The purpose of this study is to examine the influence of the flowability and the compressive strength of concrete after the improving of grain shape of the coarse aggregate and fine aggregate fineness modulus. According to the experimental results, the coarse aggregate after improvement of grain shape it lead to be down by 6% fine aggregate ratio, from 47% to 41%. The 0.5% increase of fine aggregate fineness modulus lead to 3% increase of concrete slump, and 1% reduction of concrete air content. While compressive strength on fine aggregate fineness modulus, it was increased until fineness modulus 3.0, but after it reached by 3.5 it was decreased. The compressive strength of the coarse aggregate after improving the grain shape was decreased by 6% due to loss of the adhesion of cement paste.
본 연구는 굵은골재의 입형불량과 잔골재의 조립률 저하가 초유동콘크리트의 특성에 미치는 영향을 검토한 것이다. 이론 위해 잔골재 조립률을 2.0, 2.5, 3.0, 3.5로 변화시키고 굵은골재는 입형개선전$\cdot$후 골재를 사용하여 초유동콘크리트의 유동검 및 충전성능을 검토하였다. 또한 골재입자의 분산거리를 상대비교 함으로써 잔골재의 조립률 및 굵은골재의 입형이 골재입자의 분산거리에 미치는 영향을 검토하였다. 실험 결과 굵은골재와 잔골재 혼합시의 최소공극률은 골재 입형개선 유무에 관계없이 잔골재 조립률 3.0, 2.5, 2.0, 3.5 순으로 나타나 조립률 KS 규정 값 $2.3\~3.1$보다 작거나 클 경우 공극률을 증가시키는 것으로 나타났으며, 굵은골재의 입형은 구형율 0.69의 원반상에서 구형율 0.78의 구상으로 개선할 경우 최소공극률을 나타내는 잔골재율을 $47\%$에서 $41\%$로 $6\%$ 감소시키는 것으로 나타났다. 잔골재 조립률에 따른 28일 압축강도 특성은 조립률 2.0에서 2.5, 3.0으로 증가할수록 약 3MPa씩 증가하였으나, 조립률 3.5에서는 3.0에 비해 약 9MPa 정도 감소하였다. 또한 굵은골재의 입형개선과 잔골재 조립률의 증가는 유동성, 충전성 및 V로드 상대유하시간을 향상시키는 것으로 나타났으며, 잔골재 조립률은 KS 규정 값 $2.3\~3.1$을 만족하는 범위내에서 높은 값을 사용하는 것이 페이스트 용적비를 증가시키는 것으로 나타났다.
The vacuum molding process is one of the clean-foundry molding-processes that can recycle molding sands repeatedly, because molding can be accomplished by introducing vacuum only among dry molding sands in flask. The effects of molding conditions such as sand grain fineness, vacuum pressure and coating thickness on the fluidity of A356 Al alloy were studied and the results was obtained that the fluidity length was decreased as the sand grain fineness number and coating thikness were decreased and the vacuum pressure was increased. A large amount of heat removal from the molten metal resulting from the vacuum suction during the vacuum molding process was the principal cause of this decrease in fluidity.
The manufacture and consumption of traditional Korean rice cake is being revived due to the introduction of various desserts and confectionaries in the food industry. In order to develop this traditional food of Korea and allow various types of rice cakes to enter the market, it is essential to standardize the cooking methodology. In particular, there has been little research on Dutubpyun, a traditional food famous for its good taste. In addition, the original cooking methodology varies between cookbooks. Therefore, in order to standardize the cooking methodology for Dutubpyun referring to various cookbooks, different types Dutubpyun were made by varying the grain fineness of the glutinous rice powder to 16, 20, 30 and 40 meshes, adding up water to 10%, up sugar to 10% and up soy sauce to 5%. Subsequently, a sensory evaluation, and a test on the moisture, degree of gelatinization and hardness during storage were measured to determine the optimal grain fineness of the powder. For the sensory evaluation, where the grain sizes of the glutinous rice powder were different, the 30 and 40 mesh samples received high scores for grain fineness, moisture and chewiness. The 40 mesh samples received high scores for softness, while the overall quality was the highest in the 30 mesh samples. The moisture content during storage was $38.0{\sim}40.6%$ for the samples on the day of cooking, while it was reduced to $33.3{\sim}35%$ after 3 days of storage. Regarding the degree of gelatinization during storage, the maltose content was $2.4{\sim}2.7 mg$ for the samples on the day of cooking. After 3 days, the maltose content was $2.3{\sim}2.8 mg$ but the maltose content was higher in the 40 mesh samples than in the other samples. Regarding the change in hardness during storage, the hardness marked high in the 20 mesh samples on the day of cooking (p<0.05), while it was high in the 16 mesh samples after 3 days of storage (p<0.001). The hardness tended to increase with increasing storage time. Regarding the surface structure of the glutinous rice powder and Dutubpyun, a difference in grain fineness was clearly seen in the 15x-magnifications photograph of the rice powder structure taken by SEM. At 60x and 180x magnifications of surface of Dutubpyun, the 16 mesh samples had a uniform air gap, and a lumpy configuration. Smaller air gaps were dispersed homogeneously and similar to a net in the 20 and 30 mesh samples. The 40 mesh samples showed to a net-likes structure with cracks. Overall, for the best conditions for cooking Dutubpyun, the grain fineness of the glutinous rice power needs to be 30 mesh.
