-246
    • /
    • 2003
  • 정상 성인을 대상으로 언어생성과제의 시각적 지시과제와 청각적 지시과제에 대한 기능적 MR영상들을 비교하고자 하였다. 6명의 정상 성인을 대상으로 자기공명영상기기를 이용하였다 시각적, 청각적 언어 지시과제는 명사의 언어를 이용하여. 휴지기. 확성기를 각각 6번 구성하였다. 뇌의 활성영역의 휴지기와 확성기의 신호변화에 따른 데이터는 MRDx 프로그램으로 처리하였고 cross correlation 방법으로 통계 처리하였다. 시각적, 청각적 지시과제의 분석방법은 lateralization index 공식으로 뇌 반구의 활성화 voxel의 총합과 좌$.$우 반구의 픽셀 수를 구하였고, 지시 과제에 대한 활성화 영역을 “Area of Activation Cells” 값에 따라 4등급으로 분류하여 비교 분석하였다. 시간적 청각적 지시과제에서 Broca, Wernicke 영역 등에서 크기는 다르지만 모두 활성화가 관찰되었다. lateralization index에서 뇌반구의 활성화 값에 차이는 시각적 지시과제에 비해 청각적 지시과제가 높은 활성화 값을 보였다. 그러므로 언어영역에 대한 뇌의 기능적 영상을 얻는데 두 방법 모두 유용하다고 생각된다.