• Title/Summary/Keyword: FeNi alloy

Search Result 443, Processing Time 0.028 seconds

Effects of Surface Treatment of Cathode Materials on the Electrodeposition Behavior of Fe-Ni Alloy (표면처리와 전극 재료가 철-니켈 합금 도금에 미치는 영향)

  • Kang, Na Young;Lee, Jae Ho
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.29 no.4
    • /
    • pp.71-75
    • /
    • 2022
  • In this research, Fe-Ni alloy films were electrodeposited on stainless steel (SS304 and SS430) and Ti plates to investigate the effects of surface conditions of cathode on deposits. The Ti plates were electropolished in 3 M H2SO4-methanol electrolytes at various conditions before electrodeposition, and unpolished Ti and the optimized specimen, polished at 10 V for 8 min, were used as cathode. The anomalous codeposition, the phenomenon which more active Fe is reduced preferentially, occurred on all substrate, however, there were differences in composition of all deposits. As the results of potential monitoring during electrodeposition, it was confirmed that the larger overpotential was applied to the deposition cell when using Ti cathode, leading to high Fe content of deposits from unpolished Ti due to increase in nucleation of Fe. Also, it was founded that the polished Ti can reduced deposition overpotential.

A study on the fabrication process development of FeTi type alloy for Ni/MH battery (니켈-수소 2차전지용 철-티타늄계 전극용 합금제조 공정에 관한 연구)

  • Lee, Moon-Goo;Kim, Eul-Su;Jeong, Sun-Dol;Kim, Ki-Won;Ahn, Hyo-Jun
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.10 no.1
    • /
    • pp.1-7
    • /
    • 1999
  • In order to study on the effect of fabrication methods on the changes of hydrogenation properties of FeTi alloy, FeTi samples were prepared using three different methods, i.e., arc melting, mechanical alloying and combination of the two methods. The FeTi prepared by mechanical alloying represented amorphous structure. The hydrogen storage capacity of arc melted FeTi alloy is larger than any other samples. However, FeTi electrode fabricated by mechanical alloying after arc melting showed largest discharge capacity among them.

  • PDF

Finite Element Analysis and Experimental Verification for the Cold-drawing of a FCC-based High Entropy Alloy (FCC계 고엔트로피 합금의 냉간 인발 유한요소해석 및 실험적 검증)

  • Cho, H.S.;Bae, S.J.;Na, Y.S.;Kim, J.H.;Lee, D.G.;Lee, K.S.
    • Transactions of Materials Processing
    • /
    • v.29 no.3
    • /
    • pp.163-171
    • /
    • 2020
  • We present a multi-step cold drawing for a non-equiatomic Co10Cr15Fe25Mn10Ni30V10 high entropy alloy (HEA) with a simple face-centered cubic (FCC) crystal structure. The distribution of strain in the cold-drawn Co10Cr15Fe25Mn10Ni30V10 HEA wires was analyzed by the finite element method (FEM). The effective strain was expected to be higher as it was closer to the surface of the wire. However, the reverse shear strain acted to cause a transition in the shear strain behavior. The critical effective strain at which the shear strain transition behavior is completely shifted was predicted to be 4.75. Severely cold-drawn Co10Cr15Fe25Mn10Ni30V10 HEA wires up to 96% of the maximum cross-sectional reduction ratio were successfully manufactured without breakage. With the assistance of electron back-scattering diffraction and transmission electron microscope analyses, the abundant deformation twins were found in the region of high effective strain, which is a major strengthening mechanism for the cold-drawn Co10Cr15Fe25Mn10Ni30V10 HEA wire.

