Si(100)기판상에 3C-SiC결정성장 (Crystal growth of 3C-SiC on Si(100) Wafers)

  • 정연식;정귀상
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2002년도 하계학술대회 논문집 C
    • /
    • pp.1593-1595
    • /
    • 2002
  • Single crystal 3C-SiC(cubic silicon carbide) thin-films were deposited on Si(100) wafers up to a thickness of 4.3 ${\mu}m$ by APCVD method using HMDS(hexamethyildisilane) at $1350^{\circ}C$. The HMDS flow rate was 0.5 sccm and the carrier gas flow rate was 2.5 slm. The HMDS flow rate was important to get a mirror-like crystal surface. The growth rate of the 3C-SiC films was 4.3 ${\mu}m/hr$. The 3C-SiC epitaxial films grown on Si(100) were characterized by XRD, AFM, RHEED, XPS and raman scattering, respectively. The 3C-SiC distinct phonons of TO(transverse optical) near 796 $cm^{-1}$ and LO(longitudinal optical) near $974{\pm}1cm^{-1}$ were recorded by raman scattering measurement. The hetero-epitaxially grown films were identified as the single crystal 3C-SiC phase by XRD spectra($2{\theta}=41.5^{\circ}$).

  • PDF

Target-Composition Effect on Hydroxyapatite Thin Films Coated on Titanium by r.f. Sputtering

  • Hamagami, Jun-ichi;Kokubu, Daisuke;Umegaki, Takao;Yamashita, Kimihiro
    • The Korean Journal of Ceramics
    • /
    • 제4권4호
    • /
    • pp.372-376
    • /
    • 1998
  • Using calcium-phosphate-powder targets with the Ca/P ratios of 1.0-1.67, hydroxyapatite ($Ca_{10}(PO_4)_6(OH)_2$, HAp) thin films with 4-7㎛ thickness were prepared on titanium metal plates by r.f. magnetron sputtering, followed an annealing at $200^{\circ}C$ for 24 hr under a high water vapor pressure using an autoclave. All the specimens were systematically characterized by XRD, FT-IR, SEM and EDS analyses. The post-annealed films were confirmed to be a nonstoichiometric oxyhydroxyapatite by XRD and FT-IR measurements.

  • PDF

Local Structure and Magnetic Properties of Fe-Mn Nanocrystalline Alloys Fabricated by Mechanical Alloying Technique as a Function of Milling Time

  • Tarigan, Kontan;Yang, Dong Seok;Yu, Seong Cho
    • Journal of Magnetics
    • /
    • 제18권1호
    • /
    • pp.1-4
    • /
    • 2013
  • Structural and magnetic properties of $Fe_{50}Mn_{50}$ nanocrystalline alloys prepared by the mechanical alloying technique (using commercial Fe and Mn powders as the precursors) are studied as a function of milling time, 1 hr to 48 hrs. The nano-crystallite size and shape are examined by using scanning electron microscopy (SEM). The effect of milling time on structural characterization was investigated using X-ray diffractometer (XRD) and extended X-ray absorption fine structure spectroscopy (EXAFS). Both XRD and EXAFS studies showed that the alloying process should be completed after 36 hrs milling. Concerning the magnetic behavior, the data obtained from superconducting quantum interference devices (SQUID) exhibited both magnetic saturation ($M_s$) and coercivity ($H_c$) depend strongly on the milling time, which are related to the changes in the crystallite size and magnetic dilution.

수소제조용 CdS 입자막 전극의 표면처리 효과 (Effect of Surface Treatment on Hydrogen Production of Cadmium Sulfide Particulate Film Electrodes)

  • 장점석;장혜영;소원욱;이영우;문상진
    • 한국수소및신에너지학회논문집
    • /
    • 제11권3호
    • /
    • pp.119-125
    • /
    • 2000
  • 가시광선을 이용하여 수용액 상태의 황화수소부터 수소를 제조하기 위해 사용되는 CdS 입자막전극의 광효율 개선과 광안정성 향상을 위해 막전극을 표면처리하였다. CdS 입자막 전극에 사용되는 CdS 입자는 $Cd{NO_3}{\cdot}9H_2O$$Na_2S{\cdot}4H_2O$의 혼합 침전법에 의해 제조하였다. 입자 결정상을 제어하기 위해 고압반응기에서 온도를 바꿔가며 12시간 동안 수열처리하였다. 이렇게 제조된 CdS 졸을 이용하여 캐스팅법으로 막전극을 제조하였으며, $TiCl_4$ 수용액을 사용하여 후처리 하였다. CdS 입자의 결정상은 XRD pattern으로 확인하였고, 평균 일차입자크기는 XRD pattern과 Scherrer 식에 의해 계산하였다. 입자 형상과 막 표면 형태는 SEM으로 관찰하였다. 수소 발생은 Xe램프가 장착된 연속흐름 광반응 장치를 이용하여 광전기화학적 방법과 광화학적 방법으로 각각 측정하였다. $TiCl_4$로 표면처리한 막전극의 광전류는 처리하지 않았을 때 보다 평균 2배가량 증가한 $4.0mA/cm^2$ 정도를 나타내었다. 수소발생량도 $2.4{\times}10^4mol/hr$ 정도로서 처리하지 않았을 때 보다 크게 증가하였다.

