• Title/Summary/Keyword: HDI-Biuret

Search Result 3, Processing Time 0.019 seconds

Preparation and Flame-Retardant Optimization of PU Coatings Using Pyrophosphoric Modified Polyester/HDI-Biuret (피로포스포릭 변성폴리에스테르/HDI-Biuret에 의한 PU 난연도료의 제조 및 난연최적화)

  • Shin, Dong-Il
    • Journal of the Korean Applied Science and Technology
    • /
    • v.20 no.2
    • /
    • pp.110-117
    • /
    • 2003
  • Pyrophosphoric modified polyesters (TATBs) were synthesized by polycondensation of adipic acid, trimethylolpropane, 1,4-butanediol, and tetramethylene bis(orthophosphate). Two-component PU flame-retardant coatings (TATBCs) were prepared by blending TATBs with HDI-Biuret. Most of the physical properties of the flame-retardant coatings were comparable to those of non-flame-retardant coatings. Coatings containing 10 and 15wt% 1,4-butanediol, TATBC-10C and TATBC-15C were not flammable in the vertical flame-retardancy test.

Preparation and Curing Behavior of Polyurethane Coatings by Polyester/Lactone Polyol and HDI-biuret (폴리에스테르/락톤 폴리올과 HDI-Biuret에 의한 폴리우레탄 도료의 제조 및 경화거동)

  • 최용호;김대원;황규현;박홍수;김태옥
    • Polymer(Korea)
    • /
    • v.24 no.1
    • /
    • pp.72-81
    • /
    • 2000
  • Benzoic acid polyester/lactone polyol were synthesized by polycaprolactone 0201 as diol, trimethylolpropane as triol, adipic acid as dibasic acid, and benzoic acid as monobasic acid. Polyisocyanate prepolymer Desmodur N-100 of HDI-biuret type was used in this study. Two-component polyurethane coatings were prepared by blending benzoic acid polyester/polycaprolactone, polyisocyanate, wetting/dispersing agent, white pigment, and flowing agent. Various properties were examined on the film coated with the prepared polyurethane. They showed excellent physical properties such as abrasion resistance, accelerated weathering resistance, and yellowness index. They also showed good physical properties such as flexibility, impact resistance, 60$^{\circ}$ specular gloss, cross hatch adhesion, hydrocarbon resistance, and lightness index difference. Hardness of coating showed a little poor character. The introduction of polycaprolactone 0201 as diol in the polyurethane coatings improved the hydrocarbon resistance, impact resistance, and flexibility of coatings. According to the drying and curing behavior with the contents of benzoic acid, they seem to have reasonable coating properties such as drying time of 2 to 4 hours and pot-life time of 20 to 37 hours.

  • PDF

Preparation and Curing Behavior of Two-Packaged Polyurethane Coatings by Benzoic Acid Lactone Modified Polyester/HDI-Biuret (벤조산 락톤 변성폴리에스테르/HDI-Biuret에 의한 2액형 폴리우레탄 도료의 제조 및 경화거동)

  • Seo, Kum-Jong;Kwon, Soon-Yong;Park, Hong-Soo
    • Journal of the Korean Applied Science and Technology
    • /
    • v.15 no.2
    • /
    • pp.59-66
    • /
    • 1998
  • Two-packaged polyurethane coatings were prepared by blending benzoic acid lactone modified polyester polyol(BLMPs) and HDI-biuret. BLMPs were synthesized by polycondensation of benzoic acid, viscosity depression component, with 1,4-butanediol, adipic acid, and polycaprolactone polyol. Kinematic viscosity of BLMP was gradually decreased with increasing benzoic acid content in BLMP. The low viscosity of modified polyester has an advantage of making a high-solid content coatings. After the film was coated with the prepared polyurethane coatings and cured at room temperature, the various physical properties were measured. They showed good physical properties such as flexibility, impact resistance, cross hatch adhesion, yellowness index, and rust resistance. These advantages are the results of introducing polycaprolactone polyol.