Effect of Tempering Treatment on Mechanical Properties of Ausformed Martensite in Fe-30% Ni-0.35%C Alloy (Fe-30%Ni-0.35%C 합금에서 Ausformed Martensite의 기계적 성질에 미치는 Tempering처리의 영향)

  • Lee, E.K.;Lee, K.B.;Kim, H.S.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.7 no.1
    • /
    • pp.44-52
    • /
    • 1994
  • In order to investigate the effect of tempring treatment on the mechanical properties of ausformed martensite in Fe-30%Ni-0.35%C alloy, the hardness, yield strength and elongation were examined by tensile test. 1. The strength of deformed austenite in Fe-30%Ni-0.35%C alloy was increased due to the work hardening induced from the dislocation density increased during deformation. The strength of ausformed martensite was increased because of defects inherited from deformed austenite by martensitic transformation. 2. The ductility of ausformed martensite was shown a nearly constant values independent of deformation degrees because of the interaction of multiple factors such as increased retained austenite, formation of void and decrement of twin in ausformed martensite. 3. The strength of ausformed martensite by tempering treatment was shown a little decrement up to $340^{\circ}C$, especially showed remarkable softening resistance in higher deformation degrees. 4. Virgin martensite and ausformed martensite were shown a maximum yield strength by clustering in tempering at $100^{\circ}C$ and above $100^{\circ}C$, yield strength was very small decreased due to the decrement of solute carbon by the destruction of clustering. 5. The decomposition of retained austenite was not shown up to $450^{\circ}C$ in ausformed martensite with tempering treatment, and the matrix was rapidly softening because of the decomposition of martensite and the formation of reversed austenite with tempering above $400^{\circ}C$.

  • PDF

ANALYSIS OF THE PHASE STABILITY OF FINE $Fe_{90}Ni_{10}$ ALLOY PARTICLES

  • Widatallah, H.M.;Huang, R.S.;Hsia, Y.F.;Lee, X.M.;Wang, J.H.;Lu, H.X.
    • Journal of the Korean Magnetics Society
    • /
    • v.5 no.5
    • /
    • pp.543-547
    • /
    • 1995
  • A set of $Fe_{1-x}Ni_{x}$ (x=0.10, 0.25, 0.30, 0.35, 0.50, 0.60, 0.75, 0.85) fine particles prepared by the gas evaporation technique was studied by $M\"{o}ssbauer$, XRD and other techniques. The XRD and $M\"{o}ssbauer$ patterns of the sample with x=0.10 ($Fe_{90}Ni_{10}$) were found to be exceptionally different, showing an austenite phase stability when the particles are quenched. This phase stability is quite different from that of the corresponding bulk alloy. Using binomial distrbution fits of the $M\"{o}ssbauer$ spectra of the particles in terms of nearest and next nearest neighbour configurations around the Fe atoms, an analysis of this phase stability is given. The changes in the relative intensities of the resulting magnetic sextets are used to determine the increase in martensite following the austenite-martensite transformation process. The stable austenite can, therefore, be determined. This stability may be related to the oxide surface layer and the small number of atoms of these fine particles.

  • PDF

Effect of Bonding Condition on High Temperature Mechanical Properties of TLP Bonded Joints of FE-35Ni-26Cr Alloy (Fe-35Ni-26Cr 주강 액상확산접합부의 고온기계적 특성에 미치는 접합조건의 영향)

  • 김대업
    • Journal of Welding and Joining
    • /
    • v.18 no.4
    • /
    • pp.96-103
    • /
    • 2000
  • This study investigated the effects of bonding temperature and bonding atmosphere on high temperature mechanical properties of transient liquid phase(TLP) bonded joints of heat resistant alloy using MBF-50 insert metal. Specimens were bonded at 1,423~1,468K for 600s. Microconstituents of {TEX}$Cr_{7}(C,B)_{3}${/TEX}were formed in the bonded region when the bonding temperature was low. The amount of microcostituents in the bonded layer decreased with increasing the bonding temperature, and the microconstituents in the bonded layer disappeared at the bonding temperature above 1,468K. The tensile strength of the joints at elevated temperatures increased with the increase the bonding temperature and was the same level as one of the base metal in the bonding temperature over 1,453K. Microstructure and alloying element distributions of the bonded region bonded in Ar and $N_2$atmosphere were similar to those of the bonded in vacuum. The creep rupture strength and rupture lives of joints were almost identical to those of base metal.

