• 제목/요약/키워드: Fatigue safety factor

검색결과 198건 처리시간 0.033초

교대근무자의 피로와 수행영향인자 간의 상관관계 분석 (반도체 산업을 중심으로) (Correlation Analysis between Fatigue and Performance Shaping Factor for Alternation Worker's (Focused on the Semiconductor industry))

  • 윤용구;박범
    • 대한안전경영과학회:학술대회논문집
    • /
    • 대한안전경영과학회 2008년도 추계학술대회
    • /
    • pp.303-316
    • /
    • 2008
  • For the past 25 years, Korean semiconductor has experienced enormous growth to be the highest production country in the world. Semiconductor industry is very time sensitive and driven by technology and process, and requires 24-hour full operation. The environment includes many different types of equipment, utilities, different gases and toxic chemicals as well as high voltage electricity. We have performed a survey with 3-shift engineers and workers in one line. The content of the questionnaire was about the correlation between fatigue and performance shaping factor (work type and work ability), and as a result we were able to deduce the correlation, p-value and the pattern of scatter plot. The shape of the model was made of 4 blocks for fatigue, 5 blocks for work type and 5 blocks for work ability, i. e. 14 blocks in total. As a conclusion to this findings, there was a correlation between fatigue and work type and work ability specifically in semiconductor industry, and we need some effort to reduce this.

  • PDF

해기사의 피로도 현황에 대한 조사 분석 (Analysis on the Results of Fatigue Survey for Marine Officers)

  • 양원재
    • 해양환경안전학회지
    • /
    • 제18권6호
    • /
    • pp.551-556
    • /
    • 2012
  • 피로도는 인간의 업무수행능력에 유해한 영향을 미치는 것으로 알려져 있다. 또한 피로도는 해기사와 선박승무원의 효율성과 능률을 감소시킬 수 있다. 본 연구의 목적은 해기사들의 피로도 현황을 파악하기위한 것이다. 본 연구에서는 해기사의 피로도 요소와 관련된 근무, 수면 및 휴식시간이나 기간, 졸음, 유발요인, 피로도 증상 등에 대한 설문조사를 실시하였다. 설문조사는 25문항 이었으며, 1,033명의 해기사(항해사 607명, 기관사 426명)를 대상으로 실시하였다. 설문조사 결과 해기사의 피로도는 충돌, 좌초와 같은 해양사고 유발요인의 하나이며, 항해사와 기관사의 피로도는 서로 차이가 있었다.

동역학 시뮬레이션을 통한 농업부산물 수집기 체결장치의 안전성 분석 (Simulation Study on the Safety of a Fastening Device of Agricultural By-product Collector)

  • 김정훈;황석준;남주석
    • 드라이브 ㆍ 컨트롤
    • /
    • 제20권3호
    • /
    • pp.42-49
    • /
    • 2023
  • In this study, the safety of fastening device for the agricultural by-product collector was evaluated according to the driving ground conditions by deriving the stress, static safety factor, and fatigue life using dynamic simulation. A 3D modeling of agricultural by-product collector was carried out, and simulation model was developed by applying the material properties. As a result of dynamic simulation, the magnitude of the maximum stress generated in the fastening device was the highest when driving on the flat off-road, followed by sloped pave-road and flat pave-road. Static safety factor and fatigue life were the highest when driving on the flat pave-road, followed by sloped pave-road and flat off-road. The safety of fastening device was confirmed that static safety factor was more than 1.0 and service life exceeded 9 years in all driving ground conditions.

