Confined Pt and CoFe2O4 Nanoparticles in a Mesoporous Core/Shell Silica Microsphere and Their Catalytic Activity

  • Kang, Dong-Hyeon;Eum, Min-Sik;Lee, Byeong-No;Bae, Tae-Sung;Lee, Kyu-Reon;Lim, Heung-Bin;Hur, Nam-Hwi
    • Bulletin of the Korean Chemical Society
    • /
    • 제32권10호
    • /
    • pp.3712-3719
    • /
    • 2011
  • Confined Pt and $CoFe_2O_4$ nanoparticles (NPs) in a mesoporous core/shell silica microsphere, Pt-$CoFe_2O_4$@meso-$SiO_2$, were prepared using a bi-functional linker molecule. A large number of Pt NPs in Pt-$CoFe_2O_4$@meso-$SiO_2$, ranging from 5 to 8 nm, are embedded into the shell and some of them are in close contact with $CoFe_2O_4$ NPs. The hydrogenation of cyclohexene over the Pt-$CoFe_2O_4$@meso-$SiO_2$ microsphere at $25^{\circ}C$ and 1 atm of $H_2$ yields cyclohexane as a major product. In addition, it gives oxygenated products. Control experiments with $^{18}O$-labelled water and acetone suggest that surface-bound oxygen atoms in $CoFe_2O_4$ are associated with the formation of the oxygenated products. This oxidation reaction is operative only if $CoFe_2O_4$ and Pt NPs are in close contact. The Pt-$CoFe_2O_4$@meso-$SiO_2$ catalyst is separated simply by a magnet, which can be re-used without affecting the catalytic efficiency.

다중반사에 의한 금속다층막의 자기광학 Kerr 효과 분석 (Analysis for the magneto-optical Kerr effect of metal multilayers by optical multiple reflection)

  • 최영준;서용원
    • 한국자기학회지
    • /
    • 제4권4호
    • /
    • pp.307-312
    • /
    • 1994
  • (Fe, Co)/(Pd, Pt, Cu, Ag)로 이루어진 금속 다층박막에 대한 자기광학 Kerr 효과(${\theta}_{k}$) 스펙트럼을 박막내에서 빛의 다중간섭 이론을 적용하여 계산하였고, 그 결과를 보고된 실험값과 비교하였다. Co/Pd 다층막의 경우, ${\theta}_{k}$ 스펙트럼의 조성에 따른 파장 의존성에 대한 계산값이 서로 잘 일치하였으며, Fe/Cu 및 Fe/Ag 다층막에 있어서는 Cu와 Ag의 광흡수단 영역에서 다층막 고유의 새로운 peak가 나타나는 실험현상을 계산결과로 설명이 가능하였다. 그러나 Co/Pt 다층막의 경우에는 실험으로 측정된 300 nm파장 영역에서의 거대한 자기 광학 효과를 다중간섭이론으로는 설명할 수 없었으며, 이는 Co 또는 Pt 고유의 광학정수가 다층막을 이루면서 변화되어 나타나는 현상으로 생각된다.

  • PDF

FeRAM 소자 제작 중에 발생하는 Pt/Al 반응 기구 (Pt/Al Reaction Mechanism in the FeRAM Device Integration)

  • 조경원;홍태환;권순용;최시경
    • 한국재료학회지
    • /
    • 제14권10호
    • /
    • pp.688-695
    • /
    • 2004
  • The capacitor contact barrier(CCB) layers have been introduced in the FeRAM integration to prevent the Pt/Al reaction during the back-end processes. Therefore, the interdiffusion and intermetallic formation in $Pt(1500{\AA})/Al(3000{\AA})$ film stacks were investigated over the annealing temperature range of $100\sim500^{\circ}C$. The interdiffusion in Pt/Al interface started at $300^{\circ}C$ and the stack was completlely intermixed after annealing over $400^{\circ}C$ in nitrogen ambient for 1 hour. Both XRD and SBM analyses revealed that the Pt/Al interdiffusion formed a single phase of $RtAl_2$ intermetallic compound. On the other hand, in the presence of TiN($1000{\AA}$) barrier layer at the Pt/Al interface, the intermetallic formation was completely suppressed even after the annealing at $500^{\circ}C$. These were in good agreement with the predicted effect of the TiN diffusion barrier layer. But the conventional TiN CCB layer could not perfectly block the Pt/Al reaction during the back-end processes of the FeRAM integration with the maximum annealing temperature of $420^{\circ}C$. The difference in the TiN barrier properties could be explained by the voids generated on the Pt electrode surface during the integration. The voids were acted as the starting point of the Pt/Al reaction in real FeRAM structure.