  • PDF

Hydrogen Absorption and Desorption Characteristics of Microencapsulated Hydrogen Storage Alloy Powders and Their Compacts (마이크로 캡슐화한 수소저장합금 분말 및 그 성형체의 수소흡수·방출 특성)

  • Kim, Chan Jung;Choi, Byung Jin;Kim, Dai Ryong
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.4 no.1
    • /
    • pp.41-50
    • /
    • 1993
  • The hydrogen absorption and desorption characteristics of microencapsulated (CFM)$Ni_{4.7}Al_{0.2}Fe_{0.1}$ and $MmNi_4Fe$ powder with Ni and/or Cu by means of chemical plating method have been investigated. Initial hydrogen absorption rate and activation property were increased remarkably by encapsulation and subsequent compacting. Pellets abtained by compacting of Cu-encapsulated fine powder have fairly good strength even after 30 cycles of hydriding and dehydriding. Encapsulated alloy powder and their compacts show a good resistance to degradation by $O_2$ or CO in hydrogen.

  • PDF

Characteristics of Liquid Phase Diffusion Bonded Joints Using Newly Developed Ni-3Cr-4Si-3B Insert Metal of Heat Resistant Alloy (신개발 Ni-3Cr-4Si-3B 삽입금속으로 액상확산접합한 내열주강 접합부의 특성)

    • Journal of Welding and Joining
    • /
    • v.18 no.6
    • /
    • pp.62-67
    • /
    • 2000
  • Metallurgical characteristics of bonded region and high temperature mechanical properties of heat resistant alloy, Fe-35Ni-26Cr during liquid phase diffusion bonding were investigated employing AM17 insert metal. The insert metal for bonding, AM17 was newly developed Ni-base metal using interpolation method. Bonding of specimens were carried out at 1,403~1,463K for 600s in vacuum. The microconstituents in the bonded interlayer disappeared in the bonding temperature over 1,423K. The microstructures, alloying elements and hardness distribution in the base metal. The tensile strength and elongation of the joints at elevated temperatures were the same level as one of the base metal in the bonding temperature over 1,423K. The creep rupture strength and rupture lives of joints were almost identical to those of base metal.

  • PDF

Study on the Characteristics of Hydride Heat Pump Using the Zr-based Laves Phase Alloys (Zr-based 합금을 이용한 hydride heat pump의 작동 특성에 관한 연구)

  • Lee, Soo-Geun;Lee, Jai-Young
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.2 no.1
    • /
    • pp.39-46
    • /
    • 1990
  • In order to improve the power of hydride heat pump, prototype heat pump was constructed using $Zr_{0.95}Ti_{0.05}Cr_{0.9}Fe_{1.1}$-$Zr_{0.9}Ti_{0.1}Cr_{0.6}Fe_{1.4}$ which had very good hydrogenation properties. The power changed with operating parameter such as cycle time, air flow rate, and temperature of hot air was investigated. The power shows maximum value with cycle time. The power increased with air flow rate and temperature of hot air. The power of the heat pump was $65-72 Kcal/Kg-alloy{\cdot}h$ under optimum operating condition, which was superior to that the system using $LaNi_{0.9}Al_{0.3}-MmNi_{4.15}Al_{0.66}Fe_{0.2}$ alloy pairs.

  • PDF

Development of Ti-Fe-X metal hydride electrode by mechanical alloying (기계적 합금화법에 의한 Ti-Fe-X계 수소 저장합금의 제조에 관한 연구)

  • Ha, Chang-Jin;Lee, Gyeong-Seop
    • Korean Journal of Materials Research
    • /
    • v.5 no.1
    • /
    • pp.112-122
    • /
    • 1995
  • Metal hydride alloys of TiFe based system have been produced by mechanical alloying(MA) method and their electrochemical characteristics have been evaluated for application for Ni/MH battery electrode. These alloys became amorphous after 36hrs ball milling and easily activated electrochemically. All MA amorphous alloys reached at the first charge/discharge cycle the maximum capacity which was 2-3 times higher than the crystalline state. But their cyclic lives were much inferior to the crystalline state. Alloying elements such as Ni, Co, Cr, Mo substituting Fe greatly improved the capacity and 180 mAh/g capacity was obtained in an alloy of TiFe_{0.6}Ni_{0.1}Co_{0.1}Cr_{0.1}Mo_{0.1}$.

  • PDF