Composite resins, commonly used in clinical practice, have been developed to improve aesthetics to obtain smooth surfaces. Although the restored composite resin has a smooth surface, it gradually becomes rough over time. Therefore, this study measured glossiness to evaluate the surface of various composite resins and attempted to evaluate the maintenance of glossiness of composite resins by observing surfaces that change to roughness. Specimens were produced using resin used in clinical practice: Gradia direct anterior (GA), Tetric N-Ceram (TN), Ceram.X Sphere TEC one (CX), Filtek Z350XT (FT), Estelite sigma quick (ES). After creating a smooth surface with slide glass, five locations were randomly selected to measure surface gloss, and the average was the representative value of the specimen. Roughness was applied to the specimen under water pouring at the same speed and pressure using SiC paper #2400, 1200, and 400. The gloss unit of different SiC papers was measured. To evaluate the gloss unit and gloss retention between composite resins, one-way analysis of variance and Tukey multiple comparisons test were used. As a result of the study, there was a difference in gloss unit of specimens produced under the same conditions. Although the degree differed depending on the composite resin, there was also a difference in gloss retention. Based on the findings, composite resins show differences in gloss due to their different characteristics. Ceram.X Sphere TEC one (CX) showing the lowest gloss retention and Estelite sigma quick (ES) showing the highest.
Gustavo Fabian Molina;Ricardo Juan Cabral;Ignacio Mazzola;Michael Burrow
Restorative Dentistry and Endodontics
/
제47권4호
/
pp.43.1-43.13
/
2022
Objectives: This study compared the surface gloss (SG), gloss retention (GR), and color stability (CS) of 2 universal resin composites after chemical (CA) and mechanical (MA) aging. Materials and Methods: Twenty disc-shaped samples of G-ænial A'Chord (GC-Europe) and Filtek Universal (3M-ESPE) were polished with sequential abrasive papers. For CA, specimens were stored in 1 mL of 75% ethanol for 15 days at 37℃, and readings (SG, GR, and CS) were obtained at baseline and 5, 10, and 15 days. For MA, specimens were subjected to 10,750 simulated brushing cycles. SG and CS were evaluated after every 3,583 cycles. SG was measured with a glossmeter (geometrical configuration: 60°), and values were expressed in gloss units. Color was measured with a spectrophotometer using the CIE-L*a*b* color system. The Student's t-test, 1-way analysis of variance, and Scheffé test were used for statistical analysis (α = 0.05). Results: G-ænial presented significantly higher SG values than Filtek (p = 0.02), with GR reductions of 5.2% (CA) and 5.3% (MA) for G-ænial and 7.6% (CA) and 7.2% (MA) for Filtek. The aging protocol had no statistically significant effect on SG or GR (p = 0.25) from baseline to the final readings. G-ænial-MA presented the lowest color difference (ΔE = 1.8), and G-ænial-CA and Filtek-CA had the largest changes (ΔE = 8.6 and ΔE = 11.8, respectively). Conclusion: G-ænial presented higher SG values and better CS. Both restorative materials demonstrated acceptable GR and CS. Aging protocols impacted these properties negatively.
자동차용 선도장 베이스코트 도료에서 사용되는 알루미늄의 입자 크기와 배향에 따른 내후성을 연구하였다. UV를 촉진하여 조사할 수 있는 QUV$^{(R)}$ (Q-LAB) 장비를 이용하여 UV 투과율의 차이에 의한 소재의 손상 정도를 관찰하였다. Conflake 형태의 입자 크기가 서로 다른 3종의 알루미늄 paste를 이용하여 자동차용 선도장 조건으로 베이스코트를 도장하고 투명 클리어를 도장하여 필름과 시편을 제조하였다. 작성된 필름을 UV 투과 장비로 측정한 결과 입자 크기가 작고 수평 배향인 EKART사의 #790을 사용 시 낮은 UV 투과율을 나타내었다. 실제 내후성 시편의 단면 조사에서도 #790, #770, #750 순으로 높은 광택 유지율을 나타내었다.
This study was carried out in order to evaluate the effects of ultra fine precipitated calcium carbonate (UFPCC) on properties of coating color, coated paper and off-set printability. It was found that blending of UFPCC increased the low-shear viscosity and water retention of coating color. The smaller the particle size, the more significant the effect of it. When the blending ratio of UFPCC was increased, brightness, whiteness and opacity of the coated paper were improved, while paper gloss was decreased due to the increase in roughness. When the UFPCC with the average particle size of $0.12{\mu}m$ was used, the ink receptivity during off-set printing was improved while print gloss was maintained or a little decreased. It was also observed that the dry-pick and wet-pick strength of coated paper were improved by the use of UFPCC. In conclusion, it is possible to produce the low gloss matt paper with the use of UFPCC since it could improve the optical properties and ink receptivity of coated paper.
