• 제목/요약/키워드: Flexible OLED Display

검색결과 124건 처리시간 0.027초

Barix Thin Film Encapsulation of OLED's on Flexible and Rigid Glass substrates; high temperature performance and manufacturing aspects.

  • Chu, X.;Moro, L.;Rutherford, N.;Visser, R.J.
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2007년도 7th International Meeting on Information Display 제7권2호
    • /
    • pp.1699-1702
    • /
    • 2007
  • We will discuss encapsulation of OLEDs on both flexible and rigid glass substrates. Accelerated testing at 6CC/90RH and 85C/85RH is compared and acceleration factors for OLED and Calcium test samples are discussed.We have tested the stability and performance of our barrier coating to much higher temperatures: up to 140 C. Water Vapor Transmission rates at temperatures from 60 to 140 C are presented. Rates and methods for low cost manufacturing on a large scale are analysed

  • PDF

Multilayer transparent electrodes for flexible and inverted-geometry OLEDs

  • Yoo, Seung-Hyup;Yun, Chang-Hun;Park, Jae-Woo;Cho, Hyun-Su
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2008년도 International Meeting on Information Display
    • /
    • pp.1019-1021
    • /
    • 2008
  • Multilayer transparent electrodes (MTE) based on an ultrathin metal layer assisted by additional dielectric or semiconducting layers are investigated as electrodes in OLEDs including an inverted geometry. A special attention is paid to their tuning capability in injection behavior and to their potential for ultra-flexible electrodes.

  • PDF

Towards Super Thin OLED TVs: Barix Thin Film Encapsulation of Glass and Flexible Displays

  • Xi, Chu;Lin, Steven;Rosenblum, Marty;Visser, R.J.
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2008년도 International Meeting on Information Display
    • /
    • pp.1634-1637
    • /
    • 2008
  • We will discuss encapsulation of OLEDs on both flexible and rigid glass substrates. Accelerated testing at 6CC/90RH and 85C/85RH is compared and acceleration factors for OLED and Calcium test samples are discussed.We have tested the stability and performance of our barrier coating to much higher temperatures: up to 140 C. Water Vapor Transmission rates at temperatures from 60 to 140 C are presented. Rates and methods for low cost manufacturing on a large scale are analysed.

  • PDF

Top Emitting Organic Light Emitting Diode with a Cr Anode on Flexible Substrate

  • Chung, Sung-Mook;Hwang, Chi-Sun;Lee, Jeong-Ik;KoPark, Sang-hee;Yang, Yong-Suk;Do, Lee-Mi;Chu, Hye-Yong
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2005년도 International Meeting on Information Displayvol.II
    • /
    • pp.1374-1377
    • /
    • 2005
  • Top-emitting organic light-emitting diode (TEOLED) was fabricated on flexible substrate of PES film. Aluminum and Chromium multilayer was used as an anode of TEOLED and the TEOLEDs of Cr(20nm)/Al(100nm)/Cr(20nm)/NPB(60nm)/Alq(60nm)/LiF(1nm)/Al(2nm)/Ag(20nm)/NPB(200nm) has been fabricated on PES film and Si wafer for control device. The TEOLED on PES film which had good anode surface morphology, showed very similar device characteristics to that on Si wafer.

  • PDF

High-Performance Flexible Organic Light-Emitting Devices using Amorphous Indium Zinc Oxide Anode

  • Kang, Jae-Wook;Jeong, Won-Ik;Kim, Han-Ki;Kim, Do-Geun;Lee, Gun-Hwan;Kim, Jang-Joo
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2007년도 7th International Meeting on Information Display 제7권2호
    • /
    • pp.1425-1428
    • /
    • 2007
  • The amorphous IZO on flexible substrate (PC) shows similar electrical conductivity and optical transmittance with commercial ITO glass even though it was prepared at $<50\;^{\circ}C$. Moreover, it exhibits little resistance change during 5000 bending cycles, demonstrating good mechanical robustness. A green phosphorescent OLED fabricated on amorphous IZO on flexible PC shows maximum external quantum efficiency of ${\eta}_{ext}=13.7\;%$ and power efficiency of ${\eta}_p=32.7\;lm/W$, which are higher than a device fabricated on a commercial ITO on glass (${\eta}_{ext}=12.4%$ and ${\eta}_p=30.1\;lm/W$) and ITO on flexible PC (${\eta}_{ext}=8.5%$ and ${\eta}_p=14.1\;lm/W$).

  • PDF

Silicon Carbide Barrier Technology to Enable Flexible OLED Displays

  • Kim, Sang-Jin;Zambov, Ludmil;Weidner, Ken;Shamamian, Vasgen;Cerny, Glenn
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2007년도 7th International Meeting on Information Display 제7권1호
    • /
    • pp.452-455
    • /
    • 2007
  • This paper provides an overview on the characteristics of a-SiC:H barrier film deposited for flexible display applications. Key characteristics such as high crack resistance, high thermal/hydro stability, excellent adhesion to the polymer substrate, as well as very low permeance has been demonstrated. The excellence of this barrier film has been shown from competitive analysis compared with other barrier coating materials. Finally, flexible Polymer Light Emitting Diode (PLED) test pixels have been fabricated on the barrier coated plastic substrate, demonstrating the viability of the device with lifetime data.

