• 제목/요약/키워드: Fe-Cr-Mo

검색결과 224건 처리시간 0.023초

Effect of Alloying Elements on the Thermal Creep of Zirconium Alloys

  • Cheol Nam;Kim, Kyeong-Ho;Lee, Myung-Ho;Jeong, Yong-Hwan
    • Nuclear Engineering and Technology
    • /
    • 제32권4호
    • /
    • pp.372-378
    • /
    • 2000
  • The effect of alloying elements on the creep resistance of Zr alloys was investigated using thermal creep tests that were performed as a part of advanced fuel cladding development. The creep tests were conducted at 40$0^{\circ}C$ and 150 MPa for 240 hr. A statistical model was derived from the relationship between the steady-state creep rate and the content of individual alloying elements. The creep strengthening effect decreased in the following sequence : Nb, Sn, Mn, Cr, Mo, Fe and Cu. The high creep resistance of Sn and the opposite effect of Fe on zirconium alloys seem to be associated with their lowering and enhancing, respectively, the self-diffusivity of the zirconium matrix.

  • PDF

더덕 ( 사삼 )의 재배방법별 일반성분 및 무기성분에 관한 연구 ( Proximate and Mineral of Dried Wild and Cultivated Codonopsis lanceolata Benth , et Hook , Fil , of Different Cultivated Groups )

  • 신수철
    • 한국자원식물학회지
    • /
    • 제4권2호
    • /
    • pp.39-45
    • /
    • 1991
  • Proximate compositions of the roots of cultured and wild Codonopsis lanceolata were examined as tile basic reasearch for the study of their source of processed foods.No significant difference in the contents was found between the wild root and thecultivated at 3$0^{\circ}C$ in biotronroom. In view of the results to have measured mineralswhich is included in 14 sorts of Codonopsis lanceolata and surveyed their distribution.12 kinds of minerals including T1, Co, Ge, Sm, Mo, Sc, Be, Cd, As, Ga, Bi, ph are ne-vel or little included in almost source. Other twenty-one sorts of minerals (Ni, Se,Ba, Sb, Si, Ti, B, Li, Ifs, Ca, Sr, Mn, Fe, Cu, Zn, p, Al, Na, V, Cr, K) are more or less in-cluded in all source and Ca, Mg, p, K, and Fe are metals that are included in large qu-entities in comparison with others. No minerals difference in the contents was foundbetween the cultivated temperature. The content of elements of inorganic metal differsaccording to the part of C. lanceolata.

  • PDF

정상 한국인 장기조직중 중금속류의 상호관련성 (Interelationship Between the Concentration of Heavy Metals in Normal Korean Tissues)

  • 이상기;유영찬;정규혁
    • 약학회지
    • /
    • 제43권5호
    • /
    • pp.577-583
    • /
    • 1999
  • Concentrations of heavy metals, including As, Cd, Cr, Cu, Fe, Hg, Mn, Mo, Ni, Pb, Se, Si, Sn, V and Zn in the internal organs (liver, kidney, heart, lung, spleen, cerebrum and bone) of Korean obtained from 91 forensic medical autopsy cadavers, with an age range of 12-87 years, were determined by inductively coupled plasma atomic emission spectrometry. From the results, positive correlation with age was observed in the following cases : Cd in liver, kidney and cerebrum; Fe in cerebrum and bone; Pb in bone; v in lung. Copper in heart, Hg in bone and Mn in kidney correlated negatively with age. A significantly positive correlation between Se and Hg was only observed in heart. Significant correlation coefficients between Se and As were observed in liver, kidney, heart spleen and bone. The correlation between Cd and Zn was significant in liver and kidney, indicating that the distribution of Cd is similar to that of Zn in the liver and kidney.

