Verification on the Fracture Size Estimation Using Forward Modeling Approach (순산 모델링 기법을 이용한 단열크기 추정방법 고찰)

  • 김경수;김천수;배대석;정지곤
    • The Journal of Engineering Geology
    • /
    • v.8 no.1
    • /
    • pp.1-12
    • /
    • 1998
  • The fracture size among geometric parameters of the fracture system is treated as one of the most important factors in the geotechnical and hydrogeological analysis. However, several uncertainties in data acquisition and analysis pmcess about the fracture size are not clear yet. This study presents the current status on the estimation of the fracture size and verifies the estimating method using forward modeling approach. The factors considered are the variation of fracture intersection probabilities with different assumptions on the orientation of sampling planes and fracture size by using a simulated tleee dimensional fracture network model. If it is possible to analyze precisely the fracture intersection probabilities and the characteristics of probabilistic distnbution fiom cavern walls, outcrops or boreholes,the actual fracture size developed in rock rnass can be estimated confidently.

  • PDF

Texture Development in Liquid-Phase-Sintered β -SiC by Seeding with β -SiC Whiskers

  • Kim, Won-Joong;Roh, Myong-Hoon
    • Journal of the Korean Ceramic Society
    • /
    • v.43 no.3 s.286
    • /
    • pp.152-155
    • /
    • 2006
  • Silicon carbide ceramics seeded with 10-30 wt% SiC whiskers are fabricated by hot pressing and annealing. A quantitative texture analysis including calculation of the Orientation Distribution Function (ODF) is used for obtaining the degrees of preferred orientation of the fabricated samples. The microstructure and crystallographic texture are discussed with respect to the effect of ${\beta}-SiC$ whisker seeds on the resulting fracture toughness values. The SEM microstructures and the texture data reveal a correlation between texture and fracture toughness anisotropy.

Evaluation of Fracture Resistance Characteristic for Primary Piping System of Ulchin 3,4 Nuclear Power Plants (울진 원자력 발전소 3, 4호기 1차계통 배관소재의 파괴저항특성 평가)

  • 석창성;강병구;김수용;박재실;윤병곤
    • Journal of the Korean Society of Safety
    • /
    • v.14 no.1
    • /
    • pp.25-32
    • /
    • 1999
  • The objective of this paper is to evaluate the fracture resistance characteristics of SA508 CL.1a carbon steel, TP347 stainless steel and their associated welds manufactured for primary coolant system of Ulchin 3,4 nuclear power plants. The effect of various parameters such as pipe size, welding method, chemical composition, crack plane orientation, metallography and fractography on the material properties were discussed. Test results showed that the effect of pipe size on fracture toughness is negligible while the effect of welding method on fracture toughness is significant. In addition, the drop of fracture toughness in the field fabrication weld of TP347 stainless steel is probably due to the large amount of $\sigma$-phase precipitated on the $\delta$-ferrite boundary and the large size dimples.

  • PDF

Finite Element Analysis for Fracture Criterion of PolyJet Materials (PolyJet 적층재료의 파괴기준 설정을 위한 유한요소해석)

  • Kim, Dong Bum;Lee, Geun Tae;Lee, In Hwan;Cho, Hae Yong
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.14 no.4
    • /
    • pp.134-139
    • /
    • 2015
  • PolyJet technology is an additive manufacturing (AM) technology commonly used for modeling, prototyping, and production applications. It is one of the techniques used for 3D printing. The PolyJet technique is a process that joins materials to fabricate a product from 3D CAD data in a layer-by-layer manner. The orientation of a layer can affect the mechanical properties of the product manufactured by the PolyJet technique because of its anisotropy. In this paper, tensile and shearing tests of specimens were developed with the PolyJet technique in order to study the mechanical properties according to the orientation of a layer. The mechanical properties of the specimens were determined on the basis of true stress-strain curves from tensile and shearing tests. In addition, the tensile and shearing tests were simulated under the same conditions as those of experiment, and the experiment and simulated results were compared. Through this study, the fracture criteria could be established.

Development of Random fracture network for discontinuity plane (불연속면의 확률절리망 알고리즘의 개발)

  • Ko, Wang-Kyung
    • Journal of the Korean Data and Information Science Society
    • /
    • v.11 no.2
    • /
    • pp.189-199
    • /
    • 2000
  • A major deficiency of laboratory testing of rock structure is that the structures are limited in size and therefore present a very small and highly selective sample of the rock mass from which were removed. In a typical engineering project, the samples tested in the laboratory represent only a very small fraction of one percent of the volume of the rock mass. In this paper, we calculate the representative orientation of the resultant vector, the measure of the degree of clustering, the volume of rock mass, the trace length of discontinuity spacing under underlying distributions. And we generate the random fracture networks using real data. We propose the calculating the trace length.

