• Title/Summary/Keyword: Gas Tungsten Arc

Search Result 109, Processing Time 0.031 seconds

Behavior of Weld Pool Shape and Weld Surface Deformation as a Function of Spot-GTA Welding Position for 304 Stainless Steel (Spot-GTA 용접자세에 따른 304 스테인리스강 용융지 표면 및 용접부 형상 거동)

  • Kang, Nam-Hyun;Park, Yeong-Do;Cho, Kyung-Mox;Singh, Jogender;Kulkarni, Anil
    • Journal of Welding and Joining
    • /
    • v.26 no.2
    • /
    • pp.62-68
    • /
    • 2008
  • Effects of gravitational orientation on gas tungsten arc welding (GTAW) for 304 stainless steel were studied to determine the critical factors for weld pool formation, such as weld surface deformation and weld pool shape. This study was accomplished through an analytical study of weld pool stability as a function of primary welding parameters (arc current and arc holding time), material properties (surface tension and density), and melting efficiency (cross-sectional area). The stability of weld pool shape and weld surface deformation was confirmed experimentally by changing the welding position. The arc current and translational velocity were the major factors in determining the weld pool stability as a function of the gravitational orientation. A 200A spot GTAW showed a significant variation of the weld pool formation as the arc held longer than 3 seconds, however the weld pool shape and surface morphology for a 165A spot GTAW were 'stable', i.e., constant regardless of the gravitational orientation. The cross-sectional area of the weld (CSA) was one of the critical factors in determining the weld pool stability. The measured CSA ($13.5mm^2$) for the 200A spot GTAW showed a good agreement with the calculated CSA ($14.9mm^2$).

AE Characteristics for Weld HAZ in SM 490A Steel (SM 490A 강의 용접 열영향부 음향방출 특성)

  • 이장규;우창기;박성완;김봉각;윤종희;인승현
    • Proceedings of the Korean Institute of Industrial Safety Conference
    • /
    • 2002.11a
    • /
    • pp.257-262
    • /
    • 2002
  • The object of this study is to investigate the effect of compounded welding through the AE (Acoustic Emission) characteristics for weld HAZ (Heat Affected Zone) on static tensile test. This study was carried out a SM 490A, high tension steel using the low hydrogen type E4316 of electronic shield metal arc welding, compound wire of $CO_2$ gas arc welding and tungsten electrode of TIG welding.

  • PDF

Fabrication of Mechanical Fatigue Flawed Specimen with Notch Processing (노치가공법에 의한 기계적 피로결함 시험편 제조)

  • Hong, Jae-Geun;Park, Ban-Uk
    • 연구논문집
    • /
    • s.32
    • /
    • pp.55-64
    • /
    • 2002
  • Performance demonstration with real flawed specimens has been strongly required for nondestructive evaluation of safety class components in nuclear power plant. Specimen has been designed to produce mechanical fatigue flaw with tension stress and fatigue flaw has been produced to control stress and cycle, for suitable roughness. Notch condition is considered for control of fracture mode. After seal welding for fracture surface, final welding was performed to complete flaw specimen with GTAW(Gas Tungsten Arc welding) and FCAW(Flux Cored Arc Welding). It was demonstrated flaw size of flawed specimen by radiographic. testing and ultrasonic testing.

  • PDF

Performance Improvement of TIG Welders Using Intelligent Control Algorithm (지능제어 알고리즘을 이용한 펄스 인버터 TIG 용접기의 성능 향상)

  • 김규식
    • Proceedings of the KIPE Conference
    • /
    • 2000.07a
    • /
    • pp.556-559
    • /
    • 2000
  • Pulse inverter-type TIG(Tungsten Inert Gas) arc welders are studied to investigate the dynamic performance of welding. Welding currents are controlled to be pulse waveforms resulting in stable are better welding performance. The hybrid-type controller is proposed to control the welding current. Todemonstrate the practical significance of our results we present some simulation results.