균열닫힘현상을 고려한 피로균열전파식 (Fatigue Crack Growth Rate Equation by Crack Closure)

  • 김용수;강동명;신근하
    • 한국안전학회지
    • /
    • 제6권4호
    • /
    • pp.81-87
    • /
    • 1991
  • We propose the crack growth rate equation which will model fatigue crack growth rate behavior such that constant stress amplitude fatigue crack growth behavior can be predicted. Constant stress amplitude fatigue tests are conducted for four materials under three stress ratios of R=0.2, R=0.4 and R=0.6. Materials which have different mechanical properties i.e. stainless steel, low carbon steel, medium carbon steel and aluminum alloy are used. Through constant stress amplitude fatigue test by using unloading elastic compliance method, it is confirmed that crack closure is a close relationship with fatigue crack propagation. We describe simply fatigue crack propagation behavior as a function of the effective stress intensity factor range ($\Delta$ $K_{eff}$=U .$\Delta$K) for all three regions (threshold region, stable region). The fatigue crack growth rate equation is given by da / dN=A($\Delta$ $K_{eff}$­$\Delta$ $K_{o}$ )$^{m}$ / ($\Delta$ $K_{eff}$­$\Delta$K) Where, A and m are material constants, and $\Delta$ $K_{o}$ is stress intensity factor range at low $\Delta$K region. $K_{cf}$ is critical fatigue stress intensity factor.actor.

  • PDF

숏피닝 가공재의 저온 피로 강도 평가 (An Evaluation on the Fatigue Strength Characteristics for the Shot Peening Spring Steel at Low Temperature)

  • 박경동;권오헌
    • 한국안전학회지
    • /
    • 제18권3호
    • /
    • pp.1-7
    • /
    • 2003
  • In this study, CT specimens were prepared from spring steel(SPS5) processed shot peening. The fatigue crack growth tests were carried out in the environment of the room temperature md low temperature at $25^{\circ}C$, $-30^{\circ}C$, $-50^{\circ}C$, $-70^{\circ}C$ $-100^{\circ}C$ and $-150^{\circ}C$ in the range of stress ratio of 0.05 by means of opening mode displacement. The threshold stress intensity factor range ΔKth in the early stage of fatigue crack growth (Region I) and stress intensity factor range $\Delta$K in the stable of fatigue crack growth (Region II) were decreased in proportion to descend temperature. It was shown that the fatigue resistance characteristics and fracture strength at low temperature are considerable higher than those of mom temperature in the early stage and stable of fatigue crack growth region.

피로균열이 발생한 강판형 철도교 세로보의 보수보강효과 (An Effect of Repair & Retrofit of Stringer in Steel Plate Girder Railway Bridge with Fatigue Cracks)

  • 홍성욱
    • 한국안전학회지
    • /
    • 제25권1호
    • /
    • pp.65-71
    • /
    • 2010
  • In this study, a series of finite element analysis using LUSAS were performed in order to assess the quantitative effects of repair and retrofit of stringer in steel plate girder railway bridge with fatigue cracks. And cutoff types of end part of upper flange were considered as right-angled type and round-angled type. Also, as a method of repair and retrofit of fatigue cracks in stringer, perforation of stop-hole and installation of bracket were considered. From the analysis result, it was possible to assess the fatigue safety and fatigue life of stringer with fatigue cracks, and to estimate the stress intensity factor range in cut-off part of stringer using J-integral method. Also, according to the method of perforation of stop-hole and installation of bracket, it was possible to calculate the crack propagation life at the cut-off part of stringer.

Nb 함량에 따른 마르에이징강의 유한요소해석에 관한 연구 (A Study on the FEM Analysis of Maraging Steel according to Nb content)

  • 최병기;최병희;권택용
    • 한국안전학회지
    • /
    • 제20권4호
    • /
    • pp.1-8
    • /
    • 2005
  • Effects of Nb(Niobium) contents and solution annealing on the strength and fatigue life of 18%Ni maraging steel commonly using in aircraft, space field, nuclear energy, and vehicle etc. were investigated. Also the fatigue life stress intensity factor were compared experiment result and FEA(finite element analysis) result. The more Nb content, the higher or the lower fatigue life on base metal specimens or solution annealed specimens showing that the fatigue lift was almost the same. The maximum stresses of X, Y, and Z axis direction showed about $2.12{\times}10^2MPa,\;4.40{\times}10^2MPa\;and\;1.32{\times}10^2MPa$ respectively. The Y direction stress showed the highest because of the same direction as the loading direction. The fatigue lives showed about 7% lower FEA result than experiment result showing almost invariable error every analyzed cycle. Stress intensity factor of the FEA result was lower about $3.5{\sim}10%$ than that of the experiment result showing that the longer fatigue crack length the higher error. It considered that the cause for the difference was the modeled crack tip having always the same shape and condition regardless of the crack growth.

