• Title/Summary/Keyword: Fe-36Ni

Search Result 110, Processing Time 0.022 seconds

Effects of Mn, Cr and Co on the Magnetic Properties of Fe-Ni Invar Alloys (Fe-Ni 인바합금의 자기적성질에 미치는 Mn, Cr 및 Co의 첨가효과)

  • 이종현;김희중;강일구;김학신
    • Journal of the Korean Magnetics Society
    • /
    • v.3 no.1
    • /
    • pp.7-12
    • /
    • 1993
  • The effects of Mn, Cr or Co addItion on the magnetic properties of Fe-Ni Invar alloys were investigated. The composition range of the three additives is up to 5wt%. In the temperature range of room temperature-$250^{\circ}C$, the variation of specific magnetization with the addition of Mn, Cr or Co in the Fe-Ni alloys except for 5wt% Co shows the phenomenon characteristics of the Invar effect, viz., the specific magnetization decreases very abrubtly with the temperature and the dependence of temperature on the specific magnetization is in the mixed form of $T^{3/2}$ and $T^{2}$. In the room temperature, the amount of increase in the specific magnetization, Curie temperature and coercivity is in order of Co > Cr > Mn. In the case of 5wt% Co an anomalous phenomena were observed due to the occurrance of ferromagnetic $\alpha$ phase which reduces the invar effect.

  • PDF

Properties Analysis for Small Elements Added Shadow Mask Materials

  • Kim, Ku-Hak;Kim, Chung-Ho;Kim, Dong-Soo;Kim, One-Seek
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2002.08a
    • /
    • pp.1053-1055
    • /
    • 2002
  • Recently CRT is getting large-sized, Flatness and High Fine Pitched in the meantime the raw material for shadow mask is in rapid progress of thinness, Low Thermal Expansion and high strength.Until now we have used AK(Aluminum Killed) & Invar(Fe-Ni alloy) materials for main raw material of shadow mask component. However recently Nb and Co addition and Nb+Co addition, which has advantage of Low Thermal Expansion and High Strength. has been developed as well as applying in mass production as CRT's trend has become more flat and fine pitch. Among of them, Co addition has been mass production as forming type (Flat CRT) with the beneficial effect of low thermal expansion & high strength for the first time. Since then Nb+Co addition has been used in mass production by the request of much higher strength of shadow mask component. In case of Nb addition, It's thermal expansion coefficient is a little lower than normal Invar and a little higher than Co addition, meanwhile Its Mechanical property is almost similar to Co Addition. The used samples of this experiment are 36%Ni + Fe, 32%Ni + 5%Co + Fe, 32%Ni + 5%Co + 0.3%Nb + Fe, 32%Ni + 0.3%Nb + Fe with heat treatment temperature of 600$^{\circ}C$, 650$^{\circ}C$, 700$^{\circ}C$, 750$^{\circ}C$, 800$^{\circ}C$, 850$^{\circ}C$, 900$^{\circ}C$ respectively under the condition of 15min holding time. After heat treatment, we have observed the change of mechanical property with addition of small elements through mechanical property investigation and metal structure observation as well as transition of thermal expansion coefficient by measuring of thermal expansion coefficient at 850$^{\circ}C$. In conclusion, 5%Co addition indicates that its thermal expansion coefficient is very similar under the condition of at 850$^{\circ}C$ for 15min 's heat treatment. From the experimental result it is suggested that Co addition is mostly suitable for Doming property and Nb addition is mostly suitable for Drop property.