  • PDF

A Study on the Failure Behavior of Reinforced Clay (보강점토의 파괴거동에 관한 연구)

  • 유한규
    • Geotechnical Engineering
    • /
    • v.13 no.1
    • /
    • pp.159-168
    • /
    • 1997
  • In order to investigate the effect of parameters such as orientation and surface roughness of a reinforcing material as well as the water content of the clay matrix on the stress-strain and failure behavior of reinforced clay, uniaxial compression tests were performed on clay samples reinforced with a steel inclusion Test results showed that the increase or decrease in strength of reinforced clay samples was found to depend on the orientation of a steel inclusion as well as water content of clay samples. The possible weakening mechanism induced by reinforcement in clay samples was related to the development of cracks along the tips of interface between steel inclusion and clay matrix. A theoretical interpretation of failure behavior of reinforced clay was made by using fracture mechanics theory, and the experimental results were compared with the theoretical predictions. The predicted crack propagation direction obtained from fracture criteria for a material containing a closed crack with friction agreed reasonably well with the measured values obtained from tests.

  • PDF

A Study on the Evaluation of the Pipe Fracture Characteristic (I) (실배관 파괴특성 평가에 관한 연구 (I))

  • Park, Jae-Sil;Seok, Chang-Sung
    • Proceedings of the KSME Conference
    • /
    • 2001.06a
    • /
    • pp.345-350
    • /
    • 2001
  • In order to perform elastic-plastic fracture mechanical analyses, fracture resistance curves for concerned materials are required. 1T-CT specimen was used to obtain fracture resistance curves. But the fracture resistance curve by the 1T-CT specimen was very conservative to evaluate the integrity of the structure. And fracture resistance curve was affected by the specimen geometry and crack plane orientation. The objective of this paper is to be certain the conservativeness of the fracture resistance curve by the 1T-CT specimen and to provide the additional safety margin. For these, the fracture tests using the real pipe specimen and standard 1T-CT specimen test were performed. 4-point bending jig was manufactured for pipe test and direct current potential drop method was used to measure the crack extension and length for pipe test. From the pipe and the 1T-CT specimen test results, it was observed that the J-integral of the 1T-CT specimen test at the crack initiation point was very small compare to that of the pipe specimen test.

  • PDF

Application of A Discrete Fracture Flow and Mass Transport Simulation Technique Assessing Tightness Criteria for Underground LPG Storage Cavern (지하 LPG 저장공동의 기밀성평가를 위한 분리열극개념의 지하수유동 및 용질이동 모형 모의기법 적용)

  • 한일영;조성만;정광필
    • The Journal of Engineering Geology
    • /
    • v.5 no.2
    • /
    • pp.155-165
    • /
    • 1995
  • Fluid flow studies of fractured rocks require three-dimensional modeling of the fracture system. The stochastic discrete fracture models constructed by Monte Carlo simulation technique were applied to the analysis of groundwater flow and mass transport in fractured rock for the assessment of tightness criteria of underground LPG storage cavern. The parameters that most affect the conceptual discrete fracture modeling proved either fracture orientation or size and on the fract'lre flow interpretation proved conductive fracture intensity. The fracture transmissivity played important role in solute transport in fractured rock simulated by particle tracking approach. It was partly recognized that the calibrated stochastic discrete fracture model can be used for the tightness criteria of underground LPG storage cavern.

  • PDF

Influence of Glass Fiber Orientation on the Bi-directional GFRP Characteristics (직교이방향 GFRP 재료 특성에 미치는 유리 섬유방향의 영향)

  • Suh, Jung-Joo;Moon, Duk-Hong
    • Journal of the Korean Society of Fisheries and Ocean Technology
    • /
    • v.21 no.1
    • /
    • pp.75-81
    • /
    • 1985
  • The tensile and dielctric strength of the epoxied resin with bi-directional woven glass fibers with a laminate of two layers(G-10) are studied, and the test parameter is the angle between fiber orientation and the tensile axis. The obtained results may be summaried as follows: 1) when the angle between fiber orientation and tensile axis was varied from 0$^{\circ}$ to 45$^{\circ}$ the yield and fracture stresses have a tendency to decrease with increase in the angle. Especially, the decrease rates in the yield and fracture stresses are changed remarkably in the range of 0$^{\circ}$ to 15$^{\circ}$. 2) The fracture strain has showed the maximum value when the angle between fiber orientation and tensile axis is 45$^{\circ}$, and showed the rapid rate of change from 15$^{\circ}$ to 45$^{\circ}$. 3) For the sample with same angle between fiber orientation and tensile axis the maximum dielectric strength under compressive stress is decreased with increase in tensile stress, when the compressive stress is increased as a parameter of tensile stress. 4) When the angle between fiber orientation and tensile axis is 45$^{\circ}$, the dielectric strength showed the worst value, as the mechanical strength did.

  • PDF