• Title/Summary/Keyword: Fiber Length

Search Result 1,434, Processing Time 0.028 seconds

Control of Shrinkage Cracking of Cement Composites with Different Length Mixture of PVA Fibers (서로 다른 길이의 PVA 섬유 혼합에 따른 시멘트 복합체의 균열제어 특성)

  • Won, Jong-Pil;Kim, Myung-Kyun;Park, Chan-Gi;Kim, Wan-Young;Park, Kyoung-Hoon;Jang, Chang-Il
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2006.05b
    • /
    • pp.405-408
    • /
    • 2006
  • The purpose of this study was to determine the optimum length distribution of hybrid PVA(Poly vinyl alcohol) fiber. To produce blended PVA fiber length, first the length distribution of PVA fiber in the cement composites were identified in an experimental study based on simplex lattice design. Among the different length distributions investigated, fiber length was found to have statistically significant effect on plastic shrinkage cracking of cement composites. Subsequently, Complex analysis techniques were used to devise an experimental program that helped determine the optimum combinations of the selected fiber length distribution based on plastic shrinkage crack. The optimum blended PVA length ratio was 0.0146% 4mm fiber, 0.0060% 6-mm fiber, 0.0285% 8-mm fiber, and 0.0209% 12-mm fiber.

  • PDF

Studies on Composites Using Wood and Nonwood Fibers - Effects of Polypropylene Fiber Length and Process Variables - (목질(木質)과 비목질계(非木質系) 섬유(纖維)를 활용한 복합재(複合材) 연구(硏究) - 폴리프로필렌의 섬유장(纖維長)과 공정변수(工程變數)의 영향(影響)을 중심(中心)으로 -)

  • Lee, Phil-Woo
    • Journal of the Korean Wood Science and Technology
    • /
    • v.25 no.2
    • /
    • pp.33-44
    • /
    • 1997
  • This study was executed to examine the effects of polypropylene fiber length and process variables of the composites made from wood fiber and nonwood fiber mixed formulations. As a nonwood fiber the polypropylene with 3 denier thickness of tow condition was selected and cut into each length of 0.5, 1.0, 1.5, 2.0 and 2.5cm to mix with wood fiber. And also western hemlock wood fiber for medium density fiberboard was prepared. First, to decide an adequate polypropylene mixing fiber length, the composites of 1.0g/$cm^3$ density were made from 10% polypropylene fiber by each of five lengths and 90% western hemlock fiber mixed formulations. Thereafter as the experiments of process variable, the composites applied with adequate polypropylene fiber length(1.5cm) were made from 4 density levels (0.6, 0.8, 1.0, 1.2g/$cm^3$). 3 mixed formulations of wood fiber to polypropylene fiber(95 : 5, 90 : 10, 85 : 15), and 3 mat moisture contents(5, 10, 20%). According to the results and discussions it was concluded as follows ; The physical and mechanical properties were shown improved tendency. as polypropylene fiber length was increased in the range from 0.5 to 1.5cm, but shown decreasing tendency from 2.0 to 2.5 cm. Accordingly, it was shown that polypropylene fiber length is limited to 1.5cm or less length in mixing wood fiber and polypropylene fiber by turbulent air mixing process. As the densities of wood fiber-polypropylene fiber composites were increased, the physical and mechanical properties were clearly improved. Also they were shown significantly increasement statistically between densities respectively. In the mixed formulations, physical and mechanical properties were shown only slightly improvement, as they changed from 95 : 5 to 85 : 15 in wood fiber to polypropylene fiber. Despite of increasement of mat moisture content, mechanical properties were not improved significantly but physical properties were improved somewhat in wood fiber-polypropylene fiber composites.

  • PDF

New Definition of the Fibrogram and Its Application to Cotton Blending

  • Jeon, Boong-Soo
    • Fibers and Polymers
    • /
    • v.6 no.4
    • /
    • pp.332-335
    • /
    • 2005
  • The fibrogram theory is newly derived from the superposition principle of the conventional staple diagram, in which the left-hand ends of the fibers have to share a common starting point in order for the fiber length distribution to be measured, and the right-hand ends of the fibers form points. It is shown that the fibrogram is the staple diagram of the fiber sample having different random starting points, as well as the double cumulative distribution function of the frequency length function in the length biased sample. Also, the various means, viz. the numerical mean length, numerical mean length in median, length biased mean length, and length biased mean length in median, and the various upper half means, viz. the numerical upper half mean length, numerical upper half mean length in median, length biased upper half mean length, and length biased upper half mean length in median, are discussed in relation to the cotton blending process.