  • PDF

Toxicity Evaluation of Metals and Metal-oxide Nanoparticles based on the Absorbance, Chlorophyll Content, and Cell Count of Chlorella vulgaris (Chlorella vulgaris의 흡광도, 클로로필 및 개체수 통합 영향에 근거한 중금속 및 나노입자 독성 조사)

  • Jang, Hyun Jin;Lee, Mun Hee;Lee, Eun Jin;Yang, Xin;Kong, In Chul
    • Clean Technology
    • /
    • v.23 no.1
    • /
    • pp.27-33
    • /
    • 2017
  • In this study, toxicities of seven metals (Cu, Cd, Cr, As(III), As(V), Zn, Ni) and five metal oxide nanoparticles (NPs: CuO, ZnO, NiO, $TiO_2$, $Fe_2O_3$) were evaluated based on the growth of Chlorella vulgaris. Effect on algae growth was evaluated by integrating the results of absorption, chlorophyll content, and cell count. The toxicity rankings of metals was observed as Cr ($0.7mgL^{-1}$) > Cu ($1.7mgL^{-1}$) > Cd ($3.2mgL^{-1}$) > Zn ($3.9mgL^{-1}$) > Ni ($13.2mgL^{-1}$) > As(III) ($17.8mgL^{-1}$) ${\gg}$ As(V) (> $1000mgL^{-1}$). Slightly different orders and sensitivities of metal toxicity were examined depending on endpoints of algal growth. In case of NPs, regardless of endpoints, similar toxicity rankings of NPs ($TEC_{50}$) were observed, showing ZnO ($2.4mgL^{-1}$) > NiO ($21.1mgL^{-1}$) > CuO ($36.6mgL^{-1}$) > $TiO_2$ ($62.5mgL^{-1}$) > $Fe_2O_3$ ($82.7mgL^{-1}$). These results indicate that an integrating results of endpoints might be an effective strategy for the assessment of contaminants.

Evaluation of the Corrosion Resistance of Plated Ni and Ni-Cr Layers on Fe Substrate by Using Salt Spray, CASS and EC Tests (철소지 위에 형성된 니켈 및 니켈-크롬 도금층의 염수분무, 캐스, 전해부식시험법을 이용한 내식성평가)

  • 신재호;이동훈;이재봉;신성호
    • Journal of Surface Science and Engineering
    • /
    • v.36 no.4
    • /
    • pp.307-316
    • /
    • 2003
  • Salt spray, CASS(copper accelerated acetic salt spray) and EC(electrolytic corrosion) tests were performed in order to evaluate the corrosion resistance of plated Ni and Ni-Cr layers on Fe substrate. Compared with the conventional methods such as salt spray and CASS, the electrochemical method such as EC test may be beneficial in terms of test time span and quantitative accuracy. Furthermore, EC test can also become the alternative method to evaluate the resistance to corrosion of coatings by measuring the corrosion potentials of the coated layers in the electrolyte during the off-time of EC cycles. Compared with the corrosion potentials of pure iron, nickel, chromium, those potentials of coated layers can be used to anticipate the extent of corrosion. Results showed that in terms of the test time span, EC test gave 14 times and 21 times faster results than the salt spray test in cases of $5\mu\textrm{m}$ Ni and $20\mu\textrm{m}$ Ni plated layers, respectively. In addition, EC test also offered the shorter test time span than CASS test in cases of $5 \mu\textrm{m}$ Ni + $0.5\mu\textrm{m}$ Cr, and $20\mu\textrm{m}$ Ni + $0.5\mu\textrm{m}$ Cr on Fe substrate by 78 times and 182 times, respectively. Therefore, EC test can be regarded as the better method to evaluate the resistance to corrosion of coated layers than the conventional methods such as salt spray and CASS.

Variation in the Magneto-Impedance (MI) Effect According to the Shape of Patterned Co30Fe34Ni36 Alloys