  • PDF

IMPROVEMENT OF GAS TUNGSTEN ARC WELDABILITY FOR FERRlTIC STAINLESS STEELS

  • Cui Li;Jeong, Ho-shin;Park, Byung-Il;Kim, Sung-Kab
    • Proceedings of the KWS Conference
    • /
    • 2002.10a
    • /
    • pp.107-112
    • /
    • 2002
  • Ferritic stainless steels would be the most important alloys under the chloride environment. They are a cheaper alternative to austenitic stainless steels [1]. The present study is related to gas tungsten arc welding (GTAW) characteristics of Type 444 stainless steels. The heat of welding leads to grain coarsening in the HAZ and in the weld metal of ferritic stainless steels because they solidify directly from the liquid to the ferritc phase without any intermediate phase transformation. It is therefore recommended that these alloys be welded with a low heat input and at high welding speeds. Attempts to improve weldability were made by using of direct current straight polarity (DCSP) and pulsed current GTAW processes in this study. Measuring weld bead, grain size and Erichsen test were performed and the effects of heat input, pulse frequency on the weld metal and HAZ were studied. The main results were obtained as followings: decreasing heat input was effective to control the width of weld both in DCSP welding and in pulsed current welding; pulsed current welding was found to refine the grain size effectively and the finest grain size was found at the frequency of 150Hz in pulsed current welding; it was found that decreasing heat input also refine the HAZs effectively and the frequency had no different effect on HAZ at the same heat input; the ductility could be improved effectively in pulsed current welding.

  • PDF

An Experimental Investigation on Low Cycle Fatigue Behavior of Alloy 617 Base Metal and Alloy 617/Alloy 617 Weld Joints (Alloy 617 모재와 용접부재의 저사이클피로 거동에 관한 실험적 고찰)

  • Choi, Pil-Ho;Kim, Seon-Jin;Kim, Woo-Gon;Kim, Min-Hwan
    • Journal of Power System Engineering
    • /
    • v.18 no.5
    • /
    • pp.115-121
    • /
    • 2014
  • Alloy 617 is the one of the leading candidate materials for intermediate heat exchangers(IHX) of a very high temperature reactor(VHTR) system. Some of the components are joined by many welding techniques and therefore the welded joints are inevitable in the construction of systems. In the present paper, the low cycle fatigue(LCF) behaviors of Alloy 617 base metal(BM) and the gas tungsten arc welded (GTAWed) weld joints(WJ) are investigated experimentally under strain controlled LCF tests. Fully axial total-strain controlled tests have been conducted at room temperature with total strain ranges of 0.6, 0.9, 1.2 and 1.5%. The weld joints have shown a lower fatigue lives compared with base metals at all the testing conditions. The weld joints have shown a higher cyclic stress response behavior than base metal. Both BM and WJ exhibited cyclic strain hardening behavior, depending on the total strain range. In addition, the strain-life parameters for BM and WJ were determined, based on Coffin-Manson equations.

Effect of weldability in shielding gases on the GTAW process of austenitic stainless steel (스테인레스강의 GTAW 기법에서 보호가스가 용접성에 미치는 영향)

  • Kim, Dae-Ju;Baek, Ho-Seong;Ryu, Seung-Hyeop;Go, Seong-Hun;Kim, Gyeong-Ju;Kim, Dae-Sun
    • Proceedings of the KWS Conference
    • /
    • 2006.10a
    • /
    • pp.63-65
    • /
    • 2006
  • The paper deals with the effect of hydrogen or helium in argon as a shielding gas on GTA welding of austenitic stainless steel. The studies were carried out in GTA(Gas Tungsten Arc) welding with a non-consumable electrode in case with different volume additions of hydrogen or helium to the argon shielding gas, i.e $5%H_2,\;10%H_2$, 30%He and 67%He. The penetration, welding voltage, microstructure and mechanical property were examined. The deepest penetration was obtained from the sample which was welded under shielding gas of $10%H_2$. The studies showed that hydrogen or helium addition to argon changes the static characteristic of the welding arc. The hydrogen or helium addition to argon increases arc power and the quantity of the material melted. The weld metal penetration depth and its width increased with increasing hydrogen or helium content. Additionally, welding voltage increased with increasing hydrogen or helium content.