To, Thi Xuan Hang;Pham, Gia Vu;Vu, Ke Oanh;Trinh, Anh Truc;Kodama, Toshiaki;Tanabe, Hiroyuki;Taki, Tohru;Nagai, Masanori
Corrosion Science and Technology
/
제2권5호
/
pp.207-211
/
2003
The weather resistance of five coatings systems based on alkyd, chlorinated rubber, epoxy, polyurethane and fluoropolymer were studied by natural exposure test and accelerated test. The coatings were exposed at Hanoi station with urban industry atmosphere and at Baichay station with marine atmosphere. The degradation of coatings was evaluated by gloss measurement and surface analysis by scanning electronic microscopy. The results obtained show that among coatings tested the gloss of polyurethane and fluoropolymer coatings remained highly and those of alkyd, chlorinated rubber and epoxy coatings were very low after two years of atmospheric exposure. Under accelerating conditions the gloss of fluoropolymer coatings remained highly after 80 cycles of testing. By comparison with accelerating test in UV-condensation chamber the conditions at atmospheric stations are more aggressive.
This study was carried in order to manufacture the high quality coated paper. High quality includes not only physical and optical properties of coated paper but also final print quality. In this study, new acrylic-styrene emulsion was polymerized in laboratory and compared with conventional styrene-butadiene latex. Low-shear viscosity of coating color was decreased with increasing acrylic-emulsion dosage. Small amount of acrylic emulsion addition increased water retention, but further addition decreased it. Acrylic-emulsion addition improved paper gloss, brightness and whiteness, but decreased PPS and opacity slightly. Ink gloss was increased with using No. 3 acrylic-emulsion due to lower ink setting properties. However No. 1 and 2 emulsion showed the opposite result. Surface strength of coated paper was increased with using No. 3 acrylic-emulsion. These results indicate that high quality coated paper can be manufactured with using No. 3 acrylic-emulsion.
Bio-binder is well known as a promising alternative binder for SB latex because it is eco-friendly and inexpensive, compared to synthetic latex. SB latex in top coating color was substituted with starch-based bio-binder to investigate its effects on the coating color and its coated paper properties. Bio-binder contributed to the increase of coating color viscosity, and the improvement of water retention. Most optical properties except opacity were deteriorated by the increase of bio-binder dosage. It was also found that the increase of bio-binder substitution in top coating color brought about the increase of roughness, and decrease of coated paper gloss, print gloss, dry and wet pick strength. However the stiffness and the ink set-off of the bio-binder coated paper were improved. Overall, mostly adverse effects of bio-binder on the properties of coating color and its paper were observed. Therefore, it is not recommended to use bio-binder as top coating color.
The water retention of coating colors can be accurately measured by devices such as an AA-GWR water retention meter whose principle of measurement is based on pressure filtration of coatings under an externally applied air pressure over a certain period of time. It was hypothesized that such devices could be also used to determine the immobilization solids(IMS) of coating colors by determining a sudden drop in the rate of dewatering, that is, a sudden change in the drainage curves. To test this hypothesis, the immobilization solids of coating colors containing various thickeners and water retention additives at different levels were first accurately measured by a modified immobilization tester based on the well-known gloss drop method, and then their values were compared with those obtained by an AA-GWR water retention tester. They agreed very well and showed that the mean of the solids differences is 0.36% in the IMS points between both methods. This good agreement was not surprising because both test methods are based on the same end-point, that is, the immobilization solids point at which menisci begin to form at the coating surface. Theoretical considerations supporting this new method for measuring the immobilization solids of coating colors are presented and some recommendations for the test method are discussed. Also, the effect of various thickeners and water retention additives on the properties and printability of coated papers is discussed.
Sole-binder formulation has been recently introduced to solve the problems of coating process and printability caused by use of natural polymer However, the decrease of natural polymer application causes another problem in paper coating. Therefore, synthetic thickener is used to get similar effect to natural polymer usage. In this study. low shear viscosity, dewatering of coating colors were measured to evaluate the performance of the alkali sensitive water retention and rheology modifiers. The effects of alkali sensitive thickener on the physical properties of coated paper and printability were also investigated. The gloss and printability of coated paper containing the synthetic flow modifier were similar or superior to those of CMC containing coated paper. This modifier was also effective to improve the problems caused by the use of starch. The results indicated that the flow modifier synthesized with alkali sensitive thickener can reduce the problems of natural polymer and could be a good substitute f3r a natural polymer.
The water retention of coating colors can be accurately measured by devices such as an AA-GWR water retention meter whose principle of measurement Is based on pressure filtration of coatings under an externally applied air pressure over a certain period of time. It was hypothesized that such devices could be also used to determine the immobilization solids (IMS) of coating colors by determining a sudden drop in the rate of dewatering, that is, a sudden change in the drainage curves. To test this hypothesis, the immobilization solids of coating colors containing various thickeners and water retention additives at different levels were first accurately measured by a modified immobilization tester based on the well-known gloss drop method, and then their values were compared with those obtained by an AA-GWR water retention tester. They agreed very well and showed that the standard deviation is only 0.14% in the IMS points between both methods. This good agreement was not surprising because both test methods are based on the same end-point, that is, the immobilization solids point at which menisci begin to form at the coating surface. Theoretical considerations supporting this new method for measuring the immobilization solids of coating colors are presented and some recommendations for the test method are discussed. Also, the effect of various thickeners and water retention additives on the properties and printability of coated papers is discussed.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.