  • PDF

유연 기판 위에 증착된 IZO 박막의 구조적 및 전기적 특성 (Structural and electrical characteristics of IZO thin films deposited on flexible substrate)

  • 이봉근;이규만
    • 반도체디스플레이기술학회지
    • /
    • 제10권2호
    • /
    • pp.39-44
    • /
    • 2011
  • In this study, we have investigated the structural and electrical characteristics of IZO thin films deposited on flexible substrate for the OLED (organic light emitting diodes) devices. For this purpose, PES was used for flexible substrate and IZO thin films were deposited by RF magnetron sputtering under oxygen ambient gases (Ar, $Ar+O_2$) at room temperature. In order to investigate the influences of the oxygen, the flow rate of oxygen in argon mixing gas has been changed from 0.1sccm to 0.5sccm. All the samples show amorphous structure regardless of flow rate. The electrical resistivity of IZO films increased with increasing flow rate of $O_2$ under $Ar+O_2$. All the films showed the average transmittance over 85% in the visible range. The OLED device was fabricated with different IZO electrodes made by configuration of IZO/a-NPD/DPVB/$Alq_3$/LiF/Al to elucidate the performance of IZO substrate. OLED devices with the amorphous-IZO (a-IZO) anode film show better current density-voltage-luminance characteristics than that of OLED devices with the commercial crystalline-ITO (c-ITO) anode film. It can be explained that very flat surface roughness and high work function of a-IZO anode film lead to more efficient hole injection by reduction of interface barrier height between anode and organic layers. This suggests that a-IZO film is a promising anode materials substituting conventional c-ITO anode in OLED devices.

Application of Organic TFTs to Flexible AMOLED Display Panel

  • Song, Chung-Kun;Ryu, Gi-Seong;Choe, Ki-Beom;Jung, Hyun
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2005년도 International Meeting on Information Displayvol.I
    • /
    • pp.64-67
    • /
    • 2005
  • We fabricated an array consisting of organic TFTs(OTFT) and organic LEDs (OLED) in order to demonstrate the possible application of OTFTs to flexible active matrix OLED (AMOLED). The panel was composed of $64{\times}64$ pixels on 4 inch size polyethylene-terephehalate (PET) substrate in which each pixel had one OTFT integrated with one green OLED. The panel successfully displayed some letters and pictures by emitting green light with a luminance of $1.5\;cd/m^2$ at 6 V, which was controlled by the gate voltage of OTFT.

  • PDF

전기적 기법을 통한 플렉서블 OLED 봉지막의 파괴특성 연구 (Fracture Analysis of a $SiN_x$ Encapsulation Layer for Flexible OLED using Electrical Methods)

  • 김혁진;오승하;김성민;김형준
    • 반도체디스플레이기술학회지
    • /
    • 제13권4호
    • /
    • pp.15-20
    • /
    • 2014
  • The fracture analysis of $SiN_x$ layers, which were deposited by low-temperature plasma enhanced chemical vapor deposition (LT-PECVD) and could be used for an encapsulation layer of a flexible organic light emitting display (OLED), was performed by an electrical method. The specimens of metal-insulator-metal (MIM) structure were prepared using Pt and ITO electrodes. We stressed MIM specimen mechanically by bending outward with a bending radius of 15mm repeatedly and measured leakage current through the top and bottom electrodes. We also observed the cracks, were generated on surface, by using optical microscope. Once the cracks were initiated, the leakage current started to flow. As the amount of cracks increased, the leakage current was also increased. By correlating the electrical leakage current in the MIM specimen with the bending times, the amount of cracks in the encapsulation layer, generated during the bending process, was quantitatively estimated and fracture behavior of the encapsulation layer was also closely investigated.

사용자 경험을 위한 플렉시블 디스플레이 인터페이스 디자인 (Flexible display interface design for user experience)

  • 이영주;강재신
    • 디지털융복합연구
    • /
    • 제16권1호
    • /
    • pp.287-292
    • /
    • 2018
  • ICT(Information and Communications Technologies)기술이 중심이 되는 디지털 멀티미디어 환경은 우리의 상상을 현실의 다양한 경험으로 바꾸어주었다. 고도의 정보화 사회에서 요구되는 인간과 기계의 커뮤니케이션 수단으로 탄생한 플렉시블 디스플레이(Flexible display)는 시장을 다변화시키고, 사물인터넷등과의 연계를 통해 새로운 시장을 창출해 내고 있다. 플렉시블 디스플레이의 인터페이스는 입력 또는 출력의 결과로 물리적 형태를 제공할 수 있기 때문에 사용자 중심의 인터페이스 디자인이 무엇보다 중요하다. 이에 본 논문의 연구자는 플렉시블 디스플레이의 사용자 조작에 따른 물리적 변형과 특성에 대해 문헌과 사례조사를 통해 연구했다. 연구 결과 사용자 경험을 위한 플렉시블 디스플레이 인터페이스 디자인 가이드라인을 다음과 같이 제시한다. 첫째, 다양한 형태의 디스플레이 환경에서 사용자에게 필요한 기능을 최대한 제공할 수 있도록 디자인되어야 한다. 둘째, 인터페이스를 활용함에 있어서 다중 사용자의 시야각에 방해 요소는 제거되어야 한다. 셋째 터치와 접촉 이외에 플렉시블 디스플레이에서 가능한 사용자의 모든 조작행위가 고려되어야 한다. 넷째 플렉시블 디스플레이의 가변적 상황에 따라 사용자 경험을 위한 인터페이스디자인도 달라져야 한다. 위 가이드라인은 향후 다양한 플렉시블 디스플레이가 출시된 후, 실증적인 사용자 경험에 대한 분석과 연구에 도움이 될 것으로 기대된다.