  • PDF

Fe-2%Mn-0.5%Si강판의 $600-800^{\circ}C$, $N_2/H_2O/H_2S$분위기에서의 고온부식 (Corrosion of Fe-2.25%Cr-1%Mo Steels at $600-800^{\circ}C$ in $N_2/H_2O/H_2S$ atmospheres)

  • 김민정;봉성준;이동복
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2011년도 춘계학술대회 및 Fine pattern PCB 표면 처리 기술 워크샵
    • /
    • pp.77-78
    • /
    • 2011
  • 저비용, 고효율, 안정적 수급이 가능한 전력 에너지원이 요구되면서 석탄이 새로운 에너지원으로 급부상하게 됨에 따라 차세대 친환경 석탄화력 발전기술인 IGCC (Integrated Gasification Combined Cycle) 발전 시스템 의 개발이 필요하게 되었다. 석탄가스화 공정(IGCC: integrated coal gasification combined cycle)은 석탄을 가스화한 후 이를 이용하여 복합발전소를 운전하는 발전기술로서 석탄을 고온, 고압아래에서 수소와 일산화탄소를 주성분으로 한 합성가스로 전환한 뒤 합성가스 중에 포함 된 분진과 황 화합물 등 유해물질을 제거하고 천연가스와 유사한 수준으로 정제하여 전기를 생산하는 친환경 발전 기술이다.

  • PDF

대청호 상류, 회남일대에 분포하는 탄질 변성니질암과 하상 퇴적물의 환경유해원소에 관한 지화학적 거동, 분산 및 부화 (Geochemical Behavior, Dispersion and Enrichment of Environmental Toxic Elements in Coaly Metapelites and Stream Sediments at the Hoenam Area, up the Taecheong Lake, Korea)

  • 이찬희;이현구
    • 자원환경지질
    • /
    • 제30권3호
    • /
    • pp.209-222
    • /
    • 1997
  • The Hoenam area, up the Taecheong lake, composed mainly of low grade coal-bearing metapelites within the Ogcheon Supergroup. These coal formations are developed discontinuously several hundred meters and swelling from 10 to 300 cm along the host metapelites. Although the formations have been mined for coal, but already mined out, and the formations were higher content (mean value of 42 samples) of environmental toxic elements as As (13 ppm). Ba (1.81 wt. %), Cd (2 ppm), Cr (188 ppm), Cu (87 ppm), Mo (214 ppm), Pb (25 ppm), Sb (3 ppm), Se (12 ppm), U (55 ppm), V (2124 ppm) and Zn (234 ppm) than the host metapelites and the NASC. The Al, Ti, Mg, K and Na contents in stream sediments derived from the Hando and Bugook mine area were highly concentrations than the samples from the Samseongjeil mine area. The mean value (wt. %) of Fe (10.07), Mn (0.15), Ca (0.84), P (0.18) and Ba (0.77) influenced by the Samseongjeil mine were higher than the other mine drainage sediments. The mean content (ppm) of environmental toxic elements in drainage sediments from the Samseongjeil mine were taken As (2083), Cu (447), Mo (202), Ni (720), Pb (42), U (250), V (1070) and Zn (2632), which are extremely high concentrations against NASC and EPA. Characteristics of elemental behavior and dispersion of the all toxic elements are the same as increased with increasing U, V, and Cu. Rare earth elements in the sediments are enriched with LREE (La, Ce and Nd) from the drainage on strong concentration of toxic elements. The pH of stream water is neutral, but pH of the sediments ranged from 4.92 to 6.93 (mean 6.22), those are slightly acid in the Hando mine area. Major elements in the host rocks at the Hoenam area are mostly depleted especially Ca, excepting Ti and Ba, normalized with NASC. The sediments were highly enriched of Ti, Fe, Mg, Mn and Ba, but depleted of Al, K, Ca, Na and P on the basis of host rocks and NASC. Minor and environmental toxic elements in the host rocks were strongly enriched all elements (As, Cd, Mo, Se, D, V and Zn), excepting Co, Ni and Sr. Enrichment index (mean value) about toxic elements (As, Cr, Cu, Fe, Ni, Pb and Zn) of the sediments in this area have taken 41.35 (Hando mine drainage; 2.73, Samseongjeil mine drainage; 113.14 and Bugook mine drainage; 8.19), those are seriously contaminated by environmental toxic elements.

