Fabrication of Core-Sheath Nanocomposite Fibers by Co-axial Electrospinning (공축 전기방사를 이용한 Core-Sheath형 복합나노섬유의 제조)

  • Kang, Minjung;Lee, Seungsin
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.37 no.2
    • /
    • pp.224-234
    • /
    • 2013
  • This study investigates the fabrication of core-sheath nanocomposite fibers by locating germanium (Ge) and silicon dioxide ($SiO_2$) nanoparticles selectively in the sheath layer by co-axial electrospinning. Co-axially spun fibers were prepared by electrospinning a pure PVA solution and Ge/$SiO_2$/PVA solution as the core and sheath layer, respectively. Core-sheath nanocomposite fibers were electrospun under a variety of conditions that include various feed rates for the core and sheath solutions, voltages, and concentric needle diameters, in order to find an optimum spinning condition. Ge/$SiO_2$ nanocomposite fibers were also prepared by uniaxial electrospinning to compare fiber morphology and nanoparticle distribution with core-sheath nanofibers. Using scanning electron microscopy, transmission electron microscopy, and energy dispersive X-ray analysis, it was demonstrated that the co-axial approach resulted in the presence of nanoparticles near the surface region of the fibers compared to the overall distribution obtained for uni-axial fibers. The co-axially electrospun Ge/$SiO_2$/PVA nanofiber webs have possible uses in high efficiency functional textiles in which the nanoparticles located in the sheath region provide enhanced functionality.

A Study on the Removal of an Heavy Metal Ions by an Functional Nano Fibers (기능성 나노섬유에 의한 중금속 이온의 제거에 관한 연구)

  • An Hyung-Hwan
    • Journal of the Korean Society of Safety
    • /
    • v.19 no.3 s.67
    • /
    • pp.57-64
    • /
    • 2004
  • This is the study for the removal of a toxic heavy metal ions and the recycling of expanded polystyrene wastes. Thus expanded polystyrene wastes collected from the packing materials of TV or chemicals and dissolved by $80wt.\%$ solvent(N, N-Dimethylacrylamide), electrospun in DC 20kV by power supply. Generally, the electrospinning is a process of manufacture to the fibers of nanosize from polymer solution. Manufactured nanofiber mats by electrospinning were sulfonated by cone.-sulphuric acid with $Ag_2S_O_4$ catalysts for the exchange capacity of heavy metal ions and the properties of structure with sulfonated time investigated by FESEM(Feild Emission Scaning Electron Microscope). The ion exchange capacity of light metal$(Na^+)$, Cd(II) and Ni(II), and by a nanofiber mats were 1.94[mmo1/g-dry-mat), 1.72(mmol/g-dry-mat), 1.24(mmol/g-dry-mat), respectively., and water uptake content showed a similar trend with IEC. and The selectivity coefficients $K^M_H$ of Cd(II), Ni((II) ions showed 0.324, 0.228. respectively.

Nanofibers Comprising Mo2C/Mo2N Nanoparticles and Reduced Graphene Oxide as Functional Interlayers for Lithium-Sulfur Batteries (Mo2C/Mo2N 나노 입자와 환원된 그래핀 옥사이드가 복합된 나노 섬유 중간층이 적용된 리튬-황 전지)

  • Lee, Jae Seob;Yang, Ji Hoon;Cho, Jung Sang
    • Korean Chemical Engineering Research
    • /
    • v.60 no.4
    • /
    • pp.574-581
    • /
    • 2022
  • Nanofibers comprising reduced graphene oxide (rGO) and Mo2C/Mo2N nanoparticles (Mo2C/Mo2N rGO NFs) were prepared for a functional interlayer of Li-S batteries (LSBs). The well-dispersed Mo2C and Mo2N nanoparticles in the nanofiber structure served as active polar sites for efficient immobilization of dissolved lithium polysulfide. The rGO nanosheets in the structure also provide conductive channels for fast ion/electron transport during charging-discharging and ensured reuse of lithium polysulfide during redox reactions through a fast charge transfer process. As a result, the cell assembled with Mo2C/Mo2N rGO NFs-coated separator and pure sulfur electrode (70 wt% of sulfur content and 2.1 mg cm-2 of sulfur loading) showed a stable discharge capacity of 476 mA h g-1 after 400 charge-discharge cycles at 0.1 C. Furthermore, it exhibited a discharge capacity of 574 mA h g-1 even at a high current density of 1.0 C. Therefore, we believe that the proposed unique nanostructure synthesis strategy could provide new insights into the development of sustainable and highly conductive polar materials as functional interlayers for high performance LSBs.

