• Title/Summary/Keyword: Fe-Co-Ni

Search Result 994, Processing Time 0.035 seconds

A study on the exchange anisotropy of Ni-Fe/Co-Fe/Mn-Ir/Cu/buffer/Si multialyers (Ni-Fe/Co-Fe/Mn-Ir/Cu/buffer/Si 다층박막의 교환이방성에 관한 연구)

  • 윤성용;노재철;전동민;임흥순;서수정
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.10 no.1
    • /
    • pp.36-41
    • /
    • 2000
  • We studied the exchange anisotropy of Ni-Fe/Co-Fe/Mn-Ir/Cu/buffer/Si multilayers using D.C magnetron sputtering technique. Generally, Ni-Fe/Mn-Ir/buffer(Cu)/Si multilayers cannot pin the ferromagnetic layer for the lower exchange biased field. We got $H_{ex}$ ex/ increased by two times, after using Cu/Ta as buffer layer to get larger grain size of Mn-Ir layer and inserting very thin Co-Fe layer between the Ni-Fe layer and the Mn-Ir layer to get improved grain-to-grain epitaxy relation at the interface between Ni-Fe layer and Mn-Ir layer. The variation of $H_{ex}$ by thickness of Mn-Ir layer in ferromagnete/Mn-Ir/buffer/Si multilayers is different to that in Mn-Ir/ferromagnete/buffer/Si multilayers, because the volume distribution of grain size of Mn-Ir layer and the exchange energy at the interface between the Mn-Ir and the ferromagnetic layers is different for stacking sequence.

  • PDF

Fabrication and Electrical Properties of Ni-Mn-Co-Fe Oxide Thick Film NTC Thermistors (Ni-Mn-Co-Fe 산화물 후막 NTC 서미스터의 제조 및 전기적 특성)

  • Park, Kyeong-Soon;Bang, Dae-Young;Yun, Sung-Jin;Choi, Byung-Hyun
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.10
    • /
    • pp.912-918
    • /
    • 2002
  • Ni-Mn-Co-Fe oxide thick films were coated on an alumina substrate by screening printing technique. The microstructure and electrical properties of the thick films, as a function of composition and sintering temperature, were investigated. The components of the NTC thick films sintered at 1150${\circ}C$ were distributed homogeneously. On the other hand, in the case of the NTC thick films sintered at 1200 and 1250${\circ}C$, Co element was distributed homogeneously, but Ni, Mn and Fe elements were distributed heterogeneously, resulting in the formation of Ni rich and Mn-Fe rich regions. All the thick film NTC thermistors prepared showed a linear relationship between log resistance (log R) and the reciprocal of absolute temperature (1/T), indicative of NTC characteristics. At a given NiO and $Mn_3O_4$ content, the resistance, B constant and activation energy of $(Ni_{1.0}Mn_{1.0}Co_{1-x}Fe_x)O_4$ (0.25${\le}$x${\le}$0.75) and $(Ni_{0.75}Mn_{1.25}Co_{1-x}Fe_x)O_4$ (0.25${\le}$x${\le}$0.75) thermistors increased with increasing $Fe_2O_3$ content.

Dry Etching of NiFe, NiFeCo, and Ta in Cl2/Ar Inductively Coupled Plasma (Cl2/Ar 유도 결합 플라즈마를 이용한 NiFe, NiFeCo, Ta의 건식식각)

  • Ra, Hyun-Wook;Park, HyungJo;Kim, Ki Ju;Kim, Wan-Young;Hahn, Yoon-Bong
    • Korean Chemical Engineering Research
    • /
    • v.43 no.1
    • /
    • pp.76-79
    • /
    • 2005
  • Dry etching of NiFe, NiFeCo, and Ta for magnetic random access memory (MRAM) by inductively coupled plasmas (ICPs) of $Cl_2/Ar$ has been carried out. NiFe and NiFeCo showed maximum etch rates at a particular ICP source power, but the etch rate of Ta increased with the ICP source power. The etch rates of the magnetic thin films increased with the RF chuck power, but decreased with the operating pressure and the $Cl_2$ concentration. To avoid a corrosion problem by chlorine, the etched samples were rinsed with de-ionized water for 5 minutes after etching. The etch profile showed a clean and smooth surface at 50% $Cl_2$ concentration.

