• Title/Summary/Keyword: Fire Resistance Covering

Search Result 27, Processing Time 0.027 seconds

An Experimental Study on The Fire Resistance Performance of Steel Encased Reinforcement Concrete and Steel Framed Mortar Beam with Loading Condition (철골 철근콘크리트 보 및 철골철망 모르타르조 보의 전열특성 및 화재거동에 관한 실험적 연구)

  • Kim, Hyung-Jun;Kim, Heung-Youl;Yeo, In-Hwan;Kwon, Ki-Hyuck;Kwon, In-Kyu
    • Fire Science and Engineering
    • /
    • v.26 no.1
    • /
    • pp.80-88
    • /
    • 2012
  • This study evaluates the fire resisting capacity of the beam of the legal fire resistance construction, which establishes the Article 3 of the Regulations on Escape and Fire Resistance of Buildings. There are a total of five structures that we consider as legal fire resistance constructions, however, this study has a primary target of the reinforced concrete beam, and tests the fire-resistant performance depend on the covering depth of reinforce concrete. The results showed that it meets the three hours, the maximum statutory fire resistance time, if it was a load ratio of 0.5 and covering depth of 40 cm. Steel framed mortar beam is legal fire resistance structure that it was possessed three hours fire resistance performance, if it was a load ratio of 0.4 and covering depth of 60 mm.

An Experimental Study on the Fire Resistance Performance of the Reinforced Concrete Columns According to the Cross Section Size and Depth of Concrete Cover (단면크기 및 피복두께 변화에 따른 철근콘크리트 기둥의 내화성능에 관한 실험적 연구)

  • Cho, Kyung-Suk;Yeo, In-Hwan;Cho, Bum-Yeon;Kim, Heung-Youl;Min, Byung-Yeol
    • Fire Science and Engineering
    • /
    • v.25 no.1
    • /
    • pp.78-84
    • /
    • 2011
  • Recent researches of the fire resistance in concrete focus on how to secure relevant functions in the high strength concrete. However, the demand of normal strength concrete less than 40 MPa takes most of the total concrete demand. Therefore, fire resistance study needs to cover not only high strength concretes but also normal strength concretes. This study evaluated the fire resistance performance of 40 MPa concrete columns, taking the concrete covering thickness and the size of section as variables. Consequently, the fire resistance performance improved as the section size and the covering thickness became larger.

Properties of Temperature History and Spatting Resistance of High Performance RC Column with Finishing Material (내화 마감재 종류에 따른 고성능 RC기둥의 폭열방지 및 온도이력 특성)

  • Heo Young-Sun;Kim Ki-Hoon;Lee Jin-Woo;Lee Bo-Hyeung;Lee Jae-Sam;Han Cheon-Goo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2005.05a
    • /
    • pp.37-40
    • /
    • 2005
  • High Performance Concrete(HPC) has been widely used in high-rise building. The HPC has several benefits including high strength, high fluidity and high durability. However. spatting is susceptible to occur in HPC and HPC also tends to be deteriorated in the side of fire resistance performance at fire. This paper focuses on the analysis of the temperature history and residual compressive strength with finishing material, in order to protect HPC from sudden-high-temperature, which is one of the main reason spatting occurs. Test results show that spalling occurs in all specimens. The most serious spalling took placed in HPC covering fire enduring spray-on material, whose covering thickness is 20mm but temperature history indicates that fire enduring spray effectively protected HPC from fire for more than 2hours. In addition, residual compressive strength ratio of HPC using fire enduring paint was more than $90\%$ of original strength, thus minimizing spatting and indicating significant fire resistance performance.

