• Title/Summary/Keyword: Fe-Mn alloy

Search Result 216, Processing Time 0.035 seconds

Effects of carbon content and Titanium Addition on Damping Capacity in Fe-17wt%Mn Alloy (Fe-17wt%Mn 합금의 진동감쇠능에 미치는 탄소와 티타늄 첨가의 영향)

  • Baik, S.H.;Kim, J.C.;Jee, K.K.;Shin, M.C.;Choi, C.S.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.9 no.1
    • /
    • pp.53-61
    • /
    • 1996
  • Effects of carbon and Ti on damping capacity are investigated in an Fe-17%Mn alloy. The suppressive force of carbon against ${\gamma}{\rightarrow}{\varepsilon}$ transformation increases linearly with an increase in its content, lowering Ms temperature and volume fraction of ${\varepsilon}$ martensite. Carbon deteriorates damping capacity by reducing the interfacial area of damping sources and mobility of the boundaries contributing to anelastic deformation. The reduction in damping capacity is accelerated when carbon-containing alloy is aged at higher temperatures above room temperature. The effect of Ti on damping capacity is found to be benificial in carbon-containing alloy, which is attributed to the depletion of carbon solute due to the formation of TiC.

  • PDF

Effect of Thermo-mechanical Treatment on the Tensile Properties of Fe-20Mn-12Cr-3Ni-3Si Damping Alloy (Fe-20Mn-12Cr-3Ni-3Si 합금의 인장성질에 미치는 가공열처리의 영향)

  • Han, H.S.;Kang, C.Y.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.32 no.2
    • /
    • pp.61-67
    • /
    • 2019
  • This study was carried out to investigate the effect of thermo-mechanical treatment on the tensile properties of Fe-20Mn-12Cr-3Ni-3Si alloy with deformation induced martensite transformation. ${\alpha}^{\prime}$ and ${\varepsilon}$-martensite, dislocation, stacking fault were formed, and grain size was refined by thermo-mechanical treatment. With the increasing cycle number of thermo-mechanical treatment, volume fraction of ${\varepsilon}$ and ${\alpha}^{\prime}$-martensite, dislocation, stacking fault were increased, and grain size decreased. In 5-cycle number thermo-mechanical treated specimens, more than 10% of the volume fraction of ${\varepsilon}$-martensite and less than 3% of the volume fraction of ${\alpha}^{\prime}$-martensite were attained. Tensile strength was increased and elongation was decreased with the increasing cycle number of thermo-mechanical treatment. Tensile properties of thermo-mechanical treated alloy with deformation induced martensite transformation was affected to formation of martensite by thermo-mechanical treatment, but was large affected to increasing of dislocation and grain refining.

Effect of Mn-Addition on the Cavitation Erosion Resistance of Surface-hardened Fe-20Cr-1Si-1C Aolly (Fe-20Cr-1Si-1C계 경면처리 합금의 cavitation erosion 저항성에 미치는 Mn 첨가의 영향)

  • 김수철;박인호;장세기;김선진;강성군
    • Journal of the Korean institute of surface engineering
    • /
    • v.33 no.1
    • /
    • pp.10-16
    • /
    • 2000
  • Characteristics of cavitation erosion resistance of Fe-20Cr-1Si-1C-xMn(x=0, 5, 15) alloys were investigated by SEM and XRD analysis. The effects on strain-induced transformations were considerably reduced with increasing the amounts of Mn due to twining that occurred at 5, 15Mn alloys, activating cavitation erosion rates(mg/$\textrm{cm}^2$) which varied as 0.055, 0.114 and 0.160mg/$\textrm{cm}^2$ for 0, 5, 15Mn. From the results, it was found that the addition of Mn element in Fe-base alloy provides more cracking sites at twins rather than absorbing strain energies, so accelerates cavitation erosion rates.

  • PDF

Effects of Alloying Elements(C, Si) and Hot-Rolling on Damping Capacity and Mechanical Properties of Fe-17%Mn Alloys (Fe-17%Mn 합금의 진동감쇠능과 기계적 성질에 미치는 합금원소(C, Si) 및 열간압연의 영향)

  • Kim, J.C.;Han, D.W.;Back, J.H.;Kim, T.H.;Baik, S.H.;Lee, Y.K.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.18 no.2
    • /
    • pp.99-104
    • /
    • 2005
  • In this study, the effects of C and Si on damping capacity and mechanical properties of as-cast and as-rolled Fe-17%Mn alloys were investigated as a basic study for the purpose of the commercialization of the alloy. The $M_s$ temperature of ${\gamma}{\rightarrow}{\varepsilon}$ martensitic transformation in Fe-17%Mn alloy was decreased with increasing C and Si contents, resulting in the less volume fraction of ${\varepsilon}$ martensite. The damping capacity was also decreased with increasing alloying content because of less ${\varepsilon}$ amount and the reduction in mobility of the damping sources such as the stacking fault boundaries and ${\gamma}/{\varepsilon}$ interfaces due to the pinning effect by alloying elements. The mechanical properties of as-rolled alloys were superior to those of as-cast alloys probably because of finer ${\gamma}$ grains, larger amount of ${\varepsilon}$ martensite, and chemical homogeneity.

