• Title/Summary/Keyword: Fracture stress

Search Result 2,425, Processing Time 0.028 seconds

Study on the Fatigue Test and the Accelerated Life Test for Dental Implant using Universal-Joint Test Type (유니버설조인트 시험방식을 이용한 치과용 임플란트의 피로시험 및 가속수명시험에 관한 연구)

  • Do, Gyeong Hun;Lee, Seok Jin;Kim, Jong Mi;Kim, Sung Min
    • Journal of Applied Reliability
    • /
    • v.17 no.1
    • /
    • pp.50-57
    • /
    • 2017
  • Purpose : This paper is a comparative analysis results of the fatigue test for dental implants and accelerated life test by using a static type loading device commonly used in Korea and a dynamic type loading device (universal-joint) recommended by FDA. Methods : Fatigue tests of dental implant is based on ISO 14801 and classified into static load test and dynamic load test. The tests were carried out on three test specimens by four load stress steps under each loading device. For analysis on failure mode such as crack, fracture and permanent deformation of test specimens, we used X-ray three-dimensional computed tomography on test specimens before and after the fatigue tests. The design of the accelerated life test was based on the analysis results of the fatigue life data obtained from the dynamic load test and the statistical analysis software (Minitab ver.15) was used to analyze the appropriate life distribution. Results : As a result of the fatigue tests and the accelerated life tests at same acceleration condition under each test method, the fatigue life under the dynamic type loading device (universal-joint) was shorter than when static type loading device was applied. Conclusion : This paper can be used as a reference when the universal-joint type loading device for implants fatigue test is applied as ISO 14801.

Effect of Aging Treatment on the Microstructure and Low Temperature Tensile Properties in 5083 Aluminum Alloy Weldments (5083 Al합금 용접재의 조직 및 저온 인장성질메 미치는 시효처리의 영향)

  • Lee, T.C.;Lee, H.W.;Joo, D.W.;Lee, J.H.;Sung, J.H.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.13 no.1
    • /
    • pp.1-9
    • /
    • 2000
  • The microstructural characteristics and low temperature tensile properties between $25^{\circ}C$ and $-196^{\circ}C$ for as-welded and age hardened specimen by using Al 5083-H321 for base metal, 5083-5356 and 5083-4043 weldments have been investigated. The hardness of 5083-5356 weldment decreases with aging treatment, whereas the weld region of 5083-4043 weldment shows remarkable increase in hardness after aging due to the precipitation of fine Si particle at the grain boundaries and interiors. Low temperature tensile properties of 5083 AI base metal, 5083-5356 and 5083-4043 weldments appear to be the increment of tensile strengths and elongations at the room temperature and $-196^{\circ}C$, while the decrement of tensile properties around $-50^{\circ}C$ is shown. Through the observation of fine serration to fracture in the stress-strain curve and tensile fractography, the increment of localized deformation leading to promote the neck initiation and the increment of the dimple size cause to decrease in tensile strengths and elongations around $-50^{\circ}C$. For the tensile specimen of the 5083 base metal, 5083-5356 and 5083-4043 weldments, the reason to increase in elongation after solution and aging treatment is the diminishment of fine pit, the resolution of Mg into the matrix and the spheridization of the eutectic Si.

  • PDF

Free Vascularized Fibular Graft for the Treatment of Giant Cell Tumor (생비골 이식술을 이용한 거대세포종의 치료)

  • Han, Chung-Soo;Yoo, Myung-Chul;Chung, Duke-Whan;Nam, Gi-Un;Park, Bo-Yeon
    • Archives of Reconstructive Microsurgery
    • /
    • v.1 no.1
    • /
    • pp.31-38
    • /
    • 1992
  • The management of giant cell tumor involving juxta-articular portion has always been a difficult problem. In certain some giant cell tumors with bony destruction, a wide segmental resection may be needed for preventing to recur. But a main problem is preserving of bony continuity in bony defect as well as preservation of joint function. The traditional bone grafts have high incidence in recurrence rate, delayed union, bony resorption, stress fracture despite long immobilization and stiffness of adjuscent joint. We have attemped to overcome these problems by using a microvascular technique to transfer the fibula with peroneal vascular pedicle as a living bone graft. From Apr. 1984 to Nov. 1990, we performed the reconstruction of wide bone defect after segmental resection of giant cell tumor in 4 cases, using Vascularized Fibular Graft, which occur at the distal radius in 3 cases and at the proximal tibia in 1 case. An average follow-up was 2 years 8 months, average bone defect after wide segmental resection of lesion was 11.4cm. These all cases revealed good bony union in average 6.5months, and we got the wide range of motion of adjacent joint without recurrence and serious complications.