Effect of Volume Fraction and Length of Fiber on the Mechanical Properties of Fiber Reinforced Concrete (섬유보강 콘크리트의 역학적 특성에 대한 섬유 체적비와 길이의 영향)

  • Yang, Keun-Hyeok;O, Seung-Jin
    • Journal of the Korea Institute of Building Construction
    • /
    • v.8 no.1
    • /
    • pp.43-48
    • /
    • 2008
  • Fifteen concrete specimens were mixed and tested to explore the significance and limitation of appling the polyvinyl alcohol (PVA) fiber and steel fiber with end hook to concrete. Main parameters investigated were volume fraction and length of the fibers. The measured mechanical properties of fiber reinforced concrete are analyzed according to the equivalent fiber amount index explaining the adding amount and length of fibers. Test results showed that compressive strength of fiber reinforced concrete was higher than that of concrete with no fiber by $10{\sim}20%$. The normalized splitting tensile strength and flexural strength of PVA fiber reinforced concrete were similar to those of concrete with no fiber, whereas those of steel fiber reinforced concrete increased with the increase of the equivalent fiber amount index. In particular, much higher ductile behavior was observed in steel fiber reinforced concrete than in PVA reinforced concrete, indicating that the slope of descending branch of load-displacement relationship of steel fiber reinforced concrete decreased with the increase of the volume fraction and length of the fiber.

A Study on the Crack Characteristics of the Syntetic Fiber Reinforced Soil (섬유 보강토의 균열 특성 연구)

  • 송창섭
    • Magazine of the Korean Society of Agricultural Engineers
    • /
    • v.41 no.3
    • /
    • pp.59-65
    • /
    • 1999
  • This study has been performed to confirm the three dimensional effect of the crack reduction and the restrained effect of crack growth for the synthetic fiber reinforced soil. Two types of polyrpropylene fiber and low plastic clay(CL) were used for the test. And the test variable were fiber length and so on. The results of the study were summarized as follows ; 1) The mixing of synthetic fiber was effective in reducing crack growth due to adhesion between soil partlcles and synthetic fiber.l Especially initlal crack was delayed, as compared with the pure soil, for about 1 day in case of mono filament synthetic fiber and for about 1 or 2 days in case of fibrillated syntetic fiber. 2) As the content and length of synthetic fiber were increased , the effect of crack reduction was increased. It was found that 0.5% fibrillated synthetic fiber with 40mm length reinforced soil had about 3 times more effective than natural soils. 3) In case of the same fiber content and fiber length, the fibrillated synthetic fiber has nmore effective than the mono filament synthetic fiber for crack reduction.

  • PDF

Periodic-Cell Simulations for the Microscopic Damage and Strength Properties of Discontinuous Carbon Fiber-Reinforced Plastic Composites

  • Nishikawa, M.;Okabe, T.;Takeda, N.
    • Advanced Composite Materials
    • /
    • v.18 no.1
    • /
    • pp.77-93
    • /
    • 2009
  • This paper investigated the damage transition mechanism between the fiber-breaking mode and the fiber-avoiding crack mode when the fiber-length is reduced in the unidirectional discontinuous carbon fiber-reinforced-plastics (CFRP) composites. The critical fiber-length for the transition is a key parameter for the manufacturing of flexible and high-strength CFRP composites with thermoset resin, because below this limit, we cannot take full advantage of the superior strength properties of fibers. For this discussion, we presented a numerical model for the microscopic damage and fracture of unidirectional discontinuous fiber-reinforced plastics. The model addressed the microscopic damage generated in these composites; the matrix crack with continuum damage mechanics model and the fiber breakage with the Weibull model for fiber strengths. With this numerical model, the damage transition behavior was discussed when the fiber length was varied. The comparison revealed that the length of discontinuous fibers in composites influences the formation and growth of the cluster of fiber-end damage, which causes the damage mode transition. Since the composite strength is significantly reduced below the critical fiber-length for the transition to fiber-avoiding crack mode, we should understand the damage mode transition appropriately with the analysis on the cluster growth of fiber-end damage.