  • Kim, Hyun-Kyung;Kim, Do-Hun;Son, De-Rac;Jeung, Won-Young
    • Journal of Magnetics
    • /
    • v.13 no.2
    • /
    • pp.65-69
    • /
    • 2008
  • The magneto impedance (MI) behaviors of patterned $Co_{30}Fe_{34}Ni_{36}$ microwire were investigated with respect to its shape variation. After preparing $Co_{30}Fe_{34}Ni_{36}$ microwires using electrodeposition and photolithography methods, impedance measurements were conducted to compare the MI ratios of the devices with different aspect ratios. As a result, the anisotropy field and transverse permeability were found to be strongly affected by the aspect ratio of the device. The external field value at the maximum impedance and maximum sensitivity of the device was found to increase with increasing device width, which was attributed to the increased transverse anisotropy with decreasing aspect ratio. While an increase in the thickness also contributed to an increase in the MI ratio, a variation in the thickness not only increased the anisotropic field, but the variation in the MI ratio was as also affected by the skin effect. Conversely, the MI ratios of the present devices were hardly affected by variations in the length. Considering the typical aspect ratios of our devices, it was expected that the length effect would emerge when the aspect ratio was reduced to less than 10. Nevertheless, our results show that for the practical application of MI devices, the MI characteristics can be optimized by tailoring the aspect ratio of the devices.

Design of Vertical Type Probe Tip Using Finite Element Analysis (유한요소해석을 이용한 수직형 프로브 팁의 설계)

  • Oh, Young-Ryun;Kim, Yun-Jae;Nam, Hyun-Suk;Park, Ung-Gi;Lee, Hak-Joo;Kim, Jung-Yub;Park, Jun-Hyub
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.36 no.8
    • /
    • pp.851-856
    • /
    • 2012
  • The design process of a micro-probe tip is very complicated and expensive. To avoid these problems, in this study, we used element (FE) analysis. To simplify design process. A new pre-probe tip (cobra-needle type) made of Ni and Co was designed by FE analysis. Experimental results were compared with those obtained by FE analysis to verify the reliability of the analysis. The contact force and over drive were respectively found to be 12.5 gf(Contact Force) and $100{\mu}m$(Over drive). We propose the new designed probe tip. Material of new designed probe tip is NiCo. Values of Property are 1~2 gf(Contact Force) and $100{\mu}m$(Over drive).

High Temperature Oxidation Behavior of Ni-W Coatings Electrodeposited on Steel (강기판 위에 코팅된 Ni-W의 고온산화거동)

  • 고재황;권식철;장도연;이동복
    • Journal of Surface Science and Engineering
    • /
    • v.36 no.6
    • /
    • pp.430-436
    • /
    • 2003
  • The nanoocrystalline Ni-l5W(at.%) coating electrodeposited on the high carbon steel was oxidized at 700 and $800^{\circ}C$ in air, and the resultant oxidation properties were investigated using XRD, EPMA, TGA and TEM. The oxidation resistance of the coating was not so good that most of the coating was oxidized after oxidation at $800^{\circ}C$ for 5 hrs. The oxidation led to the formation of the outer, thin NiO oxide scale and the inner, porous, rather thick ($NiWO_4$+NiO) mixed layer containing a bit of $WO_2$. During oxidation, substrate elements such as Fe and Cr diffused outwardly toward the coating, according to the concentration gradient.

Assessment of heavy metals in sediments of Shitalakhya River, Bangladesh

  • Al-Razee, A.N.M.;Abser, Md. Nurul;Mottalib, Md. Abdul;Rahman, Md. Sayadur;Cho, Namjun
    • Analytical Science and Technology
    • /
    • v.32 no.5
    • /
    • pp.210-216
    • /
    • 2019
  • Concentrations of Cu, Zn, Fe, Mn, Ni and Cr have been estimated in sediments of the Shitalakhya River at Polash-Ghorashal area, Narsingdi, Bangladesh. 36 samples of sediments from nine sampling point at different locations of Shitalakhya River were collected to determine the concentration of Cu, Zn, Fe, Mn, Ni, Cr and the samples were analyzed by atomic absorption spectrophotometer (AAS). The obtained results were compared with national and international guidelines. The levels of heavy metal concentrations in sediments were found to decrease in the order of Fe > Mn > Zn > Ni > Cu > Cr, respectively. The heavy metal concentration in sediment of Shitalakhya was below the recommended safe limits of heavy metals by WHO, FAO and other international standards. Contamination factor (CF) of Zn and Cu at sampling point Fsd2 show higher (> 1) values due to the influence of external discrete sources like wastage catalysts of ZnO and CuO. Geo-accumulation index values of the study indicate as non-contaminated to moderately contaminate.

