노즐 형상변화에 따른 HVOF 용사총에서의 유동특성에 관한 수치적 연구 (A Numerical Study on Flow Characteristics in HVOF Thermal Spray with Various Torch Shapes)

  • 백재상;김윤제
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2007년도 춘계학술대회B
    • /
    • pp.3062-3067
    • /
    • 2007
  • HVOF thermal spray guns are now being widely used to produce protective coatings, on the surfaces of engineering components. HVOF technology employs a combustion process to heat the gas flow and melt the coating materials which are particles of metals, alloys or cermets. Particle flow which is accelerated to high velocities and combustion gas stream are deposited on a substrate. In order to obtain good quality coatings, the analysis of torch design must be performed. The reason is that the design parameters of torch influence gas dynamic behaviors. In this study, numerical analysis is performed to predict the gas dynamic behaviors in a HVOF thermal spray gun with various torch shapes. The CFD model is used to deduce the effect of changes in nozzle geometry on gas dynamics. Using a commercial code, FLUENT which uses Finite Volume Method and SIMPLE algorithm, governing equations have been solved for the pressure, velocity and temperature distributions in the HVOF thermal spray torch.

  • PDF

HVOF 열용사에 의한 크롬 카바이드 코팅의 마모.마찰거동 (Tribological Behaviors of Chromium Carbide Coatings by HVOF Thermal Spraying)

  • 김장엽;임대순;이상로;변응선;이구현
    • 한국세라믹학회지
    • /
    • 제32권11호
    • /
    • pp.1315-1321
    • /
    • 1995
  • The optimal coating condition for chrominum carbide coating was selected by Taguchi method. The wear tests with coated specimens by HVOF method were performed in the temperature to 80$0^{\circ}C$. Applied normal loads were selected to be from 8N to 30N. The worn surfaces and subsurfaces were characterized by XRD, EPMA, AES and SEM. The wear track increased with increasing applied normal load, and in terms of the temperature range from 400 to $600^{\circ}C$, below that range, the wear track increased, and above that temperature ragne, the wear track decreased. The degree of oxidation caused by the test temperature and the frictional heating was responsible to the unique high temperature wear behavior chromium carbide coatings.

  • PDF

HVOF 열용사 프로세스에서의 연소특성에 관한 수학적 모델링(I): 연소생성물의 화학조성 및 단열화염온도 (Mathematical Modeling of Combustion Characteristics in HVOF Thermal Spray Processes(I): Chemical Composition of Combustion Products and Adiabatic Flame Temperature)

  • 양영명;김호연
    • 한국연소학회지
    • /
    • 제3권1호
    • /
    • pp.21-29
    • /
    • 1998
  • Mathematical modeling of combustion characteristics in HVOF thermal spray processes was carried out on the basis of equilibrium chemistry. The main objective of this work was the development of a computation code which allows to determine chemical composition of combustion products, adiabatic flame temperature, thermodynamic and transport properties. The free energy minimization method was employed with the descent Newton-Raphson technique for numerical solution of systems of nonlinear thermochemical equations. Adiabatic flame temperature was calculated by using a Newton#s iterative method incorporating the computation module of chemical composition. The performance of this code was verified by comparing computational results with data obtained by ChemKin code and in the literature. Comparisons between the calculated and measured flame temperatures showed a deviation less than 2%. It was observed that adiabatic flame temperature augments with increase in combustion pressure; the influence was significant in the region of low pressure but becomes weaker and weaker with increase in pressure. Relationships of adiabatic flame temperature, dissociation ratio and combustion pressure were also analyzed.

  • PDF

SM490B 용접부의 피로균열 성장 거동에 미치는 초고속 용사코팅 효과 (The Effect of High Velocity Oxygen Fuel Thermal Spray Coating on Fatigue Crack Growth Behavior for Welded SM490B)

  • 윤명진;최성종;조원익
    • 한국자동차공학회논문집
    • /
    • 제14권4호
    • /
    • pp.99-106
    • /
    • 2006
  • High velocity oxygen-fuel thermal spray coating of the WC-Co cermet material is a well-established process for modifying the surface properties of the structural components exposed to the corrosive and wear attacks, and also these coating are well-known method to improve the fatigue strength of material. In this study, HVOF coated SM490B are prepared to evaluation of the effect of coating on tension and fatigue crack growth behavior. The pre-crack of the fatigue crack growth test specimens machined at deposited material area, heat affected zone and boundary, respectively. Through these test, the following results are obtained: 1) Tensile strength was about 498 MPa, and fracture occurred on base metal area. 2) The fatigue crack of coated specimens propagated more rapidly than non-coated specimen in all specimens. 3) In the same coating thickness specimens, the specimens with pre-crack at boundary more rapidly propagated than the specimens with pre-crack at HAZ and deposited material area. These results can be used as basic data in a structural integrity evaluation of rolled SM490B weldments considering HVOF coating.