  • PDF

HMDS 가스원을 이용한 3C-SiC의 결정성장 (Crystal Growth of 3C-SiC Using HMDS Gas Source)

  • 선주헌;정연식;정귀상
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 하계학술대회 논문집 Vol.3 No.2
    • /
    • pp.735-738
    • /
    • 2002
  • Single crystal 3C-SiC(cubic silicon carbide) thin-films were deposited on Si(100) substrate up to a thickness of $4.3{\mu}m$ by APCVD method using HMDS(hexamethyildisilane) at $1350^{\circ}C$. The HMDS flow rate was 0.5 sccm and the carrier gas flow rate was 2.5 slm. The HMDS flow rate was important to get a mirror-like crystal surface. The growth rate of the 3C-SiC films was $4.3{\mu}m/hr$. The 3C-SiC epitaxical films grown on Si(100) were characterized by XRD, AFM, RHEED, XPS and raman scattering, respectively. The 3C-SiC distinct phonons of TO(transverse optical) near $796cm^{-1}$ and LO(longitudinal optical) near $974{\pm}1cm^{-1}$ were recorded by raman scattering measurement. The heteroepitaxially grown films were identified as the single crystal 3C-SiC phase by XRD spectra$(2{\theta}=41.5^{\circ})$.

  • PDF

Si(100) 기판 위에 성장돈 3C-SiC 박막의 물리적 특성 (Physical Characteristics of 3C-SiC Thin-films Grown on Si(100) Wafer)

  • 정귀상;정연식
    • 한국전기전자재료학회논문지
    • /
    • 제15권11호
    • /
    • pp.953-957
    • /
    • 2002
  • Single crystal 3C-SiC (cubic silicon carbide) thin-films were deposited on Si(100) wafer up to the thickness of 4.3 ${\mu}{\textrm}{m}$ by APCVD (atmospheric pressure chemical vapor deposition) method using HMDS (hexamethyildisilane; {CH$_{3}$$_{6}$ Si$_{2}$) at 135$0^{\circ}C$. The HMDS flow rate was 0.5 sccm and the carrier gas flow rate was 2.5 slm. The HMDS flow rate was important to get a mirror-like crystal surface. The growth rate of the 3C-SiC film was 4.3 ${\mu}{\textrm}{m}$/hr. The 3C-SiC epitaxial film grown on Si(100) wafer was characterized by XRD (X-ray diffraction), AFM (atomic force microscopy), RHEED (reflection high energy electron diffraction), XPS (X-ray photoelecron spectroscopy), and Raman scattering, respectively. Two distinct phonon modes of TO (transverse optical) near 796 $cm^{-1}$ / and LO (longitudinal optical) near 974$\pm$1 $cm^{-1}$ / of 3C-SiC were observed by Raman scattering measurement. The heteroepitaxially grown film was identified as the single crystal 3C-SiC phase by XRD spectra (2$\theta$=41.5。).).

Si(100) 기판상에 성장된 3C-SiC의 특성 (Characterization of 3C-SiC grown on Si(100) water)

  • 나경일;정연식;류지구;정귀상
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 추계학술대회 논문집 Vol.14 No.1
    • /
    • pp.533-536
    • /
    • 2001
  • Single crystal cubic silicon carbide(3C-SiC) thin film were deposited on Si(100) substrate up to a thickness of $4.3{\mu}m$ by APCVD(atmospheric pressure chemical vapor deposition) method using hexamethyildisilane(HMDS) at $1350^{\circ}C$. The HMDS flow rate was 0.5 sccm and the carrier gas flow rate was 2.5 slm. The HMDS flow rate was important to get a mirror-like. The growth rate of the 3C-SiC films was $4.3{\mu}m/hr$. The 3C-SiC epitaxical layers on Si(100) were characterized by XRD(X-ray diffraction), raman scattering and RHEED(reflection high-energy electron diffraction), respectively. The 3C-SiC distinct phonons of TO(transverse optical) near $796cm^{-1}$ and LO(longitudinal optical) near $974{\pm}1cm^{-1}$ were recorded by raman scattering measurement. The deposition films were identified as the single crystal 3C-SiC phase by XRD spectra($2{\theta}=41.5^{\circ}$). Also, with increase of films thickness, RHEED patterns gradually changed from a spot pattern to a streak pattern.