  • PDF

Hastelloy X의 고온열화에 따른 미세구조 및 고온압축특성 (Microstructural Analysis and High Temperature Compression Behavior of High Temperature Degradation on Hastelloy X)

  • 김길수;조태선;서영익;류우석;김영도
    • 한국재료학회지
    • /
    • 제16권5호
    • /
    • pp.318-322
    • /
    • 2006
  • Short-term high temperature degradation test was conducted on Hastelloy X, a candidate tube material for high temperature gas-cooled reactors (HTGR), to evaluate the variation of microstructure and mechanical property in air at $1050^{\circ}C$ during 2000 h. The dominant oxide layer was Cr-oxide and a very shallow Cr-depleted region was observed below the oxide layer. At the beginning of degradation, the island shape $M_6C$ precipitate (M=Mo-rich, Fe, Ni, Cr) was observed in matrix region. After 2000 h degradation, precipitate shape was changed to the chain shape and increased amount of precipitate. These results influenced mechanical property of the specimen which exposed in high temperature. Yield strength was decreased from 115MPa to 89 MPa after 24 h and 2000 h exposure, respectively.

SPRAY DEPOSITION OF MECHANICALLY ALLOYED F/M ODS STEEL POWDER

  • SUK HOON KANG;CHANG-KYU RHEE;SANGHOON NOH;TAE KYU KIM
    • Archives of Metallurgy and Materials
    • /
    • 제64권2호
    • /
    • pp.607-611
    • /
    • 2019
  • Thermal/cold spray deposition were used for additive manufacture of oxide dispersion strengthened (ODS) steel layers. Mechanically alloyed F/M ODS steel powders (Fe(bal.)-10Cr-1Mo-0.25Ti-0.35Y2O3 in wt.%) were sprayed by a high velocity oxygen fuel (HVOF) and cold spray methods. HVOF, as a thermal method, was used for manufacturing a 1 mm-thick ODS steel layer with a ~95% density. The source to objective distance (SOD) and feeding rate were controlled to achieve sound manufacturing. Y2Ti2O7 nano-particles were preserved in the HVOF sprayed layer; however, unexpected Cr2O3 phases were frequently observed at the boundary area of the powders. A cold spray was used for manufacturing the Cr2O3-free layer and showed great feasibility. The density and yield of the cold spray were roughly 80% and 45%, respectively. The softening of ODS powders before the cold spray was conducted using a tube furnace of up to 1200℃. Microstructural characteristics of the cold sprayed layer were investigated by electron back-scattered diffraction (EBSD), the uniformity of deformation amount inside powders was observed.

TiN피막 코팅된 치과주조용 합금의 부식거동 (Corrosion Behaviors of TiN Coated Dental Casting Alloys)

  • 조호형;박근형;김원기;최한철
    • 대한금속재료학회지
    • /
    • 제47권2호
    • /
    • pp.129-137
    • /
    • 2009
  • Corrosion behaviors of TiN coated dental casting alloys have been researched by using various electrochemical methods. Three casting alloys (Alloy 1: 63Co-27Cr-5.5Mo, Alloy 2: 63Ni-16Cr-5Mo, Alloy 3: 63Co-30Cr-5Mo) were prepared for fabricating partial denture frameworks with various casting methods; centrifugal casting(CF), high frequency induction casting(HFI) and vacuum pressure casting(VP). The specimens were coated with TiN film by RF-magnetron sputtering method. The corrosion behaviors were investigated using potentiostat (EG&G Co, 263A. USA) in 0.9% NaCl solution at $36.5{\pm}1^{\circ}C$. The corrosion morphologies were analyzed using FE-SEM and EDX. Alloy 1 and Alloy 2 showed the ${\alpha}-Co$ and ${\varepsilon}-Co$ phase on the matrix, and it was disappeared in case of TiN coated Alloy 1 and 2. In the Alloy 3, $Ni_2Cr$ second phases were appeared at matrix. Corrosion potentials of TiN coated alloy were higher than that of non-coated alloy, but current density at passive region of TiN coated alloy was lower than that of non-coated alloy. Pitting corrosion resistances were increased in the order of centrifugal casting, high frequency induction casting and vacuum pressure casting method from cyclic potentiodynamic polarization test.