$Fe/Al_2O_3/Co$ 자기 터널링 접합 제작 및 자기수송현상에 관한 연구 (Tunneling Magnetoresistive Properties of Reactively Sputtered $Fe/Al_2O_3/Co$ Trilayer Junctions)

  • 최서윤;김효진;조영목;주웅길
    • 한국자기학회지
    • /
    • 제8권1호
    • /
    • pp.27-33
    • /
    • 1998
  • 스파터링법으로 Si(001) 기판 위에 증착된 Fe(1000 $\AA$)/Al2O3(t$\AA$)/Co(1000$\AA$) 자기 삼층 접합들의 터널링 자기저항 성질을 연구하였다. 두께 t=50~200$\AA$의 Al2O3층을 반응성 rf 스파터링법으로 바닥 자성층위에 직접 증착하였다. 비교응 위해, Pt/Al2O3/Pt 터널링 접합을 제조하여 상온에서 전류.전압(I.V)특성을 측정한 결과, 확인한 비선형 nonmhic 거동을 나타내었다. 이로부터 반응성 스파터링된 Al2O3가 상온에서도 phnhole이 없는 휼룔한 절연 터널링 장벽을 형성함을 확인할 수 있었다. Fe/Al2O3/Co 자기 터널링 접합즐은 Pt/Al2O3/Pt 접합들에 비해 상당한 접합저항의 열화를 보였으며, 상온에서 대략 0.1%의 터널링 자기저항비를 나타내었다. Fe를 꼭대기 전극으로 하는 전극으로 하는 접합들에 비해, Co을 꼭대기 전극으로 하는 대부분의 자기 터널링 접합들이 보다 안정된 I.V 및 터널링 자기저항 특성을 보였다. 이러한 실험결과들을 자기 터널링 접합들의 계면구조와 관련지어,Pt/Al2O3/Ptwjq합과 비교하여 논의하였다.

  • PDF

FePt/MgO(001) 자성박막 결정화의 두께의존성 (Thickness Dependence of the Crystallization of FePt/MgO(001) Magnetic Thin Films)

  • 정지욱;이민수;조태식
    • 한국전기전자재료학회논문지
    • /
    • 제23권2호
    • /
    • pp.153-158
    • /
    • 2010
  • The crystallization of FePt/MgO(001) magnetic thin films of various thicknesses has been studied using synchrotron x-ray scattering, atomic force microscope, and vibrating sample magnetometer. In film with a 499-$\AA$-thick, face-centered tetragonal, ordered FePt phase was dominantly crystallized into perpendicular (001) grains keeping the magnetically easy c-axis normal to the film plane during annealing. In film with a 816-$\AA$-thick, however, longitudinal (110) grains keeping the c-axis parallel to the film plane were grown on top of the perpendicular (001) grains. The behavior of the magnetic properties was consistent with the thickness dependence of the crystallization. We attribute the thickness dependence of the crystallization to the substrate effect, which prefers the growth of the c-axis oriented perpendicular grains near the film/substrate interfacial area.

MAGNETIC PROPERTIES OF $FePt_{3}$ ORDERED ALLOY

  • Yoshida, H.;Fujimori, H.;Kaneko, T.;Abe, S.;Watanabe, K.;Matsumoto, M.;Yoshida, T.;Kanomata, T.
    • 한국자기학회지
    • /
    • 제5권5호
    • /
    • pp.362-365
    • /
    • 1995
  • The magnetic properties for $Fe_{24}Pt_{76}\;and\;Fe_{26}Pt_{74}$ have been investigated. The temperature vs. magnetic susceptibility curve for $Fe_{24}Pt_{76}$ had no peak near the Neel temperature. The magnetization proccess at 4.2 K showed only a linear variation up to the high magnetic field of 240 kOe. That for $Fe_{26}Pt_{74}$ at 77 K showed a metamagnetic transition at 100 kOe. These properties were discussed on the basis of a band picture.

  • PDF

Si, Pt이 첨가된 Fe-Cr 합금의 고온 용융염에서의 부식 (Hot Corrosion of Fe-Cr-Si and Fe-Cr-Pt alloys in Molten Salts.)

  • 박철우;최송천;이동복
    • 한국표면공학회지
    • /
    • 제27권1호
    • /
    • pp.3-11
    • /
    • 1994
  • Cyclic hot corrosion studies have been carried out on(82~94) wt. % Fe-(5, 10, 15) wt. % Cr alloys con-taining either (1, 3)wt. % of Si or Pt as minor alloying elements in molten salts of($Na_2SO_4$+NaCl) between 820 and $920^{\circ}C$. Si or Pt decreased corrosion rate with the most pronounced effect being observed for alloys having 15wt. %Cr. Especially, as Si or Pt contents are increased from 1 to 3 wt. %, improved corrosion resistance was obtained. The beneficial effect of Si addition is due to the presence of the Si-rich second phase along the grain boundaries as well as the formation of the protective $SiO_2$layer between substrates and oxide scale. The Pt addition also increased the corrosion resistance by enhancing the formation ($Cr_2O_3$+layers and by increasing the adherence of the oxide scale.

