• 제목/요약/키워드: Fatigue cack growth

검색결과 4건 처리시간 0.018초

질화규소의 피로균열진전과 입자가교효과 (Bridging Effect and Fatigue Crack Growth of Silicon Nitride)

  • 유성근
    • 한국세라믹학회지
    • /
    • 제33권11호
    • /
    • pp.1203-1208
    • /
    • 1996
  • 질화규소의 균열진전시험은 정적 및 반복사중하의 균열진전특성을 명확히 밝혔다. 일정 K값의 정적하중에서 균열진전속도는 균열진전증가와 더불어 감소하고 최종적으로는 정지하였다. 또 균열진전저항은 응력반복에 의해 크게 감소하였다. 특히 균열진전저항은 균열진전증가와 더불어 증가하였고, 증가속도는 정적하중보다 반복하중하에서 훨씬 작았다.

  • PDF

마찰교반용접된 7075-T651 알루미늄 판재의 피로균열전파의 거시적 및 미시적 관찰 (Marco and Microscopic Observations of Fatigue Crack Growth in Friction Stir Welded 7075-T651 Aluminum Alloy Plates)

  • 공유식;김선진
    • 동력기계공학회지
    • /
    • 제18권2호
    • /
    • pp.62-69
    • /
    • 2014
  • In this paper, in order to investigate the effects of marco and microscopic observations of fatigue crack growth in friction stir welded (FSWed) 7075-T651 aluminum alloy plates, fatigue crack growth tests were performed under constant amplitude loading condition at room temperature with three different pre-cack locations, namely base metal (BM-CL) and two kinds of pre-crack locations in welded joints, weld metal (WM-CL) and heat affected zone (HAZ-CL) specimens. The fatigue crack growth behavior of FSWed 7075-T651 aluminum alloy plates were discussed based on the marco and microscopic fractographic observations. The marcoscopic aspects of surface crack growth path for BM-CL and HAZ-CL specimens indicate relatively straight lines, however, the crack growth paths of WM-CL specimens grow first straight and by followed toward the TMAZ and HAZ. The microscopic aspects of fatigue fracture for BM-CL and HAZ-CL specimens indicate typical fatigue striation, but WM-CL showed intergranular fracture pattern by micro structural changes of FSW process.

고장력강의 부식피로에 미치는 용액온도의 영향에 관한 연구 (Study on effect of solution temperature on corrosion fatigue of high strength steel)

  • 유헌일
    • 오토저널
    • /
    • 제8권1호
    • /
    • pp.40-51
    • /
    • 1986
  • A study has been made of the corrosion fatigue of high strength low alloy steel in 3.5% NaCl solution under tension stress for solution temperature being 25.deg. C, 55.deg. C and 85 .deg. C. The main results obtained are as follows; 1) The corrosion fatigue crack growth rate curve could be divided into the First Region, the Second Region and the Third Region. 2) The corrosion fatigue crack growth rates in the First Region and the Second Region were Arrhenius temperature-dependent in this test range. The apparent activation energies for the corrosion fatigue cack growth rate were found to be 2000cal/mol in the First Region and 3700 cal/mol in the Second Region. 3) Hematite (Fe$_{2}$O$_{3}$) as the hexahedral crystal and magnetite (Fe$_{3}$O$_{4}$) as the octahedral crystal were observed in the corrosion products on the corrosion fatigue fracture surface at 85.deg. C and the anode fusion seem to be generated in the crack tip region at high temperature. 4) The complex environment effect ratio which was defined by the ratio of fatigue crack growth rate in corrosion environment to that in air might be considered not only a criterion estimating the effect of environment quantitatively but also an important parameter in the selection of the design stress for the fail safe design. The complex environment effect was not greater than ten in this test.

  • PDF

초대형 컨테이너선의 해치 코밍 용접부의 내부 균열에 대한 파괴역학적 연구 (A Study on Embedded Crack at the Hatch Coaming FCA Butt Weldment in an Ultra Large Containership on the Basis of Fracture Mechanics)

  • 신상범;이주성
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2010년도 춘계학술발표대회 초록집
    • /
    • pp.61-61
    • /
    • 2010
  • The purpose of this study is to prevent the unstable fracture at the FCA butt weldment of hatch coaming deck in the ultra large containership during service life. In order to do it, the behavior of the embedded crack at the weldment under design loading conditions was evaluated in accordance with BS7910. Here, the level of primary stress induced by ship motion was evaluated by the design code of classification society and FEA. The level of residual stress as secondary stress was calculated in consideration of the restraint degree of weldment and welding heat input by using the predictive equation proposed by authors in the previous study. The fatigue crack growth rate at the weldment was evaluated using CT specimen in accordance with ASTM E647. According to the results, although the allowable defect for embedded crack specified in the classification society exists at the weldment, the occurrence possibility of unstable fracture at the weldment could not be negligible, regardless of CTOD value given in this study. So, in this study, the effect of initial defect size, welding heat input, restraint degree and CTOD on the fracture mechanical characteristics of embedded crack at the weldment was evaluated by the comprehensive fracture assessment. Based on the results, the design criteria including allowable defect, residual stress level and CTOD value was established to prevent the unstable fracture at the FCA butt weldment of hatch coaming deck in an ultra large containership during service life of 20years.

  • PDF