열처리 후 플럭스 사파이어와 천연 사파이어의 비교 분석 (Comparison of flux and natural sapphire after heat-treatment)

  • 김기인;안용길;서진교;박종완
    • 한국결정성장학회지
    • /
    • 제19권3호
    • /
    • pp.152-158
    • /
    • 2009
  • 산업용 뿐만 아니라 보석용으로 가치가 있는 사파이어는 매우 다양한 방법으로 합성 사파이어를 만들어 왔다. 그 중 천연 사파이어와 매우 유사하며 보석용으로 가치가 높은 Chatham사의 플럭스 사파이어를 사용하여 천연 사파이어와 비교하였다. 먼저 WD-XRF(Wavelength dispersive x-ray fluorescence spectrometer)를 사용하여 천연과 합성의 화학 조성을 비교하였다. 천연 사파이어는 화학 조성이 매우 다양하였으나 플럭스 사파이어는 천연과 유사한 화학 성분과 특히 Mo, Pt, Pb 미량원소가 검출되었다. Pt는 플럭스 사파이어라는 결정적인 증거가 된다. 다음으로 $1300^{\circ}C$$1500^{\circ}C$의 고온에서 열처리를 한 후 자외선-가시광선 분광광도계(UV-VIS Spectrophotometer)를 사용하여 분광학적 특성을 조사함으로써 천연 사파이어는 $Cr^{3+}$와 관련된 약 690nm의 형광과 관련된 흡수 피크의 변화를 관찰할 수 있었고 플럭스 사파이어는 $Cr^{3+}$와 관련된 약 690nm의 피크와 376nm, 388nm의 $Fe^{3+}$의 흡수 피크가 변화함을 볼 수 있었다. 고온 열처리에 의해 플럭스 사파이어의 흡수 피크의 변화가 천연 사파이어의 흡수 피크의 변화보다 더 큰 것을 알 수 있었다 화학조성 및 분광분석 실험을 통하여 천연 사파이어와 flux 합성 사파이어의 특성을 비교 분석하였다.

풍화 석탄연소 고형폐기물(Pulverised Fuel Ash)의 중금속 제거가능성 : I. 뱃치 용출실험 (Potential Element Retention by Weathered Pulverised Fuel Ash : I. Batch Leaching Experiments)

  • 이상훈
    • 자원환경지질
    • /
    • 제28권3호
    • /
    • pp.251-257
    • /
    • 1995
  • 영국의 2개 화력발전소로부터 석탄연소 폐기물 시료를 17년, 약40년 풍화된 것 그리고 풍화되지 않은 것의 구분으로 각각 채취하였다. 이 시료들과 증류수, 인공 침출수등을 이용, 뱃치 실험을 실시하였다. 통화되지 않은 시료의 증류수를 통한 실험에서는 Ca, Na, K, S, B, Cr, Cu, Li, Ni, Mo 그리고 $Cl^-$ 등 원소가 다량으로 방출되는 것이 관찰되었으며 이는 이들 원소들이 주로 표면에 수반된다는 증거가 된다. Mg, Al, Ba, Si, V, As 그리고 Se등은 이러한 다량방출을 하지 않는바 이들 원소들은 입자 표면보다는 PFA 입자의 유리질에 수반되는 것으로 생각된다. 풍화 PFA시료를 통한 실험에서는 유리질과 같은 상온에서 불안정한 상에 수반되는 용융성원소들이 용액으로 방출됨이 증명되었다. 인공 침출수를 이용한 실험에서는 Fe, Ca, Cr, Cu, Ni, Zn 그리고 Hg등이 제거되는것이 관찰되었으며 이는 용액으로부터 제거되어 고체 PFA의 성분에서 증가하는것을 통하여도 확인된다. 중금속 제거정도는 Meaford>Drax 풍화시료>Drax 신선한 시료의 순이며 이는 풍화의 정도와도 일치한다. 즉 풍화를 많이 받은 시료에서 더 많은 중금속이 제거되는 결과를 보여준다.

  • PDF