스프레이 코팅 기술 (Spray Coating Technology)

  • 이창희
    • 한국분무공학회지
    • /
    • 제13권4호
    • /
    • pp.193-199
    • /
    • 2008
  • Spray coating is a versatile surface modification technology in which coating is built-up based on the successive deposition of micron-scaled particles. Depending on the coating materials, the coatings can meet the required mechanical properties, corrosion resistance, and other properties of base materials. Spraying processes are mainly classified into thermal and kinetic spraying according to their bonding mechanism and deposition characteristics. Specifically, thermal spraying process can be further classified into many categories based on the design and mechanism of the process, such as frame spraying, arc spraying, atmospheric plasma spraying (APS), and high velocity oxygen-fuel (HVOF) spraying, etc. Kinetic spraying or cold gas dynamic spraying is a newly emerging coating technique which is low-temperature and high-pressure coating process. In this paper, overall view of thermal and kinetic spray coating technologies is discussed in terms of fundamentals and industrial applications. The technological characteristics and bonding mechanism of each process are introduced. Deposition behavior and properties of technologically remarkable materials are reviewed. Furthermore, industrial applications of spray coating technology and its potentials are prospected.

  • PDF

MCrAlY 열차폐 코팅의 고온산화 (High temperature oxidation of MCrAlY thermal barrier coating)

  • 고재황;이동복
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2003년도 춘계학술발표강연 및 논문개요집
    • /
    • pp.219-219
    • /
    • 2003
  • HVOF(High Velocity Oxygen Fuel)법을 사용한 MCrAlY(M=Ni, Co, Fe)계 열차폐 코팅(thermal barrier coating)은 열기관 내부의 극심한 환경 부하에 대해 구조물 표면에 열적, 화학적 장벽을 형성함으로써 구조물의 내구성을 향상시킨다 이와 동시에 열차폐 효과는 구조물의 온도상승 없이 내부 가동 온도를 높일 수 있게 함으로써 열효율을 상승시키고 연료 효율을 높여 가동비용 절감을 이룰 수 있는 동시에 고 연소를 통한 오염원의 배출을 감소시킬 수 있다. 본 연구에서는 $H_2O$$_2$=5:1 분위기 하에서 HVOF법을 사용하여 Hastelloy-X 기판위에 125$\mu\textrm{m}$의 두께로 다음 5종류의 (Ni, Co, Cr)계 MCrAlY 코팅을 용사시켰다. 준비된 (Ni, Co)-Cr-Al-(Y, Ta, Re), (Ni, Co)-Cr-Al-(Y, Re), (Ni, Co)-Cr-Al-(Y, Ta), (Ni, Co)-Cr-Al-Y, (Ni,Co)-Cr-Al-Ir 코팅시편에 대한 산화성질을 조사하기 위해 대기 중 1000, 1100, 120$0^{\circ}C$에서 50, 100, 150, 200시간 등온실험(Isothermal oxidation)을 실시하였고, XRD, SEM/EDS, EPMA를 이용하여 생성된 산화막과 코팅 시편의 조직 변화를 조사하였다. 산화온도와 산화시간이 증가할수록 산화막의 박리가 많이 발생하였으며, 분석 결과 미세하게 분포된 a-Al$_2$O$_3$ 입자, NiCr$_2$O$_4$스피넬 상, 미세한 Cr$_2$O$_3$가 관찰되었고, 코팅 조성 변화에 따라 형성되는 이들 산화물의 존재비가 달라졌으며, 산화온도가 높아질수록 산화속도가 가속화되었다.

  • PDF

TBC/CoNiCrAlY 용사코팅의 열싸이클 특성 (Thermal cyclic characteristics of TBC/CoNiCrAlY thermal barrier coatings)

  • 김의현;유근봉
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2006년도 춘계 학술대회 개요집
    • /
    • pp.45-47
    • /
    • 2006
  • The rotating components in the hot sections of land-based gas turbine are exposed to severe environments during several tens thousand operation hours at above $1100^{\circ}C$ operation temperature. To protect such components from high temperature oxidation, an intermediate bond coat is applied, typical of a MCrAlY-type metal alloy. This study is concerned with the thermal cyclic behavior of thermal barrier coatings. The MCrAlY bond coatings are deposited by HVOF (High Velocity Oxygen Fuel) method on a nickel-based superalloy (GTD-111). Thermal cyclic tests at $1100^{\circ}C$ in ambient air for various periods of time were used to evaluate the thermal cyclic resistance of the TBC coating. The microstructure and morphology of as-sprayed and of thermal cycled coatings were characterized by scanning electron microscopy (SEM) equipped with energy dispersive spectroscopy (EDS) and X-ray diffraction (XRD).