The Effect of Magnetic Property According to Size and Orientation of Crystal for Electroplated Co-Fe-Ni Alloys (전기 도금된 CoFeNi계 박막의 결정크기와 방향성이 자기특성에 미치는 영향)

  • Jeung, Won-Young;Kim, Hyun-Kyung;Park, Chang-Bean
    • Journal of the Korean Magnetics Society
    • /
    • v.16 no.5
    • /
    • pp.249-254
    • /
    • 2006
  • CoFeNi alloys are some of the most studied soft magnetic materials because of their superial properties over FeNi alloys as write head core materials in HDD and MEMS. We studied the effect of magnetic property according to size and orientation of crystal for electroplated Co-Fe-Ni alleys. In case of heat treated ternary alloy, it affect the change of crystal size and structure. In this study, it intends to improve the magnetic properties of CoFeNi thin film by heat treatment. Minimized coercivity and increased magnetization are due to heat treatment from $300^{\circ}C\;to\;400^{\circ}C$. As a bcc phase formation, it grow to amount of magnetization.

Microstructure and Magnetic Properties in Fe-Co-B/M Films for Soft Magnetic Underlayer of Perpendicular Magnetic Recording Media (수직자기기록매체용 Fe-Co-B/M 하지연자성층의 미세결정구조 및 자기특성)

  • 공석현;손인환;금민종;최형욱;박용서;김경환
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.17 no.8
    • /
    • pp.888-892
    • /
    • 2004
  • It is necessary to develop soft magnetic layer with high saturation magnetization 4 $\pi{M}_s$ and in-plane magnetic anisotropy field Hk for soft magnetic underlayer of perpendicular magnetic recording media with high signal to noise ratio. Fe-Co-B layer with high 4 $\pi$Ms of about 23 kG deposited on Ni-Fe and Ni-Fe/Si seedlayer exhibited very high in-plane magnetic anisotropy filed Hk of about 280 and 380 Oe, respectively, In-plane XRD studies clarified that the lattice spacing of planes along the easy axis direction was longer than that along the hard axis direction in the Fe-Co-B layers with high Hk. These results indicate that high Hk of Fe-Co-B/Ni-Fe and Fe-Co-B/[Ni-Fe/si] layers were resulted from magnetoelastic anisotropy owing to a residual stress. Moreover, the high Hk in the Fe-Co-B/Ni-Fe layer was maintained until 30$0^{\circ}C$ annealing temperature.

Composition and Coercivity of Fe-Co-Ni Alloy Electrodeposits (Fe-Co-Ni합금박막의 조성 및 자기적 성질)

  • 예길촌;김용웅;문근호
    • Journal of the Korean institute of surface engineering
    • /
    • v.29 no.3
    • /
    • pp.195-202
    • /
    • 1996
  • The composition, the microstructure and the magnetic properties(HC and Hk) of Fe-Co-Ni alloy electrodeposits were investigated according to the electrolysis conditions using sulfate bath paddle agitated. The current efficiency of the alloys electrodeposition was considerably low in the range of 16∼50%. The Fe content(wt.%) of the alloy increased from 20% to 57% with current density, while Ni content of them decreased in the range of 70∼24% respectively, and Co content was nearly constant. As a result, Fe/Ni ratio of the alloy increased from 0.3 to 2.0 showing the anomalous codeposition. The structure of the alloy changed from fcc to the mixed one of fcc+bcc with the increase of Fe/Ni ratio. The preferred orientation of the alloy with fcc and bcc structure were (220) and (110) respectively. The alloy with Fe/Ni ratio(0.3∼l.2) had the lowest coercivity of 0.4∼0.8 Oe.

  • PDF

MAGNETIC PROPERTIES OF THERMALLY ANNEALED $(Ni_{80}Fe_{20})_{1-x}Mn_x$ THIN FILMS

  • Kim, K. K.;Kim, C. K.;C. S. Yoon;Kim, S. J.
    • Proceedings of the Korean Magnestics Society Conference
    • /
    • 2002.12a
    • /
    • pp.190-191
    • /
    • 2002
  • Granular feromagnets는 non-magnetic maxtrix 안에 nanometer-sized의 ferromagnetic grain들 구성된다. Co-Cu,Co-Ag, Fe-Ag, NiFe-Ag $^1$을 포함하는 이미 알려진 다른 Granular 금속 합금들의 giant magnetoresistance 에 관계하여 Granular feromagnets 에 대해 조사하였다. Bulk상태의 NiFe와 Mn 혼화되기 쉽다.$^2$ 그리고 Mn은 열처리된 다층박막의 NiFe의 lattice에 쉽게 수용되어진다.$^3$ 이번 실험에서는 metastable한 fcc solid solution NiFe-Mn 박막이 열처리 하에서 NiFe과 Mn으로 분리되었다. (중략)

  • PDF