Phase Analyses and Magnetic Properties of $Mn-(M,AI)_{1-x}(Bi,Sb)_x$(M=Cu, Fe) Alloy Systems ($Mn-(M, AI)_{1-x}(Bi, Sb)_x$ (M=Cu, Fe)합금계의 상 분석 및 자기적 성질에 관한 연구)

  • Park, Jung-Eon;Go, Gwan-Yeong;Yun, Seok-Gil
    • Korean Journal of Materials Research
    • /
    • v.6 no.1
    • /
    • pp.90-98
    • /
    • 1996
  • Mn((Cu0.66AI0.34)1-x(Bi0.3Sb0.7)x) 및 Mn((Fe0.66AI0.34)1-x(Bi0.3Sb0.7)x) 합금계의 상의 변화와 자기적 특성을 조사하였다. Mn((Cu, SI)(Bi, Sb)) 합금계는 Bi상, MnSb상, MnBi상, k-상, Heuser상, Mn2Sb 및 $\beta$-Mn상의 혼합상으로 이루어졌으며 x가 증가함에 따라 Bi상과 Mn2Sb상이 증가하고 K-상, Heusler상 및 $\beta$-Mn상이 줄어들거나 사라졌다. 자기적 성질은 자성을 띄는 MnSb상, MnBi상, Mn2Sb상, k-상 및 Hseusler상과 비자성인 Bi상과 $\beta$-Mn상의 상대적 분율에 의해 결정됨을 알 수 있었고, 150K-200K 부근에서 그 이하로 온도가 감소함에 따라 자화값이 급격히 감소하는 현상이 나타났다. Mn((Fe, AI)(Bi, Sb))합금계는 Bi상, MnSb상, MnBi상, MnBi상,$\beta$-Mn상, k-상 및 Mn2Sb상의 혼합상으로 나타났으며, 자기적 성질은 조사한 전 조성에서 강자성을 띄고 있음을 알 수 있었다.

  • PDF

The Effects of Ag Addition on the Electrode Properties of Hydrogen Storage Alloys (Zr계 수소저장합금의 전극특성에 미치는 은 첨가의 영향)

  • Noh, Hak;Jeong, So-yi;Choi, Seung-jun;Choi, Jeon;Seo, Chan-yeol;Park, Choong-Nyeon
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.8 no.3
    • /
    • pp.137-141
    • /
    • 1997
  • The effects of Ag addition to Zr-based hydrogen storage alloys ($Zr_{0.7}Ti_{0.3}V_{0.4}Ni_{1.2}Mn_{0.4}$, $Zr_{0.7}Ti_{0.3}V_{0.4}Ni_{1.2}Mn_{0.3}Cr_{0.1}$ and $Zr_{0.6}Ti_{0.4}V_{0.4}Ni_{1.2}Mn_{0.3}Fe_{0.1}$) on the electrode properties were examined. Ag-free and Ag-added Ze-based alloys were prepared by arc melting, crushed mechanically, and subjected to the electrochemical measurement. In $Zr_{0.7}Ti_{0.3}V_{0.4}Ni_{1.2}Mn_{0.4}$ alloy, 0.08 wt% Ag addition to the alloy improved the activation rate. Also Ag addition improved both activation property and discharge capacity in $Zr_{0.7}Ti_{0.3}V_{0.4}Ni_{1.2}Mn_{0.3}Cr_{0.1}$. For these Ag-added alloys, discharge capacities with the change of charge-discharge current density(10mA, 15mA and 30mA) are almost constant. Showing very high rate capability, discharge capacity of $Zr_{0.6}Ti_{0.4}V_{0.4}Ni_{1.2}Mn_{0.3}Fe_{0.1}$ alloy increased by Ag addition to the alloy. When the amount of Ag addition in $Zr_{0.7}Ti_{0.3}V_{0.4}Ni_{1.2}Mn_{0.4}$ alloy increased too much, the electrode properties became worse. Unveiling mechanism of effect of Ag addition is now progressing in our laboratory.

  • PDF

Effect of Ti, B, Zr Elements on Grain Refinement and Castability of Al-4wt%Mg-0.9wt%Si-0.3wt%Mn-0.15wt%Fe Casting Alloy (주조용 Al-4wt%Mg-0.9wt%Si-0.3wt%Mn-0.15wt%Fe 합금의 결정립 미세화와 주조특성에 미치는 Ti, B, Zr 첨가원소의 영향)

  • Kim, Heon-Joo;Park, Su-Min
    • Journal of Korea Foundry Society
    • /
    • v.35 no.5
    • /
    • pp.120-127
    • /
    • 2015
  • The effects of Ti, B and Zr on grain refinement and castability were investigated in Al-4wt%Mg-0.9wt%Si-0.3wt%Mn-0.15wt%Fe alloy. Measurement of cooling curve and micro-structure observation were performed to analyze the effects of the addition of minor elements Ti, B and Zr during solidification. The prominence of effect on grain refinement was in increasing order for Ti, Zr and B element. Fine grain size and an increase of the crystallization temperature for ${\alpha}$-Al solution were evident as the amount of addition elements increased in this study. Addition of 0.15wt% Ti was most effective for grain refinement, and the resulting grain size of ${\alpha}$-Al solution for shell mold and steel mold were $72.3{\mu}m$ and $23.5{\mu}m$, respectively. Fluidity and shrinkage tests were perform to evaluate the castability of the alloy. Maximum fluidity length and minimum ratio of micro shrinkage were recorded for 0.15wt% Ti addition due to the effect of the finest grain size.