Effect of oxyfluorination on activated electrospun carbon nanofibers for $CO_2$ storage (함산소불소화 효과에 의한 전기방사 활성탄소나노섬유의 $CO_2$ 저장)

  • Bai, Byong Chol;Kim, Jong Gu;Im, Ji Sun;Lee, Young-Seak
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 2011.05a
    • /
    • pp.219.2-219.2
    • /
    • 2011
  • The oxyfluorination effects of electrospun carbon nanofibers (OFACFs) were investigated for $CO_2$ storage. Carbon nanofibers were prepared form poly acrylonitrile / N,N-dimethylformamide solution through electrospinning method and heat treatment. Chemical activation of carbon nanofibers were carried out in order to improve the pore structure. And the surface modification of activated carbon nanofibers was conducted by oxyfluorination to improve the $CO_2$ storage on effect of introduced functional groups. The samples were labeled CF (electrospun carbon nanofiber), ACF (activated carbon nanofibers), OFACF-1 ($F_2:O_2$ = 3:7), OFACF-2 ($F_2:O_2$ = 5:5) and OFACF-3 ($F_2:O_2$ = 7:3). The functional group of OFACFs was investigated by x-ray photoelectron spectroscopy analysis. The specific surface area, pore volume and pore size of OFACFs were calculated and pore shape was estimated by the BET equation. Through the adsorption isotherm, the specific surface area and pore volume significantly decreased by oxyfluorination.

  • PDF

Fabrication of ZnO and TiO2 Nanocomposite Fibers and Their Photocatalytic Decomposition of Harmful Gases (ZnO와 TiO2 함유 복합나노섬유의 제조와 유해물질분해 성능 평가)

  • Hur, Yoon-Sun;Lee, Seung-Sin
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.35 no.11
    • /
    • pp.1297-1308
    • /
    • 2011
  • This research investigates the application of ZnO (zinc oxide) nanoparticles and $TiO_2$ (titanium dioxide) nanoparticles to polypropylene nonwoven fabrics via an electrospinning technique for the development of textile materials that can decompose harmful gases. To fabricate uniform ZnO nanocomposite fibers, two types of ZnO nanoparticles were applied. Colloidal $TiO_2$ nanoparticles were chosen to fabricate $TiO_2$ nano- composite fibers. ZnO/poly(vinyl alcohol) (PVA) and $TiO_2$/PVA nanocomposite fibers were electrospun under a variety of conditions that include various feed rates, electric voltages, and capillary diameters. The morphology of electrospun nanocomposite fibers was examined with a field-emission scanning electron micro- scope and a transmission electron microscope. Decomposition efficiency of gaseous materials (formaldehyde, ammonia, toluene, benzene, nitrogen dioxide, sulfur dioxide) by nanocomposite fiber webs with 3wt% nano-particles (ZnO or $TiO_2$) and 7$g/m^2$ web area density was assessed. This study shows that ZnO nanoparticles in colloid were more suitable for fabricating nanocomposite fibers in which nanoparticles are evenly dispersed than in powder. A heat treatment was applied to water-soluble PVA nanofiber webs in order to stabilize the electrospun nanocomposite fibrous structure against dissolution in water. ZnO/PVA and $TiO_2$/PVA nanofiber webs exhibited a range of degradation efficiency for different types of gases. For nitrogen dioxide, the degradation efficiency was 92.2% for ZnO nanocomposite fiber web and 87% for $TiO_2$ nanocomposite fiber web after 20 hours of UV light irradiation. The results indicate that ZnO/PVA and $TiO_2$/PVA nano- composite fiber webs have possible uses in functional textiles that can decompose harmful gases.

Functional Ingredients of Perilla Frutescens L. Britt Extracts and Preparation of PVA Nanoweb Containing Extracts (자소 추출물의 기능성 성분과 자소 추출물을 함유하는 PVA 나노 섬유의 제조)

  • Wang, Qian Wen;Lee, Jung-Soon
    • Textile Coloration and Finishing
    • /
    • v.29 no.4
    • /
    • pp.256-267
    • /
    • 2017
  • The purpose of this study was to analyze the functional ingredients of Perilla Frutescens L. Britt extracts and to confirm the possibility of producing PVA nanofibers using extracts. Distilled water, 3% aqueous sodium hydroxide solution and ethanol were used as extraction solvents. The electrospinning was carried out at a PVA concentration of 12%, an applied voltage of 10 kV and a tip to collector distance of 15cm. The contents of volatile substances, essential oils, total polyphenols and flavonoids of the extracts were measured to examine the constituents of functional materials. Flavor components and esters were identified in 3% sodium hydroxide and ethanol extracts. The content of polyphenols and flavonoids in ethanol extracts was higher than that of medicinal plants. 1wt.% of Tween 20 was added to disperse the essential oil components of the ethanol extract. Addition of a dispersant made it possible to produce a homogeneous mixture by having some compatibility with the ethanol extracts and the PVA molecule. When the concentration of the ethanol extract was 0.25 and 0.5wt%, relatively uniform PVA nanofiber having an average diameter of 350 to 365nm could be produced. The results of FT-IR, XRD and DSC analysis confirmed that Perilla Frutescens L. Britt ethanol extract was well mixed with PVA molecules and was electrospun.