  • PDF

제일원리 계산에 의한 Fe/Pt (001) 표면의 평형 구조 및 자기이방성 연구

  • 이응관;최희채;황유빈;정용재
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2011년도 제40회 동계학술대회 초록집
    • /
    • pp.316-316
    • /
    • 2011
  • 제일원리 계산으로 Fe/Pt (001) 표면의 표면상태도를 계산하고 표면상태도로 부터 얻어진 평형 Fe/Pt (001) 표면구조의 자기이방성에너지를 계산하였음. 계산된 표면상태도로 부터 Fe-rich $L1_2$ 구조와 수직 $L1_0$ 구조가 가장 안정한 표면 Fe/Pt (001) 구조임이 밝혀졌음. 제일원리로 계산 된 두 구조의 자기이방성에너지를 관측하여 두 구조의 자기용이축이 모두 [001] 방향으로 정렬 됨을 확인하였다. 자기이방성에너지가 격자 변화와 표면 형성 중 어떤 원인에 의해 발생하는지 판단하기 위해서 표면구조, 벌크구조, 및 표면구조와 동일한 격자상수를 가진 벌크구조를 비교 하였다. 비교 결과에 의해 자기이방성에너지의 주 원인은 표면 형성임이 밝혀졌으며 이를 좀 더 명확히 하기위해 상태밀도함수를 계산하였다. 상태밀도함수 계산 결과 Fe 원자의 $3d_{z2}$ 오비탈의 페르미 준위 아래에서의 상태가 표면이 형성되면서 증가하는 것을 관측하였으며 이는 [001] 방향으로의 자기이방성을 증가시키는 오비탈이므로 표면 형성에 따른 자기이방성에너지 증가는 Fe 원자의 $3d_{z2}$ 오비탈에 의함이 판명되었다.

  • PDF

The Effect of Cr Dosage on FePt Nanoparticle Formation

  • Won, C.;Keavney, D.J.;Divan, R.;Bader, S.D.
    • Journal of Magnetics
    • /
    • 제11권4호
    • /
    • pp.182-188
    • /
    • 2006
  • The search for high-density recording materials has been one of most active and vigorous field in the field of magnetism. $FePt-L1_{0}$ nanoparticle has emerged as a potential candidate because of its high anisotropy. In this paper, we provide an overview of recent work at Argonne National Laboratory that contributes to the ongoing dialogue concerning the relation between structure and properties of the FePt nanoparticle system. In particular we discuss the ability to control structure and properties via dosing with Cr. Cr-dosed FePt films were grown via molecular beam epitaxy and annealed at $550^{\circ}C$ in an ultrahigh vacuum chamber, and were studied with the surface magneto-optic Kerr effect (SMOKE), scanning electron microscopy (SEM) and x-ray magnetic circular dichroism (XMCD). We found that small dosage of Cr helps to generate $L1_{0}$ phase FePt magnetic nanoparticles with small size, defined shape and regular spatial distribution on MgO (001) substrate. The nanostructures are ferromagnetic with high magnetic coercivity (${\sim}0.9T$) and magnetic easy axis in the desired out-of-plane orientation. We also show that controlling the lateral region where nanostructures exist is possible via artificial patterning with Cr.

Effects of Annealing Pressures on the Ordering and Microstructures of FePt:Ag Nanocomposite Films

  • Li, Xiaohong;Feng, Zhaodi;Li, Yang;Song, Wenpeng;Zhang, Qian;Liu, Baoting
    • Journal of Magnetics
    • /
    • 제18권4호
    • /
    • pp.412-416
    • /
    • 2013
  • FePt:Ag (100 nm) nanocomposite thin films were prepared on naturally-oxidized Si substrates by dc magnetron sputtering at room temperature. X-ray diffraction (XRD) and transmission electron microscopy (TEM) are used to investigate the effects of annealing pressures on the ordering processes and microstructures of these films. The average sizes for the $L1_0$ ordered domains and the FePt grains are reduced to d = 9 nm and D = 13 nm from d = 19 nm and D = 34 nm, respectively, when the annealing pressure is enhanced to 0.6 GPa from room pressure at 873 K. Furthermore, the size distribution is improved into a narrow range. With increasing pressure, the coercivity of $L1_0$-FePt:Ag thin films decreases from 15.1 to 7.6 kOe. In the present study, the effects of high pressure on the $L1_0$ ordering processes and microstructures of FePt:Ag nanocomposite films were discussed.