  • PDF

An Experimental Study on the Fireproof Covering Thickness of High Strength Concrete Members with Spray Coating (뿜칠피복재를 사용한 고강도 콘크리트 부재의 내화피복두께에 관한 실험적 연구)

  • Lee, Tae-Gyu
    • Fire Science and Engineering
    • /
    • v.24 no.4
    • /
    • pp.41-46
    • /
    • 2010
  • High strength concrete (HSC) has been mainly used in large SOC structures. HSC have superior property as well as improvement in durability compared with normal strength concrete. In spite of durability of HSC, explosive spalling in concrete front surface near the source of fire occurs serious problem in structural safety. Therefore, this study is concerned with experimentally investigation of fire resistance at high temperature due to fireproof material covering thickness in addition to concrete cover. From the test result, it was appeared that the use of fireproof material results in good performance for fire resistance and spalling prevention, and the optimal fireproof covering thickness is 1~3mm. On the other hand, the temperature was rapidly increased by explosive spalling within 30 minutes and showed very little rise caused by evaporation heat after then. It was also found that the void channel was remained at high temperature as PP fiber melts at about $200^{\circ}C$, and the pore pressure in concrete was decreased.

Spatting Resistance of High Strength RC Column Covering Spray-on Materials of Fiber Composite Spray Mortar(FCSM) (섬유복합모르터의 뿜칠마감에 의한 고강도콘크리트 기둥부재의 폭렬방지)

  • Song Yong-Won;Han Dong-Yeob;Lee Gun-Cheol;Goh Kyoung-Taek;Kim Jin-Soo;Han Cheon-Goo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2006.05a
    • /
    • pp.5-8
    • /
    • 2006
  • High strength concrete has been increasingly used in high rue building and it is very obvious re consider fire resistance performance of that. Unlike the normal strength concrete, high strength concrete in sudden elevating temperature at fire is susceptible to spalling with severe explosion and surface split, due to high density of concrete. In order to endure the spalling, inner space temperature of concrete should be control less than certain point. Therefore this study investigated the influence of covering materials on high strength concrete finishing spray-on materials of fiber composite spray mortar(FCSM). Both polypropylene(PP) and polyvinyl alcohol(PVA) fiber were used in this test. Test showed that concrete, covering 18mm mortar containing PVA fiber and confining metal lath 2.3mm thickness, decreased 50% of main bar ambient temperature. compared with control concrete. In addition, concrete covering 18mm mortar without fiber caused falling of covering materials and then it was exposed in elevating temperature. As a result, spatting of the concrete occurred same as control concrete. However, concrete covering spray-on mortar containing PVA or PP fiber resisted spatting occurrence.

  • PDF

Evaluation on Fire Resistance Performance of High Strength Concrete Containing Fibre (섬유혼입 고강도 콘크리트의 내화성능 평가)

  • Song, Young-Chan;Kim, Yong-Ro;Kim, Ook-Jong;Lee, Do-Bum
    • Journal of the Korea Institute of Building Construction
    • /
    • v.10 no.5
    • /
    • pp.129-135
    • /
    • 2010
  • The purpose of this research is to secure fundamental data on the application of fibre as a fire resistance method for more than 60 MPa high-strength concrete through an examination of mechanical properties and fire resistance performance. The results are as follows: 1) When there are less than 0.5~1.0kg/$m^3$ contents of PP and NY fibre for 60MPa and less high strength concrete, 1.0kg/$m^3$ contents of PP and NY fibre for less than 80MPa high strength concrete and 1.5kg/$m^3$ contents of NY fibre for more than 80MPa high strength concrete, the effect of fibre contents on workability and strength development is not significant. 2) Based on the result of a 3-hour fire resistance test for mock-up column, it is necessary to secure 50 mm of covering depth for the regulation of fire resistance performance of high strength concrete to the standards of The Ministry of Land, Transport and Maritime Affairs. 3) It is necessary to secure more than 400mm of column size for stable fire resistance performance.

Fire Performance of 100MPa High Strength Concrete with Fire Protection Cover (100MPa급 내화피복 고강도 콘크리트의 내화성능 인증)

  • Song, Young-Chan;Kim, Yong-Ro;Kim, Ook-Jong;Lee, Do-Bum
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2010.05b
    • /
    • pp.21-22
    • /
    • 2010
  • In this research, the purpose is to share fire resistance method to secure 3 hours fire resistance performance which is regulation noticed by Ministry of Land, Transport and Maritime Affairs for 100MPa high strength concrete which is predicted to apply to high rise building and to propose the guideline for confirmation of fire resistance performance of high strength concrete member to which fire resistance method is applied and field application in advance.