  • PDF

2 inch Si(100)기판위에 성장된 3C-SiC 박막의 결정특성 (Crystal Characteristics of 3C-SiC Thin-films Grown on 2 inch Si(100) wafer)

  • 정수용;정연식;류지구;정귀상
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 추계학술대회 논문집 Vol.15
    • /
    • pp.452-455
    • /
    • 2002
  • Single crystal 3C-SiC(cubic silicon carbide) thin-films were deposited on Si(100) substrate up to a thickness of $4.3{\mu}m$ by APCVD method using HMDS(hexamethyildisilane) at $1350^{\circ}C$. The HMDS flow rate was 0.5 sccm and the carrier gas flow rate was 2.5 slm. The HMDS flow rate was important to get a mirror-like crystal surface. The growth rate of the 3C-SiC films was $4.3{\mu}m/hr$. The 3C-SiC epitaxical films grown on Si(100) were characterized by XRD, AFM, RHEED, XPS and raman scattering, respectively. The 3C-SiC distinct phonons of TO(transverse optical) near $796cm^{-1}$ and LO(longitudinal optical) near $974{\pm}1cm^{-1}$ were recorded by raman scattering measurement. The heteroepitaxially grown films were identified as the single crystal 3C-SiC phase by XRD spectra$(2{\theta}=41.5^{\circ})$.

  • PDF

Si(100) 기판상에 성장된 3C-SiC의 특성 (Characterization of 3C-SiC grown on Si(100) wafer)

  • 나경일;정연식;류지구;정귀상
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 추계학술대회 논문집
    • /
    • pp.533-536
    • /
    • 2001
  • Single crystal cubic silicon carbide(3C-SiC) thin film were deposited on Si(100) substrate up to a thickness of 4.3 $\mu\textrm{m}$ by APCVD(atmospheric pressure chemical vapor deposition) method using hexamethyildisilane(HMDS) at 1350$^{\circ}C$. The HMDS flow rate was 0.5 sccm and the carrier gas flow rate was 2.5 slm. The HMDS flow rate was important to get a mirror-like. The growth rate of the 3C-SiC films was 4.3 $\mu\textrm{m}$/hr. The 3C-SiC epitaxical layers on Si(100) were characterized by XRD(X-ray diffraction), raman scattering and RHEED(reflection high-energy electron diffraction), respectively The 3C-SiC distinct phonons of TO(transverse optical) near 796 cm$\^$-1/ and LO(longitudinal optical) near 974${\pm}$1 cm$\^$-1/ were recorded by raman scattering measurement. The deposition films were identified as the single crystal 3C-SiC phase by XRD spectra(2$\theta$=41.5$^{\circ}$). Also, with increase of films thickness, RHEED patterns gradually changed from a spot pattern to a streak pattern

  • PDF

Si(100)기판상에 성장된 3C-SiC의 결정 특성 (Crystal Characteristics of 3C-SiC Grown on Si(100) Wafers)

  • 정연식;류지구;선주헌;정수용;정귀상
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 춘계합동학술대회 논문집
    • /
    • pp.30-34
    • /
    • 2002
  • Single crystal 3C-SiC(cubic silicon carbide) thin-films were deposited on Si(100) wafers up to a thickness of 4.3 ${\mu}m$ by APCVD method using HMDS(hexamethyldisilane) at $1350^{\circ}C$. The HMDS flow rate was 0.5 sccm and the carrier gas flow rate was 2.5 slm. The HMDS flow rate was important to get a mirror-like crystal surface. The growth rate of the 3C-SiC films was 4.3 ${\mu}m$/hr. The 3C-SiC epitaxial films grown on Si(100) were characterized by XRD, AFM, RHEED, XPS and raman scattering, respectively. The 3C-SiC distinct phonons of TO(transverse optical) near 796 $cm^{-1}$ and LO(longitudinal optical) near $974{\pm}1cm^{-1}$ were recorded by raman scattering measurement. The heteroepitaxially grown films were identified as the single crystal 3C-SiC phase by XRD spectra($2{\theta}=41.5^{\circ}$).

  • PDF