선체구조용 EH36 TMCP 후판의 FCAW 및 EGW 조합 용접부 기계적 성질에 미치는 개선조건의 영향 (Effect of Groove Conditions on the Mechanical Properties of Welds Produced by the Combined Welding Process of Flux Cored Arc and Electro Gas in EH36 TMCP Steel Plate for Hull Structures)

  • 김기혁;김기원;심호섭;배강호;홍현욱;박병규
    • Journal of Welding and Joining
    • /
    • 제33권5호
    • /
    • pp.35-40
    • /
    • 2015
  • Characterization of microstructures and mechanical properties of 83mm thickness EH36-TM welds produced by the combined flux cored arc (FCA) and electro gas (EG) welding processes has been studied with the two different groove conditions, single-V (SV) and double-V (DV) bevels. The welding consumables used for FCA and EG welding processes were ASME/AWS A5.29 (E81T1-K2) and A5.26 (EG72T), respectively. Experimental results showed that all the mechanical properties of welds such as tensile property, CVN toughness and Vickers hardness met IACS requirements. The tensile strength of EG welded plates were reduced by approximately 4% (DV: 3.8%, SV: 4.2%) compared to the base metal. The hardness value of SV-beveled weld metal was slightly lower than that of DV-beveled one. There were no significant differences as per welding groove conditions except for the weld metal. In addition, at the fusion line, the toughness of SV condition was 20J lower and the weld metal was 40J lower than DV condition, respectively. On the basis of microstructural analysis, grain boundary ferrite (GBF) structures for SV condition were 2 times higher volume fraction than for DV condition and their packet sizes were coarsened to almost double. It was thus suggested that the GBF volume fractions and packet sizes in the weld metal of EH36-TM steel plates are the most important factors affecting the mechanical properties of the combined FCA and EG welded joint. Nevertheless, all the results of welds with both DV and SV conditions were found to be excellent.

극후판 다층 FCAW 맞대기 용접부의 잔류응력 특성에 관한 연구 (A Study of the Residual Stress Characteristics of FCAW Multi-Pass Butt Joint for an Ultra-Thick Plate)

  • 방희선;방한서;이윤기;김현수;이광진
    • 한국해양공학회지
    • /
    • 제24권2호
    • /
    • pp.62-66
    • /
    • 2010
  • The goal of this work is to establish the reliability of FCA welded joints for high strength EH36-TMCP ultra thick plate. For this, heat conduction and thermo elasto-plastic analyses have been conducted on a multi-pass, X-groove, butt-joint model to clarify the thermal and mechanical behavior (residual stresses, magnitude of the stresses, and their production and distribution mechanisms) of the weld joint. In addition, the results of the welding residual stress obtained from thermo elasto-plastic analysis was verified and compared with results obtained by XRD analysis.

필릿 용접 공정에서 온도 분포 예측을 위한 해석적 모델 (Analytical Solution for Transient Temperature Distribution in Fillet Arc Welding)

  • 정선국;조형석
    • Journal of Welding and Joining
    • /
    • 제13권2호
    • /
    • pp.68-81
    • /
    • 1995
  • This paper presents an analytical solution to predict the transient temperature distribution in fillet arc welding. The analytical solution is obtained by solving a transient three -dimensional heat conduction equation with convection boundary conditions on the surfaces of an infinite plate with finite thicknesses, and mapping an infinite plate onto the fillet weld geometry with energy equation. The electric arc heat input on fillet weld and on infinite plate is assumed to have a traveling bivariate Gaussian distribution. To check the validity of the solution, GTA and FCA welding experiments were performed under various welding conditions. The actual isotherms of the weldment cross - sections at various distances from the arc start point are compared with those of simulation result. As the result shows a satisfactory accuracy, this analytical solution can be used to predict the transient temperature distribution in the fiIIet weld of finite thickness under a moving bivariate Gaussian distributed heat source. The simplicity and short calculation time of the analytical solution provides rationales to use the analytical solution for modeling the welding control systems or for an optimization tool of welding process parameters.

  • PDF

NO ROOT GAP HORIZONTAL BUTT-WELDING WITH MAG PROCESS

  • Woo, Wan-Chuck;Jang, Tae-Won;Lee, Jae-Won
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.425-429
    • /
    • 2002
  • It has been used many kinds of horizontal butt-welding methods at block-to-block erection stage in shipbuilding companies. For examples, some companies use conventional FCA W process with one side or both sides groove joint welding, others use carriage with torch holder type mechanized welding method. Although lots of efforts were done until now, some problems in quality and productivity still remain in ship's hull welding. In this study, we have attempted to raise productivity and quality on horizontal position of welding with following 3 items. 1) Prepare groove condition with no root gap for making easy fit-up work. 2) Develop improved MAG (100% $CO_2$ gas shielding) welding process with solid wire for making sound root bead from one side. 3) Develop and apply quite new automatic welding carriage. The stability of new welding process was confirmed by conducting mechanical tests of weldments to verify the soundness of weldments.

  • PDF

용접 재료 개발 단계에서 ECA 기법을 통한 재료의 인성 적합성 평가 (Application of Engineering Critical Assessment Method in the Development Stage of Welding Consumables)

  • 신용택;조영주;서대곤
    • Journal of Welding and Joining
    • /
    • 제34권6호
    • /
    • pp.16-19
    • /
    • 2016
  • Needs for structural integrity procedure such as BS 7910, the nuclear industry document R6 Rev.4 and the European FITNET procedure are being increased in industry. Especially, BS 7910 allows metallic structures to be assessed on the basis of fracture mechanics analysis rather than strict adherence to design and fabricated codes. This study is to propose the flaw assessment to judge the toughness level of welding consumables at the development stage. The FCA welding consumables with YP 690MPa and CTOD over 0.25 mm have been developed and its allowable weld flaw size considering actually applied environment has been evaluated. Since the estimated allowable defect size is sufficiently detectable in nondestructive testing, the toughness of the developed material is judged to be appropriate and no problem in securing the structural integrity.