  • PDF

A Study on the Characteristics of Silicon Nanopowders Produced by Transferred Type Arc Plasma Apparatus (이송식 아크플라즈마 장치에 의해 제조된 실리콘 나노분말의 특성에 대한 연구)

  • Kan, Woo-Seop;Park, Sang-Hee
    • Journal of the Korean Society of Industry Convergence
    • /
    • v.24 no.6_2
    • /
    • pp.909-917
    • /
    • 2021
  • This study was carried out experimentally on the production and properties of silicon nanopowders characteristics using a transferred type arc plasma apparatus. To investigate the properties of silicon nanopowder, the purity of argon gas(99.999%, 99.9%) and the partial pressure ratio of nitrogen gas(0~90%) were varied. The total pressure in chamber is 400Torr and the silicon chunk amount used as raw material is 300g. The power supplied to the cathode to generate arc plasma was 9~12kW/h, and the electrode was made of tungsten and graphite with a diameter of 13mm. The particle size, impurity elements and powder evaporation rate of the silicon powder were analyzed using the XRD, FE-SEM, TEM and electronic scale. According to the purity of argon gas, the silicon evaporation rate and the particle size were similar, and impurities were generated more in the case of 99.9% purity than 99.999%. When argon gas and nitrogen gas were mixed in the chamber, the silicon evaporation rate and particle size increased as the partial pressure ratio of nitrogen gas increased. In particular, when the partial pressure ratio of nitrogen gas was 80%, the silicon evaporation rate 80g/h, and the particle size was about 80~100nm.

Effect of Be Mixing Ratio on the Characteristics of TIG Welding with High Current and High Speed (대전류 고속 TIG 용접 특성에 미치는 He 혼합비의 영향)

  • Oh Dong-Soo;Kim Yeong-Sik;Cho Sang-Myung
    • Journal of Welding and Joining
    • /
    • v.23 no.3
    • /
    • pp.54-60
    • /
    • 2005
  • Tungsten Inert Gas(TIG) welding is today one of the most popular arc welding process because of its high quality welds and low equipment costs. Even if welding productivity increases with welding speed and current, this strategy is limited by the appearance of defects such as undercut and humping bead due to the depressed molten metal. The purpose of this study investigates the effect of He mixing ratio on the characteristics with high current and speed in TIG welding. The conclusions obtained permit to explain the arc start characteristics quantitatively and the maximum welding speed on stable bead formation with He mixing ratio for high current and speed TIG welding observed in experiments. Also through the relation of the maximum arc pressure and surface depression depth at high current and speed TIG welding, it made clear the mechanism of unstable bead formation.

Abrasion and Impact Wear Resistance of the Fe­based Hardfacing Weld by Dispersing the Recycled WC

  • Kang, N.H.;Chae, H.B.;Kim, J.K.;Kim, J.H.
    • International Journal of Korean Welding Society
    • /
    • v.3 no.2
    • /
    • pp.1-6
    • /
    • 2003
  • The abrasion and impact wear resistance were investigated on the hardfacing weld dispersed with the recycled hard metal(HM). The HM was composed of the tungsten carbide(WC) reinforced metal matrix composite. The cored wire filled with the 35 wt.% HM and 0­6 wt.% of the alloying element, Fe­75Mn­7C(FeMnC), was used for the gas metal arc(GMA) welding. The FeMnC addition to the 35 wt.% HM did not improve the abrasion wear property since the amount of the tungsten carbide formed was decreased with respect to the FeMnC amount. However, the 6 wt.% FeMnC addition to the 35 wt.% HM exhibited the better impact wear resistance than the hardfacing weld by the 40 wt.% HM.

  • PDF