Effect of Acid Treatment of Graphitized Carbon on Carbon Corrosion in Polymer Electrolyte Membrane Fuel Cells (결정성 탄소의 산처리가 고분자연료전지의 성능과 내구성에 미치는 영향 평가)

  • Oh, Hyung-Suk;Han, Hak-Soo;Kim, Han-Sung
    • Journal of the Korean Electrochemical Society
    • /
    • v.12 no.2
    • /
    • pp.181-188
    • /
    • 2009
  • Pt catalyst was adsorbed on Carbon nanofiber (CNF) by modified polyol method after acid treatment of the carbon support with $HNO_3$ and $H_{2}SO_{4}$. As the time for acid treatment increases, more oxygen functional groups on carbon surface were produced which improve the loading amount and dispersion of Pt catalyst on carbon supports. In order to inspect the effect of CNF acid treatment time on electrochemical corrosion, constant potential of 1.4 V was applied to a single cell for 30 min and the amount of $CO_2$ emitted was monitored with on-line mass spectrometry. According to the results of our experiment, more $CO_2$ was produced with Pt/ oxidized-CNF catalyst in compared to that with unoxidized-CNF. Increasing acid treatment time also induces the more $CO_2$ emission. Besides, performance degradation after corrosion test expanded with severer carbon corrosion. From the observed results, it can be concluded that the acid treatment of CNF is beneficial to catalyst loading, but it also is a significant factor declining the fuel cell durability by accelerating electrochemical oxidation of carbon support.

Electrochemical Energy Storage of Milled Carbon Nanofiber (탄소나노섬유의 밀링에 따른 전기화학적 에너지 저장 특성)

  • Lee, Hye-Min;Jeon, Hyeon;Choi, Weon-Kyung;Cho, Tae-Hwan
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.22 no.4
    • /
    • pp.527-533
    • /
    • 2011
  • CNFs had been well addressed due to numerous promising applications in science and technology. Besides the same physicochemical properties of ordinary carbon materials such as active carbons and carbon black, they exhibit specific, e.g., tubular or fibrous structures, a large surface area, high electrical conductivity stability, as well as extremely high mechanical strengh and modulus, which make them a superior material for electrochemical capacitors. In this study, CNFs were pretreated by mechanical milling with different time in mortar and pestle. The milled CNFs were used as active material of electrode whose electrochemical property was tested to find physicochemical characterization variation. CNF electrode milled for 5 min has the highest electric capacitance. XPS spectrum were employed to explore changes in functional group induced from mechanical milling. Crystal size was calculated to analyze change of peak from different milling time by XRD. The CNF milled for 5 min has the largest crystal size and the highest electric capacitance.

Electrospinning Fabrication of Poly(vinyl alcohol)/TiO2 Nanofibers (전기방사를 이용한 Poly(vinyl alcohol)/TiO2 나노섬유 제조)

  • Kim, Young Hun;Do, Kook Bae;Choi, Jae Young;Rabbani, Mohammad Mahbub;Han, Sang Ik;Yeum, Jeong Hyun
    • Textile Coloration and Finishing
    • /
    • v.25 no.2
    • /
    • pp.118-125
    • /
    • 2013
  • Poly(vinyl alcohol) (PVA)/titanium dioxide ($TiO_2$) composite nanofibers were produced at different $TiO_2$ concentrations (0.5, 1 and 1.5 wt.%) using the electrospinning method. The parameters of electrospinning including polymer contents, voltage and tip-to-collector distance (TCD) were optimized for fabrication process. The study showed that 7.5 wt.% PVA, 15 kV applied voltage and 15 cm TCD are the best condition to obtain uniform PVA/$TiO_2$ nanofibers. $TiO_2$ nanoparticles give significant effect in fiber morphology. $TiO_2$ content increases the diameter of the fibers and roughen the fiber surfaces. The PVA/$TiO_2$ nanofibers were characterized by scanning electron microscope (SEM), transmission electron microscope (TEM) and X-ray diffraction (XRD).

First-principle investigations of the binding between carbon nanotubes and poly(acrylonitrile)

  • Lee, Juho
    • Proceeding of EDISON Challenge
    • /
    • 2015.03a
    • /
    • pp.304-307
    • /
    • 2015
  • Carbon nanotubes (CNTs) have been widely accepted and used as the enhancer for polymer nano-composites due to their remarkable mechanical properties. Understandably, the CNT fiber-polymer matrix interface plays a major role in determining the properties of the CNT-polymer nano-composites. Here, using the LCAODFT Lab tool available on the EDISON Nano-Physics site, we performed first-principles density-functional theory calculations to determine the atomic configurations and binding energies of the CNTs in contact with polymers. For the polymer matrixes, we chose poly(acrylonitrile) (PAN), which is one of the most well-known polymer matrixes for the carbon nanofiber nanocomposites. Different chiralities and diameters of pristine CNTs were considered, and several PAN-CNT configurations were prepared based on the atomistic positions and directions of cyano group in PAN. The most favorable configuration of PAN was obtained when the PAN bound parallel to the surface of CNT. Our finding indicates the binding configurations are determined by the direction of the cyano group dominantly rather than the atomistic position of PAN, or the symmetry of CNTs. The result of increasing the length of CNT diameter suggests that PAN is inclinable to align evenly on the surface of relatively large size of CNT with the configuration parallel to the surface. These results obtained in this study will provide the starting point for the design of improved PAN-CNT composites for the next-generation ultra-strong and ultra-light carbon nanofibers.

  • PDF