  • PDF

Investigation of the Thermo-mechanical Crack Initiation of the Gas Turbine Casing Using Finite Element Analysis (유한요소해석을 이용한 가스터빈 케이싱 열피로 균열발생 해석)

  • Kang, M.S.;Yun, W.N.;Kim, J.S.
    • Journal of Power System Engineering
    • /
    • v.13 no.5
    • /
    • pp.52-58
    • /
    • 2009
  • A gas turbine consists of an upstream compressor and a downstream turbine with a combustion chamber, and also the compressor and the turbine are generally coupled using a single shaft. Many casing bolts are used to assemble two horizontally separated casings, the gas turbine casing and the compressor casing, in both of axial and vertical directions. Because drilled holes for casing bolts in vertical direction are often too close to drilled holes for casing bolts in axial direction, one can observe cracks in the area frequently during operations of a gas turbine. In this study of the root cause analysis for the cracking initiating from the drilled holes of the casings of a gas turbine, the finite element analysis(FEA) was applied to evaluate the thermal and mechanical characteristics of the casings. By applying the field operation data recorded from combined cycle power plants for FEA, thermal and thermo-mechanical characteristics of a gas turbine are analyzed. The crack is initiated at the geometrical weak point, but it is found that the maximum stress is relieved when the same type of cracks is introduced on purpose during FEA. So, it is verified that the local fracture could be delayed by machining the same type of defects near the hole for casing flange bolts of the gas turbine, where the crack is initiated.

  • PDF

A Study on the Prediction Model of Shear Strength of RC Beams Strengthened for Shear by FRP (섬유보강재로 전단보강된 RC보의 전단강도예측을 위한 해석모델에 대한 연구)

  • 심종성;오홍섭;유재명
    • Journal of the Korea Concrete Institute
    • /
    • v.12 no.5
    • /
    • pp.35-46
    • /
    • 2000
  • In this paper, an analytical model is proposed to predict the shear strenth of RC beams strengthened by FRP. This predictional model is composed of two basic models-the upper bound theorem for shear failure (shear tension or shear compression criteria) and a truss model based on the lower bound theorem for diagonal tension creteria. Also, a simple flexural theory based on USD is used to explain flexural failure. The major cause of destruction of RC beams shear strengthened by FRP does not lie in FRP fracture but in the loss of load capacity incurred by rip-off failure of shear strengthening material. Since interfacial shear stree between base concrete and the FRP is a major variable in rip-off failure mode, it is carefully analyzed to derive the shear strengthening effect of FRP. The ultimate shear strength and failure mode of RC beams, using different strengthening methods, estimated in this predictional model is then compared with the result derived from destruction experiment of RC beams shear strengthened using FRP. To verify the accuracy and consistency of the analysis, the estimated results using the predictional model are compared with various other experimental results and data from previous publications. The result of this comparative analysis showed that the estimates from the predictional model are in consistency with the experimental results. Therefore, the proposed shear strength predictional model is found to predict with relative accuracy the shear strength and failure mode of RC beams shear strengthened by FRP regardless of strengthening method variable.

Development of Hybrid Fiber-reinforced High Strength Lightweight Cementitious Composite (하이브리드 섬유로 보강한 고강도 경량 시멘트 복합체의 개발)

  • Bang, Jin-Wook;Kim, Jung-Su;Lee, Bang-Yeon;Jang, Young-Il;Kim, Yun-Yong
    • Composites Research
    • /
    • v.23 no.4
    • /
    • pp.35-43
    • /
    • 2010
  • The purpose of this paper is to develop a Hybrid Fiber-reinforced High Strength Lightweight Cementitious Composite (HFSLCC) incorporated with lightweight filler and hybrid fibers for lightness and high ductility. Optimal ingredients and mixture proportion were determined on the basis of the micromechanical analysis and the steady-state cracking theory considering the fracture characteristics of matrix and the interfacial properties between fibers and matrix. Then 4 mixture proportions were determined according to the type and amount of fibers and the experiment was performed to evaluate the mechanical performance of those. The HFSLCC showed 3% of tensile strain, 4.2MPa of ultimate tensile stress, 57MPa of compressive strength and $1,660kg/m^3$ of bulk density. The mechanical performance of HFSLCC incorporated with PVA fibers of 1.0 Vol.% and PE fibers of 0.5 Vol.% is similar to those of the HFSLCC incorporated with fibers of 2.0 Vol.%.