  • PDF

Fire Resistance of Repaired High Strength Concrete Column Damaged by Fire (화재 피해를 입은 고강도 콘크리트 기둥의 보수공법 변화에 따른 내화특성)

  • Park, Chun-Jin;Back, Dae-Hyun;In, Gi-Ho;Yeo, In-Hwan;Min, Byung-Yeol;Han, Cheon-Goo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2009.11a
    • /
    • pp.113-116
    • /
    • 2009
  • This study analyzed fire-resistant characteristics according to changes in repair methods of PFH mixed high-strength concrete roof structures having undergone fire damage. The results of the study are as follows. First, as a repulsive characteristics of structures, the remaining repulsion was shown to increase following fire-resistance tests according to increases in depth of coverings. The results of the relationship between depth of coverings and remaining repulsion rates following fire-proofing tests showed a high correlation. At a covering depth of 67.3mm, remaining repulsion rate was estimated to be 100%. For fire-resistant characteristics following repairs of structure, as for spalling, severe separation was shown in the case of general plaster while general plaster + Metal Lath showed overall superior spalling prevention. For internal structure temperatures, general plaster showed max temperatures of 705℃, average temperatures of 636℃ while general plaster + metal lath showed max temperature of 660℃ and average temperature of 520℃, demonstrating lower temperature distributions than use of only general plaster. In conclusion, after removing the covering of structures damaged due to high temperatures of fires within high-strength concrete installations, the use of fire-resistant mortars and applying metal laths on surfaces of general plaster will provide superior fire-resistance performance in the occurrence of a 2nd fire.

  • PDF

A Study on the Properties of Fire Endurance and Spalling of High Performance RC Column with the Finishing and Covering Material (고성능 RC 기둥의 마감재 변화에 따른 폭열 및 내화특성에 관한 연구)

  • Han, Cheon-Goo;Hwang, Yin-Seong;Ji, Suk-Won;Kim, Kyoung-Min
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.10 no.2
    • /
    • pp.143-152
    • /
    • 2006
  • High performance concrete(HPC) has been widely used in high-rise building. The HPC has several benefits including high strength, high fluidity and high durability. However, spalling is susceptible to occur in HPC and HPC also tends to be deteriorated in the side of fire resistance performance at fire. This paper investigated the spalling prevention of high performance RC column. Control concrete showed severe failure and a case of concrete with fire enduring spraying material exhibited more severe spalling failure than even control concrete. In addition, concrete with fire enduring paint reported the most favorable spalling resistance effect for preventing spall, compared with other concrete covered with finishing materials, such as fire enduring spraying material, gypsum board, marble board and fire enduring PC board. Meanwhile, concrete adding 0.1% of PP fiber demonstrated spalling resistance performance after 3hours load bearing test.

Behavior Characteristics of PCM Infilled Floor System at Elevated Temperature (고온에 노출된 PCM 충진형 바닥 시스템의 거동 특성)

  • Park, Min-Jae;Min, Jeong-Ki;Yoon, Sung-Won;Ju, Young K.
    • Journal of Korean Association for Spatial Structures
    • /
    • v.17 no.2
    • /
    • pp.33-41
    • /
    • 2017
  • Composite Floor system infilled with PCM(Phase Change Material) between upper and lower steel plates was developed to apply the steel frame. When steel frames were applied this system, it can absolutely reduce the duration of construction due to dry construction method. However to apply this system as a structural floor member without fire resistance covering, it must have 2 hours fire resistance performance. Because PCM consisted of three quarters of section with thermal insulation performance, fire resistance performance of this floor system was expected to easily have 2 hours fire resistance performance. This paper was to investigate behavior characteristics of PCM infilled floor system at elevated temperature using FEM analysis to develop the fire resistance performance of it.