Crystallograpbic and Magnetic Properties of $Ni_{0.65}Zn_{0.35}Cu_{0.3}Fe_{1.7}O_4$ ($Ni_{0.65}Zn_{0.35}Cu_{0.3}Fe_{1.7}O_4$의 결정학적 및 자기적 특성 연구)

  • 김우철;김삼진;김철성;이승화
    • Journal of the Korean Magnetics Society
    • /
    • v.9 no.3
    • /
    • pp.136-142
    • /
    • 1999
  • $Ni_{0.65}Zn_{0.35}Cu_{0.3}Fe_{1.7}O_4$ has been studied with x-ray diffraction, Mossbauer spectroscopy, and vibrating sample magnetometer. The crystal structure is found to be a cubic spinel with the lattice constant $a_0=8.403{\AA}$. Mossbauer spectra of have been taken at various temperatures ranging from 12 K to 665 K. as the temperature increases toward $T_N$ a systematic line broadening effect in the Mossbauer spectrum is observed and interpreted to originate from different temperature dependencies of the magenetic hyperfine fields at various iron sites. Also, by using binomial distribution equation we obtained the hyperfine fields of tetrahedral[A] and octahedral sites[B], $H_{hf}(A)=470\;kOe,\; H_{hf}(B0)=495 \;kOe,\; H_{hf}(B1)=485\;kOe, \;H_{hf}(B2)=453\;kOe,\; H_{hf}(B3)=424\;kOe,\; H_{hf}(B4)=390\;kOe,\; H_{hf}(Bavr)=451\;kOe$ respectively at room temperature. The isomer shift indicates that the iron ions are ferric at tetrahedral[A] and octahedral sites[B], respectively. The Neel temperature is determined to be $T_N=665\;K$. The results of the VSM data gave the magnetic moment and coercivity values of $M_S=66\; emu/g\;and\;H_C=36\;Oe$.

  • PDF

Emission Characterization of Particulate Matters According to the Types of Wastes from Industrial Waste Incinerator (산업폐기물 소각시설에서 폐기물 유형에 따른 입자상물질의 배출특성)

  • Park, Jeong-Ho;Suh, Jeong-Min;Jo, Jeong-Gu;Ryu, Jae-Yong;Han, Seong-Jong
    • Journal of Environmental Science International
    • /
    • v.16 no.11
    • /
    • pp.1225-1230
    • /
    • 2007
  • The emissions characteristics of particulate matters(PM) according to the types of wastes from industrial waste incinerator of 800 kg/hr treatment capacity were investigated. For this study, the incinerate waste are as follows; waste resin, waste wood, waste urethane, waste gunny, and waste paper. The particulate samples were collected to be emitted in stack and air pollution control(both cyclone and bag filter). In stack, the concentrations of PM were in the range of 2.61 to $26.51 mg/Sm^3$ and the major chemical species were C, Si, Cl, K, Na, Ca in all the wastes. In cyclone fly ash, the mean content of heavy metal were in the order of Fe > Zn > Pb > Cu > Mn > Cr > Ni > Cd > As > Hg and the heavy metal content of waste resin were Zn 34,197.5 mg/kg, Fe 27,587.6 mg/kg, Pb 6,055.8 mg/kg, respectively. In bag filter fly ash, the mean content of heavy metal were in the order of Zn > Pb > Fe > Cu > Mn > Cd > Cr > Ni > As > Hg and the heavy metal content of waste wood were Pb 36,405.2 mg/kg, Fe 15,762.9 mg/kg, Cu 9,989.5 mg/kg, Cd 2,230.1 mg/kg, respectively. Comparing the heavy metal content of both cyclone and bag filter, in cyclone, the Cr, Fe, Ni content were higher than in bag filter and the Cd, Cu, Hg content were lower than in bag filter.