A study on the welding conditions that affect thermal deformation and mechanical property of Al 5083 non-ferrous alloy for eco-environmental leisure ships

  • Moon, Byung Young;Kim, Kyu Sun;Lee, Ki Yeol
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.38 no.10
    • /
    • pp.1190-1199
    • /
    • 2014
  • As a considerable, experimental approach, an autocarriage type of $CO_2$ welding machine and a MIG(metal inert gas) welding robot in the inert gas atmosphere were utilized in order to realize Al 5083 welding to hull and relevant components of green leisure ships. This study aims at investigating the effect of welding conditions(current, voltage, welding speed, etc.) on thermal deformation that occurs as welding operation and tensile characteristics after welding, by using Al 5083, nonferrous material, applied to manufacturing of eco-environmental leisure ships. With respect to welding condition to minimize the thermal deformation, 150 A and 16 V at the wire-feed rate of 6 mm/sec were acquired in the process of welding Al 5083 through an auto carriage type of $CO_2$ welding feeder. As to tensile characteristics of Al 5083 welding through a MIG welding robot, most of tensile specimens showed the fracture behavior on HAZ(heat affected zone) located at the area joined with weld metal, except for some cases. Especially, for the case of the Al specimen with 5 mm thickness, 284.62 MPa of tensile strength and 11.41 % of elongation were obtained as an actual allowable tensile stress-strain value. Mostly, after acquiring the optimum welding condition, the relevant welding data and technical requirements might be provided for actual welding operation site and welding procedure specification (WPS).

Performance Examination and Comparison of Steel Beam-Column Connection in SM570TMC for Mixed-Use (고강도강 혼용 사용을 위한 SM570TMC강 보-기둥 접합부의 성능평가 및 해석 비교)

  • Kim, Moonjeong;Cho, Sukhee;Ha, Tae-Uk;Kang, Chang-Hoon;Choi, Woo-Hyuk;Kim, Jung-Hak
    • Journal of the Korean Society for Advanced Composite Structures
    • /
    • v.4 no.3
    • /
    • pp.22-29
    • /
    • 2013
  • In recent years, the construction of high-rise buildings are promoted. According to these, there are many needs about new technologies to strengthen the building performance and high-strength steel is regarded as one of these for promoting building performance. In Korea, high-strength steels which stress are over 600MPa are on market and in aborad, super high-strength steels over 1000MPa are developing and they expected to promote the building performance. But there are still doubts about applying high-strength steel members because of size effect and worry of brittle fracture. In this reports, we propose results of performance and analysis tests for use with general steel. We propose the characteristic of high-strength steels first and next the results of performance test to show they satisfy the performance that designers expect. And last, we compare the results of test and analysis for acquire the alanysis reliability in non-linear analysis with high-strength steels.

Study on Plugging Criteria for Thru-wall Axial Crack in Roll Transition Zone of Steam Generator Tube (증기발생기 전열관 확관천이부위 축방향 관통균열의 관막음 기준에 관한 연구)

  • Park, Myeong-Gyu;Kim, Yeong-Jong;Jeon, Jang-Hwan;Kim, Jong-Min;Park, Jun-Su
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.20 no.9
    • /
    • pp.2894-2900
    • /
    • 1996
  • The stream generator tubes represent an integral part of a major barrier against the fission product release to the environment. So, the rupture of these tubes could permit flow of reactor coolant into the secondary system and injure the safety of reactor coolant system. Therefore, if the crack was detected during In-Service Inspection of tubes the cracked tube should be evaluated by the pulgging criteria and plugged or not. In this study, the fracture mechanics evaluation is carried out on the thru-wall axial crack due to Primary Water Stress Corrosion Cracking in the roll transition aone of steam generator tube to help the assurence the integrity of tubes and estabilish the plugging criteria. Due to the Inconel which is used as tube material is more ductile than others, the plastic instability repture theory was used to calculate the critical and allowable crack length. Based on Leak Before Break concept the leak rate for the critical crack length and the allowable leak rate are compared and the safety of tubes was given.

Impact Fracture Behavior of Ceramic Plates Instrumented Long Bar (계장화한 긴 바를 사용한 세라믹판의 충격 파괴 거동)

  • Shin, Hyung-Seop;Bae, Young-Jun;Oh, Sang-Yeob;Kim, Chang-Uk;Chang, Soon-Nam
    • Proceedings of the KSME Conference
    • /
    • 2001.06a
    • /
    • pp.561-566
    • /
    • 2001
  • A long bar impact test to alumina plates(AD 85 and AD 90) was carried out by using fabricated impact testing apparatus. The apparatus adopting a long bar of 2.1m in length made it possible to measure directly the applied impact force to the specimen during bar impact. The dimension of specimens was $33{\times}33mm$ and thickness was 3.4mm. Confinement of D2=18mm outer diameter and D1=10.5mm inner diameter was used to provide contact pressure to the specimen. Contact pressure of p=100 or 200MPa was applied to specimen before impact test. Damage caused in those cases were compared with the case of without contact pressure. The damage of specimen was different depending upon the pressure level of confinement. The existence of confinement had suppressed the development of radial cracks from the bottom of specimen and reduced the extent of damage as compared with cases without contact pressure(p=0MPa). Because the application of contact pressure to the specimen increased the apparent flexural stiffness of specimen during bar impact, it had produced the change of developed damage in the specimen; from the radial cracks to the local contact stress dominant damage. It would contribute to the improvement of the ballistic property in ceramic plates.