열성층을 포함하는 원자력발전소 배관의 환경피로평가 (Environmental Fatigue Evaluation for Thermal Stratification Piping of Nuclear Power Plants)

  • 김태순;김규형
    • 한국안전학회지
    • /
    • 제33권5호
    • /
    • pp.164-169
    • /
    • 2018
  • A detailed fatigue evaluation procedure was developed to mitigate the excessive conservativeness of the conventional environmental fatigue evaluation method for the pressurizer spray line elbow of domestic new nuclear power plants. The pressurizer spray line is made of austenitic stainless steel, which is relatively sensitive to the environmentally assisted fatigue, and has a low degree of design margin in terms of environmentally assisted fatigue due to the thermal stratification phenomenon on the pipe cross section as a whole or locally. In this study, to meet the environmental fatigue design requirements of the pressurizer spray line elbow, the new environmental fatigue evaluation has been performed, which used the ASME Code NB-3200-based detailed fatigue analysis and the environmental fatigue correction factor instead of the existing NB-3600 evaluation method. As a result, the design requirements for environmentally assisted fatigue were met in all parts of the pressurizer spray line elbow including the fatigue weakened zones by thermal stratification.

A182 F6A Class4 재료의 피로특성과 피로해석에 대한 연구 (A Study on Fatigue Characteristics and Analysis for A 182 F6a Class 4 Materials)

  • 이진경
    • 한국산업융합학회 논문집
    • /
    • 제26권4_2호
    • /
    • pp.585-589
    • /
    • 2023
  • Unlike general carbon steel, stainless steel's mechanical properties change depending on the content of chromium and nickel. In this study, since stainless steel for high-temperature pressure container parts is used as shafts, the fatigue strength and fatigue limit of the materials were evaluated using a rotational bending fatigue test. Meanwhile, fatigue analysis was conducted under the same conditions as the specimen for structural analysis and fatigue analysis of stainless steel for high-temperature pressure container parts. Using the fatigue analysis results, we tried to derive the life of the material and the safety factor for each part. As a result of performing a fatigue test by processing a specimen for the fatigue test of A182 F6A stainless steel, the fatigue limit was 548 MPa. The ratio between the tensile strength and fatigue limit of the material was 0.545, representing 54.5% of the tensile strength.

산악용 자전거 프레임의 피로 내구성 평가 (Evaluation of Fatigue Endurance for an MTB Frame)

  • 김택영;이만석;임웅;김호경
    • 한국안전학회지
    • /
    • 제28권3호
    • /
    • pp.1-5
    • /
    • 2013
  • In order to evaluate fatigue endurance for an MTB(mountain bike) frame, FEM(finite element method) analysis was performed. For evaluating the fatigue endurance of the MTB frame, the S-N data for Al-6061 fillet weldment were compared with the stress analysis results through FEM analysis of the frame. Three loading condition, pedalling, horizontal and vertical loading conditions were considered for fatigue endurance evaluation. Horizontal loading(+1200 N) condition was found to be the most severe to the frame. The maximum von Mises stress of the frame under horizontal loading(+1200 N) condition was determined 294 MPa through FEM analysis of the frame. Conclusively, on the basis of fatigue strength of 200 MPa at the number of cycles of 50,000, the MTB frame has an improper safety factor of approximately 0.25, suggesting that this frame needs reinforcement.