This research investigates how the fineness modulus of fine aggregates and the grain shape of coarse aggregates affects flow characteristics, packing characteristics and compressive strength characteristic. The experimental results, show that increase of the fine aggregate's fineness modulus improved concrete flow, but filling ability was high at over KS regulation extent due to segregation phenomena. It is considered that the improvement of 0.1 spherical rate was effective to concrete fluidity elevation by reducing about $6\%$ of fine aggregate ratio displays which the smallest gap rate of aggregate. Compressive strength was increased to about 0.6MPa everytime F.M. 0.1 of fine aggregate fineness is increased. However, it was decreased to about 9MPa at F.M. 3.5 compared to F.M. 3.0.
This study investigates influence of particle properties of crushed sand on the duality of concrete. The test shows that an increase of fineness modulus(FM) resulted in high slump and air contents, while compressive strength decreased due to decreased adhesion with reduction of surface area. As grain shape become rounder, the slump of concrete increased, due to reduction of internal friction, and increased air contents. The reduction of adhesion by abrasion of surface declined compressive strength during the process of manufacturing crushed sand. Increase of powder contents decreased slump and it also decreased air contents due to the effect of filling air void. In addition. using powder contents increased compressive strength, but could not find any difference of bleeding and tensile strength with particle properties.
In this paper, physical properties of fresh and hardened mortar for floor using expansion agent are described under various grain shape, grading and chloride contents of aggregates. According to experimental results, as fineness modulous increase, fluidity show high it also shows high with cement mortar using riversand and continuous distribution of grading. We can not detect any difference in fluidity according to chloride contents. Air content shows to be decreased with crushed stone having large fineness modulous and continuous distribute on of grading. chloride content does not influence on the air content. compressive strength tends to increase when crushed sand with continuous distribution of grading is used and chloride contents decreases.
An emphasis has been placed on the importance of selecting a sand for furan sand process, which ie affected by the properties of sand. Investigations have been carried out to use the domestic artificial sands for the furan sand process. For laboratory investigations, the sands have been prepared and tested for chemical analysis, loss on ignition, sieve analysis, AFS grain fineness number, grain shape, PH value, acid demand, surface shape, theoretical surface area, moisture absorption, crushing durability and compressive strength and S. S. I. of molding sands. Most commercial sands have been found to be able to be used. The main requirement of the sands has been shown to be that 3 or 4 screen sands, AFS no.40-70 (or 100), of low acid demand, good surface area and good grain shape require less resin and catalyst to give an adequate strength.
In geological engineering, grouting with Portland cement is a common technique for ground improvement, during which micro-fine cement is applied as a slurry, such that it intrudes into soil voids and decreases soil porosity. To determine the utility and behavior of cements with different Blaine values (index of cement particle fineness) for stabilization of fine sand, non-destructive and destructive tests were employed, such as laser-ray determination of grain size distribution, and sedimentation, permeability, and compressive strength tests. The results of the experimental study demonstrated a suitable mix design for the upper and lower regions of the cement-grading curve that are important for grouting and stabilization. Increasing the fineness of the cement decreased the permeability and increased the compressive strength of grouted sand samples considerably after two weeks. Moreover, relative to finer (higher Blaine value) or coarser (lower Blaine value) cements, cement with a Blaine value of $5,100cm^2/g$ was optimal for void reduction in a grouted soil mass. Overall, study results indicate that cement with an optimum Blaine value can be used to satisfy the designed geotechnical criteria.
Namdae-cheon in Gangwon-do Province, Korea, is a valuable well-preserved lagoon. The estuary of Namdae-cheon Stream is closed because of the surrounding natural sand shoal. Thus, during the dry season, river water cannot easily flow to the ocean and therefore stagnates. River water congestion causes environmental deterioration of estuaries, often by eutrophication. In this study, we examined wall disintegration in the estuary area and used it to determine appropriate measures for the conservation of estuary water quality in the future. A total of 24 sites were selected, with 13 sites on the west side and 11 sites on the east side of the estuary study area. Samples were collected and analyzed for particle size and moisture content both vertically and horizontally. Sedimentary deposition rate was measured, and subsidence analysis was performed. Particle size, water content, sedimentary deposition, and subsidence analyses indicated that flow shifted to the west during the study period. In conjunction with other variables that may affect changes in flow, these parameters can be used in future research to predict shoal breaches and associated changes in water flow direction.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.