A New Method for Measuring Fiber Length and Fiber Coarseness Using Image Analysis Technique (화상분석법을 응용한 섬유장 및 섬유 조도 측정법 개발)

  • 배진한;김철환;박종열
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.34 no.2
    • /
    • pp.13-21
    • /
    • 2002
  • A new method for measuring fiber length and fiber coarseness was developed using image analysis technique. Measured fibers were transferred to a glass slide on a filter paper placed on a wire of the laboratory paper machine. After staining the fibers on the slide, mean fiber lengths and coarseness were measured by a commercial image analysis software, named KS400. The resultant data obtained from the image analysis displayed a close correlation with those from FS-200 and also showed excellent reproducibility as well as those from FS-200. The length of synthetic fibers over 10 mm long could be readily measured by this new analysis technique. Finally, a substantial improvement in precision for measuring fiber length and coarseness was made with less operator's effort for a given time.

단일 모드 광섬유의 길이에 따른 유효차단파장의 특성 측정

  • Jeon, Yeong-Yun;Park, Jae-Dong;Sim, Chang-Seop
    • ETRI Journal
    • /
    • v.9 no.2
    • /
    • pp.55-61
    • /
    • 1987
  • The effective cutoff wavelength of $LP_11$mode is measured as a function of fiber length for three types of single-mode optical fiber which have different characteristics in the index profile or the coating structure. The measured cutoff wavelength decreased linearly in a logarithmic scale of fiber length as increasing fiber length, and eventually became constant after 3km for two fiber types. It is found that the length dependence of cutoff wavelength is due to a mode coupling between the $LP_01$ and $LP_11$ modes.

  • PDF

Effect of Mechanical Impact Treatment on Fiber Morphology and Handsheet Properties

  • Yung B. Seo;Kim, Dukki;Lee, Jong-Hoon;Yang Jeon
    • Proceedings of the Korea Technical Association of the Pulp and Paper Industry Conference
    • /
    • 2001.11a
    • /
    • pp.183-199
    • /
    • 2001
  • Alternative way of shaping fibers suitable for papermaking was introduced. Impact refining, which was done simply by hitting wet fibers with a metal weight vertically, was intended to keep the fibers from shortening and to cause mostly internal fibrillation. Virgin chemical pulp, its recycled one and OCC were used in the experiment. It was noticed from the experiment that impact refining on virgin chemical pulp kept the fiber length and Increased bonding properties greatly, However, in the recycled fibers from the chemical pulp, fiber length and bonding properties were decreased. In OCC, which seems to contain fractions of semi-chemical pulp and mechanical pulp (GP), and which is recycled pulp from corrugated boxes, fiber length and bonding properties were decreased disastrously. We believe recycled cellulosic fibers (recycled chemical pulp and OCC in this case), which went through hornification, were less resistant to the mechanical impact than virgin chemical pulp. For virgin chemical pulp, impact refining allowed no significant fiber length shortening, high WRV, and high mechanical strength.

  • PDF

Effective Utilization of Hemp Fiber for Pulp and Papermaking (I) -Morphological Characteristics of Hemp Fiber- (펄프.제지용 원료로서의 삼 섬유 이용에 관한 연구(제 1보) -대마 구성 세포의 현미경적 관찰-)

  • Yoon, Seung-Lak;Lee, Myoung-Ku
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.42 no.1
    • /
    • pp.7-12
    • /
    • 2010
  • Morphological characteristics of hemp fiber were investigated using a light microscope in order to provide fundamental data for the use of hemp as a papermaking law material. Phloem of hemp is composed of cortical parenchyma cells and bast fiber with thick walls while xylem is composed of vessel, wood fiber and ray parenchyma cells. Also there are solitary pore and radial pore multiple which exist in diffuse porous pattern. Ray cells consist of uniseriate rays and thin walled ray parenchyma cells. Wood fibers are composed of three types: a large diameter fiber with longer length; a large diameter fiber with shorter length; a small diameter fiber with medium length. Vessel elements are composed of: a medium length one; a longer length one; the one whose both end walls have ligules or tails. Parenchyma cells in xylem and pit parenchyma cells have completely different size and shape. For bast fiber, the average length is about 4.4 mm and the width is about $30.5\;{\mu}m$; for vessel element, $600.0\;{\mu}m$ in length and $493.6\;{\mu}m$ in width; for wood fiber, $1000\;{\mu}m$ and $38.9\;{\mu}m$; for parenchyma cell, $50\;{\mu}m